CategoryManufacturing & Customization
Titanium bar for auto lathes:
specify the complete feed path.
A correct alloy certificate does not establish that a bar will feed consistently through your machine. Match diameter, shape, surface and end preparation to the actual lathe and bar-feeder configuration.

Quick answer
For an automatic-lathe titanium bar order, specify the material requirement and the machine-interface requirement separately. Confirm the actual lathe, feeder, guide-bush arrangement, diameter limits, straightness definition, surface condition, bar length and end preparation. A term such as ground bar or h7 describes only part of the requirement. Ask the machine shop to approve the complete stock specification, then qualify a representative delivery against the intended production route. Do not use a generic web tolerance or speed recommendation as a substitute for the equipment manufacturer’s instructions.
01 / Identify the actual machine
Start with the lathe, feeder and guide arrangement.
A buyer requests Grade 5 titanium round bar for an automatic lathe and receives an offer for the right alloy and nominal diameter. During the shop’s review, the bar’s diameter range is not confirmed, the end preparation is unspecified and the straightness statement has no measurement method. The alloy may be correct while the production suitability remains unresolved. A material certificate and a machine-compatible supply description answer different questions, so both belong in the enquiry.
Identify the lathe model, bar feeder and relevant support or guide arrangement. A sliding-headstock machine using a conventional guide bush may impose different stock requirements from a machine operating without that bush or using an adaptive guiding system. The maximum bar length and diameter stated in a sales brochure are capacity boundaries, not a complete acceptance specification for every material and operating condition. Use the documentation for the actual installed configuration.
Locate each point where the bar must pass or be supported.
Follow the path through the feeder channel, spindle liner, collet and guide bush where fitted. Record which approved components are installed for the intended bar size. The shop should confirm the permissible stock characteristics and the setup requirements. Purchasing should not infer the working clearance by subtracting two nominal catalogue diameters, because adjustment, support design and operating conditions can affect what the equipment requires.
APSX’s loading guide for its NANO machine gives specific stock requirements, including precision grinding and defined dimensional criteria. That is a useful example of a manufacturer connecting material preparation to its own machine. It should not be copied as a universal requirement for all automatic lathes. [1] Ask the responsible machinist to identify the applicable equipment instructions before the supplier commits to a production quantity.
Check whether a claimed universal rule fits your equipment.
Tornos has described particular adjustable guide-bush options that accommodate different bar tolerance ranges. The existence of those options illustrates why a statement such as ‘every Swiss lathe requires the same ground-bar tolerance’ is too broad. It does not mean an older or differently equipped machine can use the same stock. Confirm compatibility with the installed option and current approved setup. [2]
Keep material selection separate from this compatibility review. Grade 2, Grade 5 and Grade 23 are not interchangeable simply because they can be supplied as round bar. The component drawing and product specification establish the required alloy and condition. Machine-interface requirements add another layer to that material order. For the broader product enquiry, use the titanium bar and rod supply page; this guide focuses on the stock characteristics that a machine shop must define before purchase.
02 / Translate the diameter requirement
Write the upper and lower limits in the quotation.
A nominal diameter tells the supplier the designated size, but it does not define the complete permitted range. Ask for the upper and lower limits in the controlling unit system. If the drawing specifies a tolerance designation, identify the applicable standard, nominal-size interval and edition or drawing convention. The same tolerance grade does not represent one fixed number of micrometers for every nominal diameter. Preserve the required notation while making the numerical limits clear to the purchasing and inspection teams.
Do not treat grinding as a complete dimensional specification.
Ground, turned, drawn and polished describe processing or surface routes; they are not substitutes for the required limits. A ground bar still needs a stated diameter range, shape requirements and inspection scope. A polished appearance does not prove roundness or straightness. Ask the supplier to state the delivered condition and how the proposed route establishes the agreed characteristics, rather than accepting a process name as a blanket guarantee.
For a hypothetical clearance exercise, consider an ideal circular bar ranging from 9.990 to 10.000 mm inside a fixed ideal circular opening of 10.020 mm. The diametral clearance ranges from 0.020 to 0.030 mm. If perfectly concentric, the corresponding radial gap is half that value. These numbers are deliberately chosen to explain arithmetic. They are not recommended guide-bush settings or permission to run a machine at a particular speed.
Check the limiting combination.
If the proposed bar range instead extends to 10.030 mm, that same fixed opening no longer provides clearance at every permitted size. The illustration shows why comparing only nominal dimensions can hide a mismatch. Real equipment review also needs the opening’s actual condition and tolerance, adjustment, bar shape, cleanliness and the manufacturer’s operating requirements. A paper clearance calculation cannot prove safe or stable feeding by itself.
When the machine uses an adjustable guide or collet, document the stock requirement approved for that configuration instead of pretending the opening is an unchanging nominal hole. The operator should set and verify the equipment according to the manufacturer’s procedure. A supplier’s dimensional report can support that review, but it does not authorize a different guide setting, clamping force or spindle-speed limit.
Agree how diameter variation will be assessed.
Discuss measurement positions along the bar and around the section, including whether the ends have a separate permitted condition. A few two-point readings do not establish every possible roundness characteristic. If roundness, cylindricity or a special local-size requirement matters, identify it separately and specify an appropriate method. Record actual results with units and bar identity rather than only a pass stamp when the agreed quality plan calls for measured values.
Use calibrated equipment with capability appropriate to the tolerance, and agree how results close to a limit will be handled. Avoid silently mixing millimeter and inch reports or rounding an out-of-range reading into compliance. The useful purchasing outcome is a written range and an agreed acceptance method that both supplier and receiving shop can apply to the same material.

Hypothetical ideal geometry: a 10.020 mm opening and 9.990–10.000 mm bar give 0.020–0.030 mm diametral clearance. These are not machine setup recommendations.
03 / Define bar shape
A straightness number needs a measurement method.
Diameter conformity does not guarantee that a long rotating bar behaves acceptably in a feeder. Straightness, local bends, support and the machine configuration all matter. INDEX’s stock guidance for single-spindle lathes explicitly links bar straightness with attainable operating behavior, vibration and workpiece quality. Its document also describes a particular support-and-indicator assessment. Use it as an example of an equipment-specific method, not as a universal tolerance table for every titanium bar. [3]
Separate overall bow from local defects.
A long gradual curve and a short kink near an end can cause different problems even when someone describes both as a straightness issue. State whether the requirement applies over the full bar, over a defined local length, at the ends or through another agreed evaluation. A ‘per meter’ statement is incomplete if the method, support and evaluation length are unclear. Do not extrapolate a full-length acceptance rule from one short section without technical justification.
Where an indicator method is used, record the support positions, indicator locations, rotation or measurement procedure and the quantity being reported. A maximum-minus-minimum indicator reading is not automatically identical to every geometric straightness definition. Different setups can include different contributions from shape and contact. The responsible quality team should decide which method corresponds to the equipment requirement and how the result will be interpreted.
Do not promise spindle performance from stock data alone.
Bar length, unsupported portions, feeder support, spindle liners, setup and operating speed interact. A supplier should not promise that a particular straightness value guarantees a chosen production speed on an unspecified machine. The machine manufacturer and qualified operator must establish the operating limits. If the shop reports vibration or feeding trouble, retain the material identity and setup information so the investigation can distinguish stock, tooling, support and operating factors.
Never use a procurement article as an instruction to run an unsupported projecting bar or exceed equipment limits. The purchasing action is to obtain the correct stock requirement and verify compatibility before production. If the equipment instructions require a particular end preparation, support arrangement or bar-length restriction, include that in the approved shop specification. Do not trade it away because another stock length is easier to source.
Protect shape after the supplier’s inspection.
Long bars can be affected by lifting, stacking, transport and storage. Ask for packaging and support appropriate to the agreed straightness and surface requirements. A shipment that leaves the source with acceptable measurements still needs handling that preserves its condition. At receipt, inspect packaging and visible bends before mixing the bars into available inventory. Identify any damaged pieces separately so a receiving issue does not become an unexplained production interruption.
For a disagreement, compare the original and receiving methods, bar lengths, supports, measurement positions and temperatures where relevant. Keep raw readings and the bar’s identity. An average of results across several bars does not establish that each bar meets a requirement that applies individually. Use the agreed nonconformance review to decide rework, replacement or an authorized concession.

Support, measurement positions, evaluated length and the reported quantity belong together. This schematic does not prescribe universal support spacing or tolerances.
04 / Specify surface and preparation
Surface finish, cleanliness and ends belong in the order.
A bar can have an acceptable nominal size and still present a poor interface to a guide or collet if its surface or ends are unsuitable. Describe the required surface condition, permitted defects and any specified roughness parameter. The word ‘bright’ is an appearance description; it does not by itself define texture, damage, dimensional form or cleanliness. Ask the shop which characteristics matter to the installed equipment and to the final component.
Keep roughness separate from geometric form.
A roughness value describes a defined surface-texture assessment. It does not prove roundness, straightness or the absence of an isolated scratch. If a roughness requirement is specified, state the parameter, applicable evaluation method and relevant measurement direction or conditions through the approved drawing or procedure. Do not replace one parameter with another merely because the numerical values look similar. The supplier should confirm the stated requirement, not supply a generic surface-finish claim.
Discuss defects that may affect feeding or the retained surface of the component. If the bar’s outer surface will be fully removed, the manufacturing plan still needs enough stock to remove permitted defects while reaching the final diameter. If part of the supplied surface remains on the finished component, its acceptance requirement may be more direct. Define that distinction before choosing a cheaper preparation route.
Specify the ends that the feeder actually uses.
Front and rear ends can serve different functions. One may pass through the clamping or guiding components; the other may engage a pusher or other feeder interface. State the required chamfer, deburring, end squareness or other preparation from the actual equipment instructions. Do not copy an angle from another feeder manual and treat it as a universal titanium-bar requirement. Include any end portion that is excluded from usable machining length.
Cleanliness and protective treatments also need agreement. Ask what surface protection or residue, if any, will be present and what preparation the shop requires before loading. A supplier should not introduce an unspecified lubricant, coating or marking material into a controlled process. Conversely, a request for ‘clean bar’ needs a practical definition when the application has particular contamination restrictions. Put special cleaning, packaging or handling requirements into the quoted scope.
Preserve the supplied material condition.
If additional straightening, grinding or another operation is proposed, ask the supplier to identify the route and the delivered condition. Verify that the material specification and any customer restrictions still apply after processing. ASTM B348/B348M addresses titanium and titanium alloy bars and billets within its scope; an order may need further dimensional or processing requirements for the machine interface. [4] Do not interpret a product-standard designation as confirmation of every supplementary shop requirement.
Link the final inspection and material documentation to the bars actually shipped after the contracted preparation. If marking is removed during grinding or cutting, agree how identity transfers to the finished bar or controlled bundle. A certificate for the starting material is useful only when the traceability chain to the delivered stock remains credible.
05 / Calculate usable length
Count parts from the approved bar-length budget.
The length bought and the length that becomes accepted components are different quantities. Confirm feeder capacity, permitted bar-length variation, front preparation, remnant length and the amount consumed by each parting or facing cycle. The shop’s production plan should establish those allowances. A supplier can quote cut lengths, but it cannot infer the safe usable length or remnant rule for an unspecified feeder.
Use a transparent yield calculation.
In a hypothetical planning example, a 3,000 mm bar loses a combined 200 mm to approved front preparation and the unusable remnant. That leaves 2,800 mm for repeated cycles. If each cycle consumes 25 mm of finished-part length plus 3 mm for parting and associated allowance, the planned count is floor(2,800 / 28) = 100 pieces. The 200 mm and 3 mm values are assumptions for the example, not recommended machine settings or guaranteed yields.
If the quoted bar length can be as short as 2,980 mm under the agreed range, the same simplified budget gives floor((2,980 − 200) / 28) = 99 pieces. A small difference at the bar level can change the total across a large delivery. This is why the purchase specification should state the acceptable length range and quantity basis rather than treating all nominal three-meter bars as identical production units.
Separate planned count from accepted output.
The calculation does not include setup pieces, qualification samples, defects, process losses or rejection of finished parts unless the shop explicitly adds them. Estimate those items from relevant evidence and keep the assumptions separate. Do not present the theoretical count as a production guarantee. If the customer buys by mass while the shop plans by pieces per bar, reconcile both bases with the actual diameter, length and agreed commercial weight rule.
Shorter bars can be suitable for a particular loading arrangement, but a change in length can affect handling, cycle logistics and remnant proportion. Longer bars may improve a planning ratio while exceeding the installed equipment’s permissible range. Ask the shop to approve any alternative length before purchasing. Avoid choosing the length with the lowest price per kilogram without checking the number of usable parts and the loading configuration.
Define quantities and partial deliveries.
State whether the order is by number of bars, total length, net mass or an agreed combination. Specify whether mixed lengths are permitted and how they will be listed on packing documents. A delivery of the correct total mass may still disrupt production if it contains an unexpected mixture of short bars. For scheduled releases, identify the dimensions, heat or lot and records required in each shipment.
When the order includes trial material, identify whether it comes from the proposed production route and whether it counts toward the production quantity. Reserve enough representative material for the planned evaluation without assuming that a short offcut proves full-length feeding behavior. The trial should address the uncertainty that prompted it.

Hypothetical example: (3,000 − 200) / (25 + 3) = 100 planned pieces. Actual equipment limits, trial pieces and production losses must be reviewed separately.
06 / Qualify the supply requirement
Approve the stock specification before scaling the order.
Bring the material, machine-interface and commercial requirements into one controlled enquiry. Include grade, product specification and edition, delivery condition, diameter limits, shape requirements with methods, surface condition, end preparation, length range, quantity and traceability. Add the machine or feeder information needed for the review, the destination and the requested delivery date. Identify the drawing and shop-specification revisions so the supplier can respond to a stable requirement.
Compare complete offers.
One quotation may include grinding and individual bar identification while another prices untreated stock with bundle-level documents. A third may offer a different tolerance or length. Ask each supplier to mark requirements as accepted, proposed alternative or pending clarification. Keep the alternatives separate from the compliant base offer and obtain the required approval before changing the purchase line. Our titanium quotation guide covers the broader commercial comparison.
Evaluate the cost of usable production stock, including any preparation your own shop must add. A lower material price can be offset by regrinding, cutting, inspection, handling or lost usable length. Equally, a tighter requirement than the machine and component need may add unnecessary cost or limit supply. The objective is an approved, sufficient stock specification supported by evidence, rather than automatically choosing the tightest tolerance available.
Design the trial around observable outcomes.
For a new source or preparation route, agree a representative trial with the machine shop. Record the material identity, dimensions, condition and approved machine configuration. Define what will be reviewed: loading and feeding behavior under the authorized procedure, relevant surface observations, dimensional stability of the process and accepted-part results. The qualified operator controls the machine; the supplier’s role is to provide traceable stock matching the trial scope.
Set a clear decision after the trial. Accept the specified route, request a defined correction, or revise the stock requirement through the authorized technical process. Avoid open-ended statements such as ‘sample approved’ without recording what the sample represented. A trial on a different grade, short length or special finish may not qualify the later delivery. Preserve the approved scope and change-control requirements with the order.
Make repeat orders reproducible.
Require the supplier to disclose proposed changes to source, preparation, dimensional range, condition or inspection method. At receipt, confirm identification, quantity, length distribution, condition and the agreed dimensional evidence before releasing stock to the machine. If a problem occurs, keep affected bars separate and document the setup and observations; do not erase the evidence by mixing the remaining pieces into another lot.
TiHubs can coordinate titanium-bar supply enquiries and source clarification against your approved requirements. Send the drawing and shop stock specification, marking open questions clearly. That gives the supplier a concrete target and lets your production team evaluate the delivered bar as part of the actual feeding and machining system, rather than relying on an alloy name alone.
07 / Build your RFQ
Prepare an automatic-lathe bar enquiry.
Include the shop-approved stock requirement and the installed machine or feeder details relevant to it. If the diameter limits, straightness method or end preparation are unresolved, mark them as pending. TiHubs can coordinate a supply review; machine setup and operating approval remain with the responsible shop personnel.
Information to include
- Grade, product standard, edition and delivery condition
- Lathe, feeder and guide arrangement relevant to the stock requirement
- Diameter limits, shape requirements and inspection methods
- Surface condition, cleaning and front/rear end preparation
- Bar-length range, usable-length assumptions and quantity basis
- Traceability, trial scope, destination and delivery date
Build your RFQ checklist
Choose the product and add the information you have. Copy the resulting brief or send your requirements to TiHubs. Submitting an enquiry does not place an order.
08 / FAQs
Questions buyers ask
Is h7 titanium bar mandatory for every Swiss-type lathe?
No universal statement covers every machine and guide arrangement. Use the stock requirement approved for the installed equipment and component. Conventional, adjustable and guide-bush-free configurations can have different requirements; a tolerance designation alone is not a complete bar specification.
Does ground titanium bar guarantee straightness?
The process description does not establish a particular straightness limit or inspection method. Specify diameter, relevant shape characteristics, surface condition and acceptance separately, and verify the delivered bars after the contracted preparation.
Can a material certificate prove the bar will feed correctly?
A certificate can support the stated material requirements and traceability. Feeding suitability also depends on dimensions, shape, surface, end preparation, support and the actual equipment configuration. Review those characteristics independently.
Is indicator runout the same as bar straightness?
Not automatically. The reported result depends on supports, rotation, contact positions and the quantity being evaluated. Use the method required by the approved stock specification and avoid substituting one geometric measure for another without review.
Should I order the longest available bar to reduce waste?
Only within the approved equipment and handling limits. Compare usable length, remnant rules, loading arrangement and actual production yield. A longer available stock size is not evidence that the installed feeder can accept it.
What should accompany a trial delivery?
Identify the grade, condition, source route, dimensions, preparation and heat or lot represented by the trial. Provide the agreed inspection records and define which production scope the trial can qualify. Keep any approved changes with the order.
09 / Key takeaways
Keep the purchase requirements connected.
- Start with the actual lathe and feeder configuration.
- State numerical diameter limits and separate shape requirements.
- Define straightness by a method, span and support arrangement.
- Include surface, end preparation and usable-length assumptions.
- Approve a representative trial and preserve the scope for repeat orders.
Technical references
Sources and data scope
References reviewed November 13, 2026. Public source summaries support the discussion; the controlled specification, agreed edition and approved project requirements govern acceptance.
- APSX — Workpiece loading guide for APSX-NANO — Machine-specific stock and loading information; not a universal tolerance or setup rule for all lathes.
- Tornos decomagazine 02-2019 — Guide-bush options, page 20 — Manufacturer example of an adjustable guide arrangement. Confirm the installed option and current equipment instructions.
- INDEX — Requirements for bar stock, single-spindle lathes — Manufacturer guidance illustrating the importance of straightness, end condition and a defined assessment method.
- ASTM B348/B348M-21 — Titanium and titanium alloy bars and billets — Public product-specification scope. Use the contracted edition and supplementary machine-stock requirements for the actual order.