TiHubs Grade 5 / TC4 titanium material sourcing and product forms

Ti-6Al-4V · ASTM, AMS & Chinese TC4 requirements

Grade 5 / TC4 titanium.To your specification.

Source Grade 5 and Chinese TC4 titanium for aerospace and industrial manufacturing. TiHubs coordinates Ti-6Al-4V sheet, plate, bar, wire and custom hollow-stock enquiries through one technical and commercial contact in Baoji.

Start with a specification, drawing or application. We’ll help identify the details still needed.

Material review. Supply coordination.
One contact in Baoji, China.

Ti-6Al-4VGrade 5 · UNS R56400 · Alpha-beta alloy
ASTM & AMS routesMatched to product form and specification
One contactTechnical review to delivery coordination

01 / Product forms

Grade 5 / TC4 products.
Defined for your drawing.

Choose the material form, then define the standard revision, condition, dimensions and acceptance. For TC4 titanium, include the Chinese product standard and any drawing or customer additions.

Grade 5 titanium sheet and plate for TC4 and ASTM specification enquiries

01 / 04

Ti-6Al-4V · Grade 5 / TC4 flat products

Grade 5 / TC4 titanium sheet & plate

For machined brackets, structural parts and drawing-specified formed components. Send thickness, cut size and the finished-part drawing to review stock condition and machining allowance.

Specification
ASTM B265 Grade 5 or the specified AMS 4911 revision; TC4 plate and sheet to GB/T 3621-2022 form a Chinese ordering route.
Dimensions
Thickness × width × length; flatness, tolerances, rolling direction and cut-edge requirements.
Condition
Annealed or drawing-specified condition; surface finish and any forming or subsequent heat treatment.
Acceptance
Heat identity, material records and required dimensional, mechanical or ultrasonic inspection.
Grade 5 titanium bar and rod for TC4 and ASTM specification enquiries

02 / 04

Ti-6Al-4V · Grade 5 / TC4 machining stock

Grade 5 / TC4 titanium bar & rod

For precision machining, fastener stock and drawing-based structural components. Define usable stock size, material condition and the inspection evidence needed.

Specification
ASTM B348 Grade 5 or the specified AMS 4928 revision; TC4 bars to GB/T 2965-2023 require the applicable condition and product requirements.
Dimensions
Diameter or section × length; straightness, machining allowance and quantity per size.
Condition
Annealed or specified heat treatment; turned, ground or other required surface.
Acceptance
Material certificate, heat traceability and agreed ultrasonic testing, structure and tensile requirements.
Ti-6Al-4V TC4 forged tube illustration with Chinese standard marking; a separate specification option

03 / 04

Ti-6Al-4V / TC4 · Custom hollow-product review

Ti-6Al-4V / TC4 tube & hollow stock

For drawing-defined TC4 hollow stock or a Grade 5 tube enquiry. Review the starting material, forging or machining route and finished dimensions before setting the supply specification.

Specification
Specify the TC4 or Grade 5 material requirement, manufacturing route and finished-product standard. ASTM B338 is not a Grade 5 tube route.
Dimensions
Outside diameter × inside diameter or wall × length; concentricity, end details and machining allowance.
Manufacturing
Confirm a forged, machined or other specified route. A hollow part machined from bar is not automatically certified seamless tubing.
Acceptance
Define material identity, condition, dimensional inspection, NDT and any pressure or leak test required by the design.
Grade 5 titanium wire for TC4 and ASTM specification enquiries

04 / 04

Ti-6Al-4V · Grade 5 / TC4 wire

Grade 5 / TC4 titanium wire

For specified forming and component manufacture. Include the intended process, diameter, supplied condition, surface and delivery format in your enquiry.

Specification
ASTM B863 Grade 5 or the applicable AMS 4928 revision; TC4 wire to GB/T 3623-2022 requires the intended use and condition to be stated.
Dimensions
Diameter and tolerance; coil or straight lengths, coil weight and required quantity.
Condition
Annealed or specified condition; surface cleanliness, straightness and packaging.
Acceptance
Heat or batch records, diameter checks and process-specific testing. Welding and additive feedstock require separate qualification.

Images illustrate Grade 5 / TC4 material forms and specification options. TC4 is the Chinese Ti-6Al-4V designation; conformity follows the actual ordered standard, product form and condition. Markings in an illustration are not evidence of dual certification.

Need a finished shape or part?

Send the drawing and purchase specification for a project review.

01 / Custom requirement

Forgings & near-net shapes

Blocks, discs, rings and drawing-based forgings. Send the rough and finished geometry, machining allowance, material condition and inspection requirements.

Discuss your drawing

02 / Custom requirement

Precision machined parts

Brackets, shafts, sleeves, housings and fittings. Include the drawing revision, critical features, surface requirements and first-article scope.

Discuss your drawing

03 / Custom requirement

Titanium fasteners

Bolts, screws, studs, nuts and washers to the agreed product specification. Define threads, strength, surface treatment and lot traceability.

Discuss your drawing

02 / Material identity

Grade 5 & TC4.
One Ti-6Al-4V family.

Grade 5 titanium is the Ti-6Al-4V alpha-beta alloy identified as UNS R56400 in ASTM specifications. TC4 is the Chinese Ti-6Al-4V alloy designation. TiHubs handles both buying terms on this page for sheet, plate, bar, wire and drawing-based material enquiries.

The shared nominal alloy composition does not make every ASTM, AMS and GB/T requirement interchangeable. Specify the complete grade, product standard and edition, heat-treatment condition, dimensions and acceptance requirements. TC4ELI is a distinct low-interstitial requirement.

895MPa

Published minimum tensile strength
ATI Grade 5 plate reference

828MPa

Published minimum yield strength
ATI Grade 5 plate reference

10%

Published minimum elongation
ATI Grade 5 plate reference

Property or condition Reference Ordering implication
Density Approximately 4.43 g/cm³ Useful for preliminary mass estimates; not an acceptance test.
Annealed material Specified product route AMS 4911L and AMS 4928R cover annealed Ti-6Al-4V products in different forms.
Solution treated and aged Separate requirements Do not transfer annealed values to an STA order. Confirm the applicable specification and test basis.

Numerical reference: ATI Grade 5 — plate data ↗. These published plate values are not universal minimums for every size, form or condition and are not aerospace design allowables. The purchase specification and material records govern acceptance.

For a TC4 order, apply the mechanical requirements in the selected Chinese product standard, heat-treatment condition and size range. The headline Grade 5 reference is not a universal acceptance table for TC4 or aerospace forgings.

Element Symbol Selected plate reference, wt %
Aluminum Al 5.50–6.75
Vanadium V 3.50–4.50
Iron Fe 0.30 maximum
Oxygen O 0.20 maximum
Carbon C 0.08 maximum
Nitrogen N 0.05 maximum
Hydrogen H 0.015 maximum
Titanium Ti Balance

Selected values from ATI Grade 5 plate chemistry ↗. Check all elements, analysis tolerances, sampling and product-form requirements against the specified standard revision. Do not apply this table to Grade 23 or use it as a dual-certification statement for TC4.

TC4 chemistry must satisfy its specified GB/T designation and all purchaser additions. Compare every required element and the analysis rules when ASTM / AMS and Chinese conformity are both requested.

Grade 5 and TC4: specify the route

TC4 identifies the Chinese Ti-6Al-4V alloy. Use GB/T 3620.1 with the relevant plate, bar or wire standard; for aerospace work, include the controlling drawing and purchaser specification. Dual-standard supply requires an explicit review of the actual lot and records.

GB/T 3620.1-2016 View PDF ↗

TC4 versus TC4ELI / Grade 23

TC4ELI is the extra-low-interstitial Ti-6Al-4V variant, commonly associated with Grade 23 enquiries. Do not shorten TC4ELI to TC4 or use a Grade 5 certificate as evidence of ELI conformity. State the exact alloy and material specification.

Grade 5 and Grade 2

Grade 5 is alloyed Ti-6Al-4V; Grade 2 is commercially pure titanium. Review strength, forming, joining and service conditions rather than treating Grade 5 as a universal upgrade.

Material and finished-part approval

A material certificate does not approve a component for flight. The drawing, processing route, testing and customer approval requirements must also be met.

03 / Aerospace & industrial applications

Ti-6Al-4V for
aerospace procurement.

Grade 5 and TC4 titanium enquiries often connect lightweight structural design with demanding manufacturing and inspection requirements. Define the approved material route and evidence before selecting stock.

Application review / 01

Grade 5 / TC4 stock for airframe components

Ti-6Al-4V is used in aircraft structures where strength, mass and fatigue requirements must be considered together.

Products to discuss

Plate for machined brackets and fittings; bar or forging stock for drawing-based structural parts.

What we need to review

Drawing revision, material specification, grain direction, machining allowance, fatigue-critical features and inspection class.

Send your application details

Application review / 02

Fasteners for defined aerospace requirements

Ti-6Al-4V is used for aerospace fasteners, but the raw-material designation is only one part of the finished-fastener requirement.

Products to discuss

Bar and wire feedstock; finished screws, bolts, studs or nuts subject to a separate product review.

What we need to review

Applicable fastener standard or drawing, thread and strength requirements, manufacturing route, surface treatment and lot traceability.

Send your application details

Application review / 03

Fan & compressor-region components

Ti-6Al-4V has applications in fan and cooler compressor-region components. The actual part temperature, duty and approved material condition control selection.

Products to discuss

Specified forging or bar stock and plate for qualified component routes.

What we need to review

OEM material callout, temperature history, cyclic loading, microstructure, NDT and approved-source or process requirements.

Send your application details

Application review / 04

Ti-6Al-4V / TC4 spacecraft structural enquiries

For a spacecraft structural requirement, start with the released drawing and material callout. We coordinate a supply review against that defined scope.

Products to discuss

Plate, bar and custom forgings for machining structural brackets, interfaces and housings.

What we need to review

Mission and part classification, material condition, fracture-control or fatigue requirements, cleanliness and the required traceability package.

Send your application details

Application review / 05

Aerospace fixtures & test hardware

Prototype and ground-test hardware need a clearly stated purpose. Keep qualification articles, test fixtures and flight-deliverable parts identified separately.

Products to discuss

Machined plate or bar components, fixtures and project-specific hollow sections.

What we need to review

Test loads and environment, dimensional requirements, inspection records and whether the material must represent the final flight configuration.

Send your application details

Application review / 06

Lightweight brackets & mechanical interfaces

For lightweight systems, review the complete requirement: mass, stiffness, fatigue, joining and fabrication. A material name alone does not resolve these tradeoffs.

Products to discuss

Thin plate, bar stock and machined fittings or connectors to a controlled drawing.

What we need to review

Geometry, mating materials, dynamic loads, production quantity and dimensional acceptance.

Send your application details

Application review / 07

High-performance mechanical components

Ti-6Al-4V is also used for selected performance components. Define the operating loads and surface or wear requirements before choosing a supply condition.

Products to discuss

Bar, plate and forgings for connecting parts, retainers, brackets and specified fasteners.

What we need to review

Cyclic loads, temperature, contact conditions, heat treatment and finished-part inspection.

Send your application details

Application review / 08

A drawing turns titanium into a component

Send the drawing, operating environment and quantity. We can review the material and manufacturing questions that affect quotation.

Products to discuss

Shafts, sleeves, housings, fittings, forgings and custom components subject to feasibility review.

What we need to review

Critical tolerances, corrosion environment, sliding contact, surface treatment, inspection and delivery priorities.

Send your application details

Aircraft material-use reference: Kobe Steel — titanium alloys for aircraft ↗. Spaceflight materials also need application-specific verification: NASA — Ti-6Al-4V environment-assisted cracking research ↗. These references describe material applications, not TiHubs project history or flight approval.

Aerospace enquiry checklist

What should an aerospace RFQ include?

Give us the controlling requirements early so the supply route, evidence and quotation can be evaluated together.

01

Define the material route

Send the exact ASTM / AMS revision or TC4 Chinese specification and edition, form, dimensions and heat treatment. Include any drawing-specified GJB, HB or customer requirements, melt route and microstructure criteria.

02

Define the acceptance evidence

List heat and lot traceability, material test reports, dimensional records, NDT methods and acceptance classes. State any first-article, retained-sample or independent inspection requirements.

03

Identify required approvals

Include approved-source restrictions and any customer-required quality-system or special-process approvals. TiHubs reviews the required evidence and feasible supply route before commitment.

Example: a useful TC4 aerospace plate enquiry

TC4 titanium plate; GB/T 3621 [required edition] plus the controlling aerospace drawing or purchaser specification; specified condition; thickness × width × length and tolerances; quantity; grain direction; machining allowance; material and inspection records; approved-source restrictions; destination and target date.

If AMS 4911 conformity is also required, state the revision and request an explicit review against both specifications. A commercial TC4 plate description alone does not establish aerospace approval.

Discuss an aerospace requirement ↗

04 / Standards & documentation

Grade 5 / TC4 standards.
Matched to the product.

Use ASTM / AMS for the specified Grade 5 or Ti-6Al-4V route, and the applicable Chinese standard for TC4. A grade/composition reference supports material identification; the product standard, condition and purchaser requirements complete the order.

9 reference files on TiHubs · Select a standard to preview or download.
Product form ASTM / AMS route Chinese standard route Clarify before quotation
Material identity & composition United StatesTi-6Al-4V · UNS R56400

Use the chemical requirements in the specified ASTM or AMS product standard.

ChinaGB/T 3620.1-2016 View PDF ↗

TC4 designation and chemistry. Apply with the relevant product standard; it does not set all dimensions, properties or inspection requirements.

Grade designation, all specified elements and the agreed analysis and acceptance basis.
Sheet & plate United StatesASTM B265-08 View PDF ↗AMS 4911L View PDF ↗ ChinaGB/T 3621-2022 View PDF ↗

TC4 plate and sheet: specify condition, thickness and flatness tolerances, surface, rolling direction and additional inspection.

Thickness, width, length, condition, grain direction and required inspection.
Bar & rod United StatesASTM B348-08a View PDF ↗AMS 4928R View PDF ↗ ChinaGB/T 2965-2023 View PDF ↗

TC4 bars: specify section, condition, straightness, surface, machining allowance, microstructure and additional NDT where required.

Section, straightness, surface, heat treatment, structure and NDT.
Wire United StatesASTM B863-19 View PDF ↗AMS 4928R View PDF ↗ ChinaGB/T 3623-2022 View PDF ↗

TC4 wire: state intended use, condition, diameter, coil or straight-length format, surface and acceptance.

Diameter, coil or straight length, condition, intended manufacturing use and surface.
Forgings & drawn shapes United StatesAMS 4928R View PDF ↗ ChinaDrawing and specified Chinese standard

TC4 forging enquiries require a suitable forging or drawing specification, material flow, machining allowance and inspection scope.

Rough and finished geometry, material flow, machining allowance and acceptance.
Tube & hollow sections United StatesProject-specific specification

ASTM B338 does not list Grade 5. Do not use a bar or sheet standard alone as a finished-tube specification.

ChinaTC4 route reviewed separately

TC4 hollow-product enquiries require the manufacturing route, finished geometry, condition and applicable product specification.

OD, ID or wall, length, forming route, material condition and testing.
File revision and purchase requirement are separate. The linked AMS files are AMS 4911L (June 2007) and AMS 4928R (January 2007). ASTM file editions are shown in their link titles. These reference files do not set the revision for your order; quote the revision required by your drawing or contract.

Publisher scope references: SAE AMS 4911L ↗ · SAE AMS 4928R ↗. A material-specification reference does not establish approved-source status or completed-part conformity.

05 / Order coordination

Know the scope
before ordering.

Our founder’s 20 years in titanium inform the questions we ask before quotation and the supply options we review with you.

Illustration of titanium components, a micrometer, inspection documents and protective packaging
Inspection planning illustration. Actual certificates and reports are defined for the order.
A quotation you can evaluate

Agree the grade, standard edition, dimensions, tolerance, condition and quantity before comparing prices.

  • Identify whether inspection, samples and tooling are included.
  • Confirm packaging, transport and delivery terms.
  • Record items that still need technical confirmation.
Acceptance agreed before supply

Confirm the material certificate, heat or batch identity, heat-treatment condition, dimensional checks and any additional testing before supply starts. For aerospace work, include the customer-required inspection and traceability scope.

Independent inspection can be discussed with its scope, timing, acceptance criteria and cost agreed for the order.

Delivery with clear milestones

Review the proposed lead time, approvals, production sequence and dispatch requirements. For several product forms, coordinate document and packing readiness together.

Material substitutions and technical changes require written approval. A schedule deviation should identify the impact, decisions needed and next steps.

One contact when an issue arises

Contact TiHubs with the order reference, affected items and supporting photos or inspection records.

We record the issue, review it against the agreed requirements and coordinate the next steps with the relevant manufacturing parties.

01 / Material identity

Material records

Full Grade 5 or TC4 designation, standard edition, condition, test results and heat or lot identity linked to the supplied items.

  • Material certificate
  • Heat / batch ID
  • Test results
02 / Agreed acceptance

Inspection records

Dimensional and testing records for the agreed scope, including critical drawing requirements.

  • Dimensions
  • Agreed testing
  • Acceptance criteria
03 / Ready for dispatch

Dispatch records

Item identification, packing list, protective packaging and required shipment documents.

  • Packing list
  • Item labels
  • Shipping documents

06 / Questions before sourcing

Before you source
Grade 5 / TC4 titanium.

Use Grade 5 or TC4 to begin the discussion. The full material designation, product standard and edition, condition, dimensions and acceptance requirements make the quotation useful.

A useful first enquiry

  • Product and specificationGrade 5 or TC4, the complete standard callout, product form, condition and dimensions.
  • Order and deliveryQuantity, destination and any required delivery date.
  • Acceptance requirementsDrawing revision, inspection, certificates and packaging.

Not every detail is finalized? Send the information you have. We can help identify the questions to resolve before quotation.

Discuss your requirement

What happens next: requirement review, technical clarification, then a supply proposal and quotation.

What is Grade 5 titanium?

Grade 5 is Ti-6Al-4V, an alpha-beta titanium alloy identified as UNS R56400. It is used in aerospace and industrial components where strength relative to weight matters. The product standard and delivery condition still need to be specified.

What is TC4 titanium used for?

TC4 is the Chinese Ti-6Al-4V alloy designation used for specified aerospace structures, machined structural parts and other strength-to-weight applications. The drawing determines the suitable product form, condition and acceptance requirements. A generic TC4 material certificate alone does not establish flight approval.

Which standard should I specify: ASTM B265, B348, AMS 4911 or AMS 4928?

Choose the standard required by your drawing or contract and the actual product form. ASTM B265 covers strip, sheet and plate; B348 covers bars and billets. AMS 4911L covers annealed Ti-6Al-4V sheet, strip and plate; AMS 4928R covers annealed bars, wire, forgings, flash welded rings, drawn shapes and related stock. These are not automatic substitutes.

Which Chinese standards apply to TC4 titanium?

Use GB/T 3620.1 for designation and composition, with the appropriate product standard: GB/T 3621 for plate and sheet, GB/T 2965 for bars, or GB/T 3623 for wire. Forgings, hollow products and aerospace orders require their own applicable product or purchaser specifications. State all editions and additional requirements explicitly.

Can you review an aerospace or spacecraft requirement?

Yes. Send the drawing revision, material specification and revision, product form, condition, quantity and required evidence. Include approved-source restrictions and required quality-system or special-process approvals. We assess the supply route and required documentation before confirming feasibility; Grade 5 identification alone is not flight approval.

Is TC4 the same as TC4ELI?

No. TC4ELI is the extra-low-interstitial Ti-6Al-4V variant. Its chemistry and intended purchase specification must remain explicit. Do not substitute TC4 or Grade 5 for TC4ELI / Grade 23 requirements without technical review and written agreement.

Is Grade 5 titanium the same as TC4 titanium?

Grade 5 and TC4 are commonly associated designations for the Ti-6Al-4V alloy family. ASTM Grade 5, AMS Ti-6Al-4V and Chinese TC4 orders still have their own product, chemistry, property, condition and inspection requirements. TiHubs handles them on one page and reviews any substitution or dual-standard requirement before supply.

Is Grade 5 the same as Grade 23 or Ti-6Al-4V ELI?

No. Grade 23 is the extra-low-interstitial Ti-6Al-4V variant. Keep Grade 23 or ELI requirements explicit. An industrial Grade 5 order also does not establish compliance with an implant-material specification.

Can Grade 5 tube be ordered to ASTM B338?

ASTM B338 does not list Grade 5. Send the tube drawing, manufacturing route, service conditions and required specification for review. The TC4 tube shown here illustrates a separately assessed Chinese material route.

Can you quote a size or machined part that is not listed?

Send the dimensions or drawing, tolerances, material condition, quantity and destination. We will review suitable manufacturing resources and clarify feasibility before quotation. This page does not mean every size or product is held in stock.

What are the minimum order quantity and lead time?

They depend on the product form, dimensions, condition, quantity, manufacturing route and inspection. We confirm the proposed quantity basis, lead time and approval milestones with the quotation.

Can you provide material certificates, samples or independent inspection?

The required records and inspection scope are agreed during quotation. Samples and independent inspection can be discussed with acceptance criteria, timing and costs defined for the order. Final evidence must relate to the supplied heat, batch or items.

Can Grade 5 wire be used as welding or additive-manufacturing feedstock?

Only when it meets the relevant feedstock specification and process requirements. An ASTM B863 Grade 5 description alone does not establish welding-filler classification or qualification for a particular additive process.

Who handles an order issue?

TiHubs remains your technical and commercial contact. We record the issue, review it against the agreed requirements and coordinate the next steps with the relevant manufacturing parties.

07 / Your next step

Start with the
requirement you have.

Send your Grade 5 or TC4 titanium specification, drawing or application requirements. We review the material route, clarify missing details and discuss supply options before preparing a quotation.

  1. Requirement review
  2. Technical clarification
  3. Supply proposal and quotation

Combine several items in one enquiry.

Send one list of forms, sizes and quantities. Include drawing revisions, required AMS or other standards and items that must arrive together.

Share delivery and acceptance priorities.

Include the destination, target date, inspection scope and aerospace approval or traceability requirements that affect your order.

Baoji, China · info@tihubs.com

Start your Grade 5 / TC4 enquiry

Tell us what you need. Details can be clarified after your first enquiry.

Customer Feedback & RFQ Form (#6)