CategoryManufacturing & Customization

Drilling titanium.
Specify the finished hole.

Diameter is only the beginning. Connect depth, fit, edges and inspection to the function of the component.

Manufacturing guideHole / edge / evidence
Illustrative titanium plate held in a machine vise beneath a twist drill
Hole geometryDefine the function
AcceptanceVerify the feature
AI illustration; not a production or inspection record.

Quick answer

Drilling titanium requires a process matched to the alloy, condition, hole geometry and machine. Specify finished diameter, depth, datum relationships, edge condition and inspection before selecting tooling or comparing prices. Toolmaker guidance supplies a starting window; no single drill, feed, speed or coolant setting is correct for every titanium hole.

A drilled diameter is only part of the requirement

Drilling titanium means producing a hole that satisfies a drawing, not simply making an opening in a hard-to-machine material. The required result may include diameter, position, depth, straightness, surface texture, edge condition and cleanliness. Those requirements determine whether drilling alone is sufficient or whether a subsequent finishing operation is needed. Start with the finished feature before selecting a drill or comparing quotations.

The exact titanium grade and supplied condition also matter. Commercially pure titanium and Ti-6Al-4V should not be grouped under an unspecified titanium setting. State the material specification and condition on the enquiry, including any later heat treatment. A process developed on a different alloy or condition is useful experience, but it is not automatic evidence that the new component will meet its requirements.

Identify what the hole does

A clearance hole gives a fastener space to pass; a locating bore controls a mating fit; a fluid passage connects an internal flow path. A hole that precedes tapping is an intermediate feature rather than the complete thread. Each purpose changes which dimensions and surfaces matter. Calling all of them a drilled hole can hide the feature that actually governs acceptance.

Functional distinctions for an RFQ; not a universal tolerance table
Hole functionClarify on the drawingEvidence to define
Fastener clearanceSize, position and edge conditionRequired dimensional and visual checks
Locating or fitted boreFit, form, datum relationship and finishMeasurement method for the complete requirement
Blind threaded featureUsable thread depth and available drill depthThread and depth acceptance
Fluid passageIntersections, cleanliness and accessible openingsInternal edge and passage verification
Countersunk jointAngle, diameter or depth and mating functionDefined countersink and alignment checks

Separate a requirement from a manufacturing assumption

If the design requires a finished bore, write its functional limits rather than assuming a nominal drill size will deliver them. The supplier may propose drilling followed by reaming, boring or another suitable finishing route. Evaluate that route against the approved geometry and evidence. Do not reject a necessary finishing operation merely because an earlier quote used the word drilling without defining the result.

Sandvik Coromant’s drilling guidance starts with hole diameter, depth and quality, then considers the component and machine. That is a useful review order for purchasing as well: identify the feature first, describe the stock and quantity, and then ask whether the proposed process can produce and verify the specified result.

Describe the hole the tool must actually reach

Depth-to-diameter ratio, often written L/D, is a useful geometric description. A 30 mm deep hole with 6 mm diameter is 5D; the same depth at 3 mm diameter is 10D. These calculations do not establish a universal process limit. They show why two holes with the same depth can require different tooling, guidance, coolant delivery and inspection access.

Blind depth has more than one meaning

Distinguish full-diameter depth from the deepest point left by a drill tip. A drawing that gives only a depth value can be ambiguous if a mating pin needs a cylindrical envelope near the bottom. State the usable depth and bottom geometry that the function requires. If a flat bottom is necessary, make that requirement explicit rather than assuming every drilling operation produces one.

For a blind threaded hole, separate usable thread depth, tap or thread-milling requirements, runout allowance and the permitted drilled depth. The relationship depends on the approved tooling and feature design. Do not assign a universal extra-depth allowance without checking the actual thread, tool geometry and remaining material. A breakthrough into an adjacent cavity may be unacceptable even when the thread gauge passes.

Entry and exit are part of the geometry

An angled entry, curved surface, interrupted exit or intersecting passage changes the operation. Mark these features in the RFQ instead of letting them disappear inside a generic hole count. The supplier needs to review support, alignment and the transition into or out of the material. A suitable method for a flat, uninterrupted surface should not be transferred automatically to a sloping or interrupted feature.

Identify whether the hole is drilled from one side or whether access from both sides is permitted. Two-sided machining may create a meeting condition that matters to flow, fit or inspection. If the drawing requires a continuous straight bore, a pair of individually acceptable entrance diameters does not prove that condition. The manufacturing proposal and measurement plan must address the full feature.

Stock allowance and datum sequence matter

A hole located before final machining of the datum faces must retain the required relationship after those faces are finished. Ask at which stage the hole is produced and inspected. If a thin web becomes flexible late in the process, determine whether inspection occurs in a free or restrained condition. A fixture that forces the component into shape can conceal a problem that reappears after release.

For purchased bar or plate that will be drilled later, give the machine shop enough allowance and identity information for its route. For a finished component, provide the complete drawing revision and critical datums. TiHubs can review titanium bar and rod as starting stock or CNC-machined titanium components as a separate delivery scope.

Comparison of two illustrative holes with equal depth but different depth-to-diameter ratios
Industrial buying guide / 02The same depth can create a different task.

30 mm depth gives 5D at 6 mm diameter and 10D at 3 mm diameter; these ratios are geometry, not process limits.

Tooling, support and chip removal work together

The right drill is a tool selected for the alloy, condition, diameter, depth, machine and required hole quality. A label such as carbide, cobalt or titanium-coated does not define that whole combination. In particular, a tool coating name is not proof that the drill is intended for machining titanium. Ask for the tool manufacturer’s application guidance for the actual tool family and operation.

Use cutting data in its stated context

Cutting speed, spindle speed, feed per revolution and feed per minute are different quantities. Changing diameter changes the spindle speed associated with a given cutting speed. Changing spindle speed while holding feed per minute constant changes feed per revolution. A copied number without units and tool context cannot be evaluated responsibly, even if another shop once used it successfully.

For metric units, the relationship n = 1000vc/(πD) connects spindle speed n in revolutions per minute, cutting speed vc in metres per minute and diameter D in millimetres. Feed rate vf = nfn connects feed per minute with feed per revolution. These are conversion relationships, not recommended parameters. The selected tool and machine guidance must supply an appropriate operating window.

Chip evacuation is a process requirement

Sandvik’s material-specific drilling note identifies chip evacuation and hole-surface work hardening as issues for titanium and heat-resistant alloys. It also distinguishes titanium cutting-edge geometry from nickel-alloy geometry. Use that guidance to ask about the proposed tool and coolant arrangement; it does not justify one universal pressure or feed for every titanium hole.

A coolant-pressure setting alone does not prove that fluid reaches the cutting zone at the required flow. Tool channels, filtration, connections and machine capability belong in the review. Likewise, a pecking cycle is not automatically suitable for every drill. Follow the tool-specific method and validate it for the actual depth and material rather than imposing a generic cycle because the workpiece is titanium.

Support and alignment cannot be replaced by a stronger tool

Review workholding, tool overhang, alignment and runout against the selected tool system. A flexible component or poorly located tool can produce errors that a material substitution will not solve. The supplier should identify the setup that supports the critical hole, especially where the component is thin, asymmetric or accessible only with an extended tool.

For a repeat programme, ask how tool condition is managed and what signals trigger inspection or replacement. A tool-life claim has meaning only with a defined tool, workpiece, operating window and acceptance criterion. Do not treat the number of holes made before tool breakage as the number of acceptable holes delivered. Dimensional or surface drift can require intervention earlier.

Deburring is part of the delivered feature

A clean entrance does not prove that the exit or an internal intersection is acceptable. Titanium components may have burrs in locations that become inaccessible after assembly. Define the relevant edges and the condition required at delivery. A general note to deburr is less useful than identifying the surfaces where a projecting edge, loose fragment or excessive edge break affects function.

Control removal without changing the fit

Deburring should remove the unwanted edge condition while preserving the approved geometry. An uncontrolled chamfer can change the bearing area of a fastener, the effective length of a locating bore or the entrance to a sealing feature. If a chamfer or radius is functional, dimension it. If only burr removal is intended, agree the permitted edge treatment and how it will be checked.

Distinguish a sharp-edge requirement from a burr-free requirement. They are not always identical. A drawing may need a controlled small edge break, or it may restrict rounding near a functional surface. The supplier should not have to infer the intended condition from a photograph. Establish the acceptance language before a large lot has been processed.

Intersecting holes need an internal plan

A cross-hole can leave an edge inside a main passage where normal external inspection cannot see it. Identify the intersection on the drawing and ask how its condition will be verified. Depending on geometry and the approved scope, an inspection plan may use direct access, a suitable viewing method or another validated technique. Do not name a method as sufficient until its coverage and limitations are understood.

For a fluid passage, distinguish visual edge acceptance, removal of loose debris and any required cleanliness criterion. A successful flow or leak check may answer one question while leaving another unresolved. For example, a passage can pass fluid and still contain an unacceptable retained particle. Specify the required evidence separately instead of treating one functional test as proof of every internal condition.

Plan the sequence before access disappears

If later welding, plugging or assembly closes an opening, establish the inspection and cleaning stage while access remains available. Record the accepted state and control what happens afterward. A final external check cannot recreate evidence from a hidden surface that was never inspected. This is an order-planning issue as much as a shop-floor issue.

Protect finished holes during handling and packing where dents, contamination or trapped debris could affect use. Identify whether plugs or protective covers are required and whether they must be removed before installation. Keep any special cleaning or packaging requirement in the quotation so the buyer can compare equivalent deliveries. The goal is a usable, verified feature at receipt, not only an acceptable hole immediately after machining.

Schematic identifying entrance, exit and internal intersection edges
Industrial buying guide / 04Inspect the edges you cannot see from outside.

Identify internal intersections and agree verification before later assembly removes access.

Measure the requirement, not just the easiest dimension

A hole inspection plan should connect each critical characteristic to an appropriate method, coverage and acceptance limit. Diameter at the entrance, position relative to datums, full depth, form and internal surface condition are different characteristics. A single passing measurement cannot be extended to all of them. Decide what must be demonstrated for the particular function.

Size and position answer different questions

A suitable size gauge can establish the characteristic it is designed to check, within its method and use conditions. It does not automatically report a hole’s location relative to the drawing datums. A coordinate measurement can address location and sampled geometry, but the probing strategy and access determine what is actually observed. Agree a method that covers the drawing rather than selecting an instrument name as a substitute for an inspection plan.

For a long bore, define whether diameter and straightness requirements apply throughout the length. Check how inaccessible portions will be evaluated. For a counterbore or countersink, define the relationship to the main hole as well as its size. For a threaded feature, specify the governing thread and gauge requirements and the usable depth. Keep these criteria attached to the correct drawing revision.

Measurement conditions also belong in the plan where tight limits make them significant. Record the relevant temperature, restraint and surface state, and confirm that the gauge or measuring system is suitable for the tolerance. A reading taken while a part is still thermally unstable should not be silently compared with a requirement defined for a different condition. Agree how the part is prepared for acceptance measurement.

Use a first article to resolve the difficult feature

An initial sample should represent the intended material, condition, tooling route and setup where the project requires that evidence. Select the holes that create uncertainty: a deep blind bore, a thin-wall exit, an internal intersection or a precise datum relationship. A report covering only easy external dimensions cannot establish that the difficult internal requirement is controlled.

Consider a hypothetical bracket with a locating bore and an intersecting fluid passage. The bore size may pass while its position misses the datum requirement, or the passage may retain an internal burr. These are different nonconformities with different evidence. The example is a review scenario, not a TiHubs case history. Its purpose is to show why first-article acceptance must follow function rather than a simple hole count.

Make the inspection record usable

Number the critical holes or feature groups so a reported result can be matched to the drawing. For a pattern, distinguish individual size results from the position of the pattern relative to its datums. If actual measured values are required, state that requirement; a simple pass/fail entry is a different reporting scope. Identify the measurement stage and the drawing revision on the record.

Agree how sampling applies across the lot and across repeated features on one component. Inspecting one accessible hole does not automatically cover every hole in the pattern. The appropriate coverage follows the approved plan and the consequence of a missed defect, not whichever location is easiest to reach.

Troubleshoot from evidence

Sandvik’s drilling troubleshooting guidance separates problems and tool types instead of treating every defect alike. When a hole is oversized, poorly finished or inconsistent, record the observed defect, location, tool condition and relevant process state. A symptom can have several causes; changing parameters without identifying the pattern can hide the original issue.

Keep nonconforming material identifiable while the responsible team reviews disposition. Rework should follow an approved route and retain the remaining functional requirements. Enlarging a hole may remove a surface problem but invalidate its fit or wall allowance. A repair is acceptable only when the authorized requirements permit it, not simply because a later measurement is easier to pass.

Checklist linking hole size, position, depth and edges to separate verification questions
Industrial buying guide / 05A passing size does not prove every requirement.

The inspection method and coverage must match each functional characteristic.

Compare cost per accepted feature and delivered component

A drilling quote depends on more than the number of holes. Diameter, depth, access, tooling, setup, secondary finishing, deburring and inspection all change the scope. A shallow clearance pattern and a deep intersecting passage can have similar hole counts but very different manufacturing and verification needs. Organize the RFQ around feature groups rather than treating every opening as one interchangeable unit.

Separate preparation from recurring work

Programming, fixture preparation and first-article verification may be significant for a small order. Repeat quantities can distribute some preparation cost, but only when the approved drawing and route remain stable. State the first order and potential repeat forecast separately. Do not present an uncommitted future volume as though it were already a firm production release.

Ask whether the price includes starting material, drilling, finishing, deburring, cleaning, inspection and documentation. If the buyer supplies material, define incoming identity and condition requirements and responsibility for nonconforming stock. A low drilling-only price cannot be compared directly with a finished, inspected component price. The separate titanium CNC cost guide addresses the broader quotation structure.

Make alternatives explicit

If the design owner permits another route, request it as an identified alternative with its own assumptions. A proposed change to hole diameter, corner condition, depth or access may simplify manufacture, but it still needs functional approval. Keep the approved baseline and proposed revision separate. A supplier’s process suggestion is valuable input, not automatic authority to change the component.

For features that cannot be produced economically or inspected adequately by the proposed route, review alternatives with the responsible manufacturing and design teams. The existing wire EDM versus CNC milling guide covers a different process comparison; it should not be treated as a universal replacement for drilling. Access, geometry and surface requirements determine the viable options.

Preserve the approval basis in repeat orders

Keep the material heat or lot connected to cut blanks and finished components. Record drawing revision, supplied condition and agreed inspection scope. Identify changes that require renewed review, such as a different alloy, treatment, hole geometry or acceptance requirement. Reordering by an informal part nickname can lose details that were essential to the original qualification.

The finished enquiry should make four things clear: what the hole must do, what geometry and material are approved, how the supplier proposes to manufacture it, and what evidence releases it. That is the practical route to reliable drilling of titanium. It turns a broad question about drill bits into a reviewable purchase for conforming material or components.

Send a hole specification that can be quoted.

Provide the drawing revision, approved titanium grade and condition, hole groups, critical datums and acceptance requirements. Identify blind depths, internal intersections, edge limits and any later process that removes inspection access. Separate starting stock from finished-component supply.

Information to include

  • Grade, product specification and delivery condition
  • Drawing revision and feature identification
  • Diameter, usable depth, position and form requirements
  • Entry, exit, intersections and edge acceptance
  • Finishing, cleaning, inspection and required records
  • First quantity, repeat forecast and delivery destination

Build your RFQ checklist

Choose the product and add the information you have. Copy the resulting brief or send your requirements to TiHubs. Submitting an enquiry does not place an order.

TiHubs — EN — Drilling Titanium: Hole Quality, Burr Control and Acceptance Requirements

Add your details, then copy the checklist or send your requirements to TiHubs.

We use these details to respond to your enquiry. Privacy Policy.

Questions buyers ask

What drill bit is best for titanium?

Select a tool for the actual alloy, condition, diameter, depth, machine and required result. Material or coating labels alone do not establish suitability. Use the toolmaker guidance for the selected family and validate the process for the component.

Should titanium always be drilled slowly?

Slow is not a defined cutting condition. Cutting speed, spindle speed and feed must be related to diameter and the selected tool. Do not use one generic setting or reduce feed blindly; review the tool-specific operating window and observed result.

Is peck drilling always required?

No universal cycle is specified here. The appropriate method depends on the drill design, depth, coolant delivery and workpiece. Follow the selected tool guidance and verify chip evacuation and hole quality for the actual operation.

Can drilling alone produce a precision bore?

That depends on the required size, form, position and surface condition and on the demonstrated process. Some requirements need a subsequent finishing operation. Quote the finished feature instead of assuming a nominal drill size guarantees the drawing.

How should blind-hole depth be specified?

Distinguish full-diameter usable depth from drill-tip depth, and define the bottom geometry where it affects function. For a threaded feature, state usable thread depth and available drilling space separately so the manufacturing route can be reviewed.

How can internal burrs be accepted?

Identify the internal edges and agree a method with suitable access and coverage. Define edge treatment, loose-particle removal and any cleanliness criteria separately. A good external appearance or a passing flow test does not automatically demonstrate every internal requirement.

Keep the purchase requirements connected.

  1. Specify the hole function and approved material before the tool.
  2. Keep usable depth, tip depth and thread depth distinct.
  3. Review chip removal, support and tool condition as one process.
  4. Include internal edges and cleanliness in the delivered scope.
  5. Match inspection evidence to size, position, form, depth and function.

Sources and data scope

References reviewed November 16, 2026. Public source summaries support the discussion; the controlled specification, agreed edition and approved project requirements govern acceptance.

  1. Sandvik Coromant — Drilling a hole — Toolmaker framework for hole, component and machine considerations.
  2. Sandvik Coromant — Drilling tips for different materials — Titanium-specific discussion of edge geometry, work hardening and chip evacuation; not a universal operating recipe.
  3. Sandvik Coromant — Drilling wear and troubleshooting — Separate troubleshooting by defect and tool type; apply within the selected tool guidance.

About TiHubs

TiHubs coordinates titanium material and custom supply enquiries from Baoji, China. Send the product, drawing revision and acceptance requirements so the proposed supply scope can be reviewed. Learn about our sourcing role.

Contents