TB11 / Ti-15Mo · Beta titanium alloy
TB11 / Ti-15Mo. Medical starting stock, clearly specified.
Source TB11 / Ti-15Mo medical bar, wire and machining stock with an ASTM F2066 purchasing route. Define material condition, surface finish, traceability and downstream processing for your implant manufacturing programme.
Start with a specification, drawing or application. We’ll help identify the details still needed.
Material review. Supply coordination.
One contact in Baoji, China.
01 / Product forms
Find your TB11 product.
Choose a material form or application. Send the dimensions, service conditions and required records so we can match the manufacturing route to your order.

TB11 / Ti-15Mo
TB11 medical bar & rod
Starting stock for precision-machined implant components whose drawing specifies Ti-15Mo.
- Specification
- ASTM F2066 Ti-15Mo, UNS R58150, with edition and ordered condition stated.
- Size & delivery
- Diameter, length, tolerance, straightness, turned or ground surface and lot size.
- Manufacturing review
- Review thermal history, machining allowance, cleaning and any subsequent forming or heat treatment.
- Inspection priorities
- Chemical and mechanical results, required structure, surface integrity and heat-to-piece traceability.

TB11 / Ti-15Mo
TB11 medical wire
Wire and straight lengths for validated medical component manufacturing. Shape and surface requirements should reflect the intended process.
- Specification
- ASTM F2066 applicable wire requirements; identify condition and test scope.
- Size & delivery
- Diameter, tolerance, coil or straight form, cast, helix and protective packaging.
- Manufacturing review
- State the forming sequence and final function. Do not assume generic wire is a qualified welding filler or a shape-memory product.
- Inspection priorities
- Surface defects, diameter consistency, mechanical tests and any applicable bend testing under the ordered specification.

TB11 / Ti-15Mo
TB11 plate, sheet & strip
Flat product enquiries for a specified manufacturing programme, subject to actual size and supply feasibility.
- Specification
- ASTM F2066 includes strip, sheet and plate; confirm the ordered form and condition.
- Size & delivery
- Thickness, width, length, flatness, rolling direction and surface finish.
- Manufacturing review
- Provide forming strain, bend geometry, machining route and the intended final thermal state.
- Inspection priorities
- Directional testing where required, thickness and flatness, edge quality, surface inspection and traceability.

TB11 / Ti-15Mo
Ti-15Mo machining blanks
Cut bar and oversize blanks that preserve stock for machining and qualification tests.
- Specification
- Define the parent product standard and the delivered conversion stage. A custom billet is not automatically covered by every wrought-product requirement.
- Size & delivery
- Blank envelope, cut length, end allowance, datums and retained test stock.
- Manufacturing review
- Agree cutting, roughing, stabilization and final machining responsibilities.
- Inspection priorities
- Link each blank to its parent heat and certification; agree checks after any additional thermal or mechanical processing.

TB11 / Ti-15Mo
Ti-15Mo orthopedic component blanks
Application illustration: blanks for orthopedic device designs that explicitly specify Ti-15Mo.
- Specification
- Released device drawing, ASTM F2066 starting material and approved process plan.
- Size & delivery
- Component envelope, critical sections, surface allowance and marking location.
- Manufacturing review
- Review machining and surface-treatment stages without treating the illustration as an approved device design.
- Inspection priorities
- Material records and agreed component inspection; device validation and regulatory release remain with the responsible manufacturer.

TB11 / Ti-15Mo
Ti-15Mo precision machining stock
Application illustration: small blanks and machined features for development or production programmes with a defined material requirement.
- Specification
- Ti-15Mo material specification plus drawing revision and manufacturing-stage definition.
- Size & delivery
- Critical diameters, thread allowance, concentricity, surface roughness and batch size.
- Manufacturing review
- Agree deburring, cleaning, protection from contamination and handling between machining stages.
- Inspection priorities
- Dimensional reports, surface integrity and traceability to the parent material and processing lot.
Images illustrate material forms and application possibilities. Reference markings identify specification options; they do not establish dual certification, stock availability or approval of finished equipment.
Define the shape. Share the service.
These details help turn a material enquiry into a comparable quotation.
01 / Drawing review
Drawing-controlled blanks
Provide rough and finished drawings, datum positions, critical sections, machining allowance and the intended conversion route.
Discuss your drawing02 / Drawing review
Heat treatment & process sequence
Identify the required delivery condition and subsequent manufacturing steps. Agree process records, sampling stages and dimensional checks after thermal processing.
Discuss your drawing03 / Drawing review
Component inspection planning
Specify surface integrity, microstructure, NDT, dimensional acceptance and traceability. Identify which tests apply to raw material and which apply to the finished component.
Discuss your drawing02 / Material identity
What is TB11 / Ti-15Mo titanium?
TB11 is the Chinese designation for the Ti-15Mo alloy family. ASTM F2066 identifies wrought titanium-15 molybdenum alloy, UNS R58150, for surgical implant manufacture. Its beta-alloy metallurgy makes it relevant to lower-modulus material selection, but modulus and strength depend on the delivered microstructure and processing history. Medical device suitability must follow the approved design and validation plan.
Specify the exact standard edition, form and delivery condition. Nominal chemistry is only one part of an order; strength, microstructure, dimensional acceptance and traceability also need to be defined.
| Review item | Order basis | What to confirm |
|---|---|---|
| Material condition | Define the ordered heat-treatment state | Tie test results to the same conversion and thermal history as the supplied product. |
| Strength and ductility | Product- and section-dependent | Specify tensile, proof strength, elongation, sampling location and test direction in the purchase requirement. |
| Microstructure | Agree acceptance limits | Review grain structure, alpha morphology, surface alpha case and metallographic sampling for the manufacturing route. |
| Fatigue and fracture | Application-specific validation | A material tensile certificate does not establish component life. Specify any fatigue, toughness or crack-growth evaluation separately. |
| Non-destructive examination | Drawing / product specification | Define method, calibration, coverage, acceptance class and reporting before production. |
| Selected element · wt % | Reference composition |
|---|---|
| Molybdenum · Mo | 14.0–16.0 |
| Iron · Fe | 0.10 max. |
| Carbon · C | 0.10 max. |
| Nitrogen · N | 0.05 max. |
| Hydrogen · H | 0.015 max. |
| Oxygen · O | 0.20 max. |
| Titanium · Ti | Balance |
Selected TB11 limits, wt %, from GB/T 3620.1-2016. An ASTM F2066 order requires verification against the complete ordered edition, including its product, condition and testing requirements.
TB11 and ASTM F2066
The Chinese designation and the ASTM Ti-15Mo route should be linked through documented chemistry, form, condition and test compliance. A TB11 identity alone is not proof of ASTM certification.
Compared with TC4 ELI
Ti-15Mo uses molybdenum as its main intentional alloying addition. TC4 ELI is an extra-low-interstitial Ti-6Al-4V route. Their material and process qualifications remain distinct.
Compared with TC20 / Ti-6Al-7Nb
These are different alloy systems. A lower-modulus design objective may motivate a Ti-15Mo evaluation, but approved geometry, strength, fatigue and processing requirements govern the choice.
Not Ti-15Mo-5Zr-3Al
Ti-15Mo is not the zirconium-aluminium-containing alloy identified by that longer name. Keep the complete composition and material standard in the order to avoid a purchasing mismatch.
03 / Application priorities
TB11 in application.
Review each main use through its service conditions, material choice, manufacturing route and acceptance plan. These are sourcing discussions; approved drawings and qualification requirements govern the final component.
Application review / 01
Low-modulus implant material selection
Ti-15Mo is relevant when an implant design programme evaluates a beta titanium alloy with a lower elastic modulus. This is a material-selection objective, not a promise that every delivered bar has one fixed modulus or that a component automatically reduces stress shielding.
Products & manufacturing
ASTM F2066 bar, wire or flat product matching the intended manufacturing route.
Service & design review
Specify the target property, measurement method, material condition and acceptable variation. Review stiffness together with component geometry, fatigue, strength and surface processing.
Purchase & inspection priorities
Confirm the ordered chemistry and condition, representative property testing and manufacturing history. Keep design validation separate from raw-material release.
Application review / 02
Orthopedic component machining
For orthopedic designs specified in Ti-15Mo, machining begins with controlled starting stock and a defined final material state. Thin sections, transitions and surface finish can influence component performance independently of the bar tensile certificate.
Products & manufacturing
Medical bar, cut blanks and drawing-controlled rough-machined components.
Service & design review
Provide the finished drawing, critical radii, machining allowance, permissible thermal processing and the required surface-treatment sequence. Identify whether the delivery is raw stock, a rough blank or a component.
Purchase & inspection priorities
Require heat traceability, dimensional reports and surface checks at the agreed stage. Finished device fatigue, biological evaluation and regulatory release require their own evidence.
Application review / 03
Medical wire & formed components
Wire procurement should start with the intended geometry and forming process. The delivered Ti-15Mo state must support forming while remaining consistent with the final material requirements; a wire diameter alone is not an adequate order description.
Products & manufacturing
Coils or straight lengths with controlled diameter, surface and handling conditions.
Service & design review
Define bend geometry, forming sequence, springback allowance and any later thermal processing. Identify contact surfaces that must be protected from scratches or embedded contamination.
Purchase & inspection priorities
Agree diameter inspection, surface examination and the mechanical or bend tests required by the specification. Validate the final formed component separately.
Application review / 04
Plate & strip development
ASTM F2066 provides a purchasing reference for flat forms as well as bar and wire. For a new plate or strip project, establish feasible dimensions and processing condition before planning a production schedule.
Products & manufacturing
Sheet, plate, strip and cut development blanks, subject to confirmed supply capability.
Service & design review
State rolling direction, forming radius, final wall thickness, flatness and whether machining follows forming. Establish trial quantities and approval milestones for a new route.
Purchase & inspection priorities
Use the relevant flat-product requirements, directional sampling and surface inspection. Document subsequent processing that changes the delivered condition.
Application review / 05
Precision features & interfaces
A drawing may specify Ti-15Mo for a small component with threads, bores or mating interfaces. Purchasing then requires a clear relationship between stock quality, dimensional capability and the final surface condition.
Products & manufacturing
Ground or turned bar, cut blanks and agreed rough-machined parts.
Service & design review
Provide thread geometry, concentricity, fits, roughness, datum system and cleaning requirements. Define which features remain for the customer to finish.
Purchase & inspection priorities
Agree first-article dimensions, burr and surface criteria, and piece-level identification where practical. Material certification does not establish assembly performance.
Application review / 06
Process & property qualification
Cold work and thermal processing can change the microstructure and properties of a beta titanium alloy. Qualification samples should represent the intended Ti-15Mo production condition and section.
Products & manufacturing
Representative bar or wire lots, flat coupons and retained material from the manufacturing route.
Service & design review
Define the properties to be evaluated, sampling direction and location, thermal history and acceptance authority. Avoid assigning a universal modulus from an unrelated research condition.
Purchase & inspection priorities
Record the complete sample history and agreed test methods. Establish change-control requirements for recurring supply after approval.
Application review / 07
Medical lot traceability
Implant-material purchasing requires a document trail that remains intact when stock is cut, machined or divided between subcontractors. A clear supply boundary helps prevent gaps between the mill certificate and the delivered blank.
Products & manufacturing
Segregated bar, wire and machining-stock lots with controlled identification.
Service & design review
Define certificate fields, heat and lot numbering, piece marking, retained samples, packaging and the records required from subsequent processors.
Purchase & inspection priorities
Check that delivered markings match the material and processing reports. Identify the manufacturer responsible for final device release.
Application review / 08
Comparative material programmes
A buyer may compare TB11 with TC4 ELI, TC20 or TC26 during material development. Useful comparisons keep the geometry, processing condition and evaluation method explicit rather than comparing isolated catalogue numbers.
Products & manufacturing
Documented trial lots of Ti-15Mo, with each alternative ordered under its own specification.
Service & design review
Set the selection criteria for stiffness, strength, fatigue, machining, surface processing and supply continuity. Confirm the design authority before changing a released material.
Purchase & inspection priorities
Keep certificates and specimens segregated by alloy and condition. Approve any substitution through the project validation process.
TB11 procurement checklist
Connect the application to the material order.
A useful specification connects the intended component, the supplied stock and the acceptance evidence. Share the drawing and known requirements first.
Define the application
Specify the target property, measurement method, material condition and acceptable variation. Review stiffness together with component geometry, fatigue, strength and surface processing.
Define the supplied stage
ASTM F2066 bar, wire or flat product matching the intended manufacturing route. Distinguish raw stock, converted blanks and finished parts. Define who controls subsequent processing.
Define the acceptance evidence
Confirm the ordered chemistry and condition, representative property testing and manufacturing history. Keep design validation separate from raw-material release.
Example: a useful TB11 material enquiry
TB11 medical bar & rod; required dimensions and quantity; standard and drawing revision; delivery condition; intended downstream process; mechanical, structural and dimensional acceptance; traceability, destination and required date.
Identify the approved product specification and any project-specific qualification. The grade designation and chemistry standard alone do not define component acceptance.
Discuss your material requirement ↗04 / Standards & documentation
Match the standard
to the product.
Choose the specification by product form, material condition and application. Identify the required edition on the order; a chemistry standard alone does not define a finished forging or component.
| Product / review | International / project route | Chinese reference | Clarify before quotation |
|---|---|---|---|
| Identity & chemistry | ASTM F2066-23Publisher reference ↗ | GB/T 3620.1-2016View PDF ↗ | Verify the full composition and ordered product requirements. A Chinese grade name alone does not establish international or dual certification. |
| Medical bar, wire & flat products | ASTM F2066-23Publisher reference ↗ | Documented comparison with the ordered Chinese requirements | ASTM F2066 covers wrought strip, sheet, plate, bar and wire. Confirm beta-annealed condition and applicable mechanical and bend testing against the full edition. |
| Drawing-based blanks & parts | Approved drawing and controlled manufacturing plan | Agreed product / project specification | Define the supply stage, conversion route, heat treatment, structure, NDT, dimensions and traceability. Material certification is separate from finished component qualification. |
The purchase order must identify the required revision, grade, product form, condition and inspection. Reference documents do not replace design approval, manufacturing qualification or application-specific acceptance.
Request the controlled specification revision for your order. Any substitution, equivalence or dual-certification claim requires a documented comparison and agreement.
05 / Order coordination
Know the scope
before ordering.
Our founder’s 20 years in titanium inform the questions we ask before quotation and the supply options we review with you.

A quotation you can evaluate
Agree the grade, standard edition, dimensions, tolerance, condition and quantity before comparing prices.
- Identify whether inspection, samples and tooling are included.
- Confirm packaging, transport and delivery terms.
- Record items that still need technical confirmation.
Acceptance agreed before supply
Confirm material identity, delivery condition, heat-to-piece traceability, dimensional checks and required testing before production. For converted parts, define inspection after forging, heat treatment and machining, including the specified microstructure and NDT scope.
Independent inspection can be discussed with its scope, timing, acceptance criteria and cost agreed for the order.
Delivery with clear milestones
Review the proposed lead time, approvals, production sequence and dispatch requirements. For several product forms, coordinate document and packing readiness together.
Material substitutions and technical changes require written approval. A schedule deviation should identify the impact, decisions needed and next steps.
One contact when an issue arises
Contact TiHubs with the order reference, affected items and supporting photos or inspection records.
We record the issue, review it against the agreed requirements and coordinate the next steps with the relevant manufacturing parties.
Material records
Grade, standard, test results and heat or batch identity matched to the supplied items.
Inspection records
Dimensional and testing records for the agreed scope, including critical drawing requirements.
Dispatch records
Item identification, packing list, protective packaging and required shipment documents.
06 / Questions before sourcing
Before you specify
TB11 / Ti-15Mo.
A clear material designation is the beginning. Product form, specification revision, material condition and acceptance complete the requirement.
A useful first enquiry
- Product and specificationProduct form, standard edition, dimensions and material condition.
- Order and deliveryQuantity, destination and any required delivery date.
- Acceptance requirementsDrawing revision, inspection, certificates and packaging.
Not every detail is finalized? Send the information you have. We can help identify the questions to resolve before quotation.
What happens next: requirement review, technical clarification, then a supply proposal and quotation.
What is TB11 / Ti-15Mo?
TB11 is the Chinese designation for the Ti-15Mo alloy family. ASTM F2066 identifies wrought titanium-15 molybdenum alloy, UNS R58150, for surgical implant manufacture.
Which standard should I specify for Ti-15Mo medical stock?
ASTM F2066 is the dedicated wrought Ti-15Mo implant-material reference. State the required edition, form, size and condition. If Chinese certification is also needed, request a documented comparison rather than assuming equivalence.
Does ASTM F2066 include plate and wire?
Its scope includes strip, sheet, plate, bar and wire. Actual dimensions and supply capability still need confirmation, and the applicable condition and testing requirements must be stated.
Is Ti-15Mo always lower in modulus than other titanium alloys?
Modulus depends on material state and measurement conditions. Ti-15Mo is relevant to lower-modulus design studies, but an order needs a specified condition and test method if modulus is an acceptance requirement.
Is TB11 the same as Ti-15Mo-5Zr-3Al?
No. Ti-15Mo and Ti-15Mo-5Zr-3Al have different alloying compositions. Use the complete material name and standard to avoid confusing these medical titanium routes.
Can TB11 replace TC4 ELI or TC20?
Only after the responsible design authority approves the change and required validation. Chemistry, processing response and properties differ, so substitution is not established by a similar product shape.
Can TiHubs supply finished implants?
This page focuses on raw material and drawing-based manufacturing blanks. Send the exact requested delivery stage. Material compliance alone does not establish finished-device approval or release.
What surface and traceability requirements should I include?
Specify finish, permissible defects, cleaning and packaging, heat-to-piece identification, certificate fields and the required inspection records. Add the controls needed for subsequent machining or forming.
What is needed for a TB11 quotation?
Provide form, size, quantity, ASTM F2066 edition, condition, tolerance, surface finish, test requirements and destination. Include the drawing and downstream process for custom blanks or formed products.
07 / Your next step
Start with the
requirement you have.
Send the product details, drawing or operating conditions you already know. We will identify missing information and discuss a suitable supply route before quotation.
- Requirement review
- Technical clarification
- Supply proposal and quotation
Combine materials and parts in one enquiry.
Send one list of TB11 forms, sizes and quantities. Include drawing revisions, material conditions and items that must be supplied or dispatched together.
Share the service and acceptance priorities.
Include load and temperature conditions, critical sections, required material records, process qualification, inspection, destination and timing.
Baoji, China · info@tihubs.com
Start your TB11 / Ti-15Mo enquiry
Send your material form, drawing or process conditions. We will help clarify the remaining requirements.