TA25 / Ti-3Al-2.5V-Pd titanium products on a dark metallic background

TA25 / Ti-3Al-2.5V-Pd · Near-alpha titanium alloy

TA25 / Ti-3Al-2.5V-Pd. Corrosion-aware tubing and forming.

Source TA25 tube, sheet and bar with the palladium content, wall tolerance, forming condition and inspection route clearly specified.

Start with a specification, drawing or application. We’ll help identify the details still needed.

Material review. Supply coordination.
One contact in Baoji, China.

TA25 / Ti-3Al-2.5V-PdTi-3Al-2.5V-0.05Pd
Near-alpha titanium alloyTubing, formed parts & fluid systems
One contact20 years of founder experience · 100+ Baoji factories

01 / Product forms

Find your TA25 product.

Choose a material form or application. Send the dimensions, service conditions and required records so we can match the manufacturing route to your order.

TA25 titanium tube — illustrative supply form
01 / 06

TA25 / Ti-3Al-2.5V-Pd

TA25 titanium tube

Straight tubing is the priority enquiry for thin-wall fluid and heat-transfer designs specifying this palladium-bearing family.

Specification
TA25 product specification; ASTM B338-17(2026) Grade 18 only when explicitly ordered and fully demonstrated.
Size & delivery
Outside diameter, minimum or nominal wall, length, straightness and end finish.
Manufacturing review
Specify seamless or welded route, supplied condition, subsequent bending and tube-end joining.
Inspection priorities
Wall eccentricity, surface quality, chemistry and agreed tube integrity tests.
TA25 titanium sheet — illustrative supply form
02 / 06

TA25 / Ti-3Al-2.5V-Pd

TA25 titanium sheet

Flat blanks for formed covers and light fabricated details with a defined corrosion-related material requirement.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Thickness, width, length, flatness and rolling direction.
Manufacturing review
Give bend radii, draw depth, edge condition and any post-forming treatment.
Inspection priorities
Thickness uniformity, surface defects and forming acceptance on representative stock.
TA25 titanium bar — illustrative supply form
03 / 06

TA25 / Ti-3Al-2.5V-Pd

TA25 titanium bar

Matching-alloy stock for small machined fittings and fluid-system details.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Diameter, cut length, straightness and finishing allowance.
Manufacturing review
Identify sealing surfaces, threads and the intended connection to tubing.
Inspection priorities
Material identity, dimensional results and mechanical tests in the supplied condition.
TA25 wire enquiries — illustrative supply form
04 / 06

TA25 / Ti-3Al-2.5V-Pd

TA25 wire enquiries

Solid wire for project-approved forming routes, with diameter and surface capability reviewed before commitment.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Wire diameter, coil or straight length, surface finish and packaging.
Manufacturing review
State the actual use; material wire is not automatically qualified welding filler.
Inspection priorities
Surface continuity, diameter variation and ordered ductility or forming tests.
TA25 bent-tube enquiries — illustrative supply form
05 / 06

TA25 / Ti-3Al-2.5V-Pd

TA25 bent-tube enquiries

Illustrative bent tube shapes for drawing-based fabrication review.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Centerline radius, bend angle, tangent lengths, ovality and minimum wall.
Manufacturing review
Agree tooling, material condition, lubrication removal and the inspection stage.
Inspection priorities
Wall thinning, ovality, wrinkles, cracks and any required leak test after bending.
TA25 tube-end and fitting blanks — illustrative supply form
06 / 06

TA25 / Ti-3Al-2.5V-Pd

TA25 tube-end and fitting blanks

Short tubular and coupling blanks for a defined connection design.

Specification
Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
Size & delivery
Bore, outside diameter, sealing length, end preparation and machining datums.
Manufacturing review
Review joining method and compatibility between the fitting and tube specifications.
Inspection priorities
End geometry, surface cleanliness and piece identification through assembly.

Images illustrate material forms and application possibilities. Reference markings identify specification options; they do not establish dual certification, stock availability or approval of finished equipment.

Define the shape. Share the service.

These details help turn a material enquiry into a comparable quotation.

01 / Drawing review

Condenser and heat-exchanger tubing

Straight tube in the specified seamless or welded route, with tube-end preparation defined. Agree dimensional, surface and tube-integrity tests and verify the full Grade 18 specification if that certification is required.

Discuss your drawing

02 / Drawing review

Bent fluid-circuit tubing

Straight TA25 tube and drawing-controlled bent lengths. Inspect minimum wall and ovality at the bends, surface condition and the agreed integrity test after fabrication.

Discuss your drawing

03 / Drawing review

Tube-to-fitting interfaces

Tube, bar-derived fittings and short coupling blanks. Measure critical ends and sealing faces; retain separate tube and fitting certificates and the required assembly inspection.

Discuss your drawing

02 / Material identity

What is TA25 / Ti-3Al-2.5V-Pd titanium?

TA25 adds palladium to the Ti-3Al-2.5V family. The page focuses on tubing and formed-product enquiries where wall control, fabrication and corrosive-service review matter together. Grade 18 is the international family reference. A TA25 designation alone does not establish compliance with an ASTM tube standard or qualify a bent or welded assembly.

Specify the exact standard edition, form and delivery condition. Nominal chemistry is only one part of an order; strength, microstructure, dimensional acceptance and traceability also need to be defined.

Review itemOrder basisWhat to confirm
Pd-bearing identityHeat analysis and ordered standardCheck palladium as well as aluminum and vanadium; do not substitute ordinary Ti-3Al-2.5V without agreement.
Tube geometryOutside diameter and wall mapControl minimum wall, eccentricity, ovality and straightness over the ordered length.
Bend integrityFinal bend geometryAssess wall thinning, ovalization, surface damage and dimensional recovery after bending.
Corrosive fluidsProject service envelopeEvaluate fluid chemistry, operating temperature, crevices and joining materials before selecting the tube route.
Tube acceptanceApplicable tube specificationDefine examination, leak or pressure testing and end preparation under the ordered product requirements.
Selected element · wt %Reference composition
Aluminium · Al2.5–3.5
Vanadium · V2.0–3.0
Palladium · Pd0.04–0.08
Iron · Fe0.25 max
Oxygen · O0.15 max
Titanium · TiBalance

Selected composition limits, wt %, from GB/T 3620.1-2016. Use the complete ordered standard for all impurity, residual-element and analysis requirements.

TA25 versus TA18 / Grade 9

TA25 includes palladium. A standard Ti-3Al-2.5V tube does not become TA25 through a surface treatment or a change in paperwork.

TA25 versus Grade 18

The alloy-family comparison is useful for sourcing, but tube dimensions, test methods, condition and full chemical limits must also match the requested standard.

Tube versus bar certification

A bar standard cannot establish tube wall quality, leak tightness or tube-specific tests. Choose the standard by the actual supplied form.

TA25 versus TA26

TA26 uses ruthenium rather than palladium. Treat them as separate materials and evaluate any proposed substitution explicitly.

03 / Application priorities

TA25 in application.

Review each main use through its service conditions, material choice, manufacturing route and acceptance plan. These are sourcing discussions; approved drawings and qualification requirements govern the final component.

Application review / 01

Condenser and heat-exchanger tubing

Grade 18 appears in the ASTM B338 tube scope, making this a relevant international purchasing route for the TA25 alloy family. The complete tube specification and environment still govern a particular exchanger.

Products & manufacturing

Straight tube in the specified seamless or welded route, with tube-end preparation defined.

Service & design review

Provide fluid on both sides, temperature, pressure, cleaning method, fouling and tube-to-tubesheet joint design.

Purchase & inspection priorities

Agree dimensional, surface and tube-integrity tests and verify the full Grade 18 specification if that certification is required.

Send your application details

Application review / 02

Bent fluid-circuit tubing

The value of a tube order is the usable wall and shape after forming. A straight tube that meets its incoming dimensions may still need a representative bend trial for a tight circuit.

Products & manufacturing

Straight TA25 tube and drawing-controlled bent lengths.

Service & design review

State centerline radii, bend sequence, clamp zones, pressure cycles and whether ends are expanded or flared.

Purchase & inspection priorities

Inspect minimum wall and ovality at the bends, surface condition and the agreed integrity test after fabrication.

Send your application details

Application review / 03

Tube-to-fitting interfaces

Leaks and assembly problems often arise at the connection rather than the straight span. Matching the alloy name does not resolve fit, seal geometry or joining requirements.

Products & manufacturing

Tube, bar-derived fittings and short coupling blanks.

Service & design review

Provide connector design, bore transitions, sealing finish, allowable mismatch and joining procedure. Define the supplied stage of each item.

Purchase & inspection priorities

Measure critical ends and sealing faces; retain separate tube and fitting certificates and the required assembly inspection.

Send your application details

Application review / 04

Corrosion-driven Grade 9 review

A designer may consider a palladium-bearing alternative when the existing Ti-3Al-2.5V system faces a specific environmental concern. That review should preserve the original structural and fabrication requirements.

Products & manufacturing

Trial tubing or sheet in the intended production thickness and condition.

Service & design review

Describe the observed or predicted corrosion mechanism, fluid chemistry, crevices, temperature and cleaning exposure. Compare the complete original and proposed specifications.

Purchase & inspection priorities

Require palladium analysis and the project-defined corrosion and forming evaluation before approving substitution.

Send your application details

Application review / 05

Formed sheet enclosures

Sheet and light fabricated details need formability, joining access and surface control as well as nominal alloy chemistry. TA25 enquiries should identify why palladium-bearing stock is specified.

Products & manufacturing

Sheet, cut flat blanks and simple formed-part enquiries.

Service & design review

Supply bend and draw geometry, wall targets, rolling direction, joining sequence and the exposed surfaces.

Purchase & inspection priorities

Check edge integrity, final thickness, profile and any corrosion-sensitive heat-affected or worked regions under the agreed plan.

Send your application details

Application review / 06

Thin-wall inspection planning

For tubing, minimum wall and local defects can be more consequential than an average section measurement. The inspection method must suit the diameter, wall and manufacturing route.

Products & manufacturing

Tube lots with accessible ends and representative test lengths.

Service & design review

State whether wall is nominal or minimum, permitted eccentricity, surface criteria and the required examination method.

Purchase & inspection priorities

Agree calibration, coverage, rejection limits and reports for the actual tube size; do not substitute a generic bar inspection.

Send your application details

Application review / 07

Tube fabrication trials

A new size or source should be assessed using the intended bends and joining operations. A sample in a different heat-treatment state cannot establish the behaviour of recurring production stock.

Products & manufacturing

Representative straight tube, bend samples and tube-end blanks.

Service & design review

Define trial geometry, process variables, cleaning and joining stages and who approves the trial. Keep material source and condition recorded.

Purchase & inspection priorities

Compare incoming wall and surface results with post-forming dimensions and integrity; document the accepted production window.

Send your application details

Application review / 08

Mixed-form fluid-system orders

A circuit may combine tube, small machined fittings and sheet supports. A coordinated enquiry should keep these as separate material lines while matching their drawing and delivery requirements.

Products & manufacturing

Tube, bar, sheet and approved connection blanks.

Service & design review

List each form, size, condition, specification, drawing revision and assembly deadline. Identify items requiring common heat or lot relationships.

Purchase & inspection priorities

Reconcile tube, bar and sheet certificates with item markings and packing lists; verify palladium content for every material heat.

Send your application details
Material references and applicable product standards are listed below. Select the delivery condition and acceptance plan for the specific product and approved application.

TA25 procurement checklist

Connect the application to the material order.

A useful specification connects the intended component, the supplied stock and the acceptance evidence. Share the drawing and known requirements first.

01

Define the application

Provide fluid on both sides, temperature, pressure, cleaning method, fouling and tube-to-tubesheet joint design.

02

Define the supplied stage

Straight tube in the specified seamless or welded route, with tube-end preparation defined. Distinguish raw stock, converted blanks and finished parts. Define who controls subsequent processing.

03

Define the acceptance evidence

Agree dimensional, surface and tube-integrity tests and verify the full Grade 18 specification if that certification is required.

Example: a useful TA25 material enquiry

TA25 titanium tube; required dimensions and quantity; standard and drawing revision; delivery condition; intended downstream process; mechanical, structural and dimensional acceptance; traceability, destination and required date.

Identify the approved product specification and any project-specific qualification. The grade designation and chemistry standard alone do not define component acceptance.

Discuss your material requirement ↗

04 / Standards & documentation

Match the standard
to the product.

Choose the specification by product form, material condition and application. Identify the required edition on the order; a chemistry standard alone does not define a finished forging or component.

Hosted PDFs retain their stated editions. Publisher references open separately when no distributable PDF is provided.
Product / reviewInternational / project routeChinese referenceClarify before quotation
Identity & chemistryApproved product and project specificationGB/T 3620.1-2016View PDF ↗Review the complete chemical limits and product requirements; nominal alloy names do not establish automatic interchangeability.
ASTM B338-17(2026) · Grade 18 tubeASTM B338-17(2026) · Grade 18 tubePublisher reference ↗Compare the complete ordered Chinese requirementsTube-specific route for condensers and heat exchangers; verify full Grade 18 requirements.
ASTM B348/B348M-25 · Grade 18 barASTM B348/B348M-25 · Grade 18 barPublisher reference ↗Compare the complete ordered Chinese requirementsBar and billet reference; it does not replace tube-specific acceptance.
Drawing-based blanks & partsApproved drawing and controlled manufacturing planAgreed product / project specificationDefine the supply stage, conversion route, heat treatment, structure, NDT, dimensions and traceability. Material certification is separate from finished component qualification.
Agree the order basis.

The purchase order must identify the required revision, grade, product form, condition and inspection. Reference documents do not replace design approval, manufacturing qualification or application-specific acceptance.

Request the controlled specification revision for your order. Any substitution, equivalence or dual-certification claim requires a documented comparison and agreement.

05 / Order coordination

Know the scope
before ordering.

Our founder’s 20 years in titanium inform the questions we ask before quotation and the supply options we review with you.

TA25 tube-end and fitting blanks — application illustration
Component application illustration. Actual material records, inspection and performance tests are defined for the order.
A quotation you can evaluate

Agree the grade, standard edition, dimensions, tolerance, condition and quantity before comparing prices.

  • Identify whether inspection, samples and tooling are included.
  • Confirm packaging, transport and delivery terms.
  • Record items that still need technical confirmation.
Acceptance agreed before supply

Confirm material identity, delivery condition, heat-to-piece traceability, dimensional checks and required testing before production. For converted parts, define inspection after forging, heat treatment and machining, including the specified microstructure and NDT scope.

Independent inspection can be discussed with its scope, timing, acceptance criteria and cost agreed for the order.

Delivery with clear milestones

Review the proposed lead time, approvals, production sequence and dispatch requirements. For several product forms, coordinate document and packing readiness together.

Material substitutions and technical changes require written approval. A schedule deviation should identify the impact, decisions needed and next steps.

One contact when an issue arises

Contact TiHubs with the order reference, affected items and supporting photos or inspection records.

We record the issue, review it against the agreed requirements and coordinate the next steps with the relevant manufacturing parties.

01 / Material identity

Material records

Grade, standard, test results and heat or batch identity matched to the supplied items.

  • Material certificate
  • Heat / batch ID
  • Test results
02 / Agreed acceptance

Inspection records

Dimensional and testing records for the agreed scope, including critical drawing requirements.

  • Dimensions
  • Agreed testing
  • Acceptance criteria
03 / Ready for dispatch

Dispatch records

Item identification, packing list, protective packaging and required shipment documents.

  • Packing list
  • Item labels
  • Shipping documents

06 / Questions before sourcing

Before you specify
TA25 / Ti-3Al-2.5V-Pd.

A clear material designation is the beginning. Product form, specification revision, material condition and acceptance complete the requirement.

A useful first enquiry

  • Product and specificationProduct form, standard edition, dimensions and material condition.
  • Order and deliveryQuantity, destination and any required delivery date.
  • Acceptance requirementsDrawing revision, inspection, certificates and packaging.

Not every detail is finalized? Send the information you have. We can help identify the questions to resolve before quotation.

Discuss your requirement

What happens next: requirement review, technical clarification, then a supply proposal and quotation.

What is the main TA25 product focus?

Tubing and formed-product enquiries are the priority, supported by matching sheet, bar and drawing-based fitting requests where supply capability is confirmed.

How does TA25 differ from ordinary Ti-3Al-2.5V?

It includes an intentional palladium addition. TA18 or Grade 9 stock is not a substitute without an approved material comparison.

Which international grade should a buyer compare?

Grade 18 is the Ti-3Al-2.5V-Pd family. Review complete chemistry, condition, form and inspection before requiring dual certification.

Does ASTM B338 include Grade 18?

Yes. B338-17(2026) includes Grade 18 tubing for condensers, evaporators and heat exchangers. The purchased tube must meet the complete ordered requirements.

Can every TA25 tube be bent to the same radius?

No. Diameter, wall, condition, tooling and bend sequence matter. Provide the actual geometry and acceptance limits for a forming review.

Should wall thickness be nominal or minimum?

Specify which basis the design uses. Minimum wall after bending, allowed eccentricity and inspection locations should be stated explicitly.

Is TA25 wire qualified welding filler?

Not simply because the chemistry is similar. Filler classification, joining procedure and qualification must be specified separately.

Are bent tubes tested again after forming?

Where required by the design, the inspection plan should address wall thinning, ovality, surface damage and integrity after bending rather than only incoming straight tube.

What information makes a TA25 enquiry useful?

Include tube route, diameter, wall basis, length, bend drawing, condition, fluid exposure, standard edition, inspection, quantity and connection details.

07 / Your next step

Start with the
requirement you have.

Send the product details, drawing or operating conditions you already know. We will identify missing information and discuss a suitable supply route before quotation.

  1. Requirement review
  2. Technical clarification
  3. Supply proposal and quotation

Combine materials and parts in one enquiry.

Send one list of TA25 forms, sizes and quantities. Include drawing revisions, material conditions and items that must be supplied or dispatched together.

Share the service and acceptance priorities.

Include load and temperature conditions, critical sections, required material records, process qualification, inspection, destination and timing.

Baoji, China · info@tihubs.com

Start your TA25 / Ti-3Al-2.5V-Pd enquiry

Send your material form, drawing or process conditions. We will help clarify the remaining requirements.

Customer Feedback & RFQ Form (#6)