TA24 / Ti75 titanium products on a dark metallic background

TA24 / Ti75 · Near-alpha titanium alloy

TA24 / Ti75. Marine structures, specified in detail.

Discuss Ti75 plate, forged bar and structural blanks with section size, seawater exposure, welding and toughness requirements connected from the start.

Start with a specification, drawing or application. We’ll help identify the details still needed.

Material review. Supply coordination.
One contact in Baoji, China.

TA24 / Ti75Ti-3Al-2Mo-2Zr
Near-alpha titanium alloyMarine structural plate & forgings
One contact20 years of founder experience · 100+ Baoji factories

01 / Product forms

Find your TA24 product.

Choose a material form or application. Send the dimensions, service conditions and required records so we can match the manufacturing route to your order.

TA24 marine structural plate — illustrative supply form
01 / 06

TA24 / Ti75

TA24 marine structural plate

Primary stock for drawing-approved marine panels and machined structural details.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Thickness, usable area, flatness, rolling direction and cut allowance.
Manufacturing review
Identify welded edges, load direction and any through-thickness requirement.
Inspection priorities
Directional tensile and toughness tests, surface inspection and specified internal examination.
TA24 forged bar — illustrative supply form
02 / 06

TA24 / Ti75

TA24 forged bar

Round stock for seawater-exposed structural details and machining blanks.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Diameter, length, straightness and surface preparation.
Manufacturing review
Specify final section and thermal condition; review heavy stock removal.
Inspection priorities
Structure and properties representative of the supplied diameter.
TA24 forging billet — illustrative supply form
03 / 06

TA24 / Ti75

TA24 forging billet

Conversion stock for structural forgings with a planned deformation route.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Cut mass, starting section, cropping and test extensions.
Manufacturing review
Link billet acceptance to the required final forging envelope.
Inspection priorities
Chemistry, macrostructure, internal examination and heat identity.
TA24 structural ring blanks — illustrative supply form
04 / 06

TA24 / Ti75

TA24 structural ring blanks

Illustrative annular forgings for marine equipment and enclosure designs.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Outside diameter, bore, height, ovality and machining stock.
Manufacturing review
Specify pressure or mechanical loads and approved specimen positions.
Inspection priorities
Ring-direction properties, NDT coverage and dimensional allowance.
TA24 sheet and light panels — illustrative supply form
05 / 06

TA24 / Ti75

TA24 sheet and light panels

Flat stock for project-approved fabricated covers and lighter marine details.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Thickness, width, length, edge condition and forming direction.
Manufacturing review
Review radii, joining sequence and distortion control.
Inspection priorities
Surface quality, thickness uniformity and acceptance after forming.
TA24 marine machining blanks — illustrative supply form
06 / 06

TA24 / Ti75

TA24 marine machining blanks

Drawing-based blocks and housing blanks with retained finishing stock.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Datums, envelope, critical interfaces and minimum material allowance.
Manufacturing review
Separate rough machining from final assembly and pressure testing.
Inspection priorities
Heat-to-piece traceability, critical dimensions and agreed NDT.

Images illustrate material forms and application possibilities. Reference markings identify specification options; they do not establish dual certification, stock availability or approval of finished equipment.

Define the shape. Share the service.

These details help turn a material enquiry into a comparable quotation.

01 / Drawing review

Seawater-exposed structural panels

Plate and cut structural blanks. Agree directional mechanical tests, toughness where required and plate internal examination.

Discuss your drawing

02 / Drawing review

Marine equipment housings

Plate, forged bar and rough housing blanks. Separate raw-material release from dimensional inspection and the finished housing pressure test.

Discuss your drawing

03 / Drawing review

Welded structural assemblies

Plate, sheet and matched structural blanks. Specify parent-material records and the required weld examination and joint-property tests.

Discuss your drawing

02 / Material identity

What is TA24 / Ti75 titanium?

TA24, also known as Ti75, is a Ti-3Al-2Mo-2Zr alloy associated with marine material development. Its page concentrates on structural stock and fabricated assemblies rather than generic corrosion-resistant tubing. For buyers, the important combination is usable section, toughness, manufacturing route and the evidence required after joining or forging. TA24-1 is a separate composition variant and should not be silently substituted.

Specify the exact standard edition, form and delivery condition. Nominal chemistry is only one part of an order; strength, microstructure, dimensional acceptance and traceability also need to be defined.

Review itemOrder basisWhat to confirm
Marine structural strengthThickness and delivery conditionDefine tensile sampling, orientation and section coverage for load-bearing plate and forgings.
Fracture resistanceDrawing acceptance planSpecify any impact, fracture-toughness or crack-growth testing appropriate to the component.
Seawater exposureReal assembly conditionsReview crevices, galvanic contacts, biofouling and corrosion protection as part of system design.
Welded structureJoint-specific qualificationDefine weld inspection and the property requirements for joints and heat-affected regions.
Forging soundnessQualified NDT coverageAgree examination volume, reference sensitivity and acceptance for thick or complex blanks.
Selected element · wt %Reference composition
Aluminium · Al2.0–3.8
Molybdenum · Mo1.0–2.5
Zirconium · Zr1.0–3.0
Iron · Fe0.30 max
Oxygen · O0.15 max
Titanium · TiBalance

Selected composition limits, wt %, from GB/T 3620.1-2016. Use the complete ordered standard for all impurity, residual-element and analysis requirements.

TA24 versus TA24-1

The national chemistry table lists both grades separately. Specify the intended designation and complete impurity limits.

Marine structure versus tube duty

A load-bearing plate or forging needs section-specific mechanical and structural acceptance. Tube corrosion data alone cannot release a structural component.

Plate versus forged blank

Rolling direction, forging flow and specimen orientation affect how a material order supports the drawing. Compare usable material and testing, not only mass.

Ti75 versus other marine alloys

TA22, TA31 and Ti75 address different alloy systems and requirements. Select against the approved design and fabrication route.

03 / Application priorities

TA24 in application.

Review each main use through its service conditions, material choice, manufacturing route and acceptance plan. These are sourcing discussions; approved drawings and qualification requirements govern the final component.

Application review / 01

Seawater-exposed structural panels

Ti75 plate enquiries should connect seawater exposure with the actual load path. A marine label does not define the required strength or crack tolerance.

Products & manufacturing

Plate and cut structural blanks.

Service & design review

Provide load direction, thickness, welded joints, crevices and immersion conditions.

Purchase & inspection priorities

Agree directional mechanical tests, toughness where required and plate internal examination.

Send your application details

Application review / 02

Marine equipment housings

A housing may be governed by external pressure, local attachments or sealing geometry. The material order should identify which requirement drives the blank.

Products & manufacturing

Plate, forged bar and rough housing blanks.

Service & design review

Supply pressure envelope, wall transitions, seal datums and the approved manufacturing route.

Purchase & inspection priorities

Separate raw-material release from dimensional inspection and the finished housing pressure test.

Send your application details

Application review / 03

Welded structural assemblies

Weldability is useful only when the joining procedure and resulting joint meet the design. Ti75 assembly enquiries need the parent stock and joint requirements together.

Products & manufacturing

Plate, sheet and matched structural blanks.

Service & design review

Define joint geometry, access, shielding, distortion allowance and any post-weld treatment under the approved procedure.

Purchase & inspection priorities

Specify parent-material records and the required weld examination and joint-property tests.

Send your application details

Application review / 04

Forged marine attachments

Lugs and attachment details concentrate load in small sections. A forging enquiry should preserve material flow and inspection access around these regions.

Products & manufacturing

Billet, forged bar and drawing-controlled preforms.

Service & design review

Identify principal stresses, transition radii, final section and specimen placement.

Purchase & inspection priorities

Require the agreed macrostructure, local surface checks and internal soundness before final machining.

Send your application details

Application review / 05

Annular enclosure interfaces

Ring blanks provide a practical route to circular interfaces but need a defined orientation and finishing envelope. The ring is not automatically a qualified pressure part.

Products & manufacturing

Rings and annular conversion stock.

Service & design review

State radial and axial loads, sealing faces, bolt pattern and joining details.

Purchase & inspection priorities

Agree ovality, allowance, sampling direction and examination of the complete section.

Send your application details

Application review / 06

Toughness-led stock selection

Where crack tolerance drives the design, nominal chemistry and tensile strength alone are insufficient. The relevant product thickness and condition must be represented in testing.

Products & manufacturing

Plate and forgings with retained representative test stock.

Service & design review

Provide the specified toughness method, specimen orientation, service temperature and acceptance threshold.

Purchase & inspection priorities

Link results to the actual product lot and section; identify any size limitations on valid testing.

Send your application details

Application review / 07

Seawater and dissimilar-metal interfaces

A titanium component can alter the corrosion behaviour of a connected assembly. Examine mating materials and electrical contact as part of the project review.

Products & manufacturing

Machined connection blanks and plate details.

Service & design review

Describe crevices, coatings, isolation, cathodic protection and cleaning exposure for engineering assessment.

Purchase & inspection priorities

Define any environment-specific test and the surface condition to be supplied; avoid blanket seawater guarantees.

Send your application details

Application review / 08

Large-section supply planning

For Ti75, the requested section can determine the viable rolling or forging route and the test programme. Confirm these before treating a catalogue size as available stock.

Products & manufacturing

Large plate, forged bar and conversion billet enquiries.

Service & design review

Share net and rough dimensions, quantity, test extensions and staged delivery needs.

Purchase & inspection priorities

Agree source capability, usable dimensions, section-representative properties and release documents.

Send your application details
Material references and applicable product standards are listed below. Select the delivery condition and acceptance plan for the specific product and approved application.

TA24 procurement checklist

Connect the application to the material order.

A useful specification connects the intended component, the supplied stock and the acceptance evidence. Share the drawing and known requirements first.

01

Define the application

Provide load direction, thickness, welded joints, crevices and immersion conditions.

02

Define the supplied stage

Plate and cut structural blanks. Distinguish raw stock, converted blanks and finished parts. Define who controls subsequent processing.

03

Define the acceptance evidence

Agree directional mechanical tests, toughness where required and plate internal examination.

Example: a useful TA24 material enquiry

TA24 marine structural plate; required dimensions and quantity; standard and drawing revision; delivery condition; intended downstream process; mechanical, structural and dimensional acceptance; traceability, destination and required date.

Identify the approved product specification and any project-specific qualification. The grade designation and chemistry standard alone do not define component acceptance.

Discuss your material requirement ↗

04 / Standards & documentation

Match the standard
to the product.

Choose the specification by product form, material condition and application. Identify the required edition on the order; a chemistry standard alone does not define a finished forging or component.

Hosted PDFs retain their stated editions. Publisher references open separately when no distributable PDF is provided.
Product / reviewInternational / project routeChinese referenceClarify before quotation
Identity & chemistryApproved product and project specificationGB/T 3620.1-2016View PDF ↗Review the complete chemical limits and product requirements; nominal alloy names do not establish automatic interchangeability.
Ti75 deformation researchTi75 deformation researchPublisher reference ↗Compare the complete ordered Chinese requirementsPrimary research identifies Ti75 as Ti-3Al-2Mo-2Zr; reported experimental forming results are not production acceptance limits.
Drawing-based blanks & partsApproved drawing and controlled manufacturing planAgreed product / project specificationDefine the supply stage, conversion route, heat treatment, structure, NDT, dimensions and traceability. Material certification is separate from finished component qualification.
Agree the order basis.

The purchase order must identify the required revision, grade, product form, condition and inspection. Reference documents do not replace design approval, manufacturing qualification or application-specific acceptance.

Request the controlled specification revision for your order. Any substitution, equivalence or dual-certification claim requires a documented comparison and agreement.

05 / Order coordination

Know the scope
before ordering.

Our founder’s 20 years in titanium inform the questions we ask before quotation and the supply options we review with you.

TA24 marine machining blanks — application illustration
Component application illustration. Actual material records, inspection and performance tests are defined for the order.
A quotation you can evaluate

Agree the grade, standard edition, dimensions, tolerance, condition and quantity before comparing prices.

  • Identify whether inspection, samples and tooling are included.
  • Confirm packaging, transport and delivery terms.
  • Record items that still need technical confirmation.
Acceptance agreed before supply

Confirm material identity, delivery condition, heat-to-piece traceability, dimensional checks and required testing before production. For converted parts, define inspection after forging, heat treatment and machining, including the specified microstructure and NDT scope.

Independent inspection can be discussed with its scope, timing, acceptance criteria and cost agreed for the order.

Delivery with clear milestones

Review the proposed lead time, approvals, production sequence and dispatch requirements. For several product forms, coordinate document and packing readiness together.

Material substitutions and technical changes require written approval. A schedule deviation should identify the impact, decisions needed and next steps.

One contact when an issue arises

Contact TiHubs with the order reference, affected items and supporting photos or inspection records.

We record the issue, review it against the agreed requirements and coordinate the next steps with the relevant manufacturing parties.

01 / Material identity

Material records

Grade, standard, test results and heat or batch identity matched to the supplied items.

  • Material certificate
  • Heat / batch ID
  • Test results
02 / Agreed acceptance

Inspection records

Dimensional and testing records for the agreed scope, including critical drawing requirements.

  • Dimensions
  • Agreed testing
  • Acceptance criteria
03 / Ready for dispatch

Dispatch records

Item identification, packing list, protective packaging and required shipment documents.

  • Packing list
  • Item labels
  • Shipping documents

06 / Questions before sourcing

Before you specify
TA24 / Ti75.

A clear material designation is the beginning. Product form, specification revision, material condition and acceptance complete the requirement.

A useful first enquiry

  • Product and specificationProduct form, standard edition, dimensions and material condition.
  • Order and deliveryQuantity, destination and any required delivery date.
  • Acceptance requirementsDrawing revision, inspection, certificates and packaging.

Not every detail is finalized? Send the information you have. We can help identify the questions to resolve before quotation.

Discuss your requirement

What happens next: requirement review, technical clarification, then a supply proposal and quotation.

What does Ti75 mean on a TA24 enquiry?

Ti75 is the commonly used alloy name associated with TA24 / Ti-3Al-2Mo-2Zr. Keep the exact national designation and product requirements on the order.

Is TA24-1 acceptable when TA24 is specified?

Not automatically. They are separately listed composition variants and require an approved comparison.

Which products receive priority on this page?

Structural plate, forged bar and billet, followed by rings and drawing-based marine blanks.

Can TA24 be used for a pressure housing?

Only within an approved design, material specification and manufacturing route. A grade description does not establish a pressure rating or diving depth.

Why specify rolling or forging direction?

Direction affects sampling and how the material supports the component load path. Identify it on the drawing and inspection plan.

Are weld properties covered by a parent-plate certificate?

No. The joining procedure, weld examination and any required joint tests are separate acceptance steps.

When should toughness testing be included?

When required by the design or product specification. State method, temperature, specimen orientation and acceptance criteria.

Does seawater service eliminate corrosion review?

No. Crevices, temperature, deposits, mating metals and protection systems still need assessment.

What dimensions should I quote for a forging?

Provide both the final component and rough-stock envelope, including machining allowance, test extensions and any critical directional requirements.

07 / Your next step

Start with the
requirement you have.

Send the product details, drawing or operating conditions you already know. We will identify missing information and discuss a suitable supply route before quotation.

  1. Requirement review
  2. Technical clarification
  3. Supply proposal and quotation

Combine materials and parts in one enquiry.

Send one list of TA24 forms, sizes and quantities. Include drawing revisions, material conditions and items that must be supplied or dispatched together.

Share the service and acceptance priorities.

Include load and temperature conditions, critical sections, required material records, process qualification, inspection, destination and timing.

Baoji, China · info@tihubs.com

Start your TA24 / Ti75 enquiry

Send your material form, drawing or process conditions. We will help clarify the remaining requirements.

Customer Feedback & RFQ Form (#6)