CategoryMaterials & Grade Selection
Titanium or
tantalum?
A quotation for solid titanium and one for a tantalum-lined item can describe entirely different pressure boundaries. Trace the liquid path and the load path before comparing sheet prices.

Quick answer
Grade 2 titanium (R50400) and unalloyed tantalum (R05200) are purchased to different product specifications. One square metre of bare sheet 1 mm thick weighs about 4.52 kg in the titanium example and 16.60 kg in tantalum. In a lined vessel, the metallic liner, its seams, the support and the inspection access require separate definitions. Service compatibility and design approval govern the selection.
01 / Identify what the two suppliers are offering
Identify what the two suppliers are offering
The drawings attached to two quotations both show a vessel nozzle. One quotation covers a solid titanium neck and flange. The other covers forming and fitting a tantalum sleeve inside an existing nozzle. The second proposal may expose tantalum to the liquid over much of the same area, yet it leaves an existing structural component in service. Before comparing metals, mark the physical limit of each quotation in colour. Include the bore, the flange face, any weld at the shell and the transition back to the original equipment.
The titanium in this comparison is commercially pure Grade 2, UNS R50400. The tantalum is unalloyed R05200. Fort Wayne Metals identifies this tantalum grade, and the NRC tantalum data sheet describes flat and tubular forms for chemical process equipment. These sources establish material identities and provide useful starting information. An order for a complete nozzle still needs the construction drawing, connection details and acceptance requirements. The grade designation on a piece of sheet cannot identify how the finished pressure boundary has been made.
Ask the owner to draw two paths. First, follow the process fluid from the vessel through the connection, identifying every reachable metal and gasket. Then follow the mechanical load through the nozzle, its attachment and the supporting wall. In a solid component, much of the same material may belong to both paths. In a lined component, the corrosion-resistant surface and the structural member may be different pieces. A hole in a liner can expose the backing without immediately producing a visible external leak. A structural defect can matter even when the visible liner looks intact.
The quotation should state whether the backing is new, existing equipment supplied by the owner or a component to be inspected before work begins. Who establishes its remaining suitability? Who provides access to its far side? If the design calls for a bonded construction, define what the bond is expected to do and which qualification applies. A loose liner, a bonded plate and an applied weld overlay have different interfaces. Listing them under one general description of protected metal can hide an important exclusion in the price.
Separate an early material comparison from a release to fabricate. A chemical engineer may have enough data to retain both metals on a shortlist while still lacking the inspection results needed to reuse a particular nozzle. The resulting action might be a survey, a small material purchase or a request for construction drawings. Record which action the owner authorized. It avoids turning a preliminary statement about chemical compatibility into an assumed approval of the existing shell or the proposed lining detail.
02 / Put equal areas on a defensible mass basis
Put equal areas on a defensible mass basis
Equal volume is a useful first comparison because it exposes a common commercial error. ATI lists 4.52 g/cm³ for its Grade 2 plate and Fort Wayne Metals lists 16.60 g/cm³ for R05200 tantalum. Take one square metre of sheet, one millimetre thick, with no holes, trimming allowance, seams or attachments. Its volume is one litre, or 1,000 cm³. Its ideal bare mass is therefore 4.52 kg in the titanium example and 16.60 kg in tantalum. The ratio is about 3.67 for the same geometry.
For a second drawing example, a developed area of two square metres at a uniform thickness of 1.5 mm gives three litres of metal. The titanium mass is about 13.56 kg and the tantalum mass about 49.80 kg. These are calculated masses, not recommended thicknesses. Neither sheet has been shown suitable for corrosion, forming, pressure or fatigue. The table deliberately uses identical geometries so the effect of density can be checked without also changing the proposed construction.
To use this method on a real lining, obtain the developed area of each piece. Wall panels, nozzle returns, local reinforcement and flange faces may have different thicknesses. A curved shell cut from rectangular stock also produces offcuts. Distinguish the final installed mass from the purchased mass before comparing material costs. A workshop offering to cut a small number of complex blanks from a full sheet may need to charge for more metal than appears in the final assembly. Ask whether remaining stock is returned, retained for repairs or included as scrap in the quotation.
Geometry can change more than density does. A thin corrosion barrier over an approved structural shell and a full replacement wall of a different material may need entirely different metal volumes. For costing, calculate each actual design rather than applying the 3.67 ratio to the price of a completed vessel. Add backing, fabrication and inspection as separate line items. If installation can use an existing support, record the assumption that the support will pass the agreed examination. A price conditional on that examination should remain conditional in the purchasing comparison.
Check the arithmetic against a drawing revision. A quoted weight might include the flange backing ring or mounting hardware, while the owner’s calculation includes only the wetted metal. Request a short mass breakdown by component and material. Small rounding differences usually matter less than an omitted return at a nozzle or a panel counted twice. Once the volumes agree, the buyer has a defensible basis for discussing unit prices, material utilization and the amount of repair stock to keep on site.
| Comparison basis | Grade 2 titanium | Unalloyed tantalum |
|---|---|---|
| UNS designation | R50400 | R05200 |
| Reference density | 4.52 g/cm³ (ATI) | 16.60 g/cm³ (Fort Wayne Metals) |
| 1 m² × 1 mm, ideal bare sheet | 4.52 kg | 16.60 kg |
| 2 m² × 1.5 mm, ideal bare sheet | 13.56 kg | 49.80 kg |
| Flat-product specification to review | ASTM B265 | ASTM B708 |

Two functions in a lined wall.
03 / Trace the liquid around seams and nozzles
Trace the liquid around seams and nozzles
Follow a drop of liquid through the assembled equipment on the section drawing. At a nozzle it can meet the vessel wall, a seam, a turned lip, the bore, a gasket and the mating component before leaving the equipment. A statement that the shell is lined gives no information about the last few millimetres at the transition. At each change in material or surface, record which drawing shows the detail, which shop makes it and who verifies the completed geometry.
Consider a flanged outlet whose liner turns across the face. The gasket may bear entirely on the return or may extend beyond it, depending on the actual diameters, position and compression. Ask for the mating flange and gasket drawing, including the condition after the joint is assembled. A plan view of the unloaded liner can make the coverage look generous while leaving a narrow exposed edge in service. Identify whether the contact face is supplied finished, requires machining after assembly or is protected until site installation.
The most aggressive local exposure may occur away from the area used to select the metal. Process liquor can concentrate during drying, vapour can condense on a cooled surface and cleaning solution may remain behind a fitting after the main vessel drains. Obtain the chemistry, temperature and duration for the vulnerable location. If the material comparison relies on published corrosion information, identify the actual medium and limits of that comparison. Where the plant has experienced a failure, ask for photographs before cleaning, the operating sequence and any change in feed or maintenance practice.
For a sleeve termination, decide what happens if liquid passes the first barrier. Does it enter an accessible space, reach the structural backing, emerge at a monitored point or remain concealed? This is a design question for the owner and fabricator. A proposed inspection or leak-detection feature must suit the actual construction and operating conditions. Never add an opening to pressure equipment on the strength of a general lining illustration. The purpose of tracing the route is to find an unanswered question while it can still be resolved on the drawing.
Do the same exercise for the opposite side of the wall. Washdown, a heating jacket, an insulation cover or an external support can create a separate exposure that the process-side lining does not address. Mark which surfaces are inside and outside the enquiry. If the purchase covers only the internal lining, assign the external survey and any necessary repairs to a named party. This avoids a common shutdown delay in which the lining shop arrives ready to work but cannot proceed because nobody owns the condition of the surrounding equipment.
Pay attention to repairs already present on the removed part. A metal patch might cover an earlier change of material or a failed transition that never reached the main equipment drawing. Photograph and locate it before cutting it away. If its origin cannot be traced, document that uncertainty instead of treating the patch as an approved manufacturing detail. A replacement design should recover the function of the region, while engineering retains responsibility for deciding whether copying an undocumented repair would preserve an old problem.

Mass per square metre at 1 mm.
04 / Specify the backing and the interface
Specify the backing and the interface
A loose metallic liner follows the shape of a support while retaining an interface between the two. A bonded construction has a defined attachment across some or all of that area. A solid replacement has no separate lining interface in the wall itself. These descriptions say little about performance until the actual drawings, materials and operating cycles are known. A useful quotation names the construction in plain language and identifies which document defines the connection between the protective surface and its support.
Start with the backing condition. Ask how the shop intends to establish the dimensions, surface condition and remaining section of the area to be reused. Can it survey the backing before materials are ordered, or only after stripping the old lining during the outage? If measurements are deferred, define which differences the price allows and when a revised proposal is needed. Otherwise the lowest initial quotation may simply be the one making the most generous assumption about what will be found underneath the old material.
Temperature changes can make the interface a design issue even in a vessel whose normal bulk temperature appears steady. Start-up, cleaning and shutdown may change the relative temperatures of the wetted metal and the backing. The two parts may also be constrained differently at a seam, a nozzle or a fixed support. Ask the designer how the proposed arrangement accommodates the relevant movements and pressure differences. A list of elemental coefficients is insufficient to approve a completed joint without its dimensions, restraints and temperature history.
The sequence of fabrication affects what can be examined. A backing weld accessible on the shop floor may disappear behind a liner. A transition visible before fitting a flange may be inaccessible after it is attached. Mark the hold point before each significant feature is concealed. Specify how inspection results will be identified to the location on the drawing, and what happens if a deviation is found. A final photograph of a finished shiny surface cannot recover a missing check of an underlying connection.
Consider how a replacement will fit through the available opening. A liner that can be formed and inspected in a shop may need to arrive in several sections when installation takes place inside an existing vessel. Every additional field seam changes the work, access and inspection package. Give the supplier the manway dimensions, obstructions and handling constraints relevant to the proposed route. If shop fabrication and field installation are separate contracts, agree who will accept the handover geometry and who will own any mismatch discovered when the sections are brought together.

What a local opening can expose.
05 / Choose inspection evidence for each failure path
Choose inspection evidence for each failure path
Choose an inspection by identifying the defect that matters. A discontinuity in a wetted liner, loss of bonding in a bonded product, a leak through a seam and insufficient structural wall thickness are different conditions. Agree with the responsible engineer which method can assess each one in the proposed construction. An inspection report is more useful when it names the surface, area, sensitivity or acceptance criterion, stage of manufacture and location of the results. A general statement that the equipment was tested leaves these questions for the receiving inspector.
A visible weld bead or continuous-looking surface can be a valuable first observation. It does not reveal every subsurface condition or every possible liquid path. Conversely, an examination intended to find a structural-wall defect may not demonstrate continuity of an independent liner. Have the inspection plan show which boundary is under examination at each step. If two tests use the same access port, confirm how the equipment will be configured for each and what part is isolated. Testing arrangements require the owner’s approved procedure and competent personnel.
For a patch repair, trace the old and new metal separately. Record the perimeter of material removed, the condition found underneath, the replacement material and the joints that restore the barrier. If the repair crosses an existing seam or terminates beside a nozzle, mark those intersections on the drawing. A photograph with scale and position can help a later inspector find the exact feature. Agree in advance whether sample records, witness pieces or measurements are to accompany the repair rather than assuming they can be reconstructed after the vessel returns to service.
Plan for an ambiguous finding. Suppose a proposed final test gives an indication whose location is uncertain. The owner needs a route for isolation, investigation and retest. Establish who decides whether a repair is authorized and which previous checks must be repeated. In a lined assembly, carrying out local work on the surface can affect an adjoining joint or a protected area underneath. Tie the retest boundary to the actual repair rather than closing the issue only because the visible mark has disappeared.
At handover, organize the records by equipment location. A materials certificate for each starting product, a seam map, inspection reports, approved deviations and an as-built nozzle section together let the operator answer a specific question during the next outage. Identify any inaccessible region, unexamined area or limitation of the chosen method. That limitation can then inform the in-service inspection plan. The owner benefits more from an accurately bounded record than from an unqualified claim that the complete lining has passed every conceivable test.
For example, identify the nozzle tag, the clock position at which a patch begins and the drawing revision. State the viewing direction for the clock position. Photographs taken from opposite sides of the equipment reverse left and right and could otherwise send a future inspector to a different seam.
See titanium vessels and process equipment for the equipment drawing and enquiry route.
06 / Compare repair scope and lifecycle exposure
Compare repair scope and lifecycle exposure
Build the commercial comparison around the work needed to restore service. A solid replacement may require removing a complete spool or nozzle and changing connected parts. A local lining repair may retain much of the existing structure while concentrating specialist work into a short outage. The material bill alone captures neither the access cost nor the time spent waiting for an inspection release. Ask each supplier which activities can be completed before shutdown and which depend on opening the old equipment.
Separate firm prices from conditional items. Sheet stock cut to an approved drawing is different from a field repair whose backing condition remains unknown. Obtain a basis for surveying, removing old material, preparing the backing, forming pieces, joining, examining and reinstating the assembly. List owner-supplied work such as access, isolation and lifting. If a supplier omits a task because another contractor normally performs it, record that dependency next to its price. A comparison that assigns each task once is more useful than adding two seemingly complete lump sums.
Consider spare strategy in the form actually needed. Flat sheet retained from a parent heat may help a future repair but may not reproduce a formed nozzle return or provide the qualified joining arrangement. A fabricated spare can reduce forming time yet requires protective storage and an identifiable drawing revision. Ask what dimensions or certificates will remain available if the original workshop no longer holds its records. Keep small specially shaped pieces linked to their documentation after unpacking, particularly when titanium and tantalum stock are stored in the same maintenance area.
An owner’s decision note should state why the selected construction suits the documented process, what it assumes about the backing and which inspections authorize its return to service. Where the two metals remain viable, compare the consequence of a local defect and the practical ability to detect and repair it. Where one option lacks service evidence, identify the missing evidence explicitly. A longer theoretical life entered without a source can distort a lifecycle comparison far more than a modest uncertainty in the price of sheet.
For a titanium enquiry, send TiHubs the selected grade, product form, drawing, developed area or dimensions, quantities and requested delivery. Distinguish a purchase of test sheet from an order for a formed component or a request for assessment of an existing assembly. If tantalum is included only as a commercial benchmark, say so. Identify responsibility for design, fabrication, field installation and acceptance. The resulting quotation can then be compared against the actual service task while preserving the distinction between supplying metal and approving a complete piece of plant.
When comparing outage schedules, mark the first moment at which each route can legitimately return the equipment to the operator. Delivery of the last sheet, completion of a field seam, release of an examination report and acceptance of the assembled connection are different milestones. Ask what happens if a specified witness cannot attend immediately or a backing inspection finds an unexpected condition. A route with more expensive starting material may still fit a planned stop better, but only if the fabrication, examination and release sequence actually supports the stated timetable.
07 / Build your RFQ
Request a technical quotation
A quotation for solid titanium and one for a tantalum-lined item can describe entirely different pressure boundaries. Trace the liquid path and the load path before comparing sheet prices.
Information to include
- Wetted surface and support
- Material, area and thickness
- Nozzle and seam drawings
- Leak path and inspection access
- Outage and repair responsibility
Build your RFQ checklist
Choose the product and add the information you have. Copy the resulting brief or send your requirements to TiHubs. Submitting an enquiry does not place an order.
08 / FAQs
Questions buyers ask
Does a thin tantalum liner carry the vessel pressure?
Identify the structural boundary on the approved design. A loose corrosion-resistant lining and a bonded construction are different arrangements. The presence of a liner or the strength of its starting sheet does not establish the pressure rating of the equipment.
Can the quoted price per kilogram decide the comparison?
Compare the surface area actually protected, metal thickness, seams, backing, inspection and installation scope. Equal-area sheets can have very different mass. Delivery of a formed, inspected liner includes operations absent from a quotation for flat stock.
Which dimensions are needed before quoting a nozzle repair?
Send the nozzle section, existing liner termination, flange face, bore and access envelope. Mark what can be removed during the outage and who will approve the repair design and testing. Identify unavailable measurements explicitly so that the supplier can price a survey or state a condition.
09 / Key takeaways
Keep the purchase requirements connected.
- Wetted surface and support
- Material, area and thickness
- Nozzle and seam drawings
- Leak path and inspection access
- Outage and repair responsibility
Technical references
Sources and data scope
References reviewed November 20, 2026. Public source summaries support the discussion; the controlled specification, agreed edition and approved project requirements govern acceptance.
- ATI commercially pure Grade 2 — Grade designations and published plate density.
- Fort Wayne Metals — Tantalum — R05200 identity and 16.60 g/cm³ reference density.
- NRC tantalum, PD-7035 — R05200 stock forms and chemical process equipment applications.
- ASTM B265 — Titanium strip, sheet and plate.
- ASTM B708 — Tantalum and tantalum alloy flat products.
- TIMET corrosion manual — Environmental factors affecting selection of titanium for chemical service.