titanium parts.

A drawing can contain the correct hole diameter and still leave a photo-etching shop uncertain where to measure it through the thickness. Identify the functional passage, the narrowest land and the condition in which the part is delivered.

Industrial procurementTechnical guide
Illustration of an etched titanium foil carrier with slots, apertures and retained parts
ApertureMaterial removed
LandMetal retained
AI illustration; not a production or inspection record.

Quick answer

For titanium photochemical machining, review features in relation to sheet thickness and the edge profile the process can produce. Send a dimensioned manufacturing drawing with the CAD pattern. Agree which features control passage, which remain as metal, where carrier tabs are permissible, and how the first article will be measured.

Distinguish through-etched components from surface marking

An engineer sends a file for a thin titanium plate containing several hundred metering apertures. Purchasing receives one offer for photochemical machining and another for laser cutting. Both suppliers quote the diameter shown on the screen. Before comparing unit prices, ask them to mark where that diameter would be measured on a section through the actual sheet. If a small pin must pass through every opening, a top view alone may hide a restriction inside the thickness. If the aperture controls fluid delivery, entrance shape and the geometry through the thickness can matter as well. Specify the function that prompted the dimension.

Industrial titanium etching covers several different tasks. Surface identification or decoration removes or modifies material locally and leaves the sheet intact. Cleaning or pickling serves a different purpose. Photochemical machining of a thin component removes selected metal through the sheet or forms a controlled recess where that has been specifically agreed. The enquiry here concerns manufacturing parts from a patterned sheet. A supplier quoting a marked surface has evaluated a different task from one quoting a perforated plate released from a carrier. State the required delivery condition in the subject of the enquiry.

Draw what remains as carefully as what is removed. A large open window surrounded by a narrow border can meet the opening dimensions and still leave insufficient metal for handling. A fine web between two slots can be the feature most likely to distort when the part is removed from the carrier. Show the minimum permitted metal width if the design depends on it. For an inspection template, the reference edge that sits against the work can be more important than a freely exposed decorative edge on the opposite side.

Separate the finished drawing from the manufacturing artwork. The controlled drawing describes the titanium part the customer will accept. The fabricator may need to adjust the process pattern to compensate for dimensional change during etching. If the customer supplies a file that already contains a compensation, make that fact visible. Applying a second correction at the fabricator can move every boundary in the wrong direction. A simple note recording whether the file shows finished boundaries or process artwork can prevent an entire panel of identical errors.

A useful opening enquiry gives thickness, grade, quantity and the intended operating role. Attach a dimensioned view and two enlarged details. One should show the smallest passage and the metal around it. The other should identify where the part touches its housing or locating feature. Add a sketch of a section if the through profile matters. This gives a qualified fabricator enough context to flag a design risk before buying material or making a trial panel.

Check aperture and land dimensions against sheet thickness

Photofabrication Engineering publishes a design guide specifically for titanium. It relates hole size, land width and certain corner features to starting metal thickness. Treat these relationships as that manufacturer’s design guidance. They can be used to identify features that need discussion, but they do not define a universal manufacturing limit or a TiHubs production guarantee. If two bidders quote the same drawing with different proposed tolerances, ask each how its proposed method satisfies the functional dimension on the finished part.

The thickness bands in the table illustrate why a single multiplier can mislead. For a thickness of 0.005 inch, the cited guide places the sheet in a band with a listed minimum hole of 0.008 inch. At a thickness of 0.010 inch its table gives an approximate relationship of 1.2 times thickness, corresponding to 0.012 inch. These are two distinct rows in one supplier’s guidance. Applying the second multiplier to the first example would erase the fixed minimum that the supplier actually lists for the thinner range.

Land width is measured across the metal remaining between openings. Consider two adjacent circular openings with a centre distance of 0.90 mm and diameters of 0.40 and 0.50 mm. On the line of centres, subtract their radii from the pitch. The nominal land is 0.90 minus 0.20 minus 0.25, or 0.45 mm. For equal circular holes this expression simplifies to pitch minus diameter. A note giving only pitch and the diameter of one hole is insufficient when neighbouring patterns differ.

Tolerance can change the conclusion. If the centre distance in that separate drawing example can fall to 0.88 mm and the two holes can grow to 0.42 and 0.52 mm, the smallest arithmetic land is 0.88 minus 0.21 minus 0.26, or 0.41 mm. This assumes the stated limiting geometry and examines that line only. Freeform slots, rounded ends and misaligned rows can bring two boundaries closer at another point. A dimensional check that considers only nominal centre pitch can miss that minimum.

Review the pattern at boundaries as well as the middle. A regular array may give generous metal between internal holes but leave a very narrow strip next to a corner cutout. An added locating hole may compromise a web that was acceptable on the earlier drawing. Include the full panel detail when asking about minimum features. If the manufacturer proposes enlarging a land by shrinking a hole, identify which aperture is allowed to change, whether flow or locating clearance is affected and who can approve the revised drawing.

Source or calculation Thickness or geometry Meaning for a quotation
PEI titanium guidance, thin-foil band At T = 0.005 in, the guide lists a 0.008 in minimum hole in this band 0.127 mm stock and 0.2032 mm hole after exact inch conversion
PEI thickness-band example At T = 0.010 in, its approximate 1.2T relation gives 0.012 in A vendor design-review starting point, equivalent to 0.3048 mm
PEI land guidance applied to the example 2T at T = 0.010 in gives 0.020 in Approximately 0.508 mm of metal between openings
Illustrative pitch check Pitch 0.90 mm, adjacent hole widths 0.40 and 0.50 mm Nominal intervening land 0.45 mm for centred circular holes
The hole and the metal left between holes. Clear diameter. Remaining land
Industrial buying guide / 02The hole and the metal left between holes

Compare the removed area and the load-bearing or separating metal as two different features.

Specify the edge profile and the plane of measurement

Photochemical machining can remove material laterally beneath the edge of the resist as well as through the thickness. PEI’s titanium guide describes the edge left when the material is etched from both sides. A drawing of perfectly vertical walls and sharp corners may therefore describe an ideal outline rather than an achievable edge for the selected process. Ask the supplier for the proposed cross-section, especially if a seal, pin or adjoining sheet bears on the edge. The objective is to agree which part of the profile controls service.

Three measurements on the same hole can lead to different answers. A camera looking straight at one face can measure the opening at that face. A sectioned sample can show the internal contour at a particular cut. A functional gauge can establish whether a defined object passes under agreed conditions. The optical result may be entirely correct and still be insufficient to prove the required passage. Identify the quantity measured and the decision it supports. A functional test should state the gauge dimension, direction and any constraint on the force used.

Suppose a guide sheet registers a cylindrical probe. The locating function may require a specified range on the minimum passage rather than the largest visible entrance. A neighbouring clearance hole may only need to admit a fastener head during assembly. Assign the appropriate requirement to each rather than giving every visible circle one tight tolerance. A supplier can then allocate measurement effort to the features that affect function and quote a simpler check for the remaining openings.

Corners need a similar discussion. A narrow internal corner intended to clear the corner of a housing can be drawn with a decorative sharp point that the mechanism does not need. An agreed relief may be easier to manufacture and inspect. Conversely, a corner that physically locates the part may require a well-defined profile and a mating part with a compatible radius. Show the permitted envelope or the controlling mating contour and state whether the dimension applies to one face or through the whole sheet.

For a recurring order, retain a labelled section photograph from the first article when edge profile has been agreed that way. Include a scale in the image, the face identification, sample location and drawing revision. An undocumented photograph taken at unknown magnification is difficult to reproduce and can reverse the apparent direction of an asymmetric feature. Specify which features require destructive examination of a sample and which can be checked on every delivered piece without damaging it. Keep that sampling agreement with the purchase record.

Mark the inspection direction in the case of a tapered or asymmetric feature. Suppose the customer normally inserts a locating element from the assembly side and it enters at a slight angle before seating. A straight pin inserted squarely from the opposite face may demonstrate a clear bore while failing to represent the assembly operation. Agree whether the requirement is a minimum geometrical passage, successful assembly in the actual fixture, or both. When both are required, record separate results so that a failure of one does not erase evidence from the other.

The owner of the mating component can help diagnose an apparent dimensional failure. A sharp corner on a mating pin can contact a sloped wall differently from the lead-in on the approved production pin. Record its diameter, entry geometry and orientation alongside the panel results. A supplier evaluating an unmarked gauge taken from a workshop drawer cannot know whether it represents the accepted mating design. Identifying both items on the inspection sheet is often quicker than tightening the tolerance on every etched aperture.

Face opening and minimum passage. Entry face. Narrowest section
Industrial buying guide / 03Face opening and minimum passage

A through feature can present a different contour at the face and inside the sheet. The section is illustrative.

Release artwork, datum features and carrier tabs

The design file must unambiguously identify units, finished geometry and revision. A pattern exported at a different scale can still look coherent on a screen. Include at least one verifiable overall dimension and the distance between two unambiguous reference features. Ask the recipient to report those two numbers during the drawing review. This check is particularly useful when a drawing combines a native inch grid with metric inspection requirements or when a subcontractor receives only a two-dimensional file without the original notes.

Mark the side from which the part is viewed. A symmetrical outside rectangle can carry an asymmetric slot, recess or identification mark. A mirror image can pass an outline measurement and fail in the customer’s fixture. Identify a permanent feature that distinguishes the sides, or define an agreed carrier marking that survives until the installer receives the part. If a recess is formed on one face only, show its depth or remaining thickness from a named reference surface. Specify whether the unmetallized region in the artwork represents removed material or protected metal.

Tiny parts are often easier to handle while retained in a surrounding panel. Discuss whether the customer wants loose components, parts attached to a carrier or a complete functional panel. A tab can simplify handling and counting but leave a local projection after separation. Put allowed tab zones on the drawing and mark excluded edges, especially locating corners, sealing boundaries and surfaces intended to slide into a close recess. State who removes the tabs and who accepts the final outline after removal.

A carrier also changes commercial quantities. A purchase order for one hundred parts is different from an order for one hundred carriers containing twenty parts apiece. Include the number of good pieces required, the number per carrier if that matters and the treatment of a carrier with one rejected position. A small numbering map can identify unacceptable positions without scrapping an entire panel if the buyer has approved that method. Confirm how loose parts will be counted and protected when they are supplied without the carrier.

An approved artwork revision should remain tied to the dimensional drawing, material thickness and accepted sample. If an aperture changes, the revision should show whether neighbouring lands, tabs or datum locations also changed. Keep a marked comparison of the affected features. Reusing old artwork with a new material thickness can alter the resulting dimensions even if the two-dimensional outline is identical. The supplier should identify where it needs renewed first-article approval before using an earlier pattern for a changed requirement.

Release tabs on a carrier sheet. Retained part. Tab location
Industrial buying guide / 04Release tabs on a carrier sheet

Define where separation is allowed and which residual projection is inspected after removal.

Compare etching with laser cutting and machining

Compare fabrication routes on the same finished configuration. For a flat thin part with many similar apertures, a photochemical route can create the pattern across the sheet without a separate tool path around every opening in the same sense as mechanical cutting. Tooling and production costs still depend on panel design, chemistry, material, inspection and quantity. Ask for the quotation basis and any initial artwork or first-article charges. A favourable unit price at one quantity does not automatically apply to a small replacement order.

Laser cutting can be practical for an outline or for parts that need a different thickness or feature arrangement. Review entry and exit conditions, edge quality and any heat-affected surface requirements appropriate to the selected process. Mechanical machining offers other options for controlled reference faces, a counterbore or an edge with a specified form. A combined route may be justified when most of the panel suits etching but one interface needs a separate finishing operation. Show which party performs that operation and which dimensions are inspected afterwards.

A comparable bid should state whether it includes starting titanium, manufacture, separation, edge finishing, any cleaning, documentation and packaging. One quote may supply a full carrier while another includes inspected loose parts ready for installation. A third may quote only the patterning service on customer-supplied material. Divide the total by the number of accepted finished components within the same scope. Keeping the original commercial scope visible prevents a low apparent piece price from concealing work the buyer must still purchase.

Think about the practical consequence of a failed feature. A cosmetic edge outside the active area may be repairable under an agreed concession. An undersized precision passage repeated hundreds of times in an assembled screen can be expensive to classify or rework. Specify the inspection method and sampling level in relation to that consequence. An elaborate report on overall length cannot compensate for an untested critical passage. Conversely, measuring every nonfunctional corner to a very tight tolerance can add cost without improving the assembly.

For a trial, ask for a representative panel with the smallest holes, narrowest lands, longest unsupported features and any required half-depth features. An isolated large aperture is easier to inspect but may reveal little about crowded regions of the real part. Include actual separation tabs and an example of the cut border. Inspect the trial under the same delivery conditions proposed for production. If the trial remains attached to a rigid carrier but production parts must arrive loose, inspect at least an agreed set after separation as well.

Read the related technical guide for the companion product or property.

Inspect the first panel and release repeat production

Receiving should start with identification. Check the material grade, ordered thickness, part number, revision, lot and carrier condition. Keep the relationship between the original sheet and the finished batch if traceability is required. A starting-material certificate does not establish the condition of the etched openings. The dimensional report should identify the actual first article, the inspection locations and the methods appropriate to the finished features. Define which records travel with every delivery and which remain available on request for a repeat batch.

Measure the reference features first. A camera can report plausible hole positions relative to the wrong edge when a flexible panel is located inconsistently. Use the datums identified on the approved drawing and agree how the foil is supported. A panel forced flat under a fixture can behave differently when released. Record whether flatness or position applies to the free part, a specified supported condition or the installed configuration. Include the measurement temperature or conditioning requirement only when it is relevant to the agreed inspection method.

Inspect the critical apertures and the metal between them as separate groups. Record face and through measurements separately when both are required. In a dimensional table, include the method rather than reporting an isolated diameter with no context. For a visual inspection standard, agree the lighting, magnification or reference sample that determines the disposition. A photograph taken on a bright backlight can reveal a partial obstruction while hiding the condition of the surrounding face. Another view may be necessary to answer a different acceptance question.

Packaging can damage a conforming part after inspection. Thin metal can take a permanent bend at a narrow land, and separate parts can interlock through slots. Choose trays, interleaving or retention in the carrier according to the agreed delivery state. Mark which protective materials may touch surfaces that will subsequently be joined or coated. Include opening and handling instructions when required by the customer. If a first trial arrives flat only because of a temporary supporting plate, record that packing arrangement for production shipments.

Close the review by writing an acceptance statement that each party can apply. An example would identify grade and thickness, the finished drawing revision, units of the approved artwork, the minimum functional aperture with its measurement method, the location of permitted tabs and the required sample report. Add quantity, delivery state and any unresolved assumptions. This gives the supplier a defined manufacturing scope and lets the purchaser compare the delivered titanium part with the function for which it was ordered.

Request a technical quotation

A drawing can contain the correct hole diameter and still leave a photo-etching shop uncertain where to measure it through the thickness. Identify the functional passage, the narrowest land and the condition in which the part is delivered.

Information to include

  • Material grade and sheet thickness
  • Drawing revision and CAD units
  • Functional aperture and minimum land
  • Edge inspection plane
  • Carrier condition and sample inspection

Build your RFQ checklist

Choose the product and add the information you have. Copy the resulting brief or send your requirements to TiHubs. Submitting an enquiry does not place an order.

TiHubs — EN — Titanium Etching for Thin Precision Parts: Drawings, Undercut and First-Article Inspection

Add your details, then copy the checklist or send your requirements to TiHubs.

We use these details to respond to your enquiry. Privacy Policy.

Questions buyers ask

Does an etching drawing specify the chemical recipe?

A purchasing drawing typically defines the required finished geometry, material, surface condition and evidence. Manufacturing process details belong to the qualified fabricator and any specifically agreed process-control documents.

Does one optical diameter establish through clearance?

A face measurement describes that face. If a pin must pass, identify its required clearance, the relevant through profile and the agreed functional or sectional verification.

Can a carrier tab remain on any outside edge?

Mark permitted tab zones and excluded functional edges on the drawing. Agree the condition and inspection after separation, especially where the part seats in a recess.

Keep the purchase requirements connected.

  1. Material grade and sheet thickness
  2. Drawing revision and CAD units
  3. Functional aperture and minimum land
  4. Edge inspection plane
  5. Carrier condition and sample inspection

Sources and data scope

References reviewed November 20, 2026. Public source summaries support the discussion; the controlled specification, agreed edition and approved project requirements govern acceptance.

  1. Photofabrication Engineering — Design Guidelines for Photochemical Machining of Titanium — Manufacturer-specific thickness bands, hole and land guidance and discussion of the feathered edge.
  2. Photofabrication Engineering — Titanium Etching — Material-specific manufacturing context and discussion of etched titanium components.
  3. Fotofab — Exotic Metal Photochemically Etched Parts — Second fabricator perspective on buying etched parts in specialty metals.

About TiHubs

TiHubs coordinates titanium material and custom supply enquiries from Baoji, China. Send the product, drawing revision and acceptance requirements so the proposed supply scope can be reviewed. Learn about our sourcing role.