TC26 / Ti-13Nb-13Zr · Niobium-zirconium titanium alloy
TC26 / Ti-13Nb-13Zr. Traceable stock for implant manufacture.
Source TC26 / Ti-13Nb-13Zr medical bar, wire and precision machining blanks. Build the enquiry around ASTM F1713, the required material state and a traceable manufacturing and inspection plan.
Start with a specification, drawing or application. We’ll help identify the details still needed.
Material review. Supply coordination.
One contact in Baoji, China.
01 / Product forms
Find your TC26 product.
Choose a material form or application. Send the dimensions, service conditions and required records so we can match the manufacturing route to your order.

TC26 / Ti-13Nb-13Zr
TC26 medical bar & rod
Round stock for implant manufacturers ordering Ti-13Nb-13Zr by a defined material specification.
- Specification
- ASTM F1713, UNS R58130; identify edition, size and required condition.
- Size & delivery
- Diameter, tolerance, cut length, straightness and turned or ground finish.
- Manufacturing review
- Define machining allowance and any downstream forming or thermal processing.
- Inspection priorities
- Complete material certification, required mechanical tests, surface integrity and heat-to-piece identity.

TC26 / Ti-13Nb-13Zr
TC26 medical wire
Coils and straight lengths for specified Ti-13Nb-13Zr component manufacturing.
- Specification
- ASTM F1713 wire requirements and the agreed material state.
- Size & delivery
- Diameter, tolerance, cast, helix, straightness, packaging and lot size.
- Manufacturing review
- Share the forming and finishing route. Do not treat product wire as an automatically qualified welding consumable.
- Inspection priorities
- Diameter and surface checks, mechanical testing and lot segregation under the order.

TC26 / Ti-13Nb-13Zr
TC26 precision machining blanks
Cut bar and oversize blanks for turning, milling and representative qualification specimens.
- Specification
- Specify the parent bar standard and each subsequent conversion stage.
- Size & delivery
- Blank envelope, end allowance, datum faces, test-stock locations and quantity.
- Manufacturing review
- Coordinate rough machining, thermal processing and finish allowance; identify when final material properties are established.
- Inspection priorities
- Parent heat traceability, conversion records and agreed dimensional and surface inspection.

TC26 / Ti-13Nb-13Zr
Ti-13Nb-13Zr joint-component blanks
Application illustration: oversize blanks for joint-component designs explicitly specified in Ti-13Nb-13Zr.
- Specification
- Released device drawing, starting-material specification and approved manufacturing plan.
- Size & delivery
- Envelope, load-bearing sections, interfaces, machining stock and marking areas.
- Manufacturing review
- Identify whether forging, machining, surface treatment or coating is included at delivery.
- Inspection priorities
- Material and process records plus drawing-based inspections; finished-device validation remains separately controlled.

TC26 / Ti-13Nb-13Zr
TC26 fixation-component blanks
Application illustration: material or machining blanks for specified fixation-component development and production.
- Specification
- Approved component drawing and the applicable Ti-13Nb-13Zr material route.
- Size & delivery
- Thread geometry, plate or rod envelope, hole position, critical radii and tolerance.
- Manufacturing review
- Define forming, machining, deburring, cleaning and any subsequent thermal treatment.
- Inspection priorities
- Inspect critical dimensions and surfaces; validate final component and assembly performance separately.

TC26 / Ti-13Nb-13Zr
TC26 precision interface blanks
Application illustration: small turned and milled blanks for medical designs with controlled fits and surfaces.
- Specification
- Drawing revision, raw-material condition and agreed delivery stage.
- Size & delivery
- Concentricity, bore and thread allowance, surface roughness and batch size.
- Manufacturing review
- Agree workholding surfaces, clean handling and protection of critical features in transit.
- Inspection priorities
- First-article dimensions, surface criteria and traceability to the certified parent stock.
Images illustrate material forms and application possibilities. Reference markings identify specification options; they do not establish dual certification, stock availability or approval of finished equipment.
Define the shape. Share the service.
These details help turn a material enquiry into a comparable quotation.
01 / Drawing review
Drawing-controlled blanks
Provide rough and finished drawings, datum positions, critical sections, machining allowance and the intended conversion route.
Discuss your drawing02 / Drawing review
Heat treatment & process sequence
Identify the required delivery condition and subsequent manufacturing steps. Agree process records, sampling stages and dimensional checks after thermal processing.
Discuss your drawing03 / Drawing review
Component inspection planning
Specify surface integrity, microstructure, NDT, dimensional acceptance and traceability. Identify which tests apply to raw material and which apply to the finished component.
Discuss your drawing02 / Material identity
What is TC26 / Ti-13Nb-13Zr titanium?
TC26 is the Chinese designation associated with Ti-13Nb-13Zr, a titanium-niobium-zirconium alloy identified as UNS R58130 in ASTM F1713. It provides a dedicated material route for implant manufacturers whose drawings specify this composition. Bar and wire certification, downstream processing and finished device acceptance need to be defined separately.
Specify the exact standard edition, form and delivery condition. Nominal chemistry is only one part of an order; strength, microstructure, dimensional acceptance and traceability also need to be defined.
| Review item | Order basis | What to confirm |
|---|---|---|
| Material condition | Define the ordered heat-treatment state | Tie test results to the same conversion and thermal history as the supplied product. |
| Strength and ductility | Product- and section-dependent | Specify tensile, proof strength, elongation, sampling location and test direction in the purchase requirement. |
| Microstructure | Agree acceptance limits | Review grain structure, alpha morphology, surface alpha case and metallographic sampling for the manufacturing route. |
| Fatigue and fracture | Application-specific validation | A material tensile certificate does not establish component life. Specify any fatigue, toughness or crack-growth evaluation separately. |
| Non-destructive examination | Drawing / product specification | Define method, calibration, coverage, acceptance class and reporting before production. |
| Selected element · wt % | Reference composition |
|---|---|
| Niobium · Nb | 12.5–14.0 |
| Zirconium · Zr | 12.5–14.0 |
| Iron · Fe | 0.25 max. |
| Carbon · C | 0.08 max. |
| Nitrogen · N | 0.05 max. |
| Hydrogen · H | 0.012 max. |
| Oxygen · O | 0.15 max. |
| Titanium · Ti | Balance |
Selected TC26 limits, wt %, from GB/T 3620.1-2016. Confirm complete chemistry, analysis tolerances, condition and testing against the ordered ASTM F1713 or other agreed product specification.
TC26 and ASTM F1713
ASTM F1713 addresses wrought Ti-13Nb-13Zr bar and wire for surgical implant manufacture. A Chinese grade designation alone does not establish compliance with the complete ASTM document.
Compared with TC20
TC26 uses niobium and zirconium as its main intentional alloying additions; TC20 is Ti-6Al-7Nb. Their composition and material requirements must remain distinct.
Compared with TB11
TB11 / Ti-15Mo follows a molybdenum alloy system and an ASTM F2066 route. Use the material specified by the device design, with separate evaluation of properties and processing.
Raw stock versus a component
A machined blank retains material traceability, but additional processing can introduce new requirements. Device-level fatigue, biological evaluation and final release are separate responsibilities.
03 / Application priorities
TC26 in application.
Review each main use through its service conditions, material choice, manufacturing route and acceptance plan. These are sourcing discussions; approved drawings and qualification requirements govern the final component.
Application review / 01
Specified implant-material programmes
TC26 / Ti-13Nb-13Zr is a targeted procurement choice when the device drawing already calls for this niobium-zirconium titanium alloy. The enquiry should identify the finished function and manufacturing stage without treating a material standard as device approval.
Products & manufacturing
ASTM F1713 bar and wire, plus cut or machined blanks under an agreed conversion plan.
Service & design review
State the approved material designation, standard edition, required condition and downstream processes. Resolve any proposed material substitution before purchasing qualification stock.
Purchase & inspection priorities
Match certification to the exact ordered product. Maintain heat and processing-lot identity through machining, forming and final inspection.
Application review / 02
Joint-component manufacturing
For joint designs specified in Ti-13Nb-13Zr, the blank must support the approved geometry and process sequence. Load-bearing sections and interfaces require attention to machining stock, material state and surface treatment.
Products & manufacturing
Bar, oversize machining stock and drawing-specific conversion blanks.
Service & design review
Provide critical sections, interface geometry, datum system, allowable route and final surface condition. Identify the stages performed by TiHubs supply partners and those retained by the device manufacturer.
Purchase & inspection priorities
Require the agreed material and conversion records, dimensional reports and surface examination. Device fatigue testing and regulatory release are outside raw-stock certification.
Application review / 03
Fixation-component development
Fixation parts introduce threads, holes, bends or thin transitions that may control manufacturing quality. A TC26 trial should represent the intended production geometry and process rather than rely on a generic bar coupon alone.
Products & manufacturing
Medical bar or wire and drawing-controlled blanks for specified screws, rods or other fixation concepts.
Service & design review
Define forming strain, thread method, hole geometry, edge condition and the final thermal state. Establish who approves changes after prototype evaluation.
Purchase & inspection priorities
Inspect material identity, critical dimensions and surface integrity. Establish final-part and assembly validation under the responsible design authority.
Application review / 04
Medical wire conversion
TC26 wire enquiries need both dimensional requirements and an intended conversion route. The ordered condition should support subsequent processing while keeping the final material acceptance requirements clear.
Products & manufacturing
Coiled wire, straight lengths and cut wire stock under ASTM F1713.
Service & design review
Provide diameter tolerance, straightness or coil requirements, bend geometry, thermal sequence and handling limits. Identify any surfaces that cannot be reworked after forming.
Purchase & inspection priorities
Agree incoming surface and mechanical tests, lot segregation and any additional checks after conversion. Product wire is not evidence of a qualified welding or joining process.
Application review / 05
Precision machined interfaces
A Ti-13Nb-13Zr component with small bores, threads or close fits needs a stable stock and machining specification. Raw material tolerances and final component tolerances are different purchasing requirements.
Products & manufacturing
Bar, cut cylinders and rough-machined interface blanks.
Service & design review
Share the final drawing, concentricity, surface roughness, datum references and remaining machining allowance. Define deburring, cleaning and packaging responsibilities.
Purchase & inspection priorities
Use first-article dimensional reports and agreed surface criteria. Retain the link from each machining lot to its parent heat.
Application review / 06
Material-condition qualification
ASTM F1713 material purchasing must identify the required state and applicable testing. A subsequent heat treatment or forming operation can change the properties demonstrated on the incoming certificate.
Products & manufacturing
Representative bar and wire, machining blanks and retained specimens from the planned route.
Service & design review
Define the delivered and final conditions, processing records, specimen locations and property criteria. Do not substitute a research heat treatment for an approved production instruction.
Purchase & inspection priorities
Verify the specified tensile, proof-strength, ductility and other required results at the correct stage. Document any process change requiring renewed qualification.
Application review / 07
Surface quality & clean handling
Medical starting stock needs surface controls appropriate to the amount of subsequent machining and the intended manufacturing environment. A polished appearance alone does not establish cleanliness or freedom from harmful defects.
Products & manufacturing
Turned or ground bar, controlled-surface wire and protected machining blanks.
Service & design review
State permissible defects, stock removal, cleaning method, packaging and identification requirements. Define whether surface condition is checked before or after the final conversion step.
Purchase & inspection priorities
Agree the inspection method and reject criteria. Keep surface and packaging records connected to the correct lot and delivery condition.
Application review / 08
Repeat lots & document control
Recurring TC26 procurement should preserve the same approved specification and process route unless a change is reviewed. Itemized orders help distinguish raw bar, wire and partially machined blanks with different acceptance stages.
Products & manufacturing
Scheduled lots of documented medical stock and drawing-based blanks.
Service & design review
Provide revision-controlled drawings, order quantities, certificate fields, source restrictions, inspection hold points and delivery sequence.
Purchase & inspection priorities
Reconcile markings, heat and lot numbers, material reports and packing lists. Retain the approval history for any accepted variation.
TC26 procurement checklist
Connect the application to the material order.
A useful specification connects the intended component, the supplied stock and the acceptance evidence. Share the drawing and known requirements first.
Define the application
State the approved material designation, standard edition, required condition and downstream processes. Resolve any proposed material substitution before purchasing qualification stock.
Define the supplied stage
ASTM F1713 bar and wire, plus cut or machined blanks under an agreed conversion plan. Distinguish raw stock, converted blanks and finished parts. Define who controls subsequent processing.
Define the acceptance evidence
Match certification to the exact ordered product. Maintain heat and processing-lot identity through machining, forming and final inspection.
Example: a useful TC26 material enquiry
TC26 medical bar & rod; required dimensions and quantity; standard and drawing revision; delivery condition; intended downstream process; mechanical, structural and dimensional acceptance; traceability, destination and required date.
Identify the approved product specification and any project-specific qualification. The grade designation and chemistry standard alone do not define component acceptance.
Discuss your material requirement ↗04 / Standards & documentation
Match the standard
to the product.
Choose the specification by product form, material condition and application. Identify the required edition on the order; a chemistry standard alone does not define a finished forging or component.
| Product / review | International / project route | Chinese reference | Clarify before quotation |
|---|---|---|---|
| Identity & chemistry | ASTM F1713-08(2021)e1Publisher reference ↗ | GB/T 3620.1-2016View PDF ↗ | Verify the full composition and ordered product requirements. A Chinese grade name alone does not establish international or dual certification. |
| Medical bar & wire | ASTM F1713-08(2021)e1Publisher reference ↗ | Documented comparison with the ordered Chinese requirements | ASTM F1713 covers wrought bar and wire. Specify the required material state, size and mechanical testing; do not extend this scope to every custom shape. |
| Drawing-based blanks & parts | Approved drawing and controlled manufacturing plan | Agreed product / project specification | Define the supply stage, conversion route, heat treatment, structure, NDT, dimensions and traceability. Material certification is separate from finished component qualification. |
The purchase order must identify the required revision, grade, product form, condition and inspection. Reference documents do not replace design approval, manufacturing qualification or application-specific acceptance.
Request the controlled specification revision for your order. Any substitution, equivalence or dual-certification claim requires a documented comparison and agreement.
05 / Order coordination
Know the scope
before ordering.
Our founder’s 20 years in titanium inform the questions we ask before quotation and the supply options we review with you.

A quotation you can evaluate
Agree the grade, standard edition, dimensions, tolerance, condition and quantity before comparing prices.
- Identify whether inspection, samples and tooling are included.
- Confirm packaging, transport and delivery terms.
- Record items that still need technical confirmation.
Acceptance agreed before supply
Confirm material identity, delivery condition, heat-to-piece traceability, dimensional checks and required testing before production. For converted parts, define inspection after forging, heat treatment and machining, including the specified microstructure and NDT scope.
Independent inspection can be discussed with its scope, timing, acceptance criteria and cost agreed for the order.
Delivery with clear milestones
Review the proposed lead time, approvals, production sequence and dispatch requirements. For several product forms, coordinate document and packing readiness together.
Material substitutions and technical changes require written approval. A schedule deviation should identify the impact, decisions needed and next steps.
One contact when an issue arises
Contact TiHubs with the order reference, affected items and supporting photos or inspection records.
We record the issue, review it against the agreed requirements and coordinate the next steps with the relevant manufacturing parties.
Material records
Grade, standard, test results and heat or batch identity matched to the supplied items.
Inspection records
Dimensional and testing records for the agreed scope, including critical drawing requirements.
Dispatch records
Item identification, packing list, protective packaging and required shipment documents.
06 / Questions before sourcing
Before you specify
TC26 / Ti-13Nb-13Zr.
A clear material designation is the beginning. Product form, specification revision, material condition and acceptance complete the requirement.
A useful first enquiry
- Product and specificationProduct form, standard edition, dimensions and material condition.
- Order and deliveryQuantity, destination and any required delivery date.
- Acceptance requirementsDrawing revision, inspection, certificates and packaging.
Not every detail is finalized? Send the information you have. We can help identify the questions to resolve before quotation.
What happens next: requirement review, technical clarification, then a supply proposal and quotation.
What is TC26 titanium?
TC26 is the Chinese designation associated with Ti-13Nb-13Zr, a titanium-niobium-zirconium alloy used as specified starting material for implant manufacture.
Which ASTM standard applies to Ti-13Nb-13Zr?
ASTM F1713 is the wrought Ti-13Nb-13Zr implant-material reference, identified as UNS R58130. State the exact edition, product form and material condition on the order.
Does ASTM F1713 cover every product shape?
The standard addresses bar and wire. Custom forgings, machined blanks or other shapes need a clear parent-material specification and an agreed conversion and final acceptance plan.
Is TC26 the same as TC20 or TB11?
No. TC20 is associated with Ti-6Al-7Nb and TB11 with Ti-15Mo. TC26 uses the Ti-13Nb-13Zr alloy system. Their certifications and manufacturing qualifications are not interchangeable.
Which material condition should I order?
Use the condition required by the approved material and manufacturing specification. Identify downstream thermal or mechanical processing and the stage at which final properties must be verified.
Can I order TC26 precision machining blanks?
Yes, submit the drawing and required delivery stage for review. Include parent stock requirements, dimensions, allowance, surface condition, traceability and inspection so the supply scope can be confirmed.
Does an ASTM F1713 certificate approve the finished implant?
No. Material compliance is one input to device manufacture. The responsible manufacturer must address the approved design, process validation, component performance and final regulatory release.
What documents should accompany TC26 stock?
Define chemistry, material condition, mechanical tests, dimensional and surface results, heat and lot identity, and any additional agreed examination. Converted blanks also need the relevant process records.
What should I send for a TC26 quotation?
Send product form, size, quantity, ASTM F1713 edition, condition, tolerances, finish, testing and destination. Include the drawing revision and downstream manufacturing route for custom blanks.
07 / Your next step
Start with the
requirement you have.
Send the product details, drawing or operating conditions you already know. We will identify missing information and discuss a suitable supply route before quotation.
- Requirement review
- Technical clarification
- Supply proposal and quotation
Combine materials and parts in one enquiry.
Send one list of TC26 forms, sizes and quantities. Include drawing revisions, material conditions and items that must be supplied or dispatched together.
Share the service and acceptance priorities.
Include load and temperature conditions, critical sections, required material records, process qualification, inspection, destination and timing.
Baoji, China · info@tihubs.com
Start your TC26 / Ti-13Nb-13Zr enquiry