CategoryQuality, Inspection & Standards
Buying titanium castings?
Define acceptance before production.
A certificate or an “X-ray inspected” description leaves important scope questions open. Connect the drawing, delivery stage and inspection evidence before comparing offers.

Quick answer
Specify a titanium casting by its applicable casting material standard, controlled drawing, delivery condition and inspection plan. Define critical zones, dimensional and surface requirements, NDT method and coverage, acceptance criteria, repair permissions and traceability. An X-ray report, a material certificate or HIP processing alone does not establish that every requirement of the finished component has been met.
01 / Purchase baseline
Define the casting and the stage at which it will be accepted
A titanium casting enquiry can refer to a rough casting, a cleaned and inspected blank, a partly machined component or a finished part. These delivery stages carry different dimensional and inspection responsibilities. Begin by identifying the delivered state and the operations that remain with the buyer. A quotation for an acceptable casting blank should not be read as a commitment to every requirement of a component that has not yet been machined or validated.
Attach the controlled drawing and revision, identify the applicable material specification and state the quantity and intended service information needed for review. Where the design requires a particular qualification or customer approval, retain that requirement explicitly. A supplier cannot reliably price a critical inspection package from a photograph and a general instruction to provide high quality. The task is to turn that expectation into an agreed, inspectable scope.
Use a casting designation, not an assumed wrought equivalent
ASTM’s public listing identifies B367-22 as a specification for titanium and titanium-alloy castings for general corrosion-resistant and industrial applications. It includes casting designations such as C-2 and C-5. Record the designation and edition actually required by the project. Do not replace a casting specification with a familiar wrought-product grade name solely because the alloy descriptions appear similar.
If the drawing invokes another specification, preserve it and submit proposed equivalence for technical review. Material identity is only one part of the purchase: the same alloy family does not establish an identical product form, manufacturing route or acceptance basis. Resolve conflicts between the drawing, material callout and quotation before production, and record the controlling document hierarchy in the order.
Distinguish a first article from repeat production
A first-article programme may need evidence about geometry, process capability and the proposed inspection route. A repeat order normally refers to an already accepted baseline with defined change controls. State which situation applies. Approval of a single sample should identify its actual scope and should not silently permit changes to tooling, material, processing or inspection that the production requirement does not allow.
For a replacement component, avoid treating an old part as the complete design authority. It may show wear, distortion or undocumented modifications. Use it as supplementary information while the responsible engineer establishes the required geometry and acceptance. If reverse engineering forms part of the enquiry, define that service separately from casting supply, including responsibility for approving the resulting drawing and intended application.
The titanium castings supply page provides an entry point for sharing the drawing and proposed scope. Identify open questions instead of filling them with assumed tolerances or generic inspection claims. A technically useful enquiry tells the supplier what must be demonstrated and gives the buyer a clear basis for comparing the response.
02 / Geometry and stock
Check the usable machining envelope, not just the outer shape
Dimensional acceptance needs a defined reference system. Identify drawing datums, measurement condition, tolerances and the surfaces that will be machined. A casting can resemble the final component while lacking enough material at a critical local section. Conversely, an intentionally oversize machining surface should not be rejected merely because it differs from the finished-part dimension. Keep casting and finished-part requirements distinguishable.
Budget stock against the limiting section
Consider a hypothetical wall with an as-cast nominal thickness of 8.0 mm and a permitted local minimum of 7.5 mm. If the approved machining plan removes 1.0 mm from each side at that location, the simple remaining-thickness budget is 7.5 − 1.0 − 1.0 = 5.5 mm. Against an assumed final minimum of 5.0 mm, that leaves 0.5 mm of geometric margin. These numbers are illustrative, not recommended casting tolerances.
Now suppose a local section is only 6.6 mm before the same removal. The calculated remainder is 4.6 mm, below the hypothetical final minimum. A favorable average wall thickness elsewhere cannot repair this local shortfall. The example assumes aligned surfaces and known removal amounts; real machining feasibility also depends on datums, profile, distortion and the approved setup. Use the arithmetic to expose a question for engineering review, not to certify a casting.
Identify the measurement state
Specify whether dimensions are checked before or after required heat treatment, cleaning, straightening or machining. Those stages should match the drawing and supply agreement. If a report measures an intermediate state, it should not be presented as final acceptance without the required subsequent verification. State the inspection sequence so the buyer knows which dimensions are demonstrated at delivery.
A coordinate-measurement report is useful only when its alignment, characteristic identifiers and revision match the approved requirement. Ask how inaccessible features and internal walls will be assessed where they matter. A general statement that a casting was measured does not reveal which dimensions were checked or whether the method was suitable for the feature. Record the agreed coverage rather than assuming every drawing characteristic appears in one report.
Keep appearance and usable geometry separate
Define the surface condition required on as-cast and machined areas. Where texture, local blending or cosmetic appearance matters, agree the applicable criterion and evaluation method. An attractive exterior does not demonstrate internal quality, while a permitted casting texture does not necessarily indicate a defect. Avoid subjective rejection language that neither party can apply consistently.
If material will be removed after delivery, clarify responsibility for findings exposed during that operation. The contract should identify any required examination after machining and the process for reviewing a newly visible indication. This is especially important when the buyer performs the final machining. Discuss the allocation of work and evidence before production rather than expecting an earlier inspection to answer a question that only becomes accessible at a later stage.

Hypothetical removal of 1 mm per side: 7.5 mm leaves 5.5 mm, while 6.6 mm leaves 4.6 mm. Compare with the assumed final minimum of 5 mm. Geometry and datums still require review.
03 / NDT coverage
Specify method, zone, stage and acceptance as separate fields
The phrase X-ray inspected describes an activity without fully defining its acceptance scope. Ask which parts, regions and thicknesses were examined, at what stage, under which procedure and against which criteria. The same questions apply to other nondestructive testing methods. A clear plan connects the examination to the drawing and identifies any coverage limitations that require review.
Choose methods for the question being asked
Liquid penetrant testing addresses discontinuities open or connected to the examined surface, as described in ASTM E1417/E1417M’s public scope. It does not establish the absence of every internal discontinuity. Radiographic examination addresses a different evidence question and depends on the qualified technique and geometry. The responsible NDT personnel should define suitability and coverage; procurement should preserve their approved requirements.
PCC Structurals describes radiographic, ultrasonic, penetrant and dimensional inspection among its post-cast capabilities. That is evidence of the manufacturer’s range of services, not a statement that every method is appropriate for every titanium casting or that TiHubs holds the same facilities or approvals. Specify only the methods selected for the application and require an explicit response concerning their availability and scope.
Use the reference system appropriate to the examination
The current public ASTM E1320-20(2026) listing concerns reference radiographs for titanium castings and distinguishes film references from digital reference images under E2669. Reference images support the agreed classification and acceptance framework; naming a reference standard alone does not select every acceptance level for a component. The qualified technical team must establish the applicable system and contractual criteria.
Do not substitute a severity label copied from an unrelated casting material or another examination technique. State the applicable discontinuity categories, levels and drawing zones through the approved specification. If a digital method replaces a film method, review the procedure and reference basis rather than assuming that the change is only a different way of displaying the same purchase requirement.
Make coverage visible on the drawing
For a hypothetical order of ten castings, examining a defined critical zone on every casting means all ten parts received that specified zone examination. It does not mean the entire volume of every part was examined. Likewise, examining one complete first article does not establish identical examination of the remaining nine. Keep part coverage, zone coverage and sampling frequency as separate entries in the inspection plan.
Where different zones have different criteria, use a controlled map with boundaries that the inspector can identify. A note saying critical areas without a drawing reference leaves room for inconsistent interpretation. Include the relevant inspection stage and the required report identifiers. If a geometric region cannot receive the planned examination, obtain technical disposition before treating the report as complete.
Define personnel qualifications, procedure approval and any required buyer witness or hold point through the project agreement. The buyer should receive the evidence needed to confirm compliance with that scope. Do not infer accreditation, operator certification or approval from a supplier’s use of the letters NDT. Request the actual applicable evidence when the project requires it.

Hypothetical ten-part order: inspecting Zone A on all ten parts establishes that defined coverage. It does not establish examination of every zone or the entire volume.
04 / Processing and repair
Agree the permitted route and the treatment of findings
The purchase specification should identify the required delivered condition and any approved post-cast processing. State which operations are included, which need prior authorization and which records must accompany delivery. A supplier’s general process capability does not establish that a particular operation is included in the quoted price or permitted for the component. Keep the proposed route visible during technical review.
HIP is a process step with a defined purpose
Bodycote describes hot isostatic pressing as a route for reducing internal microporosity in castings. That does not make a HIP record a universal acceptance certificate. If HIP is required, the responsible technical specification should define the approved process and relevant verification. Do not assume that the treatment establishes dimensions, chemistry, surface acceptance or every possible internal-quality requirement.
Review the location and timing of any required examinations relative to processing. The inspection plan should identify which results apply before a treatment and which are required after it. A pre-process report cannot silently stand in for a specified final-state examination. Conversely, do not add an unapproved treatment after acceptance and assume that the original evidence remains sufficient for the changed delivery condition.
Distinguish rework, repair and acceptance by concession
Use the definitions and approval rules established for the project. A permitted finishing operation, a repair and acceptance of a nonconformity can carry different responsibilities. The purchase order should identify whether repair welding or another corrective operation is allowed, who approves it, which procedure applies and what re-examination follows. Do not infer unrestricted repair permission from the supplier’s general ability to weld titanium.
If an indication is found, preserve its identity and location with the relevant inspection evidence. Submit the required information through the agreed disposition route. The responsible authority should decide whether the part is acceptable, needs an approved corrective operation or must be rejected. Procurement should not choose an arbitrary defect limit from a public article to resolve a component-specific engineering decision.
Keep the final surface and dimensions in view
A local finishing operation can change the amount of material remaining at a feature. If blending is permitted, the applicable drawing and procedure still govern geometry and surface acceptance. An indication disappearing from view is not by itself proof that the component remains dimensionally acceptable. Require the verification selected for the affected characteristics after the approved operation.
Where a surface layer or processing residue must be controlled, specify the required final condition and the approved method of verification. Avoid an unqualified instruction to remove a fixed depth from every casting. The actual requirement depends on the material, process and component. The supplier should quote against the approved condition and identify any additional information needed to establish a repeatable route.
Record the scope of any approved concession, including affected parts, requirement, authorization and limitations. A one-time acceptance should not automatically redefine future production. Keep subsequent orders tied to the intended specification revision, and carry forward only the changes that the responsible parties have deliberately approved.
05 / Records and traceability
Make the document pack identify what was actually delivered
A document pack should allow the buyer to follow the relationship between the physical casting, its material identity, processing and acceptance evidence. Agree heat or batch identification and any required individual part identifiers. The level of identification should fit the project; do not assume that a generic certificate covering an alloy name is sufficient for an order requiring serial-level traceability.
Separate material results from part-specific examinations
Chemical or mechanical test records need the relationship to the supplied casting lot required by the applicable specification. Dimensional and NDT reports need their own part or sample identities and coverage. These documents support different requirements. A material certificate does not prove every casting dimension, and a dimensional report does not establish chemical composition. Keep each report connected to the requirement it actually addresses.
The titanium material certificate guide explains how physical identification and certificate scope should remain linked. For a casting order, add the relevant processing and inspection records selected by the project. If a test coupon or specimen supplies evidence for the lot, identify that relationship under the governing specification rather than assuming the specimen represents every local condition in the finished component.
Ask for usable reports
A dimensional report should identify drawing revision, characteristic and result with the required acceptance information. An NDT report should identify the examined parts or samples, method, procedure, stage, coverage, criteria and disposition required by the agreement. Supporting images or records should be retrievable where the project requires them. A one-line pass statement may be insufficient when the order calls for a detailed, traceable report.
Make exceptions easy to find. The delivery pack should identify approved deviations and repairs that must be disclosed, rather than requiring receiving staff to search earlier correspondence. If the physical marking or paperwork disagrees, retain the material for clarification under the agreed process. Do not repair traceability by assigning a convenient identity without evidence.
Use first-article evidence for its stated purpose
A complete first-article dimensional review can establish that the evaluated sample met its specified characteristics. It does not eliminate the production inspection plan. State which checks apply to every subsequent part, which use sampling and which changes trigger renewed approval. The correct scope depends on the project and should be agreed before the production quotation is accepted.
Similarly, a supplier quality-system certificate describes an approved scope of an organization; it is not a substitute for the required product evidence. Verify any project-specific accreditation or approval actually requested, including its relevant scope and validity. Avoid copying another manufacturer’s qualifications into TiHubs marketing or treating an unspecified certified supplier description as proof of every required process.
Before shipment, reconcile the ordered quantity, part identities, report coverage and approved dispositions. The pre-shipment inspection guide can help organize that review. A missing record is easier to resolve while the supplier can still identify and access the parts. Completing the pack after delivery should not be the normal way to discover that an agreed inspection stage was never performed.
06 / RFQ and comparison
Compare accepted supply scope, not the casting price alone
Issue the same controlled enquiry package to suppliers being compared. Include the drawing, material specification, delivery stage, inspection plan and quantity basis. Identify first-article work, tooling and documentation separately where appropriate. If a supplier proposes a different route or an exception, request an explicit compliance response so the technical team can assess the change before commercial ranking.
Make exclusions visible in the price comparison
Consider a hypothetical order of ten accepted castings. Offer A is 9,000 currency units and includes the required inspection package. Offer B is 8,200 but excludes 1,200 of required examination and reporting. Adding the stated exclusion gives B an aligned comparison amount of 9,400. Under these simplified assumptions, B is 400 higher than A despite its lower headline price. These are invented arithmetic inputs, not TiHubs prices.
The comparison remains incomplete if tooling, freight, first-article work, taxes or other required items differ. List the actual inclusions and exclusions for the order, then compare on the same basis. Also establish whether the quoted quantity means poured pieces, delivered pieces or accepted components. A lower unit price is not automatically a lower cost for the required accepted delivery.
Connect schedule to approval and inspection
Separate tooling preparation, sample approval, production, processing, examination and document release in the proposed schedule. Identify buyer review or witness points that affect progress. A shorter foundry lead time may not produce an earlier usable delivery if required inspection or approval is excluded. Ask for realistic assumptions and dependencies rather than treating one undifferentiated lead-time number as a complete plan.
Before issuing the order, close technical deviations and confirm the final document revisions. Ensure the purchase order and supplier acknowledgement refer to the same requirements. If the drawing changes later, obtain an updated response for the affected work. A revised geometry may change machining stock, examination access or acceptance coverage even when the overall part appears similar.
Make the enquiry actionable
Use the worksheet below to share the casting drawing, material designation, delivered state, critical zones, inspection requirements and quantity with TiHubs. Attach or identify the approved acceptance documents and mark unresolved items for review. TiHubs can assess the proposed supply scope and information needed for quotation. Capability, tolerances, approvals, repair permissions and delivery must be confirmed for the agreed order; final design suitability remains with the responsible engineering authority.
Make the approval close the right decision
When an alternative is accepted, describe exactly what changes and which evidence supports that decision. Approving a new package, for example, does not simultaneously approve another material condition or reduced inspection coverage. Keep authorizations tied to specific requirements and identified parts. If several people review the enquiry, establish who consolidates the final version so the supplier does not receive conflicting instructions. This coordination allows production and receiving to work against the same baseline and lets purchasing decisions be reconstructed without relying on memory or isolated messages.

Hypothetical ten-part order: A includes the required scope at 9,000 units; B is 8,200 plus 1,200 required inspection, totaling 9,400. Other terms are assumed equal.
07 / Build your RFQ
Build a titanium casting acceptance enquiry
Start with the controlled drawing and delivery stage. Identify the required evidence and permitted processing so quotations can be compared against the same acceptance scope.
Information to include
- Part drawing, revision, datums and critical zones.
- Casting material designation, specification, edition and delivered condition.
- Machining stock, final dimensions and surface requirements.
- NDT method, part and zone coverage, stage, criteria and qualifications.
- Repair permissions, traceability, reports, quantity and delivery.
Build your RFQ checklist
Choose the product and add the information you have. Copy the resulting brief or send your requirements to TiHubs. Submitting an enquiry does not place an order.
08 / FAQs
Questions buyers ask
Does an X-ray inspected casting automatically meet my specification?
No. Confirm the examined parts and zones, technique, stage and acceptance criteria. A report must be linked to the supplied parts and the agreed coverage. Other requirements, including dimensions, material identity and final surface condition, need their own evidence.
Can penetrant testing replace internal examination?
Not automatically. Penetrant testing addresses surface-connected discontinuities under its applicable procedure. It does not establish every internal-quality requirement. Select the method and coverage through the responsible technical and NDT review.
Does HIP guarantee a defect-free titanium casting?
No blanket guarantee follows from a process record. HIP may be required within an approved route, but the specified final dimensions, material and inspection requirements still apply. Define the relevant verification and do not treat treatment alone as final acceptance.
Who chooses the radiographic acceptance level?
The responsible technical authority establishes the applicable criteria with the governing specification and purchase agreement. Identify the correct reference system, discontinuity categories and drawing zones. A standard name or generic quality label alone does not complete those decisions.
Why is machining allowance part of casting acceptance?
A casting must provide the usable geometry needed for the agreed delivered state or subsequent machining. Local minimum sections, datums and removal amounts can govern feasibility. A satisfactory average thickness does not prove sufficient stock at every critical location.
What should accompany a casting quotation?
Request a compliance response to the drawing, material, delivery condition, inspection scope and repair rules. Identify tooling, first-article work, reports, exclusions, quantity basis and schedule dependencies. Compare complete accepted supply rather than an isolated casting unit price.
09 / Key takeaways
Keep the purchase requirements connected.
- Define the casting material and delivered stage before requesting price.
- Check local usable geometry against the machining plan.
- Specify NDT method, coverage, stage and criteria separately.
- Approve processing and repair within a controlled disposition route.
- Connect physical identity, reports and the accepted commercial scope.
Technical references
Sources and data scope
References reviewed November 14, 2026. Public source summaries support the discussion; the controlled specification, agreed edition and approved project requirements govern acceptance.
- ASTM B367 — Titanium and titanium-alloy castings — Official B367-22 listing and casting product scope; use the controlled project specification.
- ASTM E1320-20(2026) — Reference radiographs for titanium castings — Reference-system scope and distinction between film references and digital E2669 images; no project acceptance level is selected here.
- ASTM E1417/E1417M — Liquid penetrant testing — Public method scope for surface-connected discontinuities; confirm the edition required by the project.
- PCC Structurals — Post-cast processing — Manufacturer example of separate post-cast and inspection capabilities; not a TiHubs facility or accreditation claim.
- Bodycote — Casting densification — Industrial context for HIP of internal microporosity; no process parameters or universal acceptance promise are adopted.