Mark the long diamond direction on the panel outline and identify what has to pass through the opening. Include the mating frame and maximum available depth if the mesh will sit in a groove.
Select the supply configuration
Use the drawing and the assembly configuration to identify the item to quote.
Raised expanded sheet
For the quotation, identify mesh direction, node height, free depth.
- Mesh direction
- node height
- free depth
Dimensions and acceptance
Compare raised and flattened titanium expanded sheet. Specify the mesh direction, clear opening, strand dimensions, finished envelope and cut edges for a drawing-based quote.
| Order item | Include in your enquiry | Why it matters |
|---|---|---|
| Published TA1 mesh example A | SWD 3.0 mm, LWD 6.0 mm | Listed strand 1.2 mm, listed thickness 1.5 mm |
| Published TA1 mesh example B | SWD 6.0 mm, LWD 12.0 mm | Listed strand 2.0 mm, listed thickness 2.8 mm |
| Pitch measurement | Ten equal centre-to-centre pitches across 60 mm | Illustrative mean pitch 6.0 mm in the measured direction |
| Projected open area of an ideal cell | Pitch diagonals 12 × 6 mm, clear diagonals 9 × 4 mm | Ideal planar fraction 50%; real nodes require separate verification |
| Frame example | Minimum groove 2.30 mm, maximum finished mesh depth 2.10 mm | Minimum thickness clearance 0.20 mm before other components |
| Border specification | Identify cut-through strands or an agreed framed edge | Include which direction the strands may project at the boundary |
Your starting specification.
Mark the long diamond direction on the panel outline and identify what has to pass through the opening. Include the mating frame and maximum available depth if the mesh will sit in a groove.
The table identifies the basis for the quotation. Confirm material, dimensions, inspection and delivery for the selected part before ordering.
Material and delivery condition
Identify the material on the approved drawing and confirm its product form and condition with the quotation.
Chinese designations and international names are reference routes, not automatic substitutes. Grade, product specification, condition and acceptance requirements must be agreed together.
Open grade cross reference ↗Purchasing situations
A first assembly, a replacement and a repeat order need different evidence.
Raised expanded sheet
For the quotation, identify mesh direction, node height, free depth. For related supply options, see the parent product guide.
Flattened expanded sheet
For the quotation, identify finished thickness, opening limits, panel flatness.
Mesh substrate for coating
For the quotation, identify bare or coated condition, contact tab, inspection stage.
Engineering and purchasing guide
Mark the long diamond direction on the panel outline and identify what has to pass through the opening. Include the mating frame and maximum available depth if the mesh will sit in a groove.

Pitch and opening on a diamond mesh. Node-to-node pitch, Clear aperture.
Order geometry schematic; not a dimensional drawing.Identify the diamond that controls the assembly
A rectangular sample of titanium mesh fits its frame on the bench, yet the same pattern cut for the other side of the assembly catches at the corners. Before changing the panel width, lay both samples on the assembly drawing and mark the long axis of each diamond. A ninety-degree rotation can leave the nominal outline unchanged while moving high nodes against a support or placing exposed strands at a hand-contact edge. The first sketch sent for quotation should identify the outside shape, diamond direction and viewing side. This information cannot be recovered from an outline dimension alone.
Expanded metal begins as a continuous sheet. Slitting and stretching produce interconnected strands and nodes. A woven screen crosses separate wires over and under one another. A perforated panel retains solid sheet between individual holes. These constructions present different edges, contact points and thicknesses to a frame even when photographs taken from above look similar. If the old panel is available, inspect a cut edge with magnification and look for a continuous junction between neighbouring strands. Record the construction you actually need and describe any accepted alternatives separately.
Identify the job the openings perform. A support behind another screen may need a repeatable bearing surface without blocking too much of the active area. A tray liner may need to retain particular components, drain freely and fit under a retaining lip. An electrochemical substrate may need reliable connection to a tab and a defined area for subsequent coating. These are different purchase requirements. A customer asking for an exact percentage of open area may actually be trying to control the passage of one object or the space available for flow. Write the functional condition alongside the geometric one.
A photograph is useful when its orientation and scale are known. Include a top view with the scale lying in the plane of the mesh and a separate side view of the node height. A scale placed on the bench below a raised panel introduces a perspective error when photographed at an angle. Mark the machine frame or access side on the image. Identify whether the face seen by the camera faces the contents of the equipment or its supporting frame. An isolated close-up without those details can show a pattern clearly and still lead to the wrong cut orientation.
For a repeat order, keep a controlled sample or a drawing with a labelled photograph. Identify which features the reference sample controls. Colour and reflectivity can change with lighting and surface condition, while the dimensional drawing may still govern pitch, orientation and outline. If the sample has been used, document worn strands, a bent corner and any edge work done during maintenance. A supplier copying accidental damage as a design feature would produce a faithful replica of the wrong geometry.
Specify the repeat, clear opening and projected area
The two principal repeat dimensions are usually called the long way of the diamond and the short way of the diamond, abbreviated LWD and SWD. PPG DEXMET defines them using centres of nodes. The clear opening, sometimes stated separately along each axis, is bounded by the actual inner edges of the metal. Label the points touched by each dimension arrow. A stated diamond size of six by twelve millimetres is incomplete when the reader cannot tell whether it describes the repeating pitch or the unobstructed opening.
One way to check a regular repeat uses a distance measured over several intervals. In a hypothetical panel, eleven equivalent node centres define ten pitches along a selected direction. If the distance from the first to the last is 60 mm, the mean pitch is 6.0 mm. Ten nodes would define only nine intervals. A long measurement reduces the influence of choosing the exact centre on any single node, but it does not detect every undersized opening. If the part is intended to pass an object of a specified width, examine individual clear openings at the locations required by the drawing.
The quotation table gives two examples from a manufacturer’s published TA1 mesh data. Both the geometry and the material label belong to that specific source. Its listed thickness field should be clarified before using it as a limit for either starting sheet thickness or finished panel depth. A purchasing engineer should transfer values in separate columns and retain the original names. A dimension copied under a new heading can become a different requirement even though its numerical value and unit are unchanged.
An ideal planar diamond cell illustrates the distinction between pitch and empty area. Suppose the repeating cell has diagonals of 12 and 6 mm, while its clear diamond has diagonals of 9 and 4 mm. The cell area is half the product of its diagonals, or 36 mm². The clear area is 18 mm², giving a projected open fraction of 50 percent. This is an exercise using ideal straight boundaries and a perpendicular view. Real junctions have finite shape, and an inclined surface can partially obscure the opening when viewed from another direction.
For an acceptance figure, agree the method and the region counted. An optical image taken normal to a flat coupon can represent the projected open fraction in a defined area. Mark the boundary and decide how cells intersected by the edge of that area are treated. Keep the solid border outside the calculation if the specification refers only to the active mesh. Include it if the required result is the free area of the installed panel. The same cut piece can legitimately give two different percentages depending on which area is used as the denominator.
Compare raised and flattened delivery conditions
A raised mesh has strands and junctions that project out of the original sheet plane. Flattening changes the profile offered to the frame and can also affect the final outline and opening shape. Specify whether the dimensions apply before flattening, after flattening or after subsequent finishing. A label such as “one millimetre titanium” might describe the strip from which the mesh was expanded, the material at a strand or the overall height across high nodes. Ask the supplier to sketch its thickness measurement and identify the surfaces touched by the instrument.
A sliding insert provides a useful example. If the minimum clear groove in the frame is 2.30 mm and the maximum allowed finished depth of the mesh is 2.10 mm, the thickness difference is 0.20 mm. It applies only to those surfaces and assumptions. A rolled edge, weld bead, coating buildup or trapped fastener head may occupy additional space. A bowed sheet may also resist insertion despite acceptable local node thickness. Check the envelope of the entire finished insert, including border work and the installation path, before committing to a panel size.
Flatness and thickness answer different questions. A local reading relates opposite surfaces near one set of nodes. A flatness or bow requirement concerns the form of the panel over a specified span and under a specified support condition. A thin panel can lie flat when clamped and curl when released. State whether the inspection is performed freely supported, on specified supports or in a representative frame. Describe the force, if any, used to hold it. A large clamping force can hide the very wave that prevents an installer from positioning the panel.
For a support that bears on mesh, consider which parts of the pattern actually meet the mating surface. One orientation may put node peaks against the support. Another may present a broader strand surface. Local contact is especially important when the adjacent component has a soft surface or thin coating. A visual sample should include a side view in the intended orientation. If the drawing calls for a functional assembly check, identify the mating parts and the condition in which they are tested, including spacers and protective layers.
A request for lower overall thickness may tempt a bidder to offer a completely different mesh pattern. That change can alter clear opening, number of contacts across the span, directional behaviour and retained material area. Request both the as-quoted pattern data and the expected finished profile. Evaluate the alternative as a separate configuration. A buyer can then decide whether a flattening operation on the original pattern or a new pattern better meets the actual function, with enough information to repeat the selection later.
Lay out the panel, edge cuts and frame
Position the cut outline relative to the diamonds before sending it for manufacture. Two panels of the same width can end on full junctions or on free strand ends depending on where the cut begins. A dimension from the outside of the item to a critical row of nodes can be more useful than a note saying “symmetrical.” If both opposite edges must finish on equivalent features, the width and pattern repeat have to be compatible. Ask for a proposed layout when the requested overall dimensions cannot contain the required integer number of repeats.
For a rectangular cartridge insert, sketch the visible opening of the frame separately from the outside panel dimensions. The material behind the frame can be necessary for retention but contributes little to open flow area. Locate any support rails and mounting pads. Mark where a mounting hole passes through solid material and where it would fall into a diamond opening. Drilling a nominal hole into the mesh at a point with insufficient surrounding metal cannot create the same fastener seat as a drilled solid tab.
Choose an edge detail that the installer can handle and that the assembly can accommodate. A cut through open diamonds leaves free strand ends. A bound edge or frame changes thickness, outside size and sometimes the orientation in which the panel can slide into place. Describe the maximum permitted projection and the required condition of accessible edges. Where a return bend or separate frame member is used, show its relationship to the mesh and to the nominal outside dimensions. A border included inside a fixed width reduces the available active area.
A panel with tabs or cutouts needs an unambiguous view. Give each asymmetrical feature a location from the same datums and indicate the front face. Consider a panel with one electrical tab on its upper left corner and unequal corner cutouts. A mirrored panel can have the correct width, height and tab length while placing the contact on the wrong side of the equipment. Include the direction of insertion or a clearly identifiable mounting feature on the drawing. A photograph of the installed predecessor can resolve a surprising number of questions about handedness.
When nesting several panels on a master sheet, separate the objective of material utilisation from the required diamond orientation. Rotating a part by ninety degrees to improve yield changes the pattern seen by the frame. A rotation of one hundred and eighty degrees may still alter the face or the way open strand ends enter a guide, depending on the construction. Define allowed orientations on the cutting layout and identify offcuts worth retaining. Compare bids on the basis of accepted finished panels, including border operations and any inspection of directional features.
Separate metal, surface treatment and functional evidence
Identify the titanium grade of the starting sheet and the product specification that applies to that material. Confirm how that identity will be linked to the expanded panel when the parent sheet is divided into multiple pieces. A certificate for starting sheet can establish an important part of material traceability. It does not verify the dimensions produced by expanding and flattening, the position of the cut outline or the condition of a coating applied afterwards. List those acceptance records separately and indicate who supplies each one.
The examples in the table are identified by their source as TA1. A buyer who requires a particular ASTM grade should request the exact grade and standard on the order, together with the documentation needed to support that designation. Similar trade descriptions do not establish contractual equivalence. If a supplier proposes a different national designation, review the chemistry, product form, condition and other applicable requirements against the approved purchase specification. Record who accepts the proposed substitution before the stock is committed to fabrication.
For a panel used as a coating substrate, define the boundary between metal supply and the coating operation. Identify the faces to be coated, the portion of the electrical tab that must remain available for connection, and which surfaces need protection during handling. State whether acceptance dimensions apply to bare mesh or to the finished coated component. A reading taken after coating can differ from the incoming metal dimension, particularly at a junction or edge. If the supplier only provides the bare substrate, request the records relevant to that scope and assign final coating verification to the appropriate party.
For an uncoated support in a process assembly, ask what fluid, cleaning cycle and contact materials the design must consider. The geometry of the panel may create sheltered contact points or retain deposits against the frame. A general material description cannot determine service life in that particular environment. Keep the designer’s material approval and the mesh manufacturer’s dimensional evidence distinct. When a sample exposure or a cleaning trial is required, identify the site conditions, representative surfaces and observation criteria before selecting a small coupon on appearance alone.
Packaging can affect a thin mesh long after it leaves the rolling or cutting operation. Specify how the panels will be supported and separated, where contact is allowed and whether a protective material can touch a surface intended for later treatment. A tight strap through a stack may mark the nodes or distort a corner. An unsupported overhanging edge may bend when a crate is moved. Describe the receiving inspection and any restrictions on lubricants, adhesives or identification marks in terms of the actual subsequent process.
Inspect a representative panel before releasing the order
Begin the first-panel inspection with orientation and outline. Place the part on the agreed supports and check width, length, corner details and handedness against the same view used for release. Mark the long diamond axis on the inspection record. A panel can meet both outside dimensions when turned end for end, so record how you located the front face and the reference edge. Photograph the sample next to its drawing revision, with a scale in the plane being documented.
Next check the repeat and the clear openings as separate characteristics. Record the measured span, the number of intervals and the direction for each pitch result. If the minimum opening matters, state where individual apertures were evaluated, how corners were treated and which feature bounds the passage. A rigid round object, a flat strip and a stream of fluid do not test the same aspect of the opening. A nominal pitch comparison is useful for identifying patterns, while functional acceptance may require an additional test defined for the component that must pass.
Inspect finished depth at locations representative of the panel and the border. Agree the contact size and force before comparing measurements from two instruments. A narrow tip can enter a diamond and miss the outer envelope, while excessive force can depress a raised strand. Record whether the sample was free or clamped. If a gauge frame is used, document its slot dimensions and the orientation in which the panel was inserted. A simple written statement that the part fit a fixture is hard to interpret once the fixture has been repaired or replaced.
For repeat orders, retain a complete first-panel record rather than just a photograph and the final price. Include the mesh specification, material certificate reference, final pattern direction, drawing revision, any accepted edge sample and the inspection results. Mark the handling method if it affected the outcome of a coating or assembly trial. If a later batch has a different starting gauge or flattening operation, compare it with the features that were originally approved before accepting it as a direct replacement.
A concise request for quotation can bring all of this together. Send a dimensioned panel outline with the long axis, pitch or clear dimensions identified, strand width, required finished thickness, border and delivery condition. State the quantity and whether the order includes framing, tabs or coating. Ask the bidder to identify deviations, applicable source material documents and the inspection evidence included in the quoted price. This allows the buyer to compare actual finished panels and gives the receiving team enough information to recognise the approved configuration when the crate is opened.
Inspection points
Agree the acceptance evidence before the first part is released.
Traceable from heat to shipment.
Listed strand 1.2 mm, listed thickness 1.5 mm
SWD 3.0 mm, LWD 6.0 mmListed strand 2.0 mm, listed thickness 2.8 mm
SWD 6.0 mm, LWD 12.0 mmIllustrative mean pitch 6.0 mm in the measured direction
Ten equal centre-to-centre pitches across 60 mmIdeal planar fraction 50%; real nodes require separate verification
Pitch diagonals 12 × 6 mm, clear diagonals 9 × 4 mmMinimum thickness clearance 0.20 mm before other components
Minimum groove 2.30 mm, maximum finished mesh depth 2.10 mmInclude which direction the strands may project at the boundary
Identify cut-through strands or an agreed framed edgeSource documents
Check the applicable series, revision and scope against the purchase drawing.
Library PDFs may be earlier editions. Check the document cover and your contractual revision. A reference file does not certify a supplied product.
Explore all downloads ↗Technical sources
- PPG DEXMET — Expanding Technology — Manufacturer terminology for node centres, LWD, SWD and finished mesh.
- CN Fine Wire — Titanium Expanded Mesh — Two geometry examples from the manufacturer’s listed TA1 platinum-coating mesh table. Confirm how its thickness was measured for any actual order.
- ASTM B265 — Product specification for titanium strip, sheet and plate where applicable to the starting sheet.
Baoji.
One contact.
TiHubs coordinates titanium sourcing through a local manufacturer network. Your specification guides the supplier review, technical discussion and delivery requirements.
Clarify the requirement
Confirm grade, dimensions, state, quantity and the purpose of the stock.
Review the supply route
Discuss manufacturing, finishing, inspection and documentation with the relevant supplier.
Agree the commercial scope
Confirm the quotation, lead time, acceptance requirements and delivery terms.
Coordinate inspection & delivery
Follow the agreed checks, marking, packing and shipment documentation.
Before you order
Compare raised and flattened titanium expanded sheet. Specify the mesh direction, clear opening, strand dimensions, finished envelope and cut edges for a drawing-based quote.

TITANIUM EXPANDED METAL · BAOJI SOURCING
Send your specification.
Mark the long diamond direction on the panel outline and identify what has to pass through the opening. Include the mating frame and maximum available depth if the mesh will sit in a groove.