CategoryManufacturing & Customization
Titanium honeycomb,
core or panel?
Before comparing quotations by square metre, establish what each bidder includes between the outer faces. A bare core, a faced panel and a machined panel with inserts can share one outline while carrying different mass, operations and acceptance requirements.

Quick answer
Identify the core, both skins and the joining method separately. Specify which directions matter, what the published density describes and whether the inspection coupon represents the bare core or the finished sandwich. A core-material test and a panel-interface test answer different purchasing questions.
01 / Define the product between the two outside faces
Define the product between the two outside faces
A line item reading “titanium honeycomb, one square metre” leaves a decisive question open. One shop could offer an expanded block of thin metallic foil. A second could offer a cut panel with two face sheets already joined to the core. A third could supply the same panel with a closed perimeter, drilled attachment points and protection on the show face. Each could be describing the specified plan area accurately. Only one of the three could be fitted immediately into a frame intended for the finished assembly. Start the enquiry with a section drawn through the centre and a second section through a finished edge. Identify what the supplier is to deliver on each section.
For bare core, show its length, width and height, the orientation of its cells and the condition in which it must arrive. Identify the foil material and any handling allowance. A buyer who intends to produce the final perimeter after joining skins may value additional stock on two edges. A buyer installing a precut block within an existing frame may have little space for a projecting cell wall. These are different deliveries. If the core has to follow a curved shape, include its intended orientation and the mating geometry. A photograph showing that a sample can bend in someone’s hands gives very little information about how the finished structure will fit.
For a faced panel, identify the upper and lower skins individually. Record their respective grades, thicknesses and finishes, which face the installer sees and which face meets the frame. Also identify the material between the skins, the joining route that the supplier proposes and any separate perimeter member. If the two faces differ, mark them on the part as well as on the drawing. A crate containing several identical rectangular blanks gives the receiving inspector few clues about which side is meant to face a cleaning operation. Agree on a marking location that survives handling and can be removed where required.
Give every quoted option the same boundary. For example, ask for a bare core with allowance, an untrimmed sandwich blank and a finished panel as three separate prices only if the purchasing team could actually use all three. Attach a list of operations retained by the buyer to each option. This exposes a seemingly cheap part that transfers trimming, local reinforcement or qualification testing to a different department. The commercial titanium honeycomb example in the sources describes a material form available in the market. Use the requested drawings and a written capability response to establish the specific construction available for a particular order. A trade name on a catalogue page cannot define all the interfaces in a customer’s assembly.
02 / Calculate apparent core density and panel mass
Calculate apparent core density and panel mass
Calculate core density from the mass and external volume of the defined bare-core specimen. The volume includes its open cells. It therefore represents the space occupied by the core, including the empty part, and differs from the volume of titanium metal present in the foils. The typical solid density used for a Grade 2 skin has a different purpose. Multiplying the whole panel envelope by that solid density would treat the cells as solid metal. Conversely, applying the bare core density to the entire finished thickness would charge the skins at the density of an open cellular structure. Keep a separate line for each component in the estimate.
Consider a hypothetical rectangular core measuring 300 by 200 by 12 millimetres. Its external volume is 720,000 cubic millimetres, or 720 cubic centimetres. Suppose its measured mass, after removing packaging and identification tags, is 72 grams. Dividing by external volume gives an apparent density of 0.100 gram per cubic centimetre, or 100 kilograms per cubic metre. This is an example calculation with an assumed mass. It is not a catalogue density for a particular cell size. For a purchase limit, identify the specimen condition, measurement procedure, direction, report precision and agreed sampling plan. A change in the supplied expansion condition can change measured dimensions and consequently the reported apparent density.
Now add two flat Grade 2 sheets with the same plan dimensions. At a nominal thickness of 0.40 millimetre each, each sheet occupies 24 cubic centimetres. Using the typical solid density of 4.51 grams per cubic centimetre reported by TIMET for TIMETAL 50A gives 108.24 grams per skin. Two skins plus the example core total 288.48 grams. Dividing 0.28848 kilogram by 0.060 square metre gives 4.808 kilograms per square metre. The arithmetic carries extra decimal places so another buyer can reproduce it. Inspection limits and scale resolution belong in a separate agreement. The apparent precision of the answer does not improve the accuracy of the assumed thickness or mass.
Add the mass of closures, joint material, hard points and identification hardware when comparing a finished unit to the subtotal. Decide how to handle removed material associated with holes or openings. If the framed panel has a maximum permitted installed mass, weigh it in the specified finished condition and state which detachable components accompany it on the scale. In a bid comparison, a figure quoted per square metre of bare core is useful only alongside an equally described figure. A supplier might alternatively quote an average areal mass for a specific full panel, including its edges. Doubling that panel’s area does not necessarily double the mass of its borders. Use component quantities or a fresh finished-unit calculation when the outline or attachment pattern changes.
For a quick quotation audit, ask a colleague to reproduce the mass from the inputs alone. A frequent transcription error occurs when one column contains millimetres and the supplier’s density uses cubic centimetres. Keep the original dimensions in one column and show converted volume in the next. Finish the check by reconciling the estimate with an actual weighed part and documenting the components responsible for the difference. A recorded allowance from one small panel should not automatically follow a much larger panel with a different perimeter.
| Worked example or test reference | Input or scope | Result or interpretation |
|---|---|---|
| Illustrative bare core | 300 × 200 × 12 mm external envelope, assumed specimen mass 72 g | External volume 720 cm³, apparent density 0.100 g/cm³ or 100 kg/m³ |
| Illustrative Grade 2 face | 300 × 200 × 0.40 mm solid sheet at 4.51 g/cm³ | 24 cm³ and 108.24 g per face |
| Two faces plus core | 2 × 108.24 g + 72 g | 288.48 g before joints, borders, inserts and other hardware |
| Illustrative areal mass | 0.28848 kg divided by 0.060 m² | 4.808 kg/m² for the stated subtotal |
| ASTM test families | C271/C271M, C365/C365M, C273/C273M, C297/C297M | Density, flatwise compression, core shear and flatwise sandwich tension respectively |

The same outside plan dimensions can describe a core block or a finished panel with two additional skins.
03 / Read cell dimensions, direction and trimming details
Read cell dimensions, direction and trimming details
A hexagon is easy to recognise and surprisingly easy to dimension in two different ways. Ask where the supplier measures the stated cell size. Show the reference points on a view looking down onto the broad face. A distance between opposite flats, an opening between free walls and a repeat measured across several cells can give different results. Show the orientation of the dimension line. If the controlling requirement is to mate to another pattern, state the repeat and the local feature that must line up. A single cell taken from near a trimmed border can give a poor indication of the repeating geometry across the centre.
Core manufacturers can identify a ribbon or longitudinal direction and a transverse direction in the plane, commonly marked L and W. The thickness direction is perpendicular to both. Ask the supplier to mark its own convention and relate those arrows to the finished panel axes. A direction shown on a data sheet becomes actionable when the receiving team can identify it on the actual blank. An in-plane property from a coupon aligned one way may be a poor substitute for the property in the other direction. Request separate reported directions if the purchase decision depends on both. A square panel turned through a quarter turn can keep the same outline and present a different core orientation to the assembly.
Distinguish core height from finished thickness. A drawing might show stand-off between two supporting surfaces, a skin-to-skin thickness in a particular region, or the height of unjoined core stock. Label each measurement by its contacting surfaces. Point contacts over an unsupported cell can influence a reading on a thin skin. Define the measurement support, location and acceptable contact method together with the supplier before treating two readings as evidence of a dispute. If one face has a protective film, state whether the film is present when the dimension is taken. Retain details of any temporary frame that holds loose core during the measurement.
The outline also requires an origin. Put a stable datum on a feature that remains accessible after the edge treatment is applied. State which edges are supplied oversize, which must follow the final profile, and whether the last row of cells can be interrupted. Where a decorative or exposed edge has a visual requirement, show a permitted edge sample and describe how to inspect it. An instruction to maintain perfect hexagons up to an arbitrary curved trim line may be incompatible with the pattern. Ask for a proposed trim arrangement on the drawing before approving a nest of expensive parts. Record which side retains the material at each cut and whether the supplier must return any usable offcuts.

Calculated component masses exclude the joint material, borders and local reinforcement.
04 / Specify faces, interfaces, edges and inserts
Specify faces, interfaces, edges and inserts
The face sheets do several jobs in a real purchase. They provide an exterior surface, establish part of the finished thickness and give the customer something to fasten, clean or inspect. List these requirements separately. A visible face might need a uniform finish while the opposite face must locate against an existing support. Identify any area where superficial protective film is permitted and the state in which it must be removed. If a subsequent operation heats or cleans the surface, disclose it while choosing the face finish and the joining route. Let the responsible engineering team approve the materials for the actual environment.
An interface can be hidden on the finished part. Before ordering, obtain a cross-section showing how the core meets each skin, and ask which part of that construction a proposed inspection can actually assess. A photograph of an unbroken outer sheet can establish visible appearance but says little about a hidden joint. Ask how the fabricator identifies a production run and what evidence accompanies that run. A companion coupon may be useful when it shares the relevant skins, core, direction, joining cycle and preparation. A stock coupon made earlier on unrelated material can illustrate a method without tracing the condition of the panel being shipped.
The edge detail decides whether the customer receives open cells, a filled band, a separate rail or a metal closure. State which treatment applies to each edge. Provide a section at corners where two edge details meet. Clarify whether an edge must drain, remain accessible or exclude debris. A closed-looking perimeter alone does not establish a hermetic seal. If a seal is a contractual feature, the parties need an appropriate test, boundary, acceptance criterion and record. If the assembly instead needs ventilation or drainage, the installation drawing should identify the relevant paths and how later coatings or fittings affect them. Neither condition can reasonably be inferred from an attractive exterior photograph.
A hole through a skin and a usable attachment point are also different deliverables. Draw the insert, backing element or local build-up if one is required. Identify its position relative to the finished datums and the face from which it is installed. Include any prohibition on exposed joint material near a clean surface. Request the method used to verify insert location and which mechanism a representative attachment test is intended to evaluate. A strong insert body is of limited value if its connection to the surrounding construction is the controlling feature. When two suppliers propose different attachment arrangements, record the overall thickness, local footprint, permitted access and inspection evidence for each before selecting between them.

A central cut sample and a sample near an insert can represent different construction details.
05 / Choose a specimen that answers the purchase question
Choose a specimen that answers the purchase question
Choose the test by writing the question first. If the buyer needs to confirm mass per volume for the incoming bare material, the ASTM catalogue identifies C271/C271M as the density method for sandwich core materials. If the question instead concerns compression perpendicular to the faces, C365/C365M addresses flatwise compressive properties of sandwich cores. The two resulting numbers describe different properties with different units. A density entry alone cannot establish compressive performance. On the purchase order identify the applicable edition, relevant test condition, specimen preparation and required result. Standards titles are a starting point for choosing the method, while the acceptance values come from the approved technical requirements.
When the concern is the core in shear, ASTM C273/C273M describes a shear test for sandwich core materials. Record the orientation of each specimen and the construction details needed to interpret the result. For flatwise tensile strength of sandwich constructions, ASTM C297/C297M addresses a different question involving a representative sandwich. Ask for the observed failure location as well as the result. Failure within core material, separation at an interface and a failure associated with fixtures do not support the same conclusion. The reviewer should establish whether the result is valid under the agreed method and whether it represents the location the buyer intended to evaluate.
Define what “same as production” means for each specimen. If a buyer is purchasing a panel with locally reinforced edges, a coupon cut from the interior may describe the central sandwich quite well. It may leave the reinforced detail entirely unrepresented. Mark proposed sampling sites on a drawing. Identify whether samples are cut from an actual finished unit, made as an extension of the production panel or produced as companion material. Agree which cuts the order allows and who pays for the material consumed. A test contract that requires an intact finished quantity and destructive samples from that same quantity needs an explicit sampling allowance.
Ask the supplier to return a report that a reviewer can connect to the order months later. Useful fields include drawing and revision, material identifiers, specimen dimensions, test direction, conditioning, result, units and failure description where relevant. Require enough information to distinguish a routine production check from a qualification of a new construction. Compare bids on the reports and quantities included. A lower price that covers only an outward inspection may still be appropriate when the buyer has qualified identical material separately. In a first production order, the buyer may reasonably choose to pay for better linkage between construction, test evidence and delivery. Record that decision explicitly so it is still intelligible when a replacement is ordered.
Read the related technical guide for the companion product or property.
06 / Accept delivery and manage a later replacement
Accept delivery and manage a later replacement
Plan receiving around the difference between a shipping defect and a production characteristic. A bare block can be distorted by handling at its unsupported edge. A finished panel can arrive with an intact face and a locally damaged closure or attachment detail. Ask for suitable support and separators, and agree where the unpacking crew can lift the part. Record packaging condition before discarding the supports. If the part has an identified orientation, keep the marks legible while it moves from the crate to inspection. A loose label placed beside several panels ceases to identify an individual panel as soon as the pieces are moved.
Review the bundle of records in the order the assembly is built. Link the foil documentation to the core, each skin to its material record and any joining or insert evidence to the specific panel identifier. Check the revision on the fabrication drawing against the purchase order and any approved changes. Then inspect the actual delivered features against that drawing. A correct report for one type of commercially pure titanium does not automatically identify the other skin or the core. A packing list stating “titanium panel” gives the reviewer very little help with this check. A simple component list with traceable identifiers makes the same review considerably faster.
Consider a replacement request made after the original unit has been installed. A photograph and the outer dimensions may recover the outline, but the original core orientation, foil material and local reinforcements can remain concealed. Retain the signed construction section, the panel identifier and items that changed during manufacture. If the next supplier proposes a different joining method or edge closure, ask for a clearly marked departure and the consequences for inspection and fit. A similar apparent density alone gives insufficient evidence for an interchangeable assembly. Any move to a different construction belongs with the party responsible for the design.
For a useful enquiry, send a dimensioned plan, the centre and edge sections, a component list and the required inspection evidence. Mark the features that drive cost, such as a finished edge, a small run with destructive specimens or a set of matched attachment points. Invite the fabricator to price an alternative separately where the drawing permits flexibility. On the quotation summary record the delivered form, finished dimensions, orientation, material for every layer, included tests, packaging and responsibility for final machining. This gives purchasing a price for the part it can actually use and gives inspection a practical checklist when the order arrives.
07 / Build your RFQ
Request a technical quotation
Before comparing quotations by square metre, establish what each bidder includes between the outer faces. A bare core, a faced panel and a machined panel with inserts can share one outline while carrying different mass, operations and acceptance requirements.
Information to include
- Core, skin and attachment scope
- Cell size, direction and height
- Skin thickness and material
- Edges, penetrations and inserts
- Coupon location and inspection records
Build your RFQ checklist
Choose the product and add the information you have. Copy the resulting brief or send your requirements to TiHubs. Submitting an enquiry does not place an order.
08 / FAQs
Questions buyers ask
Can core density be multiplied by finished panel volume?
Use apparent core density only for the core volume it describes. Calculate solid skins separately and add the joints, closure material, inserts and hardware that fall inside the ordered scope.
Does a flatwise compression report prove face adhesion?
It addresses compressive behaviour in the stated specimen. If the purchase question concerns the interface in tension, specify a representative sandwich construction and the appropriate tensile test and failure description.
What does titanium honeycomb specify about both skins?
Confirm the core foil and each facing individually. A titanium core can be ordered without any facing and a faced panel can combine different materials. Identify every layer on the drawing.
09 / Key takeaways
Keep the purchase requirements connected.
- Core, skin and attachment scope
- Cell size, direction and height
- Skin thickness and material
- Edges, penetrations and inserts
- Coupon location and inspection records
Technical references
Sources and data scope
References reviewed November 20, 2026. Public source summaries support the discussion; the controlled specification, agreed edition and approved project requirements govern acceptance.
- ASTM International — Composite Standards — Official test-method catalogue for core density, compression, shear and sandwich tension. Specify the agreed edition on the order.
- Stanford Advanced Materials — Titanium Honeycomb — Commercial example distinguishing titanium honeycomb core from sandwich construction and facing options.
- TIMET — TIMETAL 50A — Typical solid Grade 2 density for the example face-sheet calculation.