CategoryTitanium Applications
Felt vs mesh vs
sintered titanium PTLs
Choose the porous transport layer around the cell: water and oxygen pathways, electrical contact, assembly condition and repeatable supply.

Quick answer
No titanium PTL family is universally best. For a PEM anode, compare felt, mesh and powder-sintered structures within the same cell constraints. Specify pore measurements, contact resistance, surface treatment, loaded condition and qualification scope. Evaluate the finished component and its operating evidence rather than ranking porosity, mesh count or substrate price alone.
01 / Felt, mesh and sintered powder
Compare architectures within the same electrolyzer duty
A buyer choosing titanium felt, titanium mesh or a sintered titanium powder sheet for a porous transport layer is choosing more than a porous metal shape. The component must work with the catalyst layer, membrane, flow field, seals and assembly load. The useful comparison is the performance of a defined PTL in that system, supported by repeatable manufacturing and inspection evidence.
This guide concerns the anode-side porous transport layer in a proton exchange membrane water electrolyzer, abbreviated PEMWE. It does not establish interchangeability with a fuel-cell gas diffusion layer, an alkaline-electrolyzer component or a generic filtration sheet. Specify the actual cell side and electrochemical duty before asking for a quotation.
The PTL provides paths for liquid water and evolved oxygen while participating in electronic conduction and mechanical support at the electrode interface. These functions interact. A structure selected only for an open flow path may provide a different contact surface from a denser structure. A good contact surface alone does not demonstrate satisfactory two-phase transport.
Name the structure precisely
Titanium felt uses a network of fibers; its fiber geometry, bonding and orientation require definition. Woven mesh uses intersecting wires, while expanded mesh is formed from slitted and expanded sheet. A powder-sintered PTL forms a bonded particle structure. Do not combine woven and expanded mesh under one dimension specification or assume every felt has the same compression behavior.
A published 2026 screening study provides a useful reminder that commercial candidates can differ in thickness as well as architecture. It examined seven structures: five powder-sintered sheets, one mesh and one felt. Selected specimen dimensions are summarized below, without reproducing a performance ranking.
| Candidate family | Number of candidates | Reported thickness | Specimen plan size |
|---|---|---|---|
| Powder-sintered titanium sheets | 5 | 500 μm | 20 × 20 mm |
| Titanium mesh | 1 | 200 μm | 20 × 20 mm |
| Titanium felt | 1 | 200 μm | 20 × 20 mm |
Source: Chemical Engineering Science 328, 123786, PTL screening section. These are experimental sample descriptions, not a controlled one-variable comparison of all available products.
Define the comparison question before screening
If a buyer wants a direct replacement, retain the cell constraints that the substitute must satisfy and identify permitted changes. If the objective is a new cell design, geometry and interfaces may be optimized together. Those studies answer different questions. A successful redesigned assembly does not prove that its PTL can be dropped into an unchanged stack.
Record whether the offer is an uncoated substrate, a finished coated PTL, a multilayer component or a porous flow-field assembly. Those deliverables may look similar in a photograph while having different responsibilities and acceptance requirements. Ask the supplier to identify each included layer and operation so the quotation corresponds to the component that will actually be tested.
02 / Pores and transport
Porosity alone cannot describe water and oxygen pathways
Porosity expresses a void fraction under a defined measurement basis. It does not, by itself, describe whether the pores connect through the thickness, how narrow their connecting throats are, how tortuous the paths are or how the structure behaves when compressed. Two samples with the same bulk porosity can therefore require very different interpretation.
A 2024 study by Liu and colleagues used reconstructed fiber and powder structures to examine this issue. Its models varied porosity and mean pore diameter while distinguishing architecture and direction. It supports evaluating structure and transport together; the modeled results are not production-lot certificates or universal acceptance limits.
Separate open area, pore size and permeability
Mesh open area is usually a geometric projection of openings in a specified plane. It is not automatically the same as the volumetric porosity of a felt or powder-sintered sheet. Likewise, a nominal filter rating is not an electrolyzer transport specification. Do not place these different quantities into one column and rank the largest percentage as best.
Ask what a reported pore-size value means: an image-derived diameter, a throat-related result, a distribution statistic or another defined quantity. Include method, specimen state and units. A single mean can hide a broad distribution or a restricted connecting pathway. Where connectivity is important, the selected characterization should address connectivity rather than only a convenient visual size.
Permeability also needs direction and conditions. Through-plane transport crosses the sheet thickness, while in-plane transport follows the sheet plane. A result in one direction does not establish the other. Record the fluid, temperature, pressure range and compression state used in the measurement so the reported value can be interpreted within the intended comparison.
Use simple models within their limits
For an idealized single-phase, low-inertia Darcy comparison, pressure drop scales as viscosity times thickness times superficial velocity divided by permeability: ΔP = μLv/k. If the other terms remain fixed, doubling thickness doubles the predicted pressure drop, and halving permeability also doubles it. This is a scaling relationship, not a complete operating model for a PEM anode.
Actual water and oxygen share the pore network during electrolysis. A dry-gas permeability measurement or a fully water-saturated single-phase test does not capture every aspect of that two-phase behavior. Use such measurements as defined characterization inputs, then require cell evidence for the relevant operating regime. Do not convert a favorable single-phase result directly into a guaranteed voltage reduction.
Wettability belongs in the same review. Ask how it was measured, on which surface, after what preparation and at what time after treatment. A droplet result can change with surface condition and handling. A treatment described as hydrophilic should be connected to the actual delivered component and qualification history, rather than treated as a permanent property established by a single photograph.
For multilayer PTLs, specify layer order and which face contacts the catalyst layer. The two faces may be intentionally different. Include thickness and bonding requirements for each relevant layer, along with orientation marks if needed. Reversing a graded component during assembly can invalidate the comparison even when its overall thickness and alloy remain correct.
The existing mesh aperture and open-area guide helps define mesh geometry, while the sintered filter selection guide addresses filtration. Neither replaces PTL qualification under electrochemical duty; use each measurement for the question it actually answers.

Original conceptual map: water supply, oxygen removal, electrical contact and mechanical support must be evaluated together.
03 / Electrical contact and coatings
Treat the interface as a specified part of the component
Bulk titanium conductivity and contact resistance are different subjects. The electrical path includes the porous metal structure and its interfaces with neighboring components. A statement that titanium conducts electricity does not quantify the resistance of a particular coated or uncoated PTL against a particular catalyst layer under a defined load.
Titanium surface passivation can increase interface resistance in PEM electrolysis. Singh and colleagues’ coating study discusses the role of the TiOₓ surface and evaluates a specific protective coating system. This is a reason to specify surface condition and durability evidence, not a guarantee that every coating or uncoated substrate behaves alike.
Request an area-specific resistance with a defined fixture
When comparing contact-resistance results, retain the opposing material, applied pressure, sample area, surface condition and measurement procedure. Clarify whether the reported value includes one interface, two interfaces or additional fixture contributions. If a correction is applied, request the basis. Values with identical units can still represent different measurement arrangements.
Use consistent area definitions. Area-specific resistance expressed in Ω·cm² can be combined with current density in A/cm² to estimate its voltage contribution. A resistance reported simply in ohms requires the appropriate area relationship before comparison. Check whether the area is nominal active area or another defined contact area; do not silently switch between them.
As an original arithmetic example, 10 mΩ·cm² equals 0.010 Ω·cm². At 2 A/cm², the corresponding voltage contribution is 0.020 V, or 20 mV, for the resistance term as defined. This is not a measured PTL value or a recommended acceptance limit. It explains why a seemingly small resistance difference can matter at a specified current density.
Surface design can change performance within one family
Lee and colleagues’ 2023 laser-ablation study of sintered titanium PTLs reported voltage reductions of up to 230 mV at 4 A/cm² with 0.055 mgIr/cm² catalyst loading, and 68 mV at 3.2 A/cm² with 0.4 mgIr/cm². These are study-specific comparisons, not felt-versus-mesh rankings. See the research institution’s publication record.
The purchasing implication is to preserve interface condition in the specification. A change in surface treatment, roughness, coating or layer arrangement can change the item being qualified even when the base material family remains the same. Ask whether the evaluated sample and routine production use the same controlled surface process.
For a coated component, define coating material, intended faces, relevant loading or thickness basis, coverage and verification method. A nominal nanometer value measured on a flat witness sample may not fully describe coverage within a porous network. Ask how the supplier relates its process-control measurement to the actual delivered PTL.
Do not choose a coating solely from beginning-of-life performance. Include the operating and start-stop duty relevant to the application, post-test characterization where required and the defined failure or acceptance criterion. An attractive initial polarization curve does not establish service life. Conversely, a long test without a stated duty or failure criterion can be difficult to compare.
04 / Compression and qualification
Control the assembled condition and the test history
A PTL thickness measured without load is not necessarily its thickness inside the cell. Specify how thickness is measured and whether an additional loaded-thickness or compression characterization is required. The seal design, neighboring components and assembly procedure must accommodate the actual component rather than a nominal catalog number alone.
Keep compression, fluid operating pressure and pressure differential distinct. They describe different loads and cannot be substituted for one another in a specification. Bolt torque is also not automatically the contact pressure on the active area: the assembly geometry and load path matter. Use the cell designer’s approved procedure to define the relevant assembly conditions.
Srour and colleagues, 2024, found that contact resistance depended on clamping stress and clamping history in their setup. Their results also distinguish initial performance from durability. The lesson for a buyer is to preserve assembly history in a comparison, not to copy a laboratory tightening schedule into another stack.
Make a substitution test reproducible
Record the membrane-electrode assembly, catalyst type and loading, flow-field geometry, PTL orientation, coating, gasket arrangement, active area and assembly sequence. Define water quality and supply conditions, temperature, pressures on both sides, conditioning procedure and electrical test sequence. These details explain what the result represents and whether a comparison isolates the proposed change.
State whether a polarization curve is raw or corrected for a resistance contribution. If correction is used, report its method and keep the uncorrected result available. A corrected curve from one candidate should not be compared with an uncorrected curve from another. Also record hold times or sweep procedure; a transient result and an equilibrated operating point need not answer the same question.
High-frequency resistance can help interpret cell behavior, but it is not automatically a measurement of PTL contact resistance alone. Keep the diagnostic interpretation tied to the measurement configuration and analysis. If a claim assigns a voltage loss to the PTL, ask what evidence separates it from the membrane, other interfaces and operating changes.
Include repeatability and durability in the approval scope
Define how many independent samples, lots and assemblies are required by the program, and how results will be reported. Repeated measurements on one unchanged assembly are not the same as independent assembly repeatability. Preserve unsuccessful tests and deviations in the review so the decision does not depend only on the best curve.
Use a durability schedule relevant to the intended duty. A constant-current laboratory run does not automatically represent repeated starts, stops, load changes or extended storage. State the exposure and what constitutes acceptable drift or failure. Avoid translating a short accelerated test into a guaranteed number of operating years without a justified correlation.
After testing, compare dimensions, surfaces and other required evidence with the initial state. The investigation may need to distinguish a PTL problem from membrane damage, assembly variation or a changed operating condition. A clear sample and test history makes that investigation possible; a generic pass statement often does not.
Approve a bounded configuration: component drawing, material route, coating and surface process, relevant cell conditions and accepted change controls. If a supplier later changes fiber size, powder feedstock, mesh construction, sintering route or finishing, determine whether the approval still applies. A family name alone cannot carry every future design change.

Conceptual layer order only; not a construction drawing. Identify the catalyst-facing side, flow-field side and approved assembly state.
05 / Voltage and lifecycle cost
Translate an electrical difference into a transparent cost question
Compare finished, accepted PTLs on the same delivery basis. Substrate price alone excludes possible coating, cutting, inspection, packaging, rejected parts and qualification. A lower-cost mesh substrate may require additional interface engineering; a more expensive finished component may or may not justify its premium. The answer depends on the actual approved configuration and operating evidence.
Keep manufacturing yield and active-area utilization separate. A sheet price per square meter must be converted using the real blank size, cutting allowance, nesting and accepted quantity. Do not quote cost per active area while ignoring the material outside the active window or the scrap created by the chosen cutting process.
An original cell-level energy example
Assume an active area of 100 cm² and current density of 2 A/cm². Current is therefore 200 A. If two otherwise comparable operating cases differ by 20 mV at that current, their direct-current electrical power differs by 4 W. Over an assumed 8,000 operating hours, that is 32 kWh per cell.
| Quantity | Assumption or calculation |
|---|---|
| Active area | 100 cm² |
| Current density | 2 A/cm² |
| Current | 100 × 2 = 200 A |
| Voltage difference | 20 mV = 0.020 V |
| DC power difference | 200 × 0.020 = 4 W |
| Energy over 8,000 h | 4 × 8,000 / 1,000 = 32 kWh |
This calculation assumes the voltage difference persists over the stated hours. It does not include rectifier efficiency, auxiliary loads, changes in hydrogen production efficiency, downtime or degradation. It also does not assign the difference to felt, mesh or sintered powder. Insert measured, comparable operating data before using the calculation in an investment decision.
For variable operation, calculate energy over the relevant time intervals using the current and voltage difference in each interval. A single favorable operating point may not represent the annual duty. If the difference changes with aging, include that behavior rather than multiplying the initial result by an entire lifetime.
Then compare the energy value with component premium, qualification cost, replacement frequency and downtime assumptions. Use a documented electricity-price scenario and production schedule, not an unsupported universal payback claim. The purpose is to reveal which assumptions control the decision and which measurements would reduce uncertainty.
Supply continuity also belongs in the evaluation. Ask about repeat-lot consistency, lead time for the finished coated part, documentation availability and notification of changes. A technically promising sample is not yet a reliable series-production supply arrangement. Include acceptance and quality responsibilities in the commercial review.

Original hypothetical example: 200 A multiplied by 20 mV gives 4 W, or 32 kWh over 8,000 hours. No product performance is implied.
06 / RFQ and receiving checks
Specify the component that will actually enter the cell
Begin the enquiry with PEM anode PTL duty, the intended role in the cell, drawing revision, plan dimensions, thickness basis and quantity. State whether you need felt, woven mesh, expanded mesh, powder-sintered material or an engineered multilayer proposal. If alternatives are welcome, identify what may change and what remains fixed.
Include alloy and chemistry requirements, structural parameters with their measurement methods, surface and edge condition, coating scope, cleanliness, flatness and dimensional tolerances relevant to the design. Do not request the highest porosity or smallest pores without connecting those targets to a qualified cell requirement. A supplier cannot infer that relationship from the word PTL alone.
Ask for traceable evaluation samples and a production-control proposal. The sample report should identify the manufacturing lot and processing state. Clarify whether subsequent orders will use the same route and how changes are communicated. If characterization is subcontracted, specify which reports and sample identifiers must accompany the delivery.
At receipt, verify identification, drawing, quantity, dimensions, orientation, coating declaration and required test documents. Inspect the agreed edge and surface features without assuming visual appearance proves electrochemical performance. Hold unresolved discrepancies under the buyer’s quality process before mixing material with approved inventory or installing it in a controlled test.
TiHubs can review requirements related to titanium mesh and perforated material and the specified titanium supply scope. Confirm availability, manufacturing route, coating capability and PTL-specific evidence for each enquiry. This guide does not claim that every felt or engineered PTL is stocked, or that a TiHubs product has achieved the published research results.
The final selection should explain why the proposed structure fits the cell’s transport, contact, assembly and supply requirements. Keep the evidence and its boundaries with the approved drawing. That record is more valuable for repeat procurement than a broad statement that felt, mesh or sintered powder is always the best PTL.
07 / Build your RFQ
Prepare a PEM anode PTL enquiry
Describe the cell duty and the finished component. State which structural alternatives are permitted and which tests and approvals the actual supply must support.
Information to include
- PEM anode duty, drawing, dimensions and thickness measurement basis
- Felt, woven/expanded mesh, sintered powder or defined multilayer
- Pore structure, transport and contact-resistance test requirements
- Coating, surface condition, assembly and qualification scope
- Sample lot, production quantity, documents and change controls
Build your RFQ checklist
Choose the product and add the information you have. Copy the resulting brief or send your requirements to TiHubs. Submitting an enquiry does not place an order.
08 / FAQs
Questions buyers ask
Is titanium felt always better than mesh for a PEM PTL?
No. Compare defined components in the intended cell, including interfaces, coating, compression and operating conditions. A felt may be suitable for one configuration while a mesh or engineered multilayer is suitable for another. The family name alone does not establish cell performance.
Does higher porosity mean a better PTL?
Not necessarily. Porosity does not fully describe connectivity, pore throats, directional transport or the contact surface. Compare the relevant structural and transport measurements together with electrical and assembled-cell evidence. Do not treat projected mesh open area as the same measurement as volumetric porosity.
Can a filter micron rating specify a PEM transport layer?
It cannot define the full PTL requirement. Filtration ratings and electrochemical transport answer different questions. Specify the pore measurement method, transport direction, surface condition, contact behavior and cell qualification required for the actual component.
Can I compare contact resistance from two supplier reports directly?
Only after checking fixture, opposing material, pressure, area, surface state and included interfaces. Clarify units and any correction. Matching numerical units does not establish matching test scope, and cell high-frequency resistance is not automatically PTL contact resistance alone.
Does a good initial polarization curve prove durability?
No. Define the relevant exposure, start-stop or variable-load duty, duration and acceptance criterion. Record conditioning and assembly history. A short test or one favorable operating point does not by itself justify a lifetime claim.
How should a PTL price premium be evaluated?
Compare the finished accepted component, qualification, production yield and operating evidence. Translate measured voltage differences into energy on the actual duty cycle, then include realistic replacement and downtime assumptions. The numerical energy example here is hypothetical, not a product savings claim.
09 / Key takeaways
Keep the purchase requirements connected.
- Compare defined architectures within the same PEM anode duty.
- Keep porosity, open area, pore size and permeability distinct.
- Specify the electrical interface and coating verification basis.
- Preserve compression, conditioning and test history.
- Use measured operating evidence for lifecycle cost decisions.
Technical references
Sources and data scope
References reviewed November 15, 2026. Public source summaries support the discussion; the controlled specification, agreed edition and approved project requirements govern acceptance.
- Chemical Engineering Science, 2026 — PTL and porous flow-field study — Seven-candidate screening dimensions; sample geometry is not a universal family specification.
- Liu et al., 2024 — Fiber-based and powder-based PTLs — Reconstructed structures and modeled transport; not production acceptance data.
- Lee et al., 2023 — Interfacial engineering by laser ablation — Study-specific voltage differences with identified current densities and catalyst loadings.
- Srour et al., 2024 — Anode/PTL contact resistance — Clamping history and distinction between initial performance and durability.
- Singh et al. — Protective coating study, Energy Advances 2026 — Surface passivation and a specific coating system; not a universal coating guarantee.