TC16 Titanium Alloy titanium products on a dark metallic background

TC16 Titanium Alloy · Alpha-beta titanium alloy

TC16 Titanium Alloy. Material for fastener manufacture.

Source TC16 bar, fastener wire and conversion stock with the forming route, heat-treatment condition and inspection agreed before production.

Start with a specification, drawing or application. We’ll help identify the details still needed.

Material review. Supply coordination.
One contact in Baoji, China.

TC16 Titanium AlloyTi-3Al-5Mo-4.5V
Alpha-beta titanium alloyAircraft fasteners & precision hardware
One contact20 years of founder experience · 100+ Baoji factories

01 / Product forms

Find your TC16 product.

Choose a material form or application. Send the dimensions, service conditions and required records so we can match the manufacturing route to your order.

TC16 titanium bar — illustrative supply form
01 / 06

TC16 Titanium Alloy

TC16 titanium bar

Round stock for machined bolts, pins and drawing-controlled hardware. Quote usable size and condition, not diameter alone.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Diameter, cut length, tolerance, straightness and turned or ground surface.
Manufacturing review
State machining sequence, thread method and any subsequent thermal treatment.
Inspection priorities
Surface integrity, dimensional consistency, material condition and heat-to-piece identity.
TC16 fastener wire — illustrative supply form
02 / 06

TC16 Titanium Alloy

TC16 fastener wire

Coiled or straight wire for qualified aerospace fastener manufacturing. Surface condition and forming consistency are key procurement priorities.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Diameter, coil mass, cast and helix, straight-length option and packaging.
Manufacturing review
Provide heading geometry, reduction stages, lubrication needs and intermediate annealing requirements.
Inspection priorities
Diameter, surface defects, ductility in the ordered condition and lot-specific testing.
TC16 forging billet — illustrative supply form
03 / 06

TC16 Titanium Alloy

TC16 forging billet

Conversion stock for drawing-approved preforms, subject to the proposed size and downstream route.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Billet diameter, length, cut weight, end allowance and surface preparation.
Manufacturing review
Define deformation route, cropping allowance and the condition required after conversion.
Inspection priorities
Incoming structure, chemistry, surface quality and specified internal examination.
TC16 bolt & pin blanks — illustrative supply form
04 / 06

TC16 Titanium Alloy

TC16 bolt & pin blanks

Application illustration: headed bolt blanks and precision pin stock manufactured to the agreed drawing.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Head and shank geometry, grip length, datums and thread allowance.
Manufacturing review
Separate blank supply from thread formation, final heat treatment, surface treatment and finished-fastener qualification.
Inspection priorities
Critical transitions, dimensions and traceability; proof and fatigue tests only to the specified finished-part plan.
TC16 straight rod stock — illustrative supply form
05 / 06

TC16 Titanium Alloy

TC16 straight rod stock

Straight lengths for repetitive precision-hardware production and controlled machine feeding.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Diameter tolerance, straightness, end condition, length distribution and bundle marking.
Manufacturing review
Confirm centerless grinding, straightening and cutting responsibilities before accepting a production lot.
Inspection priorities
Dimensional capability, surface finish and consistent identity across cut lengths.
TC16 custom machining blanks — illustrative supply form
06 / 06

TC16 Titanium Alloy

TC16 custom machining blanks

Application illustration: stepped and rough-machined blanks for project-specific hardware.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Drawing envelope, datum faces, minimum machining allowance and sample quantity.
Manufacturing review
Review stock removal, stabilization, inspection access and final processing responsibility.
Inspection priorities
Require heat and lot identity, full chemical analysis, delivery condition, dimensional results and the agreed mechanical and structural tests. Define NDT method, coverage and acceptance criteria in the order.

Images illustrate material forms and application possibilities. Reference markings identify specification options; they do not establish dual certification, stock availability or approval of finished equipment.

Define the shape. Share the service.

These details help turn a material enquiry into a comparable quotation.

01 / Drawing review

Drawing-controlled blanks

Provide rough and finished drawings, datum positions, critical sections, machining allowance and the intended conversion route.

Discuss your drawing

02 / Drawing review

Heat treatment & process sequence

Identify the required delivery condition and subsequent manufacturing steps. Agree process records, sampling stages and dimensional checks after thermal processing.

Discuss your drawing

03 / Drawing review

Component inspection planning

Specify surface integrity, microstructure, NDT, dimensional acceptance and traceability. Identify which tests apply to raw material and which apply to the finished component.

Discuss your drawing

02 / Material identity

What is TC16 Titanium Alloy titanium?

TC16 is a Chinese alpha-beta titanium alloy with the nominal composition Ti-3Al-5Mo-4.5V. Fastener stock is a priority purchasing direction: the material must support the approved heading, machining, thread-forming and thermal-processing sequence. A bar or wire certificate establishes the supplied material condition; finished fastener acceptance remains a separate requirement.

Specify the exact standard edition, form and delivery condition. Nominal chemistry is only one part of an order; strength, microstructure, dimensional acceptance and traceability also need to be defined.

Review itemOrder basisWhat to confirm
Material conditionDefine the ordered heat-treatment stateTie test results to the same conversion and thermal history as the supplied product.
Strength and ductilityProduct- and section-dependentSpecify tensile, proof strength, elongation, sampling location and test direction in the purchase requirement.
MicrostructureAgree acceptance limitsReview grain structure, alpha morphology, surface alpha case and metallographic sampling for the manufacturing route.
Fatigue and fractureApplication-specific validationA material tensile certificate does not establish component life. Specify any fatigue, toughness or crack-growth evaluation separately.
Non-destructive examinationDrawing / product specificationDefine method, calibration, coverage, acceptance class and reporting before production.
Selected element · wt %Reference composition
Aluminium · Al2.2–3.8
Molybdenum · Mo4.5–5.5
Vanadium · V4.0–5.0
Iron · Fe0.25 max
Oxygen · O0.15 max
Titanium · TiBalance

Selected composition limits, wt %, from GB/T 3620.1-2016. Use the complete ordered standard for all impurity, residual-element and analysis requirements.

Chinese designation first

Keep TC16 and the applicable product specification on the purchase order. A foreign designation or simplified nominal formula requires a complete comparison before substitution.

Formability versus final strength

Starting stock intended for heading may require a different condition from a finished load-carrying fastener. Define both states and the responsible processing stages.

Wire versus machined bar

Coiled wire supports a qualified forming route; straight bar may support machining. Material utilization, surface condition and lot testing differ between these routes.

TC16 is not Grade 16

ASTM Grade 16 is a different, palladium-bearing commercially pure titanium grade. Similar numbers do not establish material equivalence.

03 / Application priorities

TC16 in application.

Review each main use through its service conditions, material choice, manufacturing route and acceptance plan. These are sourcing discussions; approved drawings and qualification requirements govern the final component.

Application review / 01

Aircraft bolt manufacture

TC16 procurement should begin with the approved bolt drawing and manufacturing route. The head-to-shank transition, thread root and final thermal state each affect the evidence required from the material and finished fastener.

Products & manufacturing

Wire for an approved heading process; bar and straight rod for machined bolt routes.

Service & design review

Identify head geometry, grip length, thread manufacturing method, forming steps and final condition. Agree which operations TiHubs coordinates and which remain with the fastener manufacturer.

Purchase & inspection priorities

Define incoming surface and material tests separately from finished-bolt dimensional, proof, tensile and fatigue acceptance.

Send your application details

Application review / 02

Precision pins & joint hardware

Pins transfer load through controlled fits and bearing surfaces. For a TC16 pin, usable bar diameter, straightness and the finishing allowance are practical purchasing priorities.

Products & manufacturing

Ground bar, straight rod and stepped machining blanks.

Service & design review

Provide fit tolerances, mating materials, critical radii and surface-treatment requirements. Identify whether the part is finished in the delivered material state or heat treated after rough machining.

Purchase & inspection priorities

Require dimensional reports, surface inspection at fatigue-sensitive locations and material records linked to the finished pieces.

Send your application details

Application review / 03

Cold-heading stock review

A forming-stock enquiry must describe the planned deformation. A material label alone does not guarantee that a particular head geometry can be produced without cracking or unacceptable surface damage.

Products & manufacturing

Coiled TC16 wire, cut wire lengths and representative trial lots.

Service & design review

State initial diameter, upset ratio, head form, tooling sequence and permitted intermediate treatments. Agree a representative forming trial when introducing a new source or size.

Purchase & inspection priorities

Evaluate incoming surface defects, material condition, formed-head integrity and dimensional consistency against the approved trial plan.

Send your application details

Application review / 04

Thread-forming coordination

Thread rolling and machining place different demands on stock condition and blank dimensions. The purchase order should identify the permitted route and the point at which final heat treatment occurs.

Products & manufacturing

Wire-derived or machined shank blanks with controlled thread allowance.

Service & design review

Share thread standard, pitch, engagement, root requirements and the approved processing sequence. Define how blank diameter and surface preparation are accepted before threading.

Purchase & inspection priorities

Inspect thread geometry and surface integrity under the drawing requirements. Retain raw-stock identity through each conversion stage.

Send your application details

Application review / 05

Heat-treatment handover

TC16 stock and finished fasteners may be delivered at different manufacturing stages. Confusion between these conditions can make two quotations or certificates appear comparable when they are not.

Products & manufacturing

Bar, wire and blanks supplied in the explicitly ordered condition.

Service & design review

List the thermal process specification, section range, processing owner and any post-treatment straightening or machining. Include distortion allowance and final inspection stage.

Purchase & inspection priorities

Match mechanical and structural results to the actual delivered condition. Later thermal processing needs its own acceptance basis.

Send your application details

Application review / 06

Forged preforms

Billet and preforms can support a qualified hardware route when their incoming structure and surface preparation are appropriate for conversion. The finished preform needs separate dimensional and material release.

Products & manufacturing

Billet, cut conversion stock and drawing-controlled preforms.

Service & design review

Define usable volume, deformation direction, end cropping, final section and specimen locations. Confirm the proposed supply capability before fixing a schedule.

Purchase & inspection priorities

Agree incoming NDT and structure checks, then identify the testing required after forging and thermal processing.

Send your application details

Application review / 07

First-article fastener lots

A trial lot should reproduce the planned production stock and process. A small successful sample from an unrelated diameter or condition does not establish the suitability of a new recurring order.

Products & manufacturing

Representative wire, bar and blank quantities with retained test stock.

Service & design review

Agree source requirements, drawing revision, manufacturing variables, inspection hold points and the approval authority before sampling.

Purchase & inspection priorities

Compile raw-material, processing and finished-part results for the defined project. Keep any later source or process change within the agreed review procedure.

Send your application details

Application review / 08

Repeat hardware procurement

Recurring TC16 orders benefit from a stable item list and explicit material-condition codes. Separate wire, straight rod and finished blanks so dimensions, inspection and delivery commitments remain clear.

Products & manufacturing

Scheduled lots of wire, bar, rod and approved blanks.

Service & design review

Provide item numbers, quantities, standard editions, delivery sequence, package sizes and certificate language. Specify how mixed heats must be separated.

Purchase & inspection priorities

Reconcile physical markings, heat numbers, test reports and packing lists before dispatch.

Send your application details
Material references and applicable product standards are listed below. Select the delivery condition and acceptance plan for the specific product and approved application.

TC16 procurement checklist

Connect the application to the material order.

A useful specification connects the intended component, the supplied stock and the acceptance evidence. Share the drawing and known requirements first.

01

Define the application

Identify head geometry, grip length, thread manufacturing method, forming steps and final condition. Agree which operations TiHubs coordinates and which remain with the fastener manufacturer.

02

Define the supplied stage

Wire for an approved heading process; bar and straight rod for machined bolt routes. Distinguish raw stock, converted blanks and finished parts. Define who controls subsequent processing.

03

Define the acceptance evidence

Define incoming surface and material tests separately from finished-bolt dimensional, proof, tensile and fatigue acceptance.

Example: a useful TC16 material enquiry

TC16 titanium bar; required dimensions and quantity; standard and drawing revision; delivery condition; intended downstream process; mechanical, structural and dimensional acceptance; traceability, destination and required date.

Identify the approved product specification and any project-specific qualification. The grade designation and chemistry standard alone do not define component acceptance.

Discuss your material requirement ↗

04 / Standards & documentation

Match the standard
to the product.

Choose the specification by product form, material condition and application. Identify the required edition on the order; a chemistry standard alone does not define a finished forging or component.

Hosted PDFs retain their stated editions. Publisher references open separately when no distributable PDF is provided.
Product / reviewInternational / project routeChinese referenceClarify before quotation
Identity & chemistryApproved product and project specificationGB/T 3620.1-2016View PDF ↗Review the complete chemical limits and product requirements; nominal alloy names do not establish automatic interchangeability.
BaoTi fastener-stock referenceBaoTi fastener-stock referencePublisher reference ↗Compare the complete ordered Chinese requirementsManufacturer catalogue identifies TC16 coiled wire for aerospace fasteners. Confirm the standard assigned to the specific grade and order; a grouped catalogue list is not a TiHubs inventory or certification claim.
Drawing-based blanks & partsApproved drawing and controlled manufacturing planAgreed product / project specificationDefine the supply stage, conversion route, heat treatment, structure, NDT, dimensions and traceability. Material certification is separate from finished component qualification.
Agree the order basis.

The purchase order must identify the required revision, grade, product form, condition and inspection. Reference documents do not replace design approval, manufacturing qualification or application-specific acceptance.

Request the controlled specification revision for your order. Any substitution, equivalence or dual-certification claim requires a documented comparison and agreement.

05 / Order coordination

Know the scope
before ordering.

Our founder’s 20 years in titanium inform the questions we ask before quotation and the supply options we review with you.

TC16 custom machining blanks — application illustration
Component application illustration. Actual material records, inspection and performance tests are defined for the order.
A quotation you can evaluate

Agree the grade, standard edition, dimensions, tolerance, condition and quantity before comparing prices.

  • Identify whether inspection, samples and tooling are included.
  • Confirm packaging, transport and delivery terms.
  • Record items that still need technical confirmation.
Acceptance agreed before supply

Confirm material identity, delivery condition, heat-to-piece traceability, dimensional checks and required testing before production. For converted parts, define inspection after forging, heat treatment and machining, including the specified microstructure and NDT scope.

Independent inspection can be discussed with its scope, timing, acceptance criteria and cost agreed for the order.

Delivery with clear milestones

Review the proposed lead time, approvals, production sequence and dispatch requirements. For several product forms, coordinate document and packing readiness together.

Material substitutions and technical changes require written approval. A schedule deviation should identify the impact, decisions needed and next steps.

One contact when an issue arises

Contact TiHubs with the order reference, affected items and supporting photos or inspection records.

We record the issue, review it against the agreed requirements and coordinate the next steps with the relevant manufacturing parties.

01 / Material identity

Material records

Grade, standard, test results and heat or batch identity matched to the supplied items.

  • Material certificate
  • Heat / batch ID
  • Test results
02 / Agreed acceptance

Inspection records

Dimensional and testing records for the agreed scope, including critical drawing requirements.

  • Dimensions
  • Agreed testing
  • Acceptance criteria
03 / Ready for dispatch

Dispatch records

Item identification, packing list, protective packaging and required shipment documents.

  • Packing list
  • Item labels
  • Shipping documents

06 / Questions before sourcing

Before you specify
TC16 Titanium Alloy.

A clear material designation is the beginning. Product form, specification revision, material condition and acceptance complete the requirement.

A useful first enquiry

  • Product and specificationProduct form, standard edition, dimensions and material condition.
  • Order and deliveryQuantity, destination and any required delivery date.
  • Acceptance requirementsDrawing revision, inspection, certificates and packaging.

Not every detail is finalized? Send the information you have. We can help identify the questions to resolve before quotation.

Discuss your requirement

What happens next: requirement review, technical clarification, then a supply proposal and quotation.

What is TC16 titanium alloy?

TC16 is a Chinese alpha-beta titanium alloy with the nominal composition Ti-3Al-5Mo-4.5V. Fastener stock is a priority purchasing direction: the material must support the approved heading, machining, thread-forming and thermal-processing sequence. A bar or wire certificate establishes the supplied material condition; finished fastener acceptance remains a separate requirement.

Is TC16 the same as ASTM Grade 16?

No. TC16 is an aluminium-molybdenum-vanadium alloy; ASTM Grade 16 is a different palladium-bearing commercially pure titanium grade. Keep the full designation and specification on the order.

Which TC16 products are the priority?

Bar and fastener wire are the main enquiries. Straight rod, conversion billet and drawing-based blanks depend on dimensions, condition and the confirmed manufacturing route.

Can I order TC16 wire for heading?

Provide wire diameter, head geometry, forming sequence and required condition. Review surface quality and a representative forming trial where the approved process requires one.

Does a wire certificate qualify a finished bolt?

No. Wire acceptance and finished-fastener qualification address different stages. Define proof, tensile, fatigue, thread and dimensional tests where required by the drawing.

What condition should I specify?

Use the condition required by your approved manufacturing route. State any subsequent heat treatment and who accepts the final condition; do not compare certificates from different states.

Can TiHubs coordinate precision blanks?

Send the drawing, raw-material specification, minimum stock allowance, quantity and inspection requirements. The supply scope and actual capability are confirmed during review.

What records should accompany TC16 stock?

Require heat and lot identity, full chemical analysis, delivery condition, dimensional results and the agreed mechanical and structural tests. Define NDT method, coverage and acceptance criteria in the order.

What should I include in a TC16 RFQ?

Include product form, size, quantity, standard edition, condition, intended forming or machining route, drawing revision, inspection and destination. Identify any approved-source restrictions.

07 / Your next step

Start with the
requirement you have.

Send the product details, drawing or operating conditions you already know. We will identify missing information and discuss a suitable supply route before quotation.

  1. Requirement review
  2. Technical clarification
  3. Supply proposal and quotation

Combine materials and parts in one enquiry.

Send one list of TC16 forms, sizes and quantities. Include drawing revisions, material conditions and items that must be supplied or dispatched together.

Share the service and acceptance priorities.

Include load and temperature conditions, critical sections, required material records, process qualification, inspection, destination and timing.

Baoji, China · info@tihubs.com

Start your TC16 Titanium Alloy enquiry

Send your material form, drawing or process conditions. We will help clarify the remaining requirements.

Customer Feedback & RFQ Form (#6)