TA23 / Ti70 · Near-alpha titanium alloy
TA23 / Ti70. Plate for complex marine shapes.
Enquire about TA23 / Ti70 plate and forming blanks for acoustic covers, sonar fairings and complex marine shells, with thickness, contour and post-forming acceptance defined together.
Start with a specification, drawing or application. We’ll help identify the details still needed.
Material review. Supply coordination.
One contact in Baoji, China.
01 / Product forms
Find your TA23 product.
Choose a material form or application. Send the dimensions, service conditions and required records so we can match the manufacturing route to your order.

TA23 / Ti70
TA23 titanium plate
Plate feedstock for Ti70 marine shell and acoustic-cover projects under a defined material specification.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Thickness basis, width, length, flatness, rolling direction and usable edge margin.
- Manufacturing review
- Connect the starting thickness to the final shell and any forming or weld preparation losses.
- Inspection priorities
- Thickness variation, surface quality, specified directional properties and plate identity.

TA23 / Ti70
TA23 forming sheet
Sheet enquiries for thinner curved parts where the supplied condition must suit the planned forming route.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Nominal or minimum thickness, blank size, surface finish and orientation.
- Manufacturing review
- Provide curvature, local strain areas, forming sequence and the required final condition.
- Inspection priorities
- Representative forming behavior, local thinning and surface integrity after the agreed trial.

TA23 / Ti70
TA23 contour-cut blanks
Flat blanks cut to a developed layout for complex curved-shell manufacture.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Contour file, trim allowance, orientation marks, quantity and edge tolerance.
- Manufacturing review
- Agree nesting, cut-edge preparation and identification before the blanks enter forming.
- Inspection priorities
- Contour dimensions, edge condition and linkage to the parent plate.

TA23 / Ti70
TA23 curved-blank enquiries
Drawing-based requests for an intermediate formed shape, subject to confirmed forming and inspection capability.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Surface model, datum scheme, trim line and minimum final wall.
- Manufacturing review
- State the supplied stage and the approved forming route, including any later welding or heat treatment.
- Inspection priorities
- Contour mapping, thickness survey and the ordered material tests at the specified stage.

TA23 / Ti70
TA23 shell-joint strips
Plate-derived strips and joint-development material for the shell fabricator’s approved design.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Width, length, thickness, rolling direction and edge preparation.
- Manufacturing review
- Define their structural role and joining sequence; do not treat matching chemistry as joint qualification.
- Inspection priorities
- Fit-up dimensions, surface cleanliness and traceable material for joint evaluation.

TA23 / Ti70
TA23 qualification coupons
Representative plate for forming, weld, impact or acoustic-assembly development under a project test plan.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Production thickness and condition, specimen orientation and reserved test allowance.
- Manufacturing review
- Define the test purpose, fabrication history and responsible acceptance authority.
- Inspection priorities
- Keep heat, plate position and processing records with each specimen set.
Images illustrate material forms and application possibilities. Reference markings identify specification options; they do not establish dual certification, stock availability or approval of finished equipment.
Define the shape. Share the service.
These details help turn a material enquiry into a comparable quotation.
01 / Drawing review
Acoustic-cover plate selection
TA23 plate and sheet in the thickness and condition specified by the design. Agree thickness and surface controls for incoming plate, then apply the designer’s acoustic and structural verification to the completed assembly.
Discuss your drawing02 / Drawing review
Complex curved-shell forming
Contour-cut blanks and production-intent forming sheet. Inspect a representative first article for contour, minimum wall and surface damage under the agreed forming plan.
Discuss your drawing03 / Drawing review
Sonar-fairing material enquiries
Plate, developed blanks and trial material for the approved fairing design. Require traceable stock and the agreed post-fabrication tests; no sonar performance or service rating is implied by a material quotation.
Discuss your drawing02 / Material identity
What is TA23 / Ti70 titanium?
TA23, commonly called Ti70, is a near-alpha titanium alloy associated with formed marine structures and acoustic-cover applications. This page centers on plate that must become a controlled curved shell: starting thickness, orientation, forming history, welded seams and the final inspection stage all matter. Acoustic performance belongs to the designed and tested assembly; it is not guaranteed by the alloy name or a raw-plate certificate.
Specify the exact standard edition, form and delivery condition. Nominal chemistry is only one part of an order; strength, microstructure, dimensional acceptance and traceability also need to be defined.
| Review item | Order basis | What to confirm |
|---|---|---|
| Final shell thickness | Minimum wall after forming | Map critical regions and define how local thinning will be measured and reported. |
| Complex contour | Drawing datums and inspection model | Agree surface-profile tolerance, trim allowance and the inspection stage after forming and joining. |
| Acoustic requirement | Complete assembly verification | Let the approved design and test plan define performance; raw plate chemistry is not an acoustic guarantee. |
| Impact acceptance | Method, orientation and condition | Specify specimen basis, temperature and whether results apply before or after fabrication. |
| Process traceability | Plate-to-panel material map | Retain heat, plate position, cut, forming, joining and specimen records throughout conversion. |
| Selected element · wt % | Reference composition |
|---|---|
| Aluminium · Al | 2.5 nominal |
| Zirconium · Zr | 2 nominal |
| Iron · Fe | 1 nominal |
| Titanium · Ti | Balance |
Nominal Ti70 composition, wt %, is shown for identification. Obtain the complete ordered TA23 chemistry and product requirements, including impurity and analysis limits, for acceptance.
TA23 and Ti70
Ti70 is the commonly used name associated with TA23. Record both on the enquiry, together with the exact product specification and condition.
TA23 and TA24 / Ti75
These are different alloy systems and purchasing routes. A common marine application does not make their chemistry, processing or acceptance interchangeable.
Acoustic material and acoustic assembly
Raw plate can be specified for an acoustic-cover design, but transmission performance depends on the complete geometry, thickness, joints and test conditions.
Incoming plate and formed shell
Forming and welding can change local thickness, shape and material condition. Define which properties and dimensions must be accepted after fabrication.
03 / Application priorities
TA23 in application.
Review each main use through its service conditions, material choice, manufacturing route and acceptance plan. These are sourcing discussions; approved drawings and qualification requirements govern the final component.
Application review / 01
Acoustic-cover plate selection
Ti70 is associated with marine acoustic-cover applications. Material selection should start from the cover design and its verification plan, rather than assigning an acoustic transmission value to stock plate.
Products & manufacturing
TA23 plate and sheet in the thickness and condition specified by the design.
Service & design review
Identify shell geometry, interfaces and required assembly testing. Keep acoustic acceptance separate from ordinary material release.
Purchase & inspection priorities
Agree thickness and surface controls for incoming plate, then apply the designer’s acoustic and structural verification to the completed assembly.
Application review / 02
Complex curved-shell forming
A doubly curved part needs more than a flat-plate size on an order. Local strain and trimming can make the useful starting blank substantially different from the finished outline.
Products & manufacturing
Contour-cut blanks and production-intent forming sheet.
Service & design review
Provide the surface model, developed blank, trim margin, forming stages and areas where thinning is critical.
Purchase & inspection priorities
Inspect a representative first article for contour, minimum wall and surface damage under the agreed forming plan.
Application review / 03
Sonar-fairing material enquiries
For a sonar fairing, Ti70 stock is one element of an engineered shell. The supplier enquiry should define material and fabrication scope while leaving system performance to the qualified design and test process.
Products & manufacturing
Plate, developed blanks and trial material for the approved fairing design.
Service & design review
Specify the required material condition, shell thickness, joint locations and component-level inspection documents.
Purchase & inspection priorities
Require traceable stock and the agreed post-fabrication tests; no sonar performance or service rating is implied by a material quotation.
Application review / 04
Post-forming thickness control
The original plate thickness is not necessarily the minimum wall in a formed component. A clear inspection map helps connect starting stock to the most demanding regions of the final shell.
Products & manufacturing
Plate and sheet with an agreed thickness basis and forming allowance.
Service & design review
Identify thinning-sensitive areas, measurement access and the stage at which minimum wall must be demonstrated.
Purchase & inspection priorities
Agree measurement method, locations and reporting for incoming stock and the formed part separately.
Application review / 05
Welded curved-panel joints
A curved shell assembled from several panels needs controlled edges and joint alignment. Material identity alone does not determine the behavior of the seam or the distortion after welding.
Products & manufacturing
Cut plate panels, joint strips and representative weld coupons.
Service & design review
Provide joint preparation, panel fit-up limits, welding sequence and the controlled joining procedure.
Purchase & inspection priorities
Inspect material and edge condition before welding, then apply the specified joint examination and final contour checks.
Application review / 06
Impact and toughness requirements
An impact requirement needs a defined specimen, direction, temperature and material stage. Published research results should not be copied into an order without considering the actual product thickness and processing.
Products & manufacturing
Representative plate and specimens associated with the supplied or fabricated condition.
Service & design review
State the applicable test standard, sample orientation, test temperature and whether results are required after forming or welding.
Purchase & inspection priorities
Agree acceptance criteria and sampling with the responsible engineer, retaining traceability to the evaluated plate and process history.
Application review / 07
Forming-route qualification
A new shell geometry or changed material route can require a forming trial. The trial is useful only if it reproduces the stock condition and critical features that matter in production.
Products & manufacturing
Matched blanks and coupons from the proposed material source and route.
Service & design review
Define the trial part, process sequence, inspection points and approval milestones before purchasing a large plate lot.
Purchase & inspection priorities
Compare dimensional, surface and required mechanical results after the full trial sequence, then document the accepted production basis.
Application review / 08
Marine shell material records
Complex fabrication divides and combines plate through cutting, forming and joining. A consistent identification plan helps connect final panels and test pieces back to their original material.
Products & manufacturing
Identified plates, nested blanks, joint strips and reserved specimens.
Service & design review
Specify the material map, marking method, protected surfaces and record transfers at each processing stage.
Purchase & inspection priorities
Reconcile plate certificates, cut records, forming lots and weld or test reports before assembly release.
TA23 procurement checklist
Connect the application to the material order.
A useful specification connects the intended component, the supplied stock and the acceptance evidence. Share the drawing and known requirements first.
Define the application
Identify shell geometry, interfaces and required assembly testing. Keep acoustic acceptance separate from ordinary material release.
Define the supplied stage
TA23 plate and sheet in the thickness and condition specified by the design. Distinguish raw stock, converted blanks and finished parts. Define who controls subsequent processing.
Define the acceptance evidence
Agree thickness and surface controls for incoming plate, then apply the designer’s acoustic and structural verification to the completed assembly.
Example: a useful TA23 material enquiry
TA23 titanium plate; required dimensions and quantity; standard and drawing revision; delivery condition; intended downstream process; mechanical, structural and dimensional acceptance; traceability, destination and required date.
Identify the approved product specification and any project-specific qualification. The grade designation and chemistry standard alone do not define component acceptance.
Discuss your material requirement ↗04 / Standards & documentation
Match the standard
to the product.
Choose the specification by product form, material condition and application. Identify the required edition on the order; a chemistry standard alone does not define a finished forging or component.
| Product / review | International / project route | Chinese reference | Clarify before quotation |
|---|---|---|---|
| Identity & chemistry | Approved product and project specification | GB/T 3620.1-2016View PDF ↗ | Review the complete chemical limits and product requirements; nominal alloy names do not establish automatic interchangeability. |
| Ti70 forming and impact research · CN109504877B | Ti70 forming and impact research · CN109504877BPublisher reference ↗ | Compare the complete ordered Chinese requirements | Sunrui patent publication, 2020. Technical background for Ti70 plate processing and impact evaluation, not a procurement standard. |
| Marine titanium alloy review · Metal World 2021 | Marine titanium alloy review · Metal World 2021Publisher reference ↗ | Compare the complete ordered Chinese requirements | Baoti-authored review identifies TA23 / Ti70 and marine plate applications. Published examples do not establish a supplied-lot guarantee. |
| CN109504877B · English translation | Project and product requirements remain separately defined | CN109504877B · English translationView PDF ↗ | High-impact-toughness and high-ductility TA23 alloy plate. Original publication: 2020-04-14. Near-alpha Ti-2.5Al-2Zr-1Fe plate; forming, welding, impact performance and sonar-fairing material research. English reference translation; original Chinese publication controls. Not a purchase specification. |
| Drawing-based blanks & parts | Approved drawing and controlled manufacturing plan | Agreed product / project specification | Define the supply stage, conversion route, heat treatment, structure, NDT, dimensions and traceability. Material certification is separate from finished component qualification. |
The purchase order must identify the required revision, grade, product form, condition and inspection. Reference documents do not replace design approval, manufacturing qualification or application-specific acceptance.
Request the controlled specification revision for your order. Any substitution, equivalence or dual-certification claim requires a documented comparison and agreement.
05 / Order coordination
Know the scope
before ordering.
Our founder’s 20 years in titanium inform the questions we ask before quotation and the supply options we review with you.

A quotation you can evaluate
Agree the grade, standard edition, dimensions, tolerance, condition and quantity before comparing prices.
- Identify whether inspection, samples and tooling are included.
- Confirm packaging, transport and delivery terms.
- Record items that still need technical confirmation.
Acceptance agreed before supply
Confirm material identity, delivery condition, heat-to-piece traceability, dimensional checks and required testing before production. For converted parts, define inspection after forging, heat treatment and machining, including the specified microstructure and NDT scope.
Independent inspection can be discussed with its scope, timing, acceptance criteria and cost agreed for the order.
Delivery with clear milestones
Review the proposed lead time, approvals, production sequence and dispatch requirements. For several product forms, coordinate document and packing readiness together.
Material substitutions and technical changes require written approval. A schedule deviation should identify the impact, decisions needed and next steps.
One contact when an issue arises
Contact TiHubs with the order reference, affected items and supporting photos or inspection records.
We record the issue, review it against the agreed requirements and coordinate the next steps with the relevant manufacturing parties.
Material records
Grade, standard, test results and heat or batch identity matched to the supplied items.
Inspection records
Dimensional and testing records for the agreed scope, including critical drawing requirements.
Dispatch records
Item identification, packing list, protective packaging and required shipment documents.
06 / Questions before sourcing
Before you specify
TA23 / Ti70.
A clear material designation is the beginning. Product form, specification revision, material condition and acceptance complete the requirement.
A useful first enquiry
- Product and specificationProduct form, standard edition, dimensions and material condition.
- Order and deliveryQuantity, destination and any required delivery date.
- Acceptance requirementsDrawing revision, inspection, certificates and packaging.
Not every detail is finalized? Send the information you have. We can help identify the questions to resolve before quotation.
What happens next: requirement review, technical clarification, then a supply proposal and quotation.
Are TA23 and Ti70 the same naming route?
Ti70 is the common alloy name associated with TA23. Use both names together with the exact product specification and supplied condition.
What is this page’s main product focus?
Plate, sheet and developed forming blanks for acoustic covers and complex marine shells. Converted shapes are project enquiries subject to confirmed capability.
Does TA23 plate guarantee acoustic transparency?
No. Acoustic performance must be defined and verified for the complete assembly, including geometry, wall thickness, joints and test conditions.
Why state minimum wall after forming?
Curved-shell forming can produce local thinning. The initial nominal plate thickness alone does not demonstrate the required finished wall.
Can complex curved blanks be quoted?
They can be reviewed from a surface model, datums, trim line, thickness limits and approved forming route. Clarify whether you need flat stock or an intermediate formed shape.
Is TA23 interchangeable with TA24 / Ti75?
No automatic substitution is claimed. They have different alloy chemistries and need a complete material, processing and acceptance comparison.
How should impact requirements be specified?
Identify the method, specimen and orientation, test temperature, sampling and material stage. Agree criteria appropriate to the product and intended fabrication.
Should weld trials use the actual plate thickness?
Use representative production material as required by the qualification plan, including thickness, condition, orientation and the intended joining sequence.
What information is needed for a TA23 quotation?
Send the application, plate or blank dimensions, surface model where relevant, condition, forming and welding stages, standard editions, inspection plan, quantity and delivery requirements.
07 / Your next step
Start with the
requirement you have.
Send the product details, drawing or operating conditions you already know. We will identify missing information and discuss a suitable supply route before quotation.
- Requirement review
- Technical clarification
- Supply proposal and quotation
Combine materials and parts in one enquiry.
Send one list of TA23 forms, sizes and quantities. Include drawing revisions, material conditions and items that must be supplied or dispatched together.
Share the service and acceptance priorities.
Include load and temperature conditions, critical sections, required material records, process qualification, inspection, destination and timing.
Baoji, China · info@tihubs.com
Start your TA23 / Ti70 enquiry
Send your material form, drawing or process conditions. We will help clarify the remaining requirements.
TiHubs specification library
CN109504877B · English translation
High-impact-toughness and high-ductility TA23 alloy plate. Original publication: 2020-04-14. Near-alpha Ti-2.5Al-2Zr-1Fe plate; forming, welding, impact performance and sonar-fairing material research. English reference translation; original Chinese publication controls. Not a purchase specification.