TA33 / Ti60 · Near-alpha high-temperature titanium
TA33 / Ti60. High-temperature stock needs time-dependent evidence.
Discuss TA33 forged bar, billet and disc or ring blanks with creep, thermal exposure, structure and lot acceptance defined for the intended duty.
Start with a specification, drawing or application. We’ll help identify the details still needed.
Material review. Supply coordination.
One contact in Baoji, China.
01 / Product forms
Find your TA33 product.
Choose a material form or application. Send the dimensions, service conditions and required records so we can match the manufacturing route to your order.

TA33 / Ti60
TA33 high-temperature forged bar
Priority machining or conversion stock for thermally loaded designs that specify TA33.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Diameter, length, finish, representative section and test allowance.
- Manufacturing review
- Identify delivered structure, thermal condition and subsequent conversion.
- Inspection priorities
- Complete chemistry, structural acceptance and specified hot-property tests.

TA33 / Ti60
TA33 conversion billet
Starting stock for approved high-temperature forging programmes.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Section, cut mass, cropping and retained test material.
- Manufacturing review
- Review homogeneity and the planned forging and thermal sequence.
- Inspection priorities
- Element distribution requirements, internal soundness and macrostructure.

TA33 / Ti60
TA33 disc forging blanks
Illustrative disc blanks for a design-approved product route.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Diameter, thickness, hub allowance and specimen extensions.
- Manufacturing review
- Define radial and tangential requirements and the supplied manufacturing stage.
- Inspection priorities
- Location-specific structure, NDT and mechanical evidence.

TA33 / Ti60
TA33 ring forging blanks
Annular stock for approved thermally loaded components and casing-related designs.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Outside diameter, bore, height, ovality and finishing stock.
- Manufacturing review
- Review section transitions, thermal cycles and final machining sequence.
- Inspection priorities
- Directional tests, internal examination and dimensional allowance.

TA33 / Ti60
TA33 flat machining blanks
Flat-stock enquiries for project-specific geometry, subject to actual product capability.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Thickness, usable envelope, direction and stock allowance.
- Manufacturing review
- Confirm whether rolled or forged flat stock is permitted by the drawing.
- Inspection priorities
- Condition, section-representative properties and specified defect limits.

TA33 / Ti60
TA33 custom high-temperature blanks
Rough annular and stepped blanks with a defined final-processing and test scope.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- CAD model, datums, critical section, allowance and trial quantity.
- Manufacturing review
- Plan final heat treatment, stabilization where required and inspection access.
- Inspection priorities
- Traceable material and process records tied to the agreed final condition.
Images illustrate material forms and application possibilities. Reference markings identify specification options; they do not establish dual certification, stock availability or approval of finished equipment.
Define the shape. Share the service.
These details help turn a material enquiry into a comparable quotation.
01 / Drawing review
Hot compressor-section forgings
Forged bar, disc blanks and project-specific forgings. Define room- and elevated-temperature tests plus structural and defect acceptance for the supplied section.
Discuss your drawing02 / Drawing review
Creep-limited components
Forgings and representative stock retained for testing. Require the agreed test report linked to the actual heat and condition; do not infer creep life from tensile strength.
Discuss your drawing03 / Drawing review
Thermal stability after exposure
Trial forgings and representative exposure-test stock. Compare post-exposure mechanical and structural results with the specified limits and original condition.
Discuss your drawing02 / Material identity
What is TA33 / Ti60 titanium?
TA33 is a near-alpha high-temperature alloy associated with the Ti60 family. This page emphasizes the evidence needed for thermally loaded forgings: elevated-temperature strength, time-dependent deformation, thermal stability and the relevant fatigue programme. Ti60 research uses varying experimental compositions, so the full TA33 chemistry in the ordered standard remains the purchasing identity. A 600°C-class research description is not a universal continuous-service guarantee.
Specify the exact standard edition, form and delivery condition. Nominal chemistry is only one part of an order; strength, microstructure, dimensional acceptance and traceability also need to be defined.
| Review item | Order basis | What to confirm |
|---|---|---|
| Creep behavior | Defined stress, temperature and duration | Request the applicable test method and acceptance at the intended duty; room-temperature tensile data are insufficient. |
| Stress rupture | Specified elevated-temperature conditions | Identify specimen location, exposure conditions and rupture acceptance in the purchase requirements. |
| Thermal stability | Exposure and residual-property checks | Define thermal exposure, microstructure review and the properties to be measured afterward. |
| Dwell-fatigue sensitivity | Application-specific evaluation | Account for hold times and load history where the approved design calls for dwell testing. |
| Heat-to-heat identity | Complete ordered chemistry | Confirm Ta, Nb, Si and carbon limits; Ti60 research variants must not silently replace the ordered TA33 composition. |
| Selected element · wt % | Reference composition |
|---|---|
| Aluminium · Al | 5.2–6.5 |
| Tin · Sn | 3.0–4.5 |
| Zirconium · Zr | 2.5–4.0 |
| Molybdenum · Mo | 0.2–1.0 |
| Niobium · Nb | 0.2–0.7 |
| Tantalum · Ta | 0.7–1.5 |
| Silicon · Si | 0.2–0.6 |
| Carbon · C | 0.04–0.08 |
| Titanium · Ti | Balance |
Selected composition limits, wt %, from GB/T 3620.1-2016. Use the complete ordered standard for all impurity, residual-element and analysis requirements.
TA33 versus an unspecified Ti60 sample
Research alloys called Ti60 do not always have identical compositions. Use TA33 and the complete standard limits on the purchase order.
TA33 versus Ti600 or IMI834
These are distinct alloy identities. Similar high-temperature development goals do not establish substitution or shared certification.
Hot tensile versus creep
A short tensile test and deformation under sustained load answer different questions. Specify both when the design requires them.
High-temperature strength versus stability
Properties after long exposure and the required fatigue response can matter as much as initial strength. Match the test programme to the service history.
03 / Application priorities
TA33 in application.
Review each main use through its service conditions, material choice, manufacturing route and acceptance plan. These are sourcing discussions; approved drawings and qualification requirements govern the final component.
Application review / 01
Hot compressor-section forgings
TA33 / Ti60-family enquiries are relevant to high-temperature compressor material programmes. The purchase must identify the approved alloy, form and condition rather than a broad temperature class.
Products & manufacturing
Forged bar, disc blanks and project-specific forgings.
Service & design review
Provide metal temperature, stress, duration, cycles and the approved component specification.
Purchase & inspection priorities
Define room- and elevated-temperature tests plus structural and defect acceptance for the supplied section.
Application review / 02
Creep-limited components
A part under sustained load may be limited by gradual deformation before a short-term strength limit is reached. Creep acceptance therefore needs explicit test conditions.
Products & manufacturing
Forgings and representative stock retained for testing.
Service & design review
State temperature, applied stress, duration, permitted strain and specimen location under the governing requirement.
Purchase & inspection priorities
Require the agreed test report linked to the actual heat and condition; do not infer creep life from tensile strength.
Application review / 03
Thermal stability after exposure
Long exposure can change a high-temperature alloy. The condition after the required exposure may be more relevant than the initial certificate values.
Products & manufacturing
Trial forgings and representative exposure-test stock.
Service & design review
Define the exposure schedule and the properties to be checked afterwards. Identify the acceptance authority.
Purchase & inspection priorities
Compare post-exposure mechanical and structural results with the specified limits and original condition.
Application review / 04
Dwell and cyclic loading review
A cycle containing a hold period can differ from a continuously varying fatigue test. Ti60-family fatigue research reinforces the need to match testing to the actual loading history.
Products & manufacturing
Representative forging coupons and approved component blanks.
Service & design review
Provide cycle shape, hold duration, stress or strain control, temperature and surface condition.
Purchase & inspection priorities
Specify the relevant fatigue programme; results from a different waveform do not establish component life.
Application review / 05
Disc-blank sampling strategy
A disc may have different local histories at the hub, web and rim. Sampling and material direction should be designed into the rough blank before machining consumes the test stock.
Products & manufacturing
Disc forgings with agreed extensions or representative sacrificial stock.
Service & design review
Identify critical zones, radial and tangential directions and the heat-treatment state for testing.
Purchase & inspection priorities
Link structure, NDT and mechanical results to the required locations and product lot.
Application review / 06
Thermally loaded ring and casing blanks
A ring-shaped component can be sensitive to thermal gradients, section changes and dimensional stability. These features should guide the blank and inspection plan.
Products & manufacturing
Ring forgings and rough annular housings.
Service & design review
State temperature cycles, attachments, sealing datums, section transitions and final-machining sequence.
Purchase & inspection priorities
Check the agreed final dimensions, direction-specific properties and internal soundness after required processing.
Application review / 07
Alloy identity and melt homogeneity
TA33 contains several intentional additions, including refractory elements and carbon. A simplified Ti60 label does not replace the full analysis required for purchasing.
Products & manufacturing
Billet and forged stock with complete heat records.
Service & design review
Specify all elements, residual limits and any required sampling for compositional uniformity.
Purchase & inspection priorities
Verify complete analysis and traceable melt and conversion records; evaluate substitutions explicitly.
Application review / 08
High-temperature development lots
A development order should produce evidence that can inform the next decision. Test material, component blanks and process records should be planned together.
Products & manufacturing
Trial bar, forging blanks and retained coupons.
Service & design review
Define the test matrix, final geometry, condition, acceptance gates and permitted changes before production.
Purchase & inspection priorities
Deliver a coherent material and test record for the defined programme without presenting research success as production approval.
TA33 procurement checklist
Connect the application to the material order.
A useful specification connects the intended component, the supplied stock and the acceptance evidence. Share the drawing and known requirements first.
Define the application
Provide metal temperature, stress, duration, cycles and the approved component specification.
Define the supplied stage
Forged bar, disc blanks and project-specific forgings. Distinguish raw stock, converted blanks and finished parts. Define who controls subsequent processing.
Define the acceptance evidence
Define room- and elevated-temperature tests plus structural and defect acceptance for the supplied section.
Example: a useful TA33 material enquiry
TA33 high-temperature forged bar; required dimensions and quantity; standard and drawing revision; delivery condition; intended downstream process; mechanical, structural and dimensional acceptance; traceability, destination and required date.
Identify the approved product specification and any project-specific qualification. The grade designation and chemistry standard alone do not define component acceptance.
Discuss your material requirement ↗04 / Standards & documentation
Match the standard
to the product.
Choose the specification by product form, material condition and application. Identify the required edition on the order; a chemistry standard alone does not define a finished forging or component.
| Product / review | International / project route | Chinese reference | Clarify before quotation |
|---|---|---|---|
| Identity & chemistry | Approved product and project specification | GB/T 3620.1-2016View PDF ↗ | Review the complete chemical limits and product requirements; nominal alloy names do not establish automatic interchangeability. |
| TA33 composition and high-temperature alloy review | TA33 composition and high-temperature alloy reviewPublisher reference ↗ | Compare the complete ordered Chinese requirements | Research context for TA33; use the complete ordered national chemistry limits. |
| Ti60 processing research | Ti60 processing researchPublisher reference ↗ | Compare the complete ordered Chinese requirements | Primary research uses a specified experimental composition and processing condition; not a universal product guarantee. |
| Ti60 long-term creep investigation | Ti60 long-term creep investigationPublisher reference ↗ | Compare the complete ordered Chinese requirements | Primary research on time-dependent behaviour; project test conditions and lot acceptance remain separate. |
| Drawing-based blanks & parts | Approved drawing and controlled manufacturing plan | Agreed product / project specification | Define the supply stage, conversion route, heat treatment, structure, NDT, dimensions and traceability. Material certification is separate from finished component qualification. |
The purchase order must identify the required revision, grade, product form, condition and inspection. Reference documents do not replace design approval, manufacturing qualification or application-specific acceptance.
Request the controlled specification revision for your order. Any substitution, equivalence or dual-certification claim requires a documented comparison and agreement.
05 / Order coordination
Know the scope
before ordering.
Our founder’s 20 years in titanium inform the questions we ask before quotation and the supply options we review with you.

A quotation you can evaluate
Agree the grade, standard edition, dimensions, tolerance, condition and quantity before comparing prices.
- Identify whether inspection, samples and tooling are included.
- Confirm packaging, transport and delivery terms.
- Record items that still need technical confirmation.
Acceptance agreed before supply
Confirm material identity, delivery condition, heat-to-piece traceability, dimensional checks and required testing before production. For converted parts, define inspection after forging, heat treatment and machining, including the specified microstructure and NDT scope.
Independent inspection can be discussed with its scope, timing, acceptance criteria and cost agreed for the order.
Delivery with clear milestones
Review the proposed lead time, approvals, production sequence and dispatch requirements. For several product forms, coordinate document and packing readiness together.
Material substitutions and technical changes require written approval. A schedule deviation should identify the impact, decisions needed and next steps.
One contact when an issue arises
Contact TiHubs with the order reference, affected items and supporting photos or inspection records.
We record the issue, review it against the agreed requirements and coordinate the next steps with the relevant manufacturing parties.
Material records
Grade, standard, test results and heat or batch identity matched to the supplied items.
Inspection records
Dimensional and testing records for the agreed scope, including critical drawing requirements.
Dispatch records
Item identification, packing list, protective packaging and required shipment documents.
06 / Questions before sourcing
Before you specify
TA33 / Ti60.
A clear material designation is the beginning. Product form, specification revision, material condition and acceptance complete the requirement.
A useful first enquiry
- Product and specificationProduct form, standard edition, dimensions and material condition.
- Order and deliveryQuantity, destination and any required delivery date.
- Acceptance requirementsDrawing revision, inspection, certificates and packaging.
Not every detail is finalized? Send the information you have. We can help identify the questions to resolve before quotation.
What happens next: requirement review, technical clarification, then a supply proposal and quotation.
What is the main TA33 page focus?
High-temperature forged stock and the time-dependent evidence needed for creep, exposure and fatigue-related acceptance.
Does Ti60 always mean exactly the same composition?
No. Experimental Ti60 compositions vary in the literature. Specify TA33 and the complete ordered chemical limits.
Is TA33 interchangeable with Ti600 or IMI834?
No automatic equivalence is claimed. A substitution needs a full technical comparison and design approval.
Does 600°C-class mean unlimited service at 600°C?
No. Stress, duration, atmosphere, condition and design qualification determine the permitted duty.
Why is a hot tensile test insufficient for creep duty?
It measures a different loading history. Sustained-load deformation needs the specified creep test conditions and acceptance.
What is a dwell-fatigue requirement?
It evaluates cyclic loading that includes a hold period. The waveform, hold time, temperature and specimen condition must be defined.
Why retain extra test stock on a forging?
It allows representative sampling at specified locations and directions before final machining removes that material.
Can high-temperature research results certify a production lot?
No. Production acceptance needs tests and records for the actual ordered material and condition.
What should a TA33 RFQ include?
Send the full alloy designation, form and rough drawing, final condition, service history, creep or fatigue requirements, sampling plan, NDT and quantity.
07 / Your next step
Start with the
requirement you have.
Send the product details, drawing or operating conditions you already know. We will identify missing information and discuss a suitable supply route before quotation.
- Requirement review
- Technical clarification
- Supply proposal and quotation
Combine materials and parts in one enquiry.
Send one list of TA33 forms, sizes and quantities. Include drawing revisions, material conditions and items that must be supplied or dispatched together.
Share the service and acceptance priorities.
Include load and temperature conditions, critical sections, required material records, process qualification, inspection, destination and timing.
Baoji, China · info@tihubs.com
Start your TA33 / Ti60 enquiry
Send your material form, drawing or process conditions. We will help clarify the remaining requirements.