TB10 Titanium Alloy titanium products on a dark metallic background

TB10 Titanium Alloy · Near-beta titanium alloy

TB10 Titanium Alloy. Forged stock with the condition under control.

Source TB10 forged bar, billet and structural preforms with the solution-treatment, ageing and inspection stages clearly assigned before quotation.

Start with a specification, drawing or application. We’ll help identify the details still needed.

Material review. Supply coordination.
One contact in Baoji, China.

TB10 Titanium AlloyTi-5Mo-5V-2Cr-3Al · nominal wt %
Near-beta titanium alloyForged bar, structural preforms & condition control
One contact20 years of founder experience · 100+ Baoji factories

01 / Product forms

Find your TB10 product.

Choose a material form or application. Send the dimensions, service conditions and required records so we can match the manufacturing route to your order.

TB10 forged round bar — illustrative supply form
01 / 06

TB10 Titanium Alloy

TB10 forged round bar

Round forged stock for project-approved aerospace and high-strength structural parts.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Diameter, length, straightness, machining allowance and delivery condition.
Manufacturing review
Review forging route, section size, solution treatment and ageing responsibility.
Inspection priorities
Microstructure, agreed mechanical results, surface integrity and internal examination.
TB10 conversion billet — illustrative supply form
02 / 06

TB10 Titanium Alloy

TB10 conversion billet

Billet for further forging or a specified conversion process.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Section, length or mass, surface finish and discard allowance.
Manufacturing review
Define the downstream deformation route and where final heat treatment and testing occur.
Inspection priorities
Chemistry, macrostructure, soundness and identification under the agreed billet specification.
TB10 rectangular stock blanks — illustrative supply form
03 / 06

TB10 Titanium Alloy

TB10 rectangular stock blanks

Cut or forged block stock for machining a defined structural envelope.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Envelope dimensions, orientation, corner allowance and datum surfaces.
Manufacturing review
Review metal-flow requirements, final load direction and heavy stock-removal stages.
Inspection priorities
Dimensional envelope, surface and internal quality, with material orientation preserved.
TB10 structural forging preforms — illustrative supply form
04 / 06

TB10 Titanium Alloy

TB10 structural forging preforms

Drawing-controlled rough preforms for subsequent machining and component qualification.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Outline, section transitions, draft, flash or trim allowance and inspection access.
Manufacturing review
Confirm feasible forging route, grain-flow objectives and heat-treatment sequence.
Inspection priorities
Structure, defects, distortion and NDT scope at the specified delivery stage.
TB10 cut bar sections — illustrative supply form
05 / 06

TB10 Titanium Alloy

TB10 cut bar sections

Short bar lengths or disks prepared for a defined machining operation.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Cut length, thickness, squareness, burr limits and machining allowance.
Manufacturing review
Agree cutting method, piece identification and whether cut faces are inspection surfaces.
Inspection priorities
Geometry, clean ends, surface condition and continuity of heat/lot records.
TB10 process-qualification stock — illustrative supply form
06 / 06

TB10 Titanium Alloy

TB10 process-qualification stock

Representative material reserved for forging, heat-treatment and inspection qualification.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Sampling position, direction, specimen sizes and retained quantity.
Manufacturing review
Define the material stages and acceptance questions before removing specimens.
Inspection priorities
Keep test pieces tied to the production heat, forging route and thermal lot.

Images illustrate material forms and application possibilities. Reference markings identify specification options; they do not establish dual certification, stock availability or approval of finished equipment.

Define the shape. Share the service.

These details help turn a material enquiry into a comparable quotation.

01 / Drawing review

Aerospace structural forging stock

Forged bar, billet and structural preforms. Agree material condition, properties, microstructure and NDT without treating the grade name as flight approval.

Discuss your drawing

02 / Drawing review

Controlled forging conversion

Conversion billet and rough structural preforms. Inspect soundness and structure at the agreed stage; retain the forging and thermal records required by the order.

Discuss your drawing

03 / Drawing review

Solution-treatment handoff

Bar and blanks in the condition required by the approved route. Define which mechanical tests apply at delivery and which apply after the buyer’s final processing.

Discuss your drawing

02 / Material identity

What is TB10 titanium?

TB10 is the Ti-5Mo-5V-2Cr-3Al near-beta titanium alloy described in Chinese forged-bar research. It was developed with a lower chromium content than TB2 and is associated with high-strength aerospace structural forgings. This page focuses on forged stock, consistent microstructure and the supplied heat-treatment condition; research strengths and process recipes are not guaranteed delivery values.

Specify the exact standard edition, form and delivery condition. Nominal chemistry is only one part of an order; strength, microstructure, dimensional acceptance and traceability also need to be defined.

Review itemOrder basisWhat to confirm
Forged structureApproved conversion routeSpecify macrostructure, microstructure and material-flow requirements relevant to the final drawing.
Delivered conditionSolution/ageing handoffState the incoming condition, remaining buyer operations and the stage for final testing.
Mechanical acceptanceOrdered section and orientationUse agreed strength, ductility and fracture requirements; do not substitute patent example values.
Inspection accessBlank geometry and surfaceAgree scan directions, coverage, preparation and defect criteria before making the preform.
Cut-piece controlParent-bar traceabilityPreserve identity, orientation, quantity and dimensional records after subdivision.
Selected element · wt %Reference composition
Molybdenum · Mo5 nominal
Vanadium · V5 nominal
Chromium · Cr2 nominal
Aluminium · Al3 nominal
Titanium · TiBalance

Nominal composition, wt %, identifies TB10. Use the complete ordered chemical limits and heat analysis for acceptance; nominal values do not establish product conformity.

TB10 and TB2

TB10 has a different nominal chromium content and is a distinct grade. Processing, properties and certification must not be transferred from TB2 without approval.

TB10 and TB15 / Ti6554

Both are high-strength titanium routes but have different chemistry and processing requirements. Select the grade specified by the approved design.

Solution-treated and aged stock

The incoming condition changes the manufacturing sequence and acceptance basis. State whether subsequent forming, machining or ageing is part of the buyer’s process.

United States reference

No direct US equivalent is claimed. A substitute requires comparison of the complete grade, product form, condition and acceptance requirements.

03 / Application priorities

TB10 in application.

Review each main use through its service conditions, material choice, manufacturing route and acceptance plan. These are sourcing discussions; approved drawings and qualification requirements govern the final component.

Application review / 01

Aerospace structural forging stock

TB10 primary research identifies aerospace structural use, including forged parts for aircraft structures. The material purchase must still follow the approved drawing and qualified supply route.

Products & manufacturing

Forged bar, billet and structural preforms.

Service & design review

Provide load-critical sections, drawing revision, source-approval requirements and the intended machining route.

Purchase & inspection priorities

Agree material condition, properties, microstructure and NDT without treating the grade name as flight approval.

Send your application details

Application review / 02

Controlled forging conversion

Deformation and temperature history influence the structure delivered to heat treatment. A billet enquiry should state what the downstream forging process is expected to achieve.

Products & manufacturing

Conversion billet and rough structural preforms.

Service & design review

Specify finished geometry, reduction, grain-flow expectations, critical transitions and where process qualification resides.

Purchase & inspection priorities

Inspect soundness and structure at the agreed stage; retain the forging and thermal records required by the order.

Send your application details

Application review / 03

Solution-treatment handoff

Some projects need stock in an intermediate condition so the buyer can complete processing. The quotation should make that handoff explicit instead of using an ambiguous description such as heat treated.

Products & manufacturing

Bar and blanks in the condition required by the approved route.

Service & design review

State the incoming condition, subsequent operations, storage limitations if specified and responsibility for final ageing.

Purchase & inspection priorities

Define which mechanical tests apply at delivery and which apply after the buyer’s final processing.

Send your application details

Application review / 04

Ageing and final property acceptance

Ageing requirements must be coordinated with section size and the preceding route. A research schedule for TB10 is not a universal production schedule.

Products & manufacturing

Final-condition bar, preforms or representative qualification pieces.

Service & design review

Agree the required property balance, thermal-record scope, sampling and acceptance stage.

Purchase & inspection priorities

Check the specified tensile, ductility, fracture and microstructural requirements against the actual delivered lot.

Send your application details

Application review / 05

Machined brackets and fittings

A structural machining blank should preserve enough sound material and allowance around holes, fillets and transitions. Procurement needs the critical geometry, not just a gross block size.

Products & manufacturing

Rectangular blanks, forged preforms and short bar sections.

Service & design review

Identify principal loads, critical bores, transition radii, orientation and roughing sequence.

Purchase & inspection priorities

Agree NDT access, surface integrity, dimensional allowance and material identity through machining.

Send your application details

Application review / 06

Internal-quality planning

Inspection requirements need to be practical for the delivered geometry. A generic NDT statement does not identify coverage or the defects that govern rejection.

Products & manufacturing

Bar or preforms with inspection-friendly surfaces and reserved material.

Service & design review

Specify the method, calibration basis, scan directions, coverage and acceptance criteria required by the project.

Purchase & inspection priorities

Agree surface preparation, records and any limits created by geometry before manufacture.

Send your application details

Application review / 07

Cut-to-length production lots

Cut sections can reduce buyer preparation work, but dividing one bar introduces identification and geometry-control steps. Those steps should be included in the ordered scope.

Products & manufacturing

Short bar lengths and disk-like sections.

Service & design review

Specify cut plan, quantity, saw or machining allowance, end squareness and piece-marking restrictions.

Purchase & inspection priorities

Reconcile piece IDs, dimensions and counts to the parent-bar certificate and processing records.

Send your application details

Application review / 08

New-route qualification

A change in forging equipment, section or heat-treatment sequence can require fresh evidence. The approval plan should identify which variables and properties are being demonstrated.

Products & manufacturing

Representative trial bar and process-qualification stock.

Service & design review

Define trial size, process records, specimen map, laboratories and release milestones.

Purchase & inspection priorities

Connect chemistry, microstructure, mechanical results and internal-quality reports to one documented route.

Send your application details
Material references and applicable product standards are listed below. Select the delivery condition and acceptance plan for the specific product and approved application.

TB10 procurement checklist

Connect the application to the material order.

A useful specification connects the intended component, the supplied stock and the acceptance evidence. Share the drawing and known requirements first.

01

Define the application

Provide load-critical sections, drawing revision, source-approval requirements and the intended machining route.

02

Define the supplied stage

Forged bar, billet and structural preforms. Distinguish raw stock, converted blanks and finished parts. Define who controls subsequent processing.

03

Define the acceptance evidence

Agree material condition, properties, microstructure and NDT without treating the grade name as flight approval.

Example: a useful TB10 material enquiry

TB10 forged round bar; required dimensions and quantity; standard and drawing revision; delivery condition; intended downstream process; mechanical, structural and dimensional acceptance; traceability, destination and required date.

Identify the approved product specification and any project-specific qualification. The grade designation and chemistry standard alone do not define component acceptance.

Discuss your material requirement ↗

04 / Standards & documentation

Match the standard
to the product.

Choose the specification by product form, material condition and application. Identify the required edition on the order; a chemistry standard alone does not define product acceptance or application approval.

Hosted PDFs retain their stated editions. Publisher references open separately when no distributable PDF is provided.
Product / reviewInternational / project routeChinese referenceClarify before quotation
Identity & chemistryApproved product and project specificationGB/T 3620.1-2016View PDF ↗Review the complete chemical limits and product requirements; nominal alloy names do not establish automatic interchangeability.
TB10 forged-bar processing · CN115007781BTB10 forged-bar processing · CN115007781BPublisher reference ↗Compare the complete ordered Chinese requirementsPrimary research published 2025-04-22, identifying the alloy and a specific forged-bar processing route; not a purchase specification or a TiHubs process claim.
TB10 bar heat-treatment research · CN114892110ATB10 bar heat-treatment research · CN114892110APublisher reference ↗Compare the complete ordered Chinese requirementsPrimary heat-treatment research. The material, section and ordered acceptance must be reviewed before adopting any procedure.
CN115007781B · English translationProject and product requirements remain separately definedCN115007781B · English translationView PDF ↗Method for processing forged bars of near-beta TB10 titanium alloy. Original publication: 2025-04-22. TB10 forged-bar process research: controlled multi-direction forging, heat treatment and reported mechanical-property comparisons. Reference translation, not a purchase specification. English reference translation; original Chinese publication controls. Not a purchase specification.
Drawing-based blanks & partsApproved drawing and controlled manufacturing planAgreed product / project specificationDefine the supply stage, conversion route, heat treatment, structure, NDT, dimensions and traceability. Material certification is separate from finished component qualification.
Agree the order basis.

The purchase order must identify the required revision, grade, product form, condition and inspection. Reference documents do not replace design approval, manufacturing qualification or application-specific acceptance.

Request the controlled specification revision for your order. Any substitution, equivalence or dual-certification claim requires a documented comparison and agreement.

05 / Order coordination

Know the scope
before ordering.

Our founder’s 20 years in titanium inform the questions we ask before quotation and the supply options we review with you.

TB10 process-qualification stock — application illustration
Component application illustration. Actual material records, inspection and performance tests are defined for the order.
A quotation you can evaluate

Agree the grade, standard edition, dimensions, tolerance, condition and quantity before comparing prices.

  • Identify whether inspection, samples and tooling are included.
  • Confirm packaging, transport and delivery terms.
  • Record items that still need technical confirmation.
Acceptance agreed before supply

Confirm material identity, delivery condition, heat-to-piece traceability, dimensional checks and required testing before production. For converted parts, define inspection after forging, heat treatment and machining, including the specified microstructure and NDT scope.

Independent inspection can be discussed with its scope, timing, acceptance criteria and cost agreed for the order.

Delivery with clear milestones

Review the proposed lead time, approvals, production sequence and dispatch requirements. For several product forms, coordinate document and packing readiness together.

Material substitutions and technical changes require written approval. A schedule deviation should identify the impact, decisions needed and next steps.

One contact when an issue arises

Contact TiHubs with the order reference, affected items and supporting photos or inspection records.

We record the issue, review it against the agreed requirements and coordinate the next steps with the relevant manufacturing parties.

01 / Material identity

Material records

Grade, standard, test results and heat or batch identity matched to the supplied items.

  • Material certificate
  • Heat / batch ID
  • Test results
02 / Agreed acceptance

Inspection records

Dimensional and testing records for the agreed scope, including critical drawing requirements.

  • Dimensions
  • Agreed testing
  • Acceptance criteria
03 / Ready for dispatch

Dispatch records

Item identification, packing list, protective packaging and required shipment documents.

  • Packing list
  • Item labels
  • Shipping documents

06 / Questions before sourcing

Before you specify
TB10 Titanium Alloy.

A clear material designation is the beginning. Product form, specification revision, material condition and acceptance complete the requirement.

A useful first enquiry

  • Product and specificationProduct form, standard edition, dimensions and material condition.
  • Order and deliveryQuantity, destination and any required delivery date.
  • Acceptance requirementsDrawing revision, inspection, certificates and packaging.

Not every detail is finalized? Send the information you have. We can help identify the questions to resolve before quotation.

Discuss your requirement

What happens next: requirement review, technical clarification, then a supply proposal and quotation.

What is the nominal composition of TB10?

TB10 is commonly identified as Ti-5Mo-5V-2Cr-3Al. Complete ordered limits, including impurities, govern acceptance.

Is TB10 the same as TB2?

No. TB10 has a different nominal chromium content and a distinct material and processing basis.

What is the main supply focus?

Forged round bar, conversion billet and drawing-defined structural blanks or preforms, subject to confirmed capability.

What does heat treated need to specify?

State the exact delivered condition and approved solution/ageing route, including who performs the remaining operations and when acceptance tests apply.

Can the patent’s strength values be used as guaranteed properties?

No. Reported research results depend on the example composition, section and process. Use the property requirements agreed in the order.

Is there a confirmed US equivalent?

No direct US equivalent is claimed on this page. Any proposed substitute needs an approved complete comparison.

Why define NDT before ordering?

Method, coverage, geometry, surface preparation and acceptance criteria determine whether the requested examination can be performed meaningfully.

Can short bar sections be quoted?

Yes, as a cut-to-length enquiry with defined dimensions, allowance, end quality, quantity and piece-traceability requirements.

What should a TB10 RFQ contain?

Include form, dimensions, quantity, drawing and standard revisions, forging and thermal condition, properties, microstructure, NDT, documents and destination.

07 / Your next step

Start with the
requirement you have.

Send the product details, drawing or operating conditions you already know. We will identify missing information and discuss a suitable supply route before quotation.

  1. Requirement review
  2. Technical clarification
  3. Supply proposal and quotation

Combine materials and parts in one enquiry.

Send one list of TB10 forms, sizes and quantities. Include drawing revisions, material conditions and items that must be supplied or dispatched together.

Share the service and acceptance priorities.

Include load and temperature conditions, critical sections, required material records, process qualification, inspection, destination and timing.

Baoji, China · info@tihubs.com

Start your TB10 Titanium Alloy enquiry

Send your material form, drawing or process conditions. We will help clarify the remaining requirements.

Customer Feedback & RFQ Form (#6)