TC24 / Ti-4.5Al-3V-2Fe-2Mo titanium products on a dark metallic background

TC24 / Ti-4.5Al-3V-2Fe-2Mo · Beta-rich alpha-beta titanium alloy

TC24 / Ti-4.5Al-3V-2Fe-2Mo. Stock for complex forming.

Source TC24 sheet, plate, bar and forming blanks. Connect the SP700 alloy family to the required microstructure, forming route and final-part inspection.

Start with a specification, drawing or application. We’ll help identify the details still needed.

Material review. Supply coordination.
One contact in Baoji, China.

TC24 / Ti-4.5Al-3V-2Fe-2MoTi-4.5Al-3V-2Fe-2Mo · SP700 family
Beta-rich alpha-beta titanium alloySheet forming & precision conversion
One contact20 years of founder experience · 100+ Baoji factories

01 / Product forms

Find your TC24 product.

Choose a material form or application. Send the dimensions, service conditions and required records so we can match the manufacturing route to your order.

TC24 titanium sheet — illustrative supply form
01 / 06

TC24 / Ti-4.5Al-3V-2Fe-2Mo

TC24 titanium sheet

Thin flat stock for qualified forming and development programmes that specify the SP700 alloy family.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Thickness, width, length, flatness, rolling direction and edge condition.
Manufacturing review
State whether superplastic forming, conventional bending or machining is intended; specify the required stock structure.
Inspection priorities
Thickness uniformity, surface condition, directional properties and the agreed microstructure or forming tests.
TC24 plate & flat blanks — illustrative supply form
02 / 06

TC24 / Ti-4.5Al-3V-2Fe-2Mo

TC24 plate & flat blanks

Plate and cut stock for drawing-approved machining or conversion, subject to actual thickness availability.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Thickness, usable width and length, flatness and cutting allowance.
Manufacturing review
Identify rolling direction, pocketing, thermal processing and distortion limits.
Inspection priorities
Directional mechanical testing, surface quality, internal examination where specified and usable dimensions.
TC24 titanium bar — illustrative supply form
03 / 06

TC24 / Ti-4.5Al-3V-2Fe-2Mo

TC24 titanium bar

Round machining stock for approved precision parts and process-development components.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Diameter, cut length, tolerance, straightness and surface finish.
Manufacturing review
Define delivered condition, downstream forging or machining and final thermal treatment.
Inspection priorities
Structure and mechanical results for the ordered condition, dimensions and traceability.
TC24 conversion billet — illustrative supply form
04 / 06

TC24 / Ti-4.5Al-3V-2Fe-2Mo

TC24 conversion billet

Billet enquiries for controlled forging routes and project-specific preforms.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Section, length, cut weight, cropping and test-stock allowance.
Manufacturing review
Agree deformation plan, process controls and final section before comparing raw-stock prices.
Inspection priorities
Incoming chemistry, structure, surface quality and specified internal examination.
TC24 formed-panel enquiries — illustrative supply form
05 / 06

TC24 / Ti-4.5Al-3V-2Fe-2Mo

TC24 formed-panel enquiries

Application illustration: a simple formed panel representing a drawing-controlled conversion route.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Panel envelope, radii, minimum wall, trim allowance and datum system.
Manufacturing review
Review stock structure, tooling, forming cycle, oxidation protection and post-forming treatment.
Inspection priorities
Thickness distribution, dimensional conformity, surface integrity and agreed mechanical checks after forming.
TC24 custom structural blanks — illustrative supply form
06 / 06

TC24 / Ti-4.5Al-3V-2Fe-2Mo

TC24 custom structural blanks

Application illustration: rough-machined brackets and precision blanks to an approved design.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Drawing revision, critical features, usable stock and first-article quantity.
Manufacturing review
Identify whether the geometry is machined from stock or converted through a qualified forming or forging route.
Inspection priorities
Require heat and lot identity, full chemical analysis, delivery condition, dimensional results and the agreed mechanical and structural tests. Define NDT method, coverage and acceptance criteria in the order.

Images illustrate material forms and application possibilities. Reference markings identify specification options; they do not establish dual certification, stock availability or approval of finished equipment.

Define the shape. Share the service.

These details help turn a material enquiry into a comparable quotation.

01 / Drawing review

Drawing-controlled blanks

Provide rough and finished drawings, datum positions, critical sections, machining allowance and the intended conversion route.

Discuss your drawing

02 / Drawing review

Heat treatment & process sequence

Identify the required delivery condition and subsequent manufacturing steps. Agree process records, sampling stages and dimensional checks after thermal processing.

Discuss your drawing

03 / Drawing review

Component inspection planning

Specify surface integrity, microstructure, NDT, dimensional acceptance and traceability. Identify which tests apply to raw material and which apply to the finished component.

Discuss your drawing

02 / Material identity

What is TC24 / Ti-4.5Al-3V-2Fe-2Mo titanium?

TC24 has the nominal composition Ti-4.5Al-3V-2Fe-2Mo, associated with the internationally known SP700 alloy family. Its purchasing focus is formable titanium stock, especially sheet for qualified forming processes and bar or billet for controlled conversion. Superplastic behaviour depends on stock structure and processing conditions; it is not an automatic property guarantee for every TC24 product.

Specify the exact standard edition, form and delivery condition. Nominal chemistry is only one part of an order; strength, microstructure, dimensional acceptance and traceability also need to be defined.

Review itemOrder basisWhat to confirm
Material conditionDefine the ordered heat-treatment stateTie test results to the same conversion and thermal history as the supplied product.
Strength and ductilityProduct- and section-dependentSpecify tensile, proof strength, elongation, sampling location and test direction in the purchase requirement.
MicrostructureAgree acceptance limitsReview grain structure, alpha morphology, surface alpha case and metallographic sampling for the manufacturing route.
Fatigue and fractureApplication-specific validationA material tensile certificate does not establish component life. Specify any fatigue, toughness or crack-growth evaluation separately.
Non-destructive examinationDrawing / product specificationDefine method, calibration, coverage, acceptance class and reporting before production.
Selected element · wt %Reference composition
Aluminium · Al4.0–5.0
Vanadium · V2.5–3.5
Iron · Fe1.7–2.3
Molybdenum · Mo1.8–2.2
Oxygen · O0.15 max
Titanium · TiBalance

Selected composition limits, wt %, from GB/T 3620.1-2016. Use the complete ordered standard for all impurity, residual-element and analysis requirements.

TC24 and SP700

These names identify the related Ti-4.5Al-3V-2Fe-2Mo alloy family. Compare full chemistry, product condition, process pedigree and acceptance requirements before dual certification or substitution.

Compared with Ti-6Al-4V

The alloy system and forming response differ from TC4 / Grade 5. A qualified Ti-6Al-4V forming cycle cannot simply be transferred to TC24 stock.

Fine-grained forming stock

Specify microstructure and forming evidence when the intended route relies on superplasticity. A generic annealed sheet certificate may not address the complete forming requirement.

Stock versus formed component

A sheet, forged blank and formed panel have different dimensional and acceptance needs. Separate incoming material tests from thickness distribution, distortion and surface inspection after conversion.

03 / Application priorities

TC24 in application.

Review each main use through its service conditions, material choice, manufacturing route and acceptance plan. These are sourcing discussions; approved drawings and qualification requirements govern the final component.

Application review / 01

Superplastic sheet forming

Sheet forming is a priority TC24 enquiry where the approved process calls for the SP700 alloy family. The practical purchasing question is whether the supplied structure and thickness support the specified forming trial and final geometry.

Products & manufacturing

Fine-structure sheet and cut forming blanks, with supply capability and test requirements confirmed.

Service & design review

Provide panel depth, radii, target wall distribution, tooling envelope and process specification. Agree stock structure, forming validation and final treatment without assuming a universal production cycle.

Purchase & inspection priorities

Inspect incoming sheet and then verify formed thickness, dimensions, surface integrity and the project-specific property requirements.

Send your application details

Application review / 02

Complex lightweight panels

A formed panel may reduce machining demand for a particular design, but the benefit depends on the permitted manufacturing route and achievable wall distribution. TC24 stock must be tied to those drawing requirements.

Products & manufacturing

Sheet, trim blanks and drawing-controlled formed panels.

Service & design review

Share the CAD model, datum scheme, minimum wall, local radii, trimming and joining requirements. Identify whether trial tooling and first-article inspection are included in the enquiry.

Purchase & inspection priorities

Agree profile, thickness mapping, surface examination and any joining or post-forming tests. A stock certificate does not release the complete assembly.

Send your application details

Application review / 03

Conventional bending & forming

SP700-family material is also discussed for formability outside a superplastic process. For a specific TC24 part, bend radius, stock condition and direction still need a validated manufacturing plan.

Products & manufacturing

Sheet and cut blanks for approved bending or forming trials.

Service & design review

Specify bend geometry, edge preparation, rolling direction, springback allowance and any intermediate treatment. Use representative material when qualifying a new thickness or source.

Purchase & inspection priorities

Review surface cracking, dimensional stability and properties after the agreed process. Do not infer an unrestricted bend limit from nominal alloy chemistry.

Send your application details

Application review / 04

Forged precision preforms

Bar or billet can be considered for project-approved hot-conversion routes. Incoming structure, deformation and thermal history must be controlled together to support the final blank requirements.

Products & manufacturing

Bar, billet and rough preforms against a defined conversion plan.

Service & design review

Provide final section, deformation direction, stock utilization, heat-treatment sequence and specimen positions. Confirm the actual product range before setting a delivery date.

Purchase & inspection priorities

Require chemistry, structure and surface acceptance on incoming stock, then define the checks after conversion.

Send your application details

Application review / 05

Fatigue-sensitive machined parts

For cyclically loaded components specified in TC24, the material route and surface condition need to be connected to the approved design. A reference fatigue result does not establish the life of a new geometry.

Products & manufacturing

Bar, plate and drawing-controlled machining blanks.

Service & design review

State load directions, critical fillets, surface finish, thermal condition and final inspection stage. Define any required component or coupon fatigue programme separately.

Purchase & inspection priorities

Use representative sampling, controlled surface preparation and traceable material records. Evaluate results within the specified qualification scope.

Send your application details

Application review / 06

Sporting-goods material review

SP700 has documented sporting-goods applications, including golf-club face material. A new TC24 enquiry should identify the actual design, forming route and applicable product rules before committing stock.

Products & manufacturing

Sheet and flat blanks for an approved sporting-goods development programme.

Service & design review

Provide thickness, face geometry, joining details, forming and thermal treatment. Confirm the finished product requirements with the responsible designer.

Purchase & inspection priorities

Agree dimensions, surface quality and the specified durability tests. Illustrations do not indicate that a finished sporting product is stocked or approved.

Send your application details

Application review / 07

Forming-process qualification

A representative trial is useful when moving from an alloy reference to a production TC24 component. Sheet thickness, microstructure and process history should match the intended recurring supply.

Products & manufacturing

Trial sheet lots, cut blanks and retained material for comparative testing.

Service & design review

Identify the controlled variables, test geometry, inspection stages and approval authority. Record acceptable changes in stock source and processing.

Purchase & inspection priorities

Compile incoming, forming and final-condition results so the accepted route can be reproduced.

Send your application details

Application review / 08

Repeat sheet & blank orders

Recurring TC24 procurement needs consistent material condition and clear revision control. Keep sheet, plate, bar and converted blanks as separate order lines with their respective release requirements.

Products & manufacturing

Scheduled stock and approved blanks against an itemized requirement.

Service & design review

State dimensions, quantities, standard editions, condition, marking, packaging and delivery sequence. Identify changes that require technical approval.

Purchase & inspection priorities

Match material certificates, piece or bundle markings, inspection results and packing lists before dispatch.

Send your application details
Material references and applicable product standards are listed below. Select the delivery condition and acceptance plan for the specific product and approved application.

TC24 procurement checklist

Connect the application to the material order.

A useful specification connects the intended component, the supplied stock and the acceptance evidence. Share the drawing and known requirements first.

01

Define the application

Provide panel depth, radii, target wall distribution, tooling envelope and process specification. Agree stock structure, forming validation and final treatment without assuming a universal production cycle.

02

Define the supplied stage

Fine-structure sheet and cut forming blanks, with supply capability and test requirements confirmed. Distinguish raw stock, converted blanks and finished parts. Define who controls subsequent processing.

03

Define the acceptance evidence

Inspect incoming sheet and then verify formed thickness, dimensions, surface integrity and the project-specific property requirements.

Example: a useful TC24 material enquiry

TC24 titanium sheet; required dimensions and quantity; standard and drawing revision; delivery condition; intended downstream process; mechanical, structural and dimensional acceptance; traceability, destination and required date.

Identify the approved product specification and any project-specific qualification. The grade designation and chemistry standard alone do not define component acceptance.

Discuss your material requirement ↗

04 / Standards & documentation

Match the standard
to the product.

Choose the specification by product form, material condition and application. Identify the required edition on the order; a chemistry standard alone does not define a finished forging or component.

Hosted PDFs retain their stated editions. Publisher references open separately when no distributable PDF is provided.
Product / reviewInternational / project routeChinese referenceClarify before quotation
Identity & chemistryApproved product and project specificationGB/T 3620.1-2016View PDF ↗Review the complete chemical limits and product requirements; nominal alloy names do not establish automatic interchangeability.
JFE SP700 technical referenceJFE SP700 technical referenceView PDF ↗Project and product requirements remain separately definedManufacturer reference on the SP700 alloy family and applications. Reference information only; TC24 supply and acceptance require a separate agreed specification.
Drawing-based blanks & partsApproved drawing and controlled manufacturing planAgreed product / project specificationDefine the supply stage, conversion route, heat treatment, structure, NDT, dimensions and traceability. Material certification is separate from finished component qualification.
Agree the order basis.

The purchase order must identify the required revision, grade, product form, condition and inspection. Reference documents do not replace design approval, manufacturing qualification or application-specific acceptance.

Request the controlled specification revision for your order. Any substitution, equivalence or dual-certification claim requires a documented comparison and agreement.

05 / Order coordination

Know the scope
before ordering.

Our founder’s 20 years in titanium inform the questions we ask before quotation and the supply options we review with you.

TC24 custom structural blanks — application illustration
Component application illustration. Actual material records, inspection and performance tests are defined for the order.
A quotation you can evaluate

Agree the grade, standard edition, dimensions, tolerance, condition and quantity before comparing prices.

  • Identify whether inspection, samples and tooling are included.
  • Confirm packaging, transport and delivery terms.
  • Record items that still need technical confirmation.
Acceptance agreed before supply

Confirm material identity, delivery condition, heat-to-piece traceability, dimensional checks and required testing before production. For converted parts, define inspection after forging, heat treatment and machining, including the specified microstructure and NDT scope.

Independent inspection can be discussed with its scope, timing, acceptance criteria and cost agreed for the order.

Delivery with clear milestones

Review the proposed lead time, approvals, production sequence and dispatch requirements. For several product forms, coordinate document and packing readiness together.

Material substitutions and technical changes require written approval. A schedule deviation should identify the impact, decisions needed and next steps.

One contact when an issue arises

Contact TiHubs with the order reference, affected items and supporting photos or inspection records.

We record the issue, review it against the agreed requirements and coordinate the next steps with the relevant manufacturing parties.

01 / Material identity

Material records

Grade, standard, test results and heat or batch identity matched to the supplied items.

  • Material certificate
  • Heat / batch ID
  • Test results
02 / Agreed acceptance

Inspection records

Dimensional and testing records for the agreed scope, including critical drawing requirements.

  • Dimensions
  • Agreed testing
  • Acceptance criteria
03 / Ready for dispatch

Dispatch records

Item identification, packing list, protective packaging and required shipment documents.

  • Packing list
  • Item labels
  • Shipping documents

06 / Questions before sourcing

Before you specify
TC24 / Ti-4.5Al-3V-2Fe-2Mo.

A clear material designation is the beginning. Product form, specification revision, material condition and acceptance complete the requirement.

A useful first enquiry

  • Product and specificationProduct form, standard edition, dimensions and material condition.
  • Order and deliveryQuantity, destination and any required delivery date.
  • Acceptance requirementsDrawing revision, inspection, certificates and packaging.

Not every detail is finalized? Send the information you have. We can help identify the questions to resolve before quotation.

Discuss your requirement

What happens next: requirement review, technical clarification, then a supply proposal and quotation.

What is TC24 titanium?

TC24 has the nominal composition Ti-4.5Al-3V-2Fe-2Mo, associated with the internationally known SP700 alloy family. Its purchasing focus is formable titanium stock, especially sheet for qualified forming processes and bar or billet for controlled conversion. Superplastic behaviour depends on stock structure and processing conditions; it is not an automatic property guarantee for every TC24 product.

Is TC24 also called SP700?

TC24 is associated with the Ti-4.5Al-3V-2Fe-2Mo / SP700 alloy family. Full specification, condition and processing requirements must be compared before declaring interchangeability.

Which product forms should I enquire about?

Sheet is the main forming-stock focus. Plate, bar, billet and drawing-based blanks are reviewed against dimensions, condition and confirmed capability.

Is every TC24 sheet superplastic forming grade?

No. The required structure, thickness and forming behaviour must be specified and demonstrated for the approved process. A generic grade designation is insufficient.

Can TC4 forming parameters be reused?

Do not assume that a Ti-6Al-4V process is transferable. TC24 has a different alloy system; the responsible manufacturer must qualify the material and forming route.

What matters when ordering formed panels?

Provide geometry, minimum wall, radii, datums, trim allowance, material condition and inspection. Include thickness mapping and surface acceptance after forming.

Can TiHubs coordinate machined blanks?

Supply the drawing, stock specification, quantity and delivered stage. We review the permitted route and supply capability before confirming the quotation.

Are datasheet fatigue values a component guarantee?

No. Geometry, condition, surface finish and loading affect performance. Use project-specific design and qualification requirements for finished components.

What belongs in a TC24 RFQ?

Include form, dimensions, quantity, standard and drawing revisions, condition, intended forming or machining route, inspection, destination and required timing.

07 / Your next step

Start with the
requirement you have.

Send the product details, drawing or operating conditions you already know. We will identify missing information and discuss a suitable supply route before quotation.

  1. Requirement review
  2. Technical clarification
  3. Supply proposal and quotation

Combine materials and parts in one enquiry.

Send one list of TC24 forms, sizes and quantities. Include drawing revisions, material conditions and items that must be supplied or dispatched together.

Share the service and acceptance priorities.

Include load and temperature conditions, critical sections, required material records, process qualification, inspection, destination and timing.

Baoji, China · info@tihubs.com

Start your TC24 / Ti-4.5Al-3V-2Fe-2Mo enquiry

Send your material form, drawing or process conditions. We will help clarify the remaining requirements.

Customer Feedback & RFQ Form (#6)