Titanium anodizing colours.
Specify the match.

Use a chart to choose the direction. Use a representative sample and a defined comparison to approve the production finish.

Colour / surfaceSample and acceptance
Conceptual illustration of six coloured titanium sample coupons beside an uncoated machined sleeve
Screen referenceChoose a colour family
Physical sampleAgree the production target
AI illustration; not a production or inspection record.

Quick answer

Titanium anodizing can produce bronze, gold, blue, purple and green-family interference colours. A screen chart helps select a direction, but the approved shade depends on the material, surface and controlled process. Specify a physical reference, visible areas and comparison method. Treat a voltage chart as process-specific information, not a universal colour recipe or an acceptance certificate.

Choose a colour family, then approve a sample

A titanium anodizing color chart is a useful starting point for choosing an appearance. It is not a substitute for an agreed physical reference when a production batch must match. Begin with the colour family, then specify the titanium surface, visible area and acceptance method. This sequence turns an attractive screenshot into a requirement that a supplier and buyer can discuss consistently.

The specialist finisher Danco publishes a titanium colour selection guide showing blue, purple, bronze, gold and green-family options. It explicitly identifies the displayed colours as reference-only. The table below groups useful colour descriptions for an enquiry; it does not reproduce Danco’s proprietary colour codes, promise an exact shade or claim that TiHubs holds those samples.

Colour-family selection guide; descriptive appearance only, not calibrated colour values or voltage settings
FamilyDescribe the targetResolve before production
BronzeBrown-gold metallic appearanceApproved sample and distinction from a yellow-gold target
GoldYellow-gold metallic appearanceBrightness, surface texture and viewing conditions
Purple / magentaViolet or pink-purple appearanceWhich hue family is intended; do not use the names interchangeably
BlueLight, medium or dark blue appearanceLightness and shade on the actual surface finish
Aqua / tealBlue-green appearanceReference sample and acceptable direction of colour variation
GreenA defined green referenceFeasible shade and consistency on the selected material

Do not purchase by colour name alone

“Blue titanium screws” leaves several decisions unresolved. Is the purpose visual identification, a decorative match across an assembly or a customer-facing finish on one surface? Should the colour match a retained titanium sample, an existing component or an image? Are hidden areas allowed to differ? Answering those questions matters more than selecting an appealing name from a chart.

A printed brochure, phone photograph and physical metallic sample are different references. State which one governs. If the buyer has only an image, treat it as a direction for sample development and ask the finisher to establish a feasible physical target. Avoid writing “exactly as photo” into a purchase order when the parties have never compared the same object under agreed conditions.

Keep appearance and functional requirements separate

A colour code may help distinguish otherwise similar components, but it does not verify alloy identity, strength or suitability for a regulated application. A beautiful surface does not replace material traceability. If a part needs wear, friction, electrical or corrosion performance, state that requirement separately and agree its evidence. Do not infer it from the presence of a particular colour.

Danco’s published guide also distinguishes a grey Type 2 finish from its colour selections. That is a reminder to identify the required process, rather than treating every titanium surface treatment as a different shade of the same operation. The broader choice between anodizing and PVD is covered in our process comparison; this page concentrates on specifying and accepting a chosen anodized appearance.

Illustrative swatches identifying bronze, gold, purple, blue, aqua and green titanium anodizing colour families
Industrial buying guide / 01Choose a family before approving a shade.

Illustrative screen colours only. These are not measured titanium samples, supplier colour codes, voltage settings or acceptance limits.

A voltage chart belongs to a defined process

Titanium colour anodizing produces an oxide layer whose optical behaviour creates interference colours. It is not simply the application of a coloured paint. Applied voltage is important in the process, but a purchasing requirement needs more than a voltage number copied from an unrelated chart. The target is the agreed appearance and product condition after the controlled finishing route.

Nippon Steel’s report on titanium oxide interference colours examines the relationship between the oxide layer, surface texture and visible appearance. The practical purchasing implication is that colour and texture cannot be considered independently. A smooth coupon and a differently finished production part may not present the same appearance even when a nominal colour instruction is shared.

Why two published charts can differ

Charts may represent different material, preparation, equipment or observation conditions. Before using one, identify who produced it, which process it represents and whether its scope matches the intended part. A chart with a clear source and limitations is more useful than a precise-looking unsourced table. The number of decimal places does not establish transferability.

The Zirkonzahn equipment manual hosted by Straumann provides a concrete example: its voltage diagrams distinguish different pretreatment conditions within the documented system. That manual is an equipment-specific reference, not a universal recipe for industrial titanium parts or evidence of medical-device qualification. Its chart should not be transplanted into a supplier order without the corresponding process context.

Use voltage as process information

If the approved supplier uses a controlled voltage setting, retain it in the process documentation together with the relevant preparation and equipment information. The order can refer to an approved process revision and sample. It should not make an isolated electrical setting the only acceptance criterion while leaving the required appearance undefined.

Conversely, a buyer should not force a supplier to reproduce another workshop’s setting when the target can only be met by a different qualified route. Ask the supplier to identify the proposed process and demonstrate the intended result on representative material. Keep the distinction between an appearance requirement and a manufacturing instruction explicit; changes to a controlled instruction still require the agreed approval.

Do not turn colour into a thickness certificate

A visible colour can inform process control within a defined system, but a screenshot cannot establish a universally valid oxide thickness. If film thickness is itself a contractual requirement, specify the relevant measurement and acceptance method. Likewise, the colour of a heat-affected titanium surface is not automatically equivalent to a deliberately anodized finish. The origin and controlled process matter.

For procurement, the useful question is whether the finisher can reproduce the approved appearance on the proposed product and document the controls that matter. A request containing grade, surface finish, drawing, sample reference and acceptance scope is therefore stronger than “make it blue at this voltage.” It also gives the supplier a clear basis for identifying an assumption before production.

Develop the sample on the production surface

A colour sample should represent the surface the customer will actually receive. Specify whether that surface is machined, polished, brushed, blasted or otherwise prepared, and identify the relevant texture or finish requirement. “Same blue” on two surfaces is not a complete instruction if the buyer expects the same brightness and visual character across them.

Record the finish before anodizing

Use the drawing or finishing specification to define the starting surface. Identify visible machining marks, grain direction and areas where polishing or blasting is prohibited. If a roughness value matters, state the parameter and measurement requirements; a single number does not necessarily describe every visual aspect. Our surface-finish guide provides the broader specification context.

A development coupon made from a polished scrap may help choose a colour family, but it may be inadequate to approve a production component with a milled face and curved edge. Establish which surfaces the coupon represents and where a first article is needed. Record its material designation and preparation so that the next supplier does not have to reconstruct the target from appearance alone.

Identify visible and hidden surfaces

Mark the appearance-critical region on the drawing. A customer-facing face, a hidden bore and a clamping surface may require different treatment. Show masked areas and permitted electrical contact locations. If a contact mark must be outside the visible zone, state its allowed position rather than asking the supplier to guess which side the customer will see.

Complex shapes deserve a representative review. A flat coupon cannot demonstrate every aspect of a recessed feature, edge or assembled interface. Ask whether the approval concerns a coupon, a complete first article or both. Where the component has several finishes, define the boundary and the order of operations so that the final appearance and dimensions are evaluated together.

Keep material changes visible

Record the grade and product condition used for the approved sample. A later change in substrate or preparation should trigger the review agreed for the process. This does not mean every change automatically causes unacceptable colour; it means the supplier should not assume equivalence without checking the relevant requirement. The approval plan should identify which changes need a new sample.

For machined titanium parts, include the finished drawing rather than only the raw-stock dimensions. For titanium bolts, identify whether colour is required on the head, entire exposed surface or another defined region. Functional interfaces and permitted contact marks should be reviewed alongside the appearance request.

Before approving the first sample, inspect it in the intended assembly where practical. Two components viewed separately may seem acceptable but create an unwanted contrast when placed together. Define whether acceptance is against one master sample, between neighbouring parts, or both. This small clarification prevents a later argument about two different meanings of “matching.”

Diagram linking substrate, surface preparation, visible region and reference sample for anodized titanium
Industrial buying guide / 03The sample must represent the part.

Keep material, surface preparation and the appearance-critical area connected to the approved reference.

Define how the colour will be judged

A sample approval becomes useful when both parties know how to compare future parts with it. Record the reference identity, viewing arrangement and acceptable scope of variation. A buyer looking under a warehouse lamp and a finisher looking under a different light can otherwise disagree without either having changed the component. The agreed assessment should reflect the intended product and the practical inspection conditions.

Establish a common viewing arrangement

The public scope of ASTM D1729 addresses visual appraisal of colours and colour differences under diffuse illumination. It provides a relevant framework to discuss with a competent finisher or laboratory; it does not automatically resolve every angle-dependent metallic appearance. Agree the appropriate viewing geometry and applicability to the actual anodized component.

For a visual method, specify the reference sample, illumination, observation distance or arrangement where relevant, background and part orientation. Decide whether surfaces are inspected clean and dry, before or after protective packaging is removed. Define which faces are compared and whether several orientations are necessary. Keep the method practical enough to repeat at both dispatch and receipt.

A numerical colour limit needs a method

ASTM D2244 covers calculation of colour differences from instrumentally measured coordinates using specified systems. Different colour-difference formulas are not interchangeable labels for the same calculation. An order that says only “Delta E below the limit” is incomplete if it omits the formula, measurement conditions and reference.

Do not invent a universal numerical tolerance for titanium anodizing. Ask whether the instrument geometry, aperture, specimen curvature and surface finish support a meaningful comparison. Where a small or curved component cannot be measured in the proposed arrangement, agree a suitable fixture, representative specimen or visual method. A number reported by an unsuitable setup can create false confidence.

Separate within-part and between-part consistency

One component may need a consistent appearance across a broad face. A batch may need consistency between separate components. An assembly may require adjacent pieces from different lots to match. These are different acceptance questions. State which one governs and identify the surfaces or comparison groups. A batch average alone may conceal an unacceptable individual part or an unwanted local variation.

Fields to complete in a project-specific acceptance record
FieldRecordPurpose
ReferencePhysical sample identifier, revision and custodianBoth parties compare against the same target
SurfaceMaterial, preparation, texture and visible regionThe reference represents production
AssessmentVisual or instrumental method and conditionsThe judgment can be repeated
VariationAgreed limits or approved boundary samplesAcceptable difference is explicit
SamplingPieces, locations and comparison groupsThe inspection covers the intended delivery
DispositionReviewer, result and action for deviationsApproval remains traceable

The table is a proposed purchasing record, not a claim that a particular sampling plan or tolerance is mandatory. Populate it with the project requirements. If boundary samples are used, identify and protect them as carefully as the master sample; an undocumented collection of old parts is not a stable acceptance system.

Diagram of the reference, viewing method, variation criteria and recorded approval needed for colour acceptance
Industrial buying guide / 04Make the comparison repeatable.

Record which sample governs, how parts are viewed, which variation is acceptable and who approves the result.

Keep approval meaningful across repeat orders

A successful first sample establishes a reference for a defined route. Repeat orders need a way to preserve that reference and identify changes. Retain the drawing revision, substrate designation, preparation description, approved sample and finishing process reference together. A purchase order that merely says “same as last time” may become ambiguous after personnel, subcontractor or product changes.

Agree which changes require review

Discuss changes in material source or condition, surface preparation, finishing subcontractor, equipment route, contact arrangement and appearance-critical geometry. The goal is not to prohibit every process adjustment. It is to identify which changes could affect the agreed result and how they will be reviewed. A controlled notification is more useful than discovering the change after a customer sees the finished assembly.

Where the supplier proposes a change, ask for its scope: all parts or one variant, one lot or future production, visible or hidden surfaces. Decide whether a new coupon, first article or additional comparison is needed. Record the approval and its limits. An accepted development trial should not silently become blanket approval for unrelated shapes or substrate conditions.

Plan the batch comparison before packing

If parts must be used as a matched set, identify that set before final packing. Record how components from different finishing runs will be allocated and whether mixing is permitted. This can matter for adjacent decorative faces or colour-coded product families. It avoids receiving individually acceptable pieces that do not satisfy the customer’s assembly-level expectation.

Specify the inspection stage relative to cleaning, marking and packaging. If a label, protective film or packing material touches the visible surface, review whether it affects the intended appearance or leaves residue. The supplied cleanliness requirement and any approved cleaning method should be clear. Do not introduce an unapproved abrasive cleaning step at receipt simply to make a colour comparison look better.

Protect the appearance after approval

Danco Medical’s technical description notes that colour-anodized oxide films are very thin and should not be assumed to provide excellent abrasion resistance. This supports a practical distinction: an approved colour is not a guarantee that parts can rub together in transit without affecting appearance. Packaging and handling need their own agreed requirements.

Choose protection appropriate to the geometry and intended delivery. Separate appearance-critical faces, identify permissible contact regions and ensure the unpacking method does not damage them. Confirm whether the buyer requires individual protection, grouped packaging or another arrangement. Do not promise a specific packaging system until it has been reviewed for the actual order.

For a discrepancy, preserve the reference, affected parts and original packing information. Compare them under the agreed conditions before attempting rework. Record whether the issue is colour, texture, staining, scratching or another surface condition. Each may need a different response; describing everything as “wrong blue” makes both investigation and commercial resolution harder.

Write a colour requirement a supplier can quote

Begin the enquiry with the component and its purpose. State whether colour provides identification, a decorative appearance or a match to an existing product. Attach the controlled drawing and mark the visible surfaces. Add the material designation, proposed preparation, quantity and destination. The finisher can then assess the actual supply task instead of quoting an undefined colour operation.

A sample specification structure

A useful draft note might read: “Colour-anodize the indicated visible face to the approved physical reference identified in the order. Substrate and surface preparation shall follow the drawing. Contact marks and masked areas are limited to the indicated regions. Assess appearance using the agreed viewing method and acceptance record. Report proposed changes before production.” This is a structure to complete, not a ready-made acceptance specification for every part.

Replace general phrases with the project’s reference identifiers and requirements. If no sample has been approved, state that the first stage is colour development and first-article review. Keep that stage separate from the production release. Otherwise, a supplier may treat a quotation request as approval to process the full quantity using its own interpretation of the target shade.

An illustrative matched-assembly case

Consider a hypothetical order for two neighbouring titanium covers. One cover has a brushed face and the other a machined face, while the buyer requests the same blue. A flat polished colour coupon could select the broad hue, but it does not settle the appearance of the finished pair. The review needs representative surfaces and the installed viewing relationship.

The buyer can ask for a first-article pair, compare it using the intended arrangement and identify the accepted surface preparation for each component. If the appearance cannot meet the original expectation, the design owner can review a common preparation or a revised target. That is a controlled development decision, not proof that anodizing always produces identical appearance on unlike surfaces.

Compare complete quotations

Separate sample development, preparation, masking, finishing, inspection, records and packaging. Ask whether the price includes the representative first article and what happens if the target changes after approval. A low finishing price may exclude the preparation or matching work that dominates the real task. Compare suppliers on the same accepted deliverable and clearly identified assumptions.

For repeat supply, retain the approved record with the order history and identify who controls the physical references. Replace damaged references through an agreed comparison process. A faded printout, scratched sample or unlabelled leftover component should not quietly become the new master. The objective is to make colour selection repeatable enough for procurement, inspection and the final customer to share one expectation.

TiHubs can review enquiries for titanium components with specified finishing requirements. Send the drawing and target reference so that the proposed supply route, sampling stage and documentation can be confirmed. Availability of a particular shade or matching tolerance must be assessed for the actual material, surface and geometry; the colour guide alone is not a production commitment.

Send the part and the colour target.

Attach the drawing and identify the colour family or physical reference. Specify the material, starting surface, visible faces, masked areas and quantity. If a sample still needs development, say so explicitly. TiHubs can review the proposed finishing and supply scope before confirming a quotation.

Information to include

  • Product, grade, drawing revision and quantity
  • Colour family and physical reference identifier if available
  • Surface preparation and appearance-critical areas
  • Masking boundaries and permitted contact locations
  • Visual or instrumental assessment and agreed variation
  • Sample-development stage, packing, destination and target date

Build your RFQ checklist

Choose the product and add the information you have. Copy the resulting brief or send your requirements to TiHubs. Submitting an enquiry does not place an order.

TiHubs — EN — Titanium Anodizing Color Chart: Samples, Finish and Batch Consistency

Add your details, then copy the checklist or send your requirements to TiHubs.

We use these details to respond to your enquiry. Privacy Policy.

Questions buyers ask

Is there one voltage for every titanium colour?

No universal setting should be assumed. Published charts represent particular processes and conditions. Use the finishing supplier’s controlled route and approve the result on representative material. An isolated voltage does not replace a physical colour reference and acceptance method.

Can titanium anodizing match a photograph exactly?

A photograph can communicate a direction, but display, lighting and the original surface affect its appearance. Develop a physical reference and agree how it will be compared with production. Do not treat an image alone as a calibrated acceptance standard.

Will polished and blasted parts have the same appearance?

Not necessarily. Surface texture is part of the visible result. If different surfaces must match, approve representative samples or first articles and define the viewing conditions. The broad colour name alone does not settle brightness or texture differences.

Does a colour-anodized finish guarantee wear resistance?

No. Appearance and functional performance require separate specifications. A colour selection does not establish abrasion, friction or service-life performance. State the relevant functional requirement and its evidence independently of the colour target.

Can contact marks be hidden?

Identify the permitted contact locations and visible surfaces on the drawing, then ask the finisher to confirm feasibility. Do not assume a complex component can be processed with no contact evidence anywhere. Approve any appearance-critical arrangement before production.

What should a repeat order retain?

Keep the drawing revision, material and surface description, approved reference, comparison method, variation criteria and relevant process revision together. Identify changes that require review and preserve the physical samples so that “same as before” has a clear meaning.

Keep the purchase requirements connected.

  1. Use colour families to begin selection and physical references to approve a target.
  2. Keep voltage information attached to the process that produced it.
  3. Develop samples on representative material, texture and geometry.
  4. Define viewing or measurement conditions and the scope of acceptable variation.
  5. Preserve the approved appearance through change control, handling and packaging.

Sources and data scope

References reviewed November 17, 2026. Public source summaries support the discussion; the controlled specification, agreed edition and approved project requirements govern acceptance.

  1. Danco — Titanium Anodizing Color Selection Guide — Published colour selections and limitations of displayed references; no supplier affiliation or colour-code equivalence is implied.
  2. Nippon Steel — Simulation Technology for Titanium Oxide Layer Interference Color — Technical report on oxide interference colour and surface texture; not TiHubs production data.
  3. Zirkonzahn — Titanium Spectral-Colouring Anodizer manual, 2019 — Equipment-specific voltage diagrams demonstrate process context; not a universal industrial recipe or device qualification.
  4. ASTM D1729-22 — Visual appraisal of colours and colour differences — Public scope for a visual appraisal framework; confirm applicability to the actual metallic surface.
  5. ASTM D2244 — Instrumental colour differences and tolerances — Public scope for specified colour-difference systems; no universal titanium acceptance limit is provided.
  6. Danco Medical — Titanium Anodizing: Color and Type 2 — Finisher reference distinguishing colour appearance from coating and handling considerations.

About TiHubs

TiHubs coordinates titanium material and custom supply enquiries from Baoji, China. Send the product, drawing revision and acceptance requirements so the proposed supply scope can be reviewed. Learn about our sourcing role.

Contents