CategoryQuality, Inspection & Standards
Titanium ultrasonic testing:
specify the evidence
For bar, billet and plate, define the class, coverage and manufacturing stage before comparing inspection offers.

Quick answer
An AMS2631 reference alone is not a complete titanium UT purchase requirement. Identify the applicable revision, product scope, acceptance class, qualified procedure, inspection stage, coverage and report package. Distinguish examination of every item from coverage of its volume and from probability of detection. Preserve the link from inspected parent stock to every delivered cut piece.
01 / Standard and product scope
Specify the inspection as precisely as the titanium
A purchase order stating titanium bar, ultrasonic tested leaves important questions unanswered. Which revision applies, what acceptance class is required, which material volume is examined and at what manufacturing stage? Without those details, two suppliers can quote different inspections while both describe the material as UT tested. Resolve the inspection basis before comparing prices.
This guide addresses purchasing ultrasonic inspection for wrought titanium bar, billet and plate. It is not a procedure for operating an instrument or accepting a safety-critical part. The responsible engineering and nondestructive-testing personnel must define and approve the actual inspection. Procurement’s job is to make that requirement unambiguous and preserve the evidence through delivery.
| Document | Published revision date | Public scope boundary |
|---|---|---|
| AMS2631G | 20 June 2022 | Wrought titanium and titanium-alloy products, cross-section thickness or diameter at least 0.25 in. (6.4 mm) |
| AMS2628C | 17 May 2024 | Enhanced immersion inspection of premium-grade wrought titanium round billet, nominal diameter at least 5 in. (127 mm) |
Sources: SAE public pages for AMS2631G and AMS2628C. The table is a scope comparison, not a reproduction of either document’s acceptance rules. Use the contractually applicable controlled edition.
The material specification and UT requirement do different jobs
The material order defines alloy, product form, condition, dimensions and the applicable material requirements. The UT requirement defines an examination of the supplied product. A material certificate and an ultrasonic report complement each other; neither automatically replaces the other. A correct alloy analysis cannot establish scan coverage, and a favorable ultrasonic result cannot establish chemical composition.
Identify whether the purchase is for a long bar, a cropped billet, a plate blank or a finished component. Do not extend a bar-and-billet requirement to a casting, weld or complex finished forging without reviewing the applicable specification and approved procedure. Similar alloy names do not make different product geometries equally inspectable.
State the revision explicitly when the drawing or customer requirement fixes it. If the order uses a current-revision convention, define how that convention is applied and how changes are reviewed. A supplier should not silently substitute a newer or older edition after quotation. Resolve differences between the drawing, material specification and inspection purchase note through the authorized technical process.
Some applications impose additional requirements beyond a generic bar inspection. For example, the FAA’s guidance for premium titanium rotating engine components discusses staged NDT and enhanced billet inspection. That is a particular application context, not a universal rule for all titanium purchases or evidence that any supplier is approved for engine hardware.

Original purchasing framework: alloy and condition must remain connected to the examination scope and delivered records.
02 / Signals and reference standards
Understand what an ultrasonic result actually compares
Ultrasonic inspection evaluates sound transmitted into material and the signals returned under a defined setup. A displayed response is an indication to interpret, not automatically a measured crack. Geometry, the inspection arrangement and material response all matter. Buyers do not need to interpret waveforms themselves, but they should understand why a report must identify the procedure and reference basis.
Evident’s display tutorial distinguishes echo amplitude from transit time in an A-scan. Amplitude describes response magnitude; time is related to sound path through calibration. A screenshot without setup and location information therefore cannot establish the size or acceptability of a discontinuity.
Instrument certification is not the complete test setup
Evident separates instrument calibration certification from reference calibration for a specific examination. The former addresses instrument performance under documented conditions; the latter establishes the test against appropriate reference standards. Buying a service from a shop with a calibrated instrument does not, by itself, define the inspection performed on your material.
Ask the inspection provider to identify the approved procedure, equipment configuration and relevant reference standard. The report or supporting records should connect those items to the examined stock. Do not request arbitrary settings copied from another supplier’s report. The qualified procedure must address the actual alloy, condition, geometry and required sensitivity.
A reference reflector is not a literal defect-size guarantee
A flat-bottom hole, often abbreviated FBH, is a controlled artificial reflector used in many ultrasonic reference arrangements. Its response supports a defined comparison. A natural discontinuity can differ in shape, orientation and acoustic behavior. A statement referring to an equivalent reflector should not be rewritten as a guarantee that every physical flaw larger than that diameter has been excluded.
Evident’s DGS explanation specifically describes equivalent reflector size as a response comparison with a flat-bottom reflector at a corresponding path. This illustrates the distinction between an acoustic equivalence and a direct geometric measurement. It does not establish that DGS is the required technique for your AMS2631 order.
For a conceptual comparison, two indications with the same screen height are not necessarily equivalent if reference gain, sound path or calibration differs. Conversely, changing display gain can change screen height without changing the material. Keep the result tied to the reference and procedure instead of comparing photographs from unrelated inspections.
Noise and attenuation also need evaluation within the approved method. A quiet-looking display is not sufficient proof of sensitivity, and simply increasing gain is not a universal solution. Ask whether the required examination was demonstrably achievable throughout the specified region and how any limitation was reported. The buyer needs a documented conclusion, not an attractive instrument screenshot.
Use terminology carefully in commercial documents. Detected, evaluated, accepted and rejected describe different steps. An indication can require evaluation without proving a rejectable defect; an accepted item can still contain responses below applicable reporting or rejection criteria. Avoid translating a conforming inspection into an unsupported claim that the stock contains absolutely no discontinuities.
03 / Coverage and manufacturing stage
Make 100% inspection a defined statement
The phrase 100% UT can refer to every piece in the order, the planned coverage of each piece, or both. It does not mean a 100% probability of detecting every possible flaw. State the population and coverage separately. If ten bars are ordered, the inspection record should identify which bars were examined and what region and directions were covered on each.
Ask for a scan plan appropriate to product geometry. For plate, identify the examined faces and how the required volume is addressed. For round bar or billet, identify the inspection arrangement and coverage of the section and length. Procurement should not prescribe a scan pattern from an illustration; it should require the provider’s qualified plan to satisfy the defined requirement.
Identify limitations before cutting the stock
Near-surface regions, ends, edges and geometric features can require special consideration. The actual limitations depend on the method, setup and product. Ask the provider to state any unexamined or inadequately examined regions and the proposed disposition. Do not assume a fixed universal dead-zone distance for all titanium products.
Consider an original arithmetic example, not a test result. A 3,000 mm bar with 50 mm at each end outside a hypothetical qualified inspection region has 2,900 mm of covered length. That is 96.7% of the original length. If both ends are removed and the retained region is correctly identified, the delivered 2,900 mm can correspond to that covered length. This calculation says nothing about cross-sectional coverage or detection probability.
The example shows why crop location and identity matter. A report for a parent bar cannot be applied to a cut piece unless the cut piece is traceably located within the inspected material. A distributor should preserve the link between parent identification, cut map and supplied pieces. If excluded ends are accidentally included, shortening the invoice description does not correct the inspection gap.
The inspection stage changes the question
UT before extensive machining can help identify unsuitable stock before additional cost is committed. However, a stock inspection does not automatically satisfy a requirement for the finished component. Subsequent forming, heat treatment, machining or joining may change the applicable examination needs. State the required stage and final deliverable rather than assuming one incoming inspection covers the entire manufacturing route.
A complex component may need an intermediate inspection shape to make relevant regions accessible. If the engineering plan requires this, include the extra machining and examination in the quotation. Discovering after final machining that a required region cannot be adequately examined creates a design-and-process problem, not merely a missing certificate.
NASA JSC PRC-6504 is an example of a controlled specification that explicitly addresses acceptance class, zones, coverage and inspection sequence. Its requirements belong to its own applicability and invocation. The useful purchasing lesson is to define those subjects, not to import its acceptance numbers into AMS2631.
Document how coverage is demonstrated and what data must be retained. Automated equipment can produce extensive records, but automation alone does not prove a suitable scan. Manual inspection also needs the required evidence and qualified execution. Compare demonstrated capability and record scope rather than assuming that either label guarantees a better examination.

Original hypothetical length calculation: 3,000 mm minus two 50 mm ends leaves 2,900 mm, or 96.7% of original length. No actual UT capability is implied.
04 / Acceptance and deviations
Choose the class through engineering, not a sales shortcut
An acceptance class belongs to a named specification and revision. A letter by itself is incomplete, and a letter from one standard should not be treated as equivalent to the same letter in another. Request the complete contractual reference. Do not build a purchase requirement from an internet table whose edition, product scope or footnotes are missing.
The responsible technical authority should select the inspection requirement from the component’s design, application and customer obligations. Procurement should communicate that decision accurately. Asking the supplier for its standard class can be useful for an initial capability discussion, but it does not establish the class your application requires.
Sensitivity, reporting and rejection are different controls
A reference level establishes a comparison within the inspection. A reporting rule determines what information must be recorded. Acceptance criteria determine disposition under the specification. These concepts may interact, but they are not interchangeable. A purchase note that gives only a reference reflector size can leave other required evaluation criteria undefined.
Review the complete applicable requirements with qualified NDT personnel. Depending on the governing document, evaluation may involve more than one type of response or limitation. Do not reduce the entire inspection to one peak amplitude. The public SAE abstracts used in this article do not expose all normative clauses, so no purported AMS2631 acceptance-limit table is reproduced here.
| Quotation statement | What to clarify before release |
|---|---|
| UT tested | Specification, revision, class, procedure, stage and result |
| 100% inspected | Every supplied item, examined volume, directions and exclusions |
| Calibrated equipment | Specific reference setup and demonstrated suitability for this product |
| No defects | Actual acceptance statement, limitations and traceable report |
| Mill certificate available | Whether the required UT record is included and covers the delivered pieces |
These are clarification prompts, not automatic reasons to reject a supplier. A short quotation may be supported by a complete technical attachment. Review the whole offer and record the agreed scope. The problem is leaving the meaning unresolved until the material arrives or a downstream customer asks for evidence.
Resolve nonconformance without rewriting the result
If a required region cannot be examined or an indication exceeds the applicable criterion, follow the agreed disposition process. Possible next steps depend on the specification and authority: further evaluation, permitted processing and reinspection, removal of material or rejection. A salesperson should not relabel an exception as passed because the delivery date is close.
Keep deviations explicit and approved by the authorized party. A concession should identify the affected material, requirement, technical basis and permitted use. It should not silently change future orders or imply general equivalence. If the customer does not permit concessions, the supply plan must respect that restriction from the outset.
Where additional customer approval of the inspection source is required, confirm it before outsourcing the work. A laboratory’s general competence and its approval for a particular program are different matters. Ask for the applicable evidence without assuming that a logo, generic accreditation or previous unrelated order covers the present requirement.
05 / Reports and traceability
Connect the examination to the pieces you receive
A useful report allows the receiver to answer four questions: what was examined, how was it examined, against what requirement, and what was the result? The format can vary, but those connections must remain clear. A certificate that only repeats a purchase-order number may not establish which pieces or regions were covered.
Identify alloy, product form, heat or lot and individual stock identifiers where required. Include dimensions and the condition at examination sufficiently to connect the report to the supplied material. If a plate was subdivided or a bar cropped after inspection, preserve the mapping. Heat identity alone can be insufficient when several parent products from the same heat had separate inspection outcomes.
Review the technical and disposition fields
The agreed report package should identify the specification and revision, acceptance class, procedure or technique revision, inspection stage and date, and the responsible inspection organization. Include coverage, limitations, relevant results and disposition as required by the contract. Supporting equipment and reference-standard records should be available at the level required by the applicable quality system and order.
Do not demand a universal report template containing every possible instrument parameter. Some information may belong in controlled supporting records rather than the shipment certificate. Agree on what is delivered, what is retained and what can be reviewed. That distinction makes the document package useful without replacing the inspection provider’s approved system.
For recorded data, specify the usable deliverable before the job. A screenshot, a PDF indication map and native acquisition files serve different purposes. Confirm whether the buyer can open and interpret the supplied format and whether supporting setup information is needed. A large data archive without traceable locations and a disposition report may be less useful than a concise, complete inspection package.
Check consistency rather than collecting more paper
Reconcile identifiers across the material certificate, UT report, cutting record, packing list and physical marking. Check that dimensions and quantities make sense after cropping or subdivision. Investigate discrepancies before releasing material to production. A matching file name is not a substitute for a documented relationship between the records and the metal.
Separate missing documentation from a failed test. A clerical omission may be resolved through a corrected traceable report; an unperformed examination cannot be fixed by adding a sentence to a certificate. If the provider issues a correction, retain revision history and the reason. Do not edit the supplier’s signed technical result yourself.
Preserve records for the period required by the project and customer. If no period has been set, resolve it before ordering rather than discovering later that acquisition data are no longer available. The retention arrangement should reflect the intended use and contract, not an arbitrary period copied from another industry.

Material identity, inspection result, cutting map and supplied piece must remain traceably connected.
06 / RFQ and receiving plan
Request a complete inspection scope with the stock
Prepare one controlled enquiry containing material designation and specification, product form, size, quantity, delivery condition and intended downstream use where relevant. Add the UT document and edition, engineer-selected class, required stage, coverage and reporting scope. Identify customer-specific source approvals and hold points before the supplier plans production.
For a hypothetical machined plate component, ask whether the purchased blank is inspected in its supplied condition and whether the component drawing requires another examination after machining. For a hypothetical billet that will be divided into shorter lengths, require the inspection and cut traceability to remain connected. These examples illustrate different purchasing questions, not actual TiHubs inspection jobs.
Ask the supplier to identify exceptions in the quotation. Confirm who performs the examination, what preparation is included, how crop losses affect delivered quantity and whether report review is a release hold point. If the inspection depends on an outside facility, include that step in the delivery schedule.
At receipt, check identity, dimensions, condition and the agreed document package before accepting the material for its intended use. The broader titanium pre-shipment inspection checklist complements this UT-specific review. Tube hydrostatic and eddy-current testing addresses different examination purposes and should not be substituted for a bar UT requirement.
Send TiHubs enquiries for titanium bar and rod, forging billet or plate with the inspection requirement attached. Source capability, approval status, class, coverage and document availability must be confirmed for the actual order. A product enquiry does not imply that every inspection class is routinely available.
The result should be a purchase that can be checked without reconstructing its meaning from sales emails. The material, examined region, governing criteria and final disposition remain linked. That is the practical value of specifying ultrasonic inspection carefully: the buyer receives evidence addressing a defined requirement rather than a reassuring but ambiguous UT label.
07 / Build your RFQ
Prepare a titanium stock and UT enquiry
Attach the engineering inspection requirement to the material enquiry. State the actual product and delivered condition so the supplier can confirm inspection capability, exceptions and records.
Information to include
- Alloy, material specification, form, dimensions and quantity
- UT specification and revision; engineer-selected acceptance class
- Required manufacturing stage, coverage and excluded-region disposition
- Inspection-source approvals, hold points and report deliverables
- Parent-stock identification, cropping and cut-piece traceability
Build your RFQ checklist
Choose the product and add the information you have. Copy the resulting brief or send your requirements to TiHubs. Submitting an enquiry does not place an order.
08 / FAQs
Questions buyers ask
Does 100% UT mean the material is completely defect-free?
No. It must be defined in terms of items and examination coverage, and it does not mean perfect detection of every possible discontinuity. Acceptance is against the specified procedure and criteria, with stated limitations. Avoid replacing that conclusion with an absolute defect-free claim.
Is AMS2631G the same as AMS2628C?
No. Their public scopes differ. AMS2628C addresses enhanced immersion inspection of premium round billet within its stated size scope. Use the document required by the application and approved engineering basis; do not substitute one solely because both concern titanium ultrasonics.
Can I choose an acceptance class from an online table?
The responsible technical authority should define the class using the applicable controlled standard and project requirements. Online summaries can omit revisions, footnotes and evaluation rules. A class letter without its document and edition is incomplete.
Does an FBH reference prove an actual crack diameter?
No. A reference reflector supports an acoustic comparison under a defined setup. Natural discontinuities can have different shapes and orientations. Equivalent reflector response should not be presented as a direct geometric measurement or a universal detection guarantee.
Can a parent-bar report cover cut pieces?
It can support them when the pieces remain traceably located within the examined material and the applicable requirements permit that arrangement. Preserve parent identity, cut mapping and any cropped or excluded regions. Heat number alone may not establish that relationship.
Does a mill material certificate replace the UT report?
Not automatically. The agreed certificate package may include UT results, but it must identify the required inspection and its connection to supplied stock. Chemical and mechanical certification does not establish scan coverage, procedure, acceptance class or inspection-stage conformity.
09 / Key takeaways
Keep the purchase requirements connected.
- Specify revision, class, stage and coverage with the material order.
- Distinguish reference response from actual discontinuity geometry.
- Identify excluded regions and preserve crop traceability.
- Resolve exceptions through the authorized technical process.
- Accept records that connect the result to the delivered metal.
Technical references
Sources and data scope
References reviewed November 15, 2026. Public source summaries support the discussion; the controlled specification, agreed edition and approved project requirements govern acceptance.
- SAE — AMS2631G — Public scope and revision; full acceptance clauses require the controlled standard.
- SAE — AMS2628C — Public scope of enhanced billet immersion inspection.
- NASA JSC — PRC-6504, revision G — Example of a separate controlled inspection specification; not substituted for AMS2631.
- Evident — Calibration concepts — Instrument certification and specific reference calibration are distinct.
- Evident — DGS/AVG — Explanation of equivalent reflector size.
- FAA — AC 33.15-1A — Application-specific guidance for premium titanium rotating engine components.