Ti-6246 / TC19 titanium materials and application forms on a dark metallic background

Ti-6246 · TC19 · UNS R56260

Ti-6246 / TC19 titanium.For compressor and aerospace structural requirements.

Source Ti-6246 / TC19 titanium bar, forging blanks, rings and structural wire for specified aerospace parts. TiHubs coordinates the drawing, material condition, processing and inspection through one contact in Baoji.

Start with a specification, drawing or application. We’ll help identify the details still needed.

Material review. Supply coordination.
One contact in Baoji, China.

Ti-6246 / TC19Ti-6246 · Ti-6Al-2Sn-4Zr-6Mo · UNS R56260
Defined material & conditionMatch the product, process and acceptance requirements
One contact20 years of founder experience · 100+ Baoji factories

01 / Product forms

Find your
Ti-6246 / TC19 product.

Choose a material form or application. Send the dimensions, service conditions and required records so we can match the manufacturing route to your order.

Ti-6246 / TC19 titanium disc forging blanks — material and specification illustration
01 / 06

Ti-6246 / TC19 · Ti-6246 · Ti-6Al-2Sn-4Zr-6Mo

Ti-6246 / TC19 titanium disc forging blanks

Forging blanks for specified compressor and structural-part requirements. Provide the blank and finished drawings so section size, process route, test locations and machining stock can be reviewed before quotation.

Specification
AMS 4981 covers the specified bars, wire, forgings and forging stock. Select the drawing-required revision and apply its product and section limits.
Geometry
Disc diameter, thickness, hub and rim geometry, section transitions, minimum machining allowance and quantity.
Processing
Required forging route, microstructure and final heat treatment. Identify whether the order is for stock, a rough forging or a heat-treated blank.
Acceptance
Material identity, sampling orientation and location, structure, NDT zones, dimensions and traceability. TC19 uses the agreed forging requirements alongside GB/T 3620.1 chemistry.
Ti-6246 / TC19 titanium bar & rod — material and specification illustration
02 / 06

Ti-6246 / TC19 · Ti-6246 · Ti-6Al-2Sn-4Zr-6Mo

Ti-6246 / TC19 titanium bar & rod

Stock for high-strength machined aerospace parts and project-specific processing. Include the finished geometry and condition so the quotation can cover the correct section, allowance and inspection basis.

Specification
AMS 4981 is an aerospace bar route for Ti-6Al-2Sn-4Zr-6Mo. For TC19, specify the required bar product document in addition to its material designation.
Geometry
Diameter or section × length, straightness, machined or ground surface, cutting allowance and quantity by size.
Condition
Confirm the ordered solution-and-precipitation-heat-treated route or another explicitly approved specification. Mechanical acceptance depends on the product and relevant section.
Acceptance
Chemistry, tensile test location and orientation, heat-treatment records, surface, dimensions and agreed ultrasonic inspection.
Ti-6246 / TC19 ring & hollow forging blanks — material and specification illustration
03 / 06

Ti-6246 / TC19 · Ti-6246 · Ti-6Al-2Sn-4Zr-6Mo

Ti-6246 / TC19 ring & hollow forging blanks

Annular blanks and drawing-based hollow forgings for reviewed engine and structural requirements. A forged ring or machined hollow blank is not described here as standard seamless pipe.

Specification
Apply AMS 4981 where the ordered forging falls within its scope, or the purchaser-approved forging document. Define the TC19 manufacturing and acceptance requirements explicitly.
Geometry
OD, ID, height, flange or step geometry, minimum section, eccentricity and stock allowance at critical surfaces.
Processing
Forging route, grain-flow or structure requirements, heat-treatment stage and any rough-machining work. Include the final drawing to identify critical transitions.
Acceptance
Test locations, dimensional datums, inspection coverage, structure and surface quality. State any additional approval or proof requirements for the intended component.
Ti-6246 / TC19 titanium structural wire — material and specification illustration
04 / 06

Ti-6246 / TC19 · Ti-6246 · Ti-6Al-2Sn-4Zr-6Mo

Ti-6246 / TC19 titanium structural wire

Wire and straight lengths for specified component manufacturing. Define the product condition and downstream process so surface and mechanical requirements can be reviewed with the manufacturing scope.

Specification
AMS 4981 includes Ti-6Al-2Sn-4Zr-6Mo wire. Specify the revision, diameter and required delivery condition.
Supply form
Diameter and tolerance, coil or straight lengths, surface, coil weight or piece length and protective packing.
Processing
Forming or machining requirements, final heat-treatment responsibility and any sample approval. Identify finished-component requirements separately from raw wire.
Acceptance
Chemistry, specified mechanical tests, surface, dimensions and lot records. Structural wire is not automatically a qualified welding consumable.
Ti-6246 / TC19 compressor disc, blade & seal requirements — material and specification illustration
05 / 06

Ti-6246 / TC19 · Ti-6246 · Ti-6Al-2Sn-4Zr-6Mo

Ti-6246 / TC19 compressor disc, blade & seal requirements

Application illustration: material and processing review for released compressor-component drawings. Begin with the material specification and critical section, then define the required supply stage and supporting evidence.

Supply boundary
Stock, forged blank, heat-treated blank or drawing-based machined item. Make the responsibilities for subsequent operations explicit.
Design duty
Specified temperature history, rotational or cyclic loads, required life-related acceptance and critical zones identified by the design authority.
Manufacturing
Forging and heat-treatment route, structure, grain flow, machining allowance and surface condition. State purchaser restrictions on sources and special processes.
Acceptance
NDT class and coverage, mechanical sampling, dimensions, traceability and required first-article or approval documents. Material conformity alone does not qualify a rotating part.
Ti-6246 / TC19 machined airframe & engine structures — material and specification illustration
06 / 06

Ti-6246 / TC19 · Ti-6246 · Ti-6Al-2Sn-4Zr-6Mo

Ti-6246 / TC19 machined airframe & engine structures

Application illustration: source blanks and drawing-based machining for specified aerospace structural parts. Agree the stock route, final condition and inspection package before comparing finished-part offers.

Starting material
Bar, disc or ring forging selected against the released material and process requirements. The drawing determines whether a particular stock route is acceptable.
Geometry
Machining envelope, critical interfaces, thin sections, thread or bore details, datums, surface finish and inspection access.
Sequence
Rough machining, final heat treatment, finish machining and any surface process. Identify approval points and allowable dimensional correction.
Acceptance
Critical dimensions, material and process records, required NDT, surface evidence and customer approval. Finished-component qualification is agreed for the particular order.

Images illustrate material forms and application possibilities. Reference markings identify specification options; they do not establish dual certification, stock availability or finished-component approval.

Define the product. Share the requirement.

These details help turn your enquiry into a comparable quotation.

01 / Requirement review

A disc or ring forging

Send blank and finished drawings, critical sections, structure and NDT requirements. State the condition and stage required at delivery.

Discuss your requirement

02 / Requirement review

A machined aerospace component

Provide datums, tolerances, interfaces, permitted stock routes and final condition. Include customer approval and first-article requirements.

Discuss your requirement

03 / Requirement review

A repeat stock order

List sizes, quantities, standard revision and records. Agree cut-piece identification, source or process change control and dispatch milestones.

Discuss your requirement

02 / Material identity

What is
Ti-6246 / TC19 titanium?

Ti-6246 / TC19 is a heat-treatable alpha-beta titanium alloy. Product form, section and processing history belong in the same material review as chemistry and required mechanical properties.

The figures below identify the alloy and support preliminary comparison. Mechanical acceptance must come from the actual product specification and final condition.

4.64g/cm³

Approximate density · producer reference

6% Mo

Nominal molybdenum addition

α + β

Alpha-beta titanium alloy family

TIMET 6-2-4-6 technical reference · density and alloy identity; these are not component design allowables.

Property or conditionReferenceOrdering implication
DensityApproximately 4.64 g/cm³Producer reference for preliminary blank-mass estimates. Include the actual stock envelope and process allowance.
Alloy familyHeat-treatable alpha-beta titaniumTi-6246 / TC19 is specified with a manufacturing route and final condition; the alloy name alone is not a strength acceptance criterion.
ConditionProduct-specific heat treatmentAMS 4981 is a solution-and-precipitation-heat-treated product route. Other conditions need an explicitly applicable specification and purchaser agreement.
Strength and ductilitySection and process dependentQuote the acceptance values for the actual product, section and orientation. Historical producer tables must not be presented as universal requirements for all TC19 or AMS 4981 material.
Forging routeMicrostructure affects the assessmentIdentify the required forging and heat-treatment route, structure and test locations. Do not switch between process routes without reviewing the specified requirements.
Service environmentTemperature, load and exposure togetherProvide thermal duty, cyclic loading and chemical exposure where relevant. Material-property tables do not establish component life or stress-corrosion suitability.

Use section- and condition-specific acceptance requirements. Historical producer tables do not replace the ordered AMS revision, TC19 product requirements or the part approval process.

Element · wt.%Ti-6246 · nominal identityGB/T 3620.1-2016 · TC19 limits
Aluminum · Al6 nominal5.5–6.5
Tin · Sn2 nominal1.75–2.25
Zirconium · Zr4 nominal3.5–4.5
Molybdenum · Mo6 nominal5.5–6.5
Oxygen · OApply the ordered product specification0.15 max.
Iron · FeApply the ordered product specification0.15 max.
Carbon · CApply the ordered product specification0.04 max.
Nitrogen · NApply the ordered product specification0.04 max.
Hydrogen · HApply the ordered product specification0.0125 max.
Titanium · TiBalanceBalance

Nominal identity and chemical acceptance limits serve different purposes. Apply the complete ordered product specification, including sampling, residuals and any product-specific exceptions.

Ti-6246 / TC19 / Ti-6Al-2Sn-4Zr-6Mo

These are the alloy designations used for this page. UNS R56260 identifies Ti-6246. Include the product specification, edition, delivered condition and required records in the enquiry.

Ti-6246 and Ti-6242S

The nominal molybdenum addition differs: 6% in Ti-6246 and 2% in Ti-6242S, with the latter also specifying a small silicon addition. Their product routes and heat-treatment requirements should remain distinct.

Forging stock and a finished forging

Feedstock for a forging operation and a heat-treated forging blank have different supply boundaries. Specify which stage is purchased and which tests relate to that stage.

Ring forging and seamless pipe

An annular forging is ordered to a forging drawing and process route. A tubular shape does not by itself make the product compliant with a pipe or pressure-tube standard.

03 / Application review

Ti-6246 / TC19 for compressor and structural parts.

Define the required manufacturing stage and critical features first. Material, forging, heat treatment and inspection can then be evaluated as one purchasing scope.

Application review / 01

Compressor discs: define the blank and its critical zones

Ti-6246 / TC19 is relevant to compressor-disc material discussions where the released design specifies the alloy and manufacturing route. A buyer should define the delivered blank stage, the thickest section and the required structure before requesting price. The machining envelope and inspection zones help establish the stock allowance and the evidence needed for the next production stage.

Products to discuss

Forging stock, rough disc blanks, heat-treated forgings and agreed machining work. Identify a development blank separately from material for an approved production programme.

What we need to review

Drawing and specification revisions, hub and rim sections, process route, grain flow, test locations and orientations. Agree critical-zone NDT, dimensional datums, traceability and purchaser hold points before releasing production.

Send your application details

Application review / 02

Blade material: connect stock selection to final geometry

A Ti-6246 / TC19 blade enquiry should identify the released root and airfoil geometry, intended manufacturing sequence and the material condition required at delivery. The starting form must suit the approved process rather than simply fit around the finished part. Define the responsibilities for blank production, machining and final acceptance so competing quotations include the same work.

Products to discuss

Specified bar or forging blanks and drawing-based machining. Material supply can be separated from downstream processing when the buyer carries out the finishing operations.

What we need to review

Root and airfoil allowance, orientation, surface requirements, thermal processing, structure and required inspection. Include first-article evidence, approved-process constraints and marking methods that preserve item traceability.

Send your application details

Application review / 03

Engine seal and ring blanks: make the interface requirements explicit

Producer literature identifies Ti-6246 in compressor seal applications. For a purchasing enquiry, provide the complete annular geometry and the released requirements for the intended component. The review should distinguish a forged blank from a finished seal and connect interface dimensions, section changes and surface requirements with the specified material and process route.

Products to discuss

Ring forgings, annular blanks and reviewed machining work for defined seal or structural-ring requirements. Final component function and approval remain drawing-specific.

What we need to review

OD, ID, wall transitions, flange or seal-contact geometry, mating materials, thermal duty and inspection access. Agree machining allowance, heat-treatment stage, surface condition, NDT coverage and acceptance documents.

Send your application details

Application review / 04

Airframe stock: specify the load path and manufacturing stage

Ti-6246 / TC19 can be considered for airframe parts where it is selected by the design specification. For procurement, identify the finished geometry, the permitted stock form and the final material condition. Review any changes in section, critical interfaces and inspection access before choosing a bar or forging envelope. This lets the supply proposal describe the actual part-related requirements.

Products to discuss

Bars, disc or ring forgings and defined machined structural components. The order can cover starting stock only or an agreed sequence of manufacturing operations.

What we need to review

Material and process revision, critical sections, grain orientation, machining allowance, final heat treatment and surface finish. State fatigue-related or fracture-control evidence required by the drawing, together with customer source restrictions and first-article requirements.

Send your application details

Application review / 05

Cases and housings: confirm the approved material route first

For a Ti-6246 / TC19 case or housing enquiry, begin with the released material selection and drawing. A ring-shaped part is not sufficient evidence that any ring forging is suitable. The supply review should connect final wall and flange geometry, design duty and process requirements with the selected blank, then identify the inspection and approval stages that must be included in the quotation.

Products to discuss

Specified annular forgings, bar-derived housings and drawing-based machined parts where the customer’s material and manufacturing requirements permit the route.

What we need to review

Design metal temperature, mechanical and cyclic duty, section transitions, interfaces, tolerances and required structure. Agree blank inspection, tests after heat treatment, final dimensional records and any proof or assembly tests defined by the purchaser.

Send your application details

Application review / 06

Repeat machining orders: preserve the approved material basis

Repeat production is easier to compare when each order carries the same material and process baseline. For Ti-6246 / TC19 machining stock, identify the approved revision, delivered condition and required records, then list each cut size and quantity. Changes in source, section or heat treatment should be reviewed against the agreed requirements before material enters the buyer’s machining line.

Products to discuss

Bar and forging blanks supplied in specified lengths or envelopes, with optional rough or finish machining subject to the released scope.

What we need to review

Drawing revision, cut-size allowance, straightness, surface, lot marking and certificate linkage. Agree which changes require approval, how nonconforming items are recorded and the documents needed for each dispatch.

Send your application details

Application review / 07

Wire requirements: distinguish stock from finished-part performance

Ti-6246 structural-wire enquiries need to define the wire itself and the later component-making steps. The relevant material specification supplies a raw-product acceptance basis; it does not describe every formed or machined component’s functional performance. State the required diameter, condition and surface, then separately identify any finished-part loading, geometry or validation requirements included in the project.

Products to discuss

AMS 4981 wire within the ordered scope, coils or straight lengths and separately reviewed processing work. Welding filler is a different procurement category.

What we need to review

Diameter tolerance, cast or straightness, surface, condition, packaging and lot identity. Identify forming steps, final treatment, dimensional acceptance, sample quantities and any component tests to be priced separately.

Send your application details

Application review / 08

Trials: use a defined evaluation plan before production release

A Ti-6246 / TC19 development order should say what the buyer intends to establish from the first delivery. The objective may be to evaluate a forging envelope, a machining sequence or a specified inspection method. Agree the sample count and evidence before starting, then define the decision needed to move from trials to a repeat supply arrangement.

Products to discuss

Small batches of specified bar, forging stock, trial blanks and drawing-based test articles. Trial lead time and later production scheduling are reviewed separately.

What we need to review

Material and condition, test-piece locations, dimensional or process objectives, destructive-test allowance and reporting format. Record acceptable changes, retained samples, approval responsibility and the next-stage requirements.

Send your application details

Purchasing checklist

Define the manufacturing route behind the material name.

A Ti-6246 / TC19 quotation should make the product, final condition, processing boundary and acceptance evidence clear before the order is placed.

01

Material and dimensions

Alloy designation, product specification, revision, stock form, section and quantity.

02

Processing and responsibility

Blank drawing, forging route, heat treatment, machining stage and purchaser hold points.

03

Inspection and acceptance

Test locations, structure, NDT class, dimensions, traceability and required approval documents.

“We need TC19 blanks for compressor components.”

We would clarify whether the order covers stock, rough forgings or heat-treated blanks; review the released drawing, critical sections and process requirements; and agree mechanical sampling, NDT, machining allowance and approval milestones.

Illustrative requirement review; it is not a claim of flight qualification or a completed customer project.

Discuss your requirement

04 / Standards & documentation

Match the standard
to the product.

Select the actual product route and required revision. The available PDFs below support material review; the official AMS catalog identifies a product standard without offering an unverified full-standard download.

Reference files · Select a standard or technical reference to preview the supplied document.
Product formASTM / AMS / ASME routeChinese standard routeClarify before quotation
Material identityUnited States / technical reference

Ti-6246 · Ti-6Al-2Sn-4Zr-6Mo · UNS R56260.

ChinaGB/T 3620.1-2016View PDF ↗

TC19 chemical composition and designation.

Full alloy identity, analysis basis and complete specified limits.
Bars & structural wireUnited States / technical reference

AMS 4981 includes these forms within its specified size and condition requirements.

ChinaGB/T 3620.1-2016View PDF ↗

TC19 identity plus the agreed bar or wire product requirements.

Section, condition, surface, testing, quantity and lot identity.
Disc & ring forgingsUnited States / technical reference

AMS 4981 forging scope; select the correct revision and section limits.

ChinaGB/T 3620.1-2016View PDF ↗

TC19 chemistry with an agreed forging specification and process route.

Blank drawing, structure, test locations, grain flow and NDT coverage.
Forging stockUnited States / technical reference

AMS 4981 separately addresses stock for forging; identify the intended conversion route.

ChinaGB/T 3620.1-2016View PDF ↗

Agree the stock supply condition and conversion requirements.

Billet envelope, downstream process, responsibility and acceptance stage.
Machined componentsUnited States / technical reference

Material specification plus the released component and process requirements.

ChinaGB/T 3620.1-2016View PDF ↗

TC19 identity plus the same defined finished-part scope.

Interfaces, tolerances, final condition, records and customer approval.
Technical referenceUnited States / technical referenceTi-6Al-2Sn-4Zr-6Mo · producer technical dataView PDF ↗

Original producer data for Ti-6Al-2Sn-4Zr-6Mo; typical and historical references are identified.

China

Use the ordered TC19 product requirements for acceptance.

Confirm that any quoted data match the intended section and condition.
Agree the order basis.

The supplied GB/T 2965-2023 bar file does not list TC19, so it is not presented here as the TC19 product route. AMS conformity and finished-component approval are separate requirements.

Use the document edition, product scope and condition specified in the purchase order. Producer technical references support discussion; they do not replace ordered product acceptance requirements.

05 / Order coordination

Know the scope
before ordering.

Our founder’s 20 years in titanium inform the questions we ask before quotation and the supply options we review with you.

Ti-6246 / TC19 machined airframe & engine structures — application illustration
Component application illustration. Actual material records, inspection and performance tests are defined for the order.
A quotation you can evaluate

Agree the grade, standard edition, dimensions, tolerance, condition and quantity before comparing prices.

  • Identify whether inspection, samples and tooling are included.
  • Confirm packaging, transport and delivery terms.
  • Record items that still need technical confirmation.
Acceptance agreed before supply

Confirm the material certificate, full grade, heat or lot identity, delivery condition, dimensional checks and required testing before supply starts. Define any process records, NDT and purchaser approval points for the ordered product.

Independent inspection can be discussed with its scope, timing, acceptance criteria and cost agreed for the order.

Delivery with clear milestones

Review the proposed lead time, approvals, production sequence and dispatch requirements. For several product forms, coordinate document and packing readiness together.

Material substitutions and technical changes require written approval. A schedule deviation should identify the impact, decisions needed and next steps.

One contact when an issue arises

Contact TiHubs with the order reference, affected items and supporting photos or inspection records.

We record the issue, review it against the agreed requirements and coordinate the next steps with the relevant manufacturing parties.

01 / Material identity

Material records

Grade, standard, test results and heat or batch identity matched to the supplied items.

  • Material certificate
  • Heat / batch ID
  • Test results
02 / Agreed acceptance

Inspection records

Dimensional and testing records for the agreed scope, including critical drawing requirements.

  • Dimensions
  • Agreed testing
  • Acceptance criteria
03 / Ready for dispatch

Dispatch records

Item identification, packing list, protective packaging and required shipment documents.

  • Packing list
  • Item labels
  • Shipping documents

06 / Questions before sourcing

Before you specify
Ti-6246 / TC19.

A clear material designation is the beginning. Product form, specification revision, material condition and acceptance complete the requirement.

A useful first enquiry

  • Product and specificationProduct form, standard edition, dimensions and material condition.
  • Order and deliveryQuantity, destination and any required delivery date.
  • Acceptance requirementsDrawing revision, inspection, certificates and packaging.

Not every detail is finalized? Send the information you have. We can help identify the questions to resolve before quotation.

Discuss your requirement

What happens next: requirement review, technical clarification, then a supply proposal and quotation.

What is Ti-6246 / TC19 titanium?

Ti-6246 / TC19 is the Ti-6Al-2Sn-4Zr-6Mo alpha-beta titanium alloy family, identified as UNS R56260 for Ti-6246. Specify the product form, standard revision, delivered condition and required manufacturing records with the alloy name.

What are its main aerospace applications?

Key producer references include intermediate compressor discs, blades and seals, together with airframe parts. TiHubs reviews material and processing requirements against the purchaser’s released drawings. A potential application does not establish approval for a specific engine or airframe part.

Which products can I enquire about?

Bar, rod, disc and ring forging blanks, forging stock and structural wire are the main forms shown here. Send dimensions, quantity, condition and inspection requirements. Sheet, conventional tube or other forms require a separate product-route review rather than assuming the bar or forging specification applies.

Which standard applies to Ti-6246 bar and forgings?

AMS 4981 covers the specified bar, wire, forgings and forging stock, subject to its product and section limits. SAE lists revision K dated October 2026; use the revision required by the drawing or purchase order. TC19 material identity is defined in GB/T 3620.1, with the actual product requirements specified separately.

How does Ti-6246 differ from Ti-6242S?

Ti-6246 has a nominal 6% molybdenum addition; Ti-6242S has 2% molybdenum with a small silicon addition. Their processing and acceptance requirements differ. Use the full alloy designation and approved product specification instead of treating the abbreviated names as substitutes.

What strength or heat-treatment condition should I order?

Use the acceptance table and condition required by the applicable product specification and drawing. Section size, test direction and manufacturing history affect the requirements. Producer examples are useful for review but should not be copied as a universal tensile value for every bar, forging or finished part.

Can you supply engine casings or finished compressor parts?

Provide the released part and blank drawings, material and process specifications, required supply stage and customer approval requirements. TiHubs reviews the relevant manufacturing resources and evidence needed for that scope. The enquiry may cover source material, a machined blank or additional processing, with qualification requirements agreed explicitly.

What inspection and traceability should be included?

Define chemistry and mechanical records, test locations, heat-treatment evidence, structure, NDT class and coverage, dimensions and lot or item identity. Add any purchaser-source approval, special-process or first-article requirements. The final document package must correspond to the actual supplied material and processing scope.

How do I request a quotation and delivery plan?

Send the drawing or stock form, Ti-6246 or TC19 designation, specification revision, dimensions, condition, quantity and destination. Include the inspection and approval stages. We clarify the missing details and confirm material, processing, samples, documentation and proposed delivery milestones in the quotation.

07 / Your next step

Start with the
requirement you have.

Send the product details, drawing or operating conditions you already know. We will identify missing information and discuss a suitable supply route before quotation.

  1. Requirement review
  2. Technical clarification
  3. Supply proposal and quotation

Combine materials and parts in one enquiry.

Send one list of Ti-6246 / TC19 forms, sizes and quantities. Include drawing revisions and items that need to be supplied together.

Define the condition and acceptance priorities.

Include the ordered specification, final application, material condition, inspection and documentation, destination and required delivery milestones.

Baoji, China · info@tihubs.com

Start your Ti-6246 / TC19 enquiry

Send your material form, drawing or process conditions. We will help clarify the remaining requirements.

Customer Feedback & RFQ Form (#6)