TA33 / Ti60 titanium products on a dark metallic background

TA33 / Ti60 · Near-alpha high-temperature titanium

TA33 / Ti60. High-temperature stock needs time-dependent evidence.

Discuss TA33 forged bar, billet and disc or ring blanks with creep, thermal exposure, structure and lot acceptance defined for the intended duty.

Start with a specification, drawing or application. We’ll help identify the details still needed.

Material review. Supply coordination.
One contact in Baoji, China.

TA33 / Ti60Ti-5.8Al-4Sn-3.5Zr-0.7Mo-0.5Nb-1.1Ta-0.4Si-0.06C
Near-alpha high-temperature titaniumHigh-temperature forgings & creep-focused acceptance
One contact20 years of founder experience · 100+ Baoji factories

01 / Product forms

Find your TA33 product.

Choose a material form or application. Send the dimensions, service conditions and required records so we can match the manufacturing route to your order.

TA33 high-temperature forged bar — illustrative supply form
01 / 06

TA33 / Ti60

TA33 high-temperature forged bar

Priority machining or conversion stock for thermally loaded designs that specify TA33.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Diameter, length, finish, representative section and test allowance.
Manufacturing review
Identify delivered structure, thermal condition and subsequent conversion.
Inspection priorities
Complete chemistry, structural acceptance and specified hot-property tests.
TA33 conversion billet — illustrative supply form
02 / 06

TA33 / Ti60

TA33 conversion billet

Starting stock for approved high-temperature forging programmes.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Section, cut mass, cropping and retained test material.
Manufacturing review
Review homogeneity and the planned forging and thermal sequence.
Inspection priorities
Element distribution requirements, internal soundness and macrostructure.
TA33 disc forging blanks — illustrative supply form
03 / 06

TA33 / Ti60

TA33 disc forging blanks

Illustrative disc blanks for a design-approved product route.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Diameter, thickness, hub allowance and specimen extensions.
Manufacturing review
Define radial and tangential requirements and the supplied manufacturing stage.
Inspection priorities
Location-specific structure, NDT and mechanical evidence.
TA33 ring forging blanks — illustrative supply form
04 / 06

TA33 / Ti60

TA33 ring forging blanks

Annular stock for approved thermally loaded components and casing-related designs.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Outside diameter, bore, height, ovality and finishing stock.
Manufacturing review
Review section transitions, thermal cycles and final machining sequence.
Inspection priorities
Directional tests, internal examination and dimensional allowance.
TA33 flat machining blanks — illustrative supply form
05 / 06

TA33 / Ti60

TA33 flat machining blanks

Flat-stock enquiries for project-specific geometry, subject to actual product capability.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Thickness, usable envelope, direction and stock allowance.
Manufacturing review
Confirm whether rolled or forged flat stock is permitted by the drawing.
Inspection priorities
Condition, section-representative properties and specified defect limits.
TA33 custom high-temperature blanks — illustrative supply form
06 / 06

TA33 / Ti60

TA33 custom high-temperature blanks

Rough annular and stepped blanks with a defined final-processing and test scope.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
CAD model, datums, critical section, allowance and trial quantity.
Manufacturing review
Plan final heat treatment, stabilization where required and inspection access.
Inspection priorities
Traceable material and process records tied to the agreed final condition.

Images illustrate material forms and application possibilities. Reference markings identify specification options; they do not establish dual certification, stock availability or approval of finished equipment.

Define the shape. Share the service.

These details help turn a material enquiry into a comparable quotation.

01 / Drawing review

Hot compressor-section forgings

Forged bar, disc blanks and project-specific forgings. Define room- and elevated-temperature tests plus structural and defect acceptance for the supplied section.

Discuss your drawing

02 / Drawing review

Creep-limited components

Forgings and representative stock retained for testing. Require the agreed test report linked to the actual heat and condition; do not infer creep life from tensile strength.

Discuss your drawing

03 / Drawing review

Thermal stability after exposure

Trial forgings and representative exposure-test stock. Compare post-exposure mechanical and structural results with the specified limits and original condition.

Discuss your drawing

02 / Material identity

What is TA33 / Ti60 titanium?

TA33 is a near-alpha high-temperature alloy associated with the Ti60 family. This page emphasizes the evidence needed for thermally loaded forgings: elevated-temperature strength, time-dependent deformation, thermal stability and the relevant fatigue programme. Ti60 research uses varying experimental compositions, so the full TA33 chemistry in the ordered standard remains the purchasing identity. A 600°C-class research description is not a universal continuous-service guarantee.

Specify the exact standard edition, form and delivery condition. Nominal chemistry is only one part of an order; strength, microstructure, dimensional acceptance and traceability also need to be defined.

Review itemOrder basisWhat to confirm
Creep behaviorDefined stress, temperature and durationRequest the applicable test method and acceptance at the intended duty; room-temperature tensile data are insufficient.
Stress ruptureSpecified elevated-temperature conditionsIdentify specimen location, exposure conditions and rupture acceptance in the purchase requirements.
Thermal stabilityExposure and residual-property checksDefine thermal exposure, microstructure review and the properties to be measured afterward.
Dwell-fatigue sensitivityApplication-specific evaluationAccount for hold times and load history where the approved design calls for dwell testing.
Heat-to-heat identityComplete ordered chemistryConfirm Ta, Nb, Si and carbon limits; Ti60 research variants must not silently replace the ordered TA33 composition.
Selected element · wt %Reference composition
Aluminium · Al5.2–6.5
Tin · Sn3.0–4.5
Zirconium · Zr2.5–4.0
Molybdenum · Mo0.2–1.0
Niobium · Nb0.2–0.7
Tantalum · Ta0.7–1.5
Silicon · Si0.2–0.6
Carbon · C0.04–0.08
Titanium · TiBalance

Selected composition limits, wt %, from GB/T 3620.1-2016. Use the complete ordered standard for all impurity, residual-element and analysis requirements.

TA33 versus an unspecified Ti60 sample

Research alloys called Ti60 do not always have identical compositions. Use TA33 and the complete standard limits on the purchase order.

TA33 versus Ti600 or IMI834

These are distinct alloy identities. Similar high-temperature development goals do not establish substitution or shared certification.

Hot tensile versus creep

A short tensile test and deformation under sustained load answer different questions. Specify both when the design requires them.

High-temperature strength versus stability

Properties after long exposure and the required fatigue response can matter as much as initial strength. Match the test programme to the service history.

03 / Application priorities

TA33 in application.

Review each main use through its service conditions, material choice, manufacturing route and acceptance plan. These are sourcing discussions; approved drawings and qualification requirements govern the final component.

Application review / 01

Hot compressor-section forgings

TA33 / Ti60-family enquiries are relevant to high-temperature compressor material programmes. The purchase must identify the approved alloy, form and condition rather than a broad temperature class.

Products & manufacturing

Forged bar, disc blanks and project-specific forgings.

Service & design review

Provide metal temperature, stress, duration, cycles and the approved component specification.

Purchase & inspection priorities

Define room- and elevated-temperature tests plus structural and defect acceptance for the supplied section.

Send your application details

Application review / 02

Creep-limited components

A part under sustained load may be limited by gradual deformation before a short-term strength limit is reached. Creep acceptance therefore needs explicit test conditions.

Products & manufacturing

Forgings and representative stock retained for testing.

Service & design review

State temperature, applied stress, duration, permitted strain and specimen location under the governing requirement.

Purchase & inspection priorities

Require the agreed test report linked to the actual heat and condition; do not infer creep life from tensile strength.

Send your application details

Application review / 03

Thermal stability after exposure

Long exposure can change a high-temperature alloy. The condition after the required exposure may be more relevant than the initial certificate values.

Products & manufacturing

Trial forgings and representative exposure-test stock.

Service & design review

Define the exposure schedule and the properties to be checked afterwards. Identify the acceptance authority.

Purchase & inspection priorities

Compare post-exposure mechanical and structural results with the specified limits and original condition.

Send your application details

Application review / 04

Dwell and cyclic loading review

A cycle containing a hold period can differ from a continuously varying fatigue test. Ti60-family fatigue research reinforces the need to match testing to the actual loading history.

Products & manufacturing

Representative forging coupons and approved component blanks.

Service & design review

Provide cycle shape, hold duration, stress or strain control, temperature and surface condition.

Purchase & inspection priorities

Specify the relevant fatigue programme; results from a different waveform do not establish component life.

Send your application details

Application review / 05

Disc-blank sampling strategy

A disc may have different local histories at the hub, web and rim. Sampling and material direction should be designed into the rough blank before machining consumes the test stock.

Products & manufacturing

Disc forgings with agreed extensions or representative sacrificial stock.

Service & design review

Identify critical zones, radial and tangential directions and the heat-treatment state for testing.

Purchase & inspection priorities

Link structure, NDT and mechanical results to the required locations and product lot.

Send your application details

Application review / 06

Thermally loaded ring and casing blanks

A ring-shaped component can be sensitive to thermal gradients, section changes and dimensional stability. These features should guide the blank and inspection plan.

Products & manufacturing

Ring forgings and rough annular housings.

Service & design review

State temperature cycles, attachments, sealing datums, section transitions and final-machining sequence.

Purchase & inspection priorities

Check the agreed final dimensions, direction-specific properties and internal soundness after required processing.

Send your application details

Application review / 07

Alloy identity and melt homogeneity

TA33 contains several intentional additions, including refractory elements and carbon. A simplified Ti60 label does not replace the full analysis required for purchasing.

Products & manufacturing

Billet and forged stock with complete heat records.

Service & design review

Specify all elements, residual limits and any required sampling for compositional uniformity.

Purchase & inspection priorities

Verify complete analysis and traceable melt and conversion records; evaluate substitutions explicitly.

Send your application details

Application review / 08

High-temperature development lots

A development order should produce evidence that can inform the next decision. Test material, component blanks and process records should be planned together.

Products & manufacturing

Trial bar, forging blanks and retained coupons.

Service & design review

Define the test matrix, final geometry, condition, acceptance gates and permitted changes before production.

Purchase & inspection priorities

Deliver a coherent material and test record for the defined programme without presenting research success as production approval.

Send your application details
Material references and applicable product standards are listed below. Select the delivery condition and acceptance plan for the specific product and approved application.

TA33 procurement checklist

Connect the application to the material order.

A useful specification connects the intended component, the supplied stock and the acceptance evidence. Share the drawing and known requirements first.

01

Define the application

Provide metal temperature, stress, duration, cycles and the approved component specification.

02

Define the supplied stage

Forged bar, disc blanks and project-specific forgings. Distinguish raw stock, converted blanks and finished parts. Define who controls subsequent processing.

03

Define the acceptance evidence

Define room- and elevated-temperature tests plus structural and defect acceptance for the supplied section.

Example: a useful TA33 material enquiry

TA33 high-temperature forged bar; required dimensions and quantity; standard and drawing revision; delivery condition; intended downstream process; mechanical, structural and dimensional acceptance; traceability, destination and required date.

Identify the approved product specification and any project-specific qualification. The grade designation and chemistry standard alone do not define component acceptance.

Discuss your material requirement ↗

04 / Standards & documentation

Match the standard
to the product.

Choose the specification by product form, material condition and application. Identify the required edition on the order; a chemistry standard alone does not define a finished forging or component.

Hosted PDFs retain their stated editions. Publisher references open separately when no distributable PDF is provided.
Product / reviewInternational / project routeChinese referenceClarify before quotation
Identity & chemistryApproved product and project specificationGB/T 3620.1-2016View PDF ↗Review the complete chemical limits and product requirements; nominal alloy names do not establish automatic interchangeability.
TA33 composition and high-temperature alloy reviewTA33 composition and high-temperature alloy reviewPublisher reference ↗Compare the complete ordered Chinese requirementsResearch context for TA33; use the complete ordered national chemistry limits.
Ti60 processing researchTi60 processing researchPublisher reference ↗Compare the complete ordered Chinese requirementsPrimary research uses a specified experimental composition and processing condition; not a universal product guarantee.
Ti60 long-term creep investigationTi60 long-term creep investigationPublisher reference ↗Compare the complete ordered Chinese requirementsPrimary research on time-dependent behaviour; project test conditions and lot acceptance remain separate.
Drawing-based blanks & partsApproved drawing and controlled manufacturing planAgreed product / project specificationDefine the supply stage, conversion route, heat treatment, structure, NDT, dimensions and traceability. Material certification is separate from finished component qualification.
Agree the order basis.

The purchase order must identify the required revision, grade, product form, condition and inspection. Reference documents do not replace design approval, manufacturing qualification or application-specific acceptance.

Request the controlled specification revision for your order. Any substitution, equivalence or dual-certification claim requires a documented comparison and agreement.

05 / Order coordination

Know the scope
before ordering.

Our founder’s 20 years in titanium inform the questions we ask before quotation and the supply options we review with you.

TA33 custom high-temperature blanks — application illustration
Component application illustration. Actual material records, inspection and performance tests are defined for the order.
A quotation you can evaluate

Agree the grade, standard edition, dimensions, tolerance, condition and quantity before comparing prices.

  • Identify whether inspection, samples and tooling are included.
  • Confirm packaging, transport and delivery terms.
  • Record items that still need technical confirmation.
Acceptance agreed before supply

Confirm material identity, delivery condition, heat-to-piece traceability, dimensional checks and required testing before production. For converted parts, define inspection after forging, heat treatment and machining, including the specified microstructure and NDT scope.

Independent inspection can be discussed with its scope, timing, acceptance criteria and cost agreed for the order.

Delivery with clear milestones

Review the proposed lead time, approvals, production sequence and dispatch requirements. For several product forms, coordinate document and packing readiness together.

Material substitutions and technical changes require written approval. A schedule deviation should identify the impact, decisions needed and next steps.

One contact when an issue arises

Contact TiHubs with the order reference, affected items and supporting photos or inspection records.

We record the issue, review it against the agreed requirements and coordinate the next steps with the relevant manufacturing parties.

01 / Material identity

Material records

Grade, standard, test results and heat or batch identity matched to the supplied items.

  • Material certificate
  • Heat / batch ID
  • Test results
02 / Agreed acceptance

Inspection records

Dimensional and testing records for the agreed scope, including critical drawing requirements.

  • Dimensions
  • Agreed testing
  • Acceptance criteria
03 / Ready for dispatch

Dispatch records

Item identification, packing list, protective packaging and required shipment documents.

  • Packing list
  • Item labels
  • Shipping documents

06 / Questions before sourcing

Before you specify
TA33 / Ti60.

A clear material designation is the beginning. Product form, specification revision, material condition and acceptance complete the requirement.

A useful first enquiry

  • Product and specificationProduct form, standard edition, dimensions and material condition.
  • Order and deliveryQuantity, destination and any required delivery date.
  • Acceptance requirementsDrawing revision, inspection, certificates and packaging.

Not every detail is finalized? Send the information you have. We can help identify the questions to resolve before quotation.

Discuss your requirement

What happens next: requirement review, technical clarification, then a supply proposal and quotation.

What is the main TA33 page focus?

High-temperature forged stock and the time-dependent evidence needed for creep, exposure and fatigue-related acceptance.

Does Ti60 always mean exactly the same composition?

No. Experimental Ti60 compositions vary in the literature. Specify TA33 and the complete ordered chemical limits.

Is TA33 interchangeable with Ti600 or IMI834?

No automatic equivalence is claimed. A substitution needs a full technical comparison and design approval.

Does 600°C-class mean unlimited service at 600°C?

No. Stress, duration, atmosphere, condition and design qualification determine the permitted duty.

Why is a hot tensile test insufficient for creep duty?

It measures a different loading history. Sustained-load deformation needs the specified creep test conditions and acceptance.

What is a dwell-fatigue requirement?

It evaluates cyclic loading that includes a hold period. The waveform, hold time, temperature and specimen condition must be defined.

Why retain extra test stock on a forging?

It allows representative sampling at specified locations and directions before final machining removes that material.

Can high-temperature research results certify a production lot?

No. Production acceptance needs tests and records for the actual ordered material and condition.

What should a TA33 RFQ include?

Send the full alloy designation, form and rough drawing, final condition, service history, creep or fatigue requirements, sampling plan, NDT and quantity.

07 / Your next step

Start with the
requirement you have.

Send the product details, drawing or operating conditions you already know. We will identify missing information and discuss a suitable supply route before quotation.

  1. Requirement review
  2. Technical clarification
  3. Supply proposal and quotation

Combine materials and parts in one enquiry.

Send one list of TA33 forms, sizes and quantities. Include drawing revisions, material conditions and items that must be supplied or dispatched together.

Share the service and acceptance priorities.

Include load and temperature conditions, critical sections, required material records, process qualification, inspection, destination and timing.

Baoji, China · info@tihubs.com

Start your TA33 / Ti60 enquiry

Send your material form, drawing or process conditions. We will help clarify the remaining requirements.

Customer Feedback & RFQ Form (#6)