TC25 Titanium Alloy · Heat-resistant alpha-beta titanium alloy
TC25 Titanium Alloy. Forged stock for thermal service.
Source TC25 forged bar, billet and compressor-part blanks. Define thermal condition, microstructure, creep or fatigue evidence and the final inspection stage.
Start with a specification, drawing or application. We’ll help identify the details still needed.
Material review. Supply coordination.
One contact in Baoji, China.
01 / Product forms
Find your TC25 product.
Choose a material form or application. Send the dimensions, service conditions and required records so we can match the manufacturing route to your order.

TC25 Titanium Alloy
TC25 forged titanium bar
Forged round stock for approved compressor and thermal-service machining routes.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Diameter, usable length, straightness and surface condition.
- Manufacturing review
- Specify delivered thermal state, subsequent conversion and removal allowance.
- Inspection priorities
- Structure, directional mechanical results, surface quality and agreed internal examination.

TC25 Titanium Alloy
TC25 conversion billet
Billet enquiries for qualified forging programmes and representative material testing.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Section, cut weight, length and test-stock allowance.
- Manufacturing review
- Define final section, deformation orientation, cropping and thermal route.
- Inspection priorities
- Incoming structure, chemistry and specified surface or internal inspection.

TC25 Titanium Alloy
TC25 stepped forgings
Application illustration: stepped stock for drawing-controlled thermal-service components.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Drawing envelope, critical section changes, datums and finish allowance.
- Manufacturing review
- Review forging route, thermal history, structural requirements and sampling.
- Inspection priorities
- Require heat and lot identity, full chemical analysis, delivery condition, dimensional results and the agreed mechanical and structural tests. Define NDT method, coverage and acceptance criteria in the order.

TC25 Titanium Alloy
TC25 compressor disc blanks
Application illustration: disc-shaped stock for a project-approved compressor design.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Outside diameter, bore, web and rim sections, and retained test material.
- Manufacturing review
- Agree deformation route, condition, specimen locations and final machining sequence.
- Inspection priorities
- Internal soundness, structure, directional properties and drawing-specific dimensional acceptance.

TC25 Titanium Alloy
TC25 compressor blade blanks
Application illustration: rough blade-shaped preforms supplied at the agreed manufacturing stage.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Airfoil and root envelopes, orientation and surface-removal allowance.
- Manufacturing review
- Review preform geometry, thermal route, final surface requirements and inspection stages.
- Inspection priorities
- Critical transitions, surface integrity, structure and the specified examination.

TC25 Titanium Alloy
TC25 ring & custom blanks
Application illustration: ring-shaped stock and custom blanks for approved thermal-service equipment.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Outside and inside diameters, height, drawing datums and usable allowance.
- Manufacturing review
- Confirm the permitted conversion route, final condition and test plan.
- Inspection priorities
- Require heat and lot identity, full chemical analysis, delivery condition, dimensional results and the agreed mechanical and structural tests. Define NDT method, coverage and acceptance criteria in the order.
Images illustrate material forms and application possibilities. Reference markings identify specification options; they do not establish dual certification, stock availability or approval of finished equipment.
Define the shape. Share the service.
These details help turn a material enquiry into a comparable quotation.
01 / Drawing review
Drawing-controlled blanks
Provide rough and finished drawings, datum positions, critical sections, machining allowance and the intended conversion route.
Discuss your drawing02 / Drawing review
Heat treatment & process sequence
Identify the required delivery condition and subsequent manufacturing steps. Agree process records, sampling stages and dimensional checks after thermal processing.
Discuss your drawing03 / Drawing review
Component inspection planning
Specify surface integrity, microstructure, NDT, dimensional acceptance and traceability. Identify which tests apply to raw material and which apply to the finished component.
Discuss your drawing02 / Material identity
What is TC25 Titanium Alloy titanium?
TC25 is a heat-resistant alpha-beta titanium alloy containing aluminium, molybdenum, zirconium, tin, tungsten and silicon. Compressor-related forged stock is a priority purchasing direction. Published research shows that thermal history and microstructure affect creep and fatigue behaviour, so a reference test temperature or tensile value must not be presented as a universal component operating limit.
Specify the exact standard edition, form and delivery condition. Nominal chemistry is only one part of an order; strength, microstructure, dimensional acceptance and traceability also need to be defined.
| Review item | Order basis | What to confirm |
|---|---|---|
| Material condition | Define the ordered heat-treatment state | Tie test results to the same conversion and thermal history as the supplied product. |
| Strength and ductility | Product- and section-dependent | Specify tensile, proof strength, elongation, sampling location and test direction in the purchase requirement. |
| Microstructure | Agree acceptance limits | Review grain structure, alpha morphology, surface alpha case and metallographic sampling for the manufacturing route. |
| Fatigue and fracture | Application-specific validation | A material tensile certificate does not establish component life. Specify any fatigue, toughness or crack-growth evaluation separately. |
| Non-destructive examination | Drawing / product specification | Define method, calibration, coverage, acceptance class and reporting before production. |
| Selected element · wt % | Reference composition |
|---|---|
| Aluminium · Al | 6.2–7.2 |
| Molybdenum · Mo | 1.5–2.5 |
| Zirconium · Zr | 0.8–2.5 |
| Tin · Sn | 0.8–2.5 |
| Tungsten · W | 0.5–1.5 |
| Silicon · Si | 0.10–0.25 |
| Iron · Fe | 0.15 max |
| Oxygen · O | 0.15 max |
| Titanium · Ti | Balance |
Selected composition limits, wt %, from GB/T 3620.1-2016. Use the complete ordered standard for all impurity, residual-element and analysis requirements.
TC25 is not ASTM Grade 25
Chinese TC25 is a heat-resistant multi-element alloy. ASTM Grade 25 is a different Ti-6Al-4V-based nickel-palladium alloy.
Thermal condition and structure
Microstructure and thermal history influence creep and fatigue behaviour. Specify the delivered state and acceptance plan rather than quoting an isolated research result.
Creep versus tensile strength
Short-duration tensile tests do not establish long-duration deformation or rupture performance. Add the tests required by the approved design.
Environment and fatigue
Surface degradation can affect fatigue performance. Service exposure and surface integrity belong in the review for cyclically loaded components.
03 / Application priorities
TC25 in application.
Review each main use through its service conditions, material choice, manufacturing route and acceptance plan. These are sourcing discussions; approved drawings and qualification requirements govern the final component.
Application review / 01
Compressor disc stock
TC25 disc enquiries should connect the forging geometry to the thermal and cyclic demands of the approved design. The bore, web and rim may need different sampling provisions and inspection access.
Products & manufacturing
Billet, forged disc blanks and conversion stock.
Service & design review
Provide the disc drawing, section map, load and temperature envelope, forging route and final thermal specification. Agree retained test stock before production.
Purchase & inspection priorities
Specify structural acceptance, NDT and directional mechanical tests. Any creep or fatigue qualification must match the project requirements and supplied condition.
Application review / 02
Compressor blade preforms
TC25 blade-shaped stock requires control of the root-to-airfoil transition, orientation and surface removal. A preform order must identify the manufacturing stages still required before the component can be released.
Products & manufacturing
Forged bar and blade preforms.
Service & design review
Share final geometry, root requirements, machining allowance, thermal sequence and surface-integrity requirements.
Purchase & inspection priorities
Agree microstructure, critical dimensions, surface inspection and specified NDT after the relevant processing stages. Finished-blade acceptance remains separate.
Application review / 03
Creep-sensitive thermal service
For sustained elevated-temperature loading, creep behaviour is a separate design consideration from room-temperature tensile strength. TC25 research demonstrates why the material state and test conditions must be identified.
Products & manufacturing
Representative bar, forgings and test blanks.
Service & design review
State the approved stress, temperature and duration requirements and the applicable test procedure. Define whether production acceptance or a qualification programme is required.
Purchase & inspection priorities
Use results tied to the actual material condition and sampling. Do not interpret a published experiment as a universal service-life or temperature guarantee.
Application review / 04
Fatigue-sensitive components
Cyclic performance depends on geometry, material condition and surface integrity. A TC25 enquiry should identify critical locations and the accepted processing route before stock is selected.
Products & manufacturing
Bar, disc blanks and structural forgings.
Service & design review
Provide load modes, critical radii, surface finish, residual processing requirements and any environmental exposure.
Purchase & inspection priorities
Specify the required coupon or component fatigue evidence separately from tensile acceptance. Maintain traceability through finishing and inspection.
Application review / 05
Ring & casing-related blanks
Ring-shaped or casing-related stock can be reviewed when the approved design specifies TC25. The enquiry should identify wall transitions, joining and the final material state.
Products & manufacturing
Ring and custom-forging enquiries.
Service & design review
Provide envelope, wall sections, datums, machining allowance and the permitted conversion route. Confirm actual manufacturing capability for the size.
Purchase & inspection priorities
Agree internal examination, structure, dimensions and tests after the specified treatment or joining stages.
Application review / 06
Heat-treatment & structure control
The thermal state of TC25 must be matched to the intended application. Processing affects the resulting structure, so an order should identify acceptance evidence as well as the name of a treatment.
Products & manufacturing
Bar, billet and forgings in the defined delivery condition.
Service & design review
Provide the controlling procedure, section range, processing owner and specimen locations. Clarify subsequent machining or thermal steps.
Purchase & inspection priorities
Review metallographic and mechanical results for the actual delivered state. Later processing requires the appropriate final-stage checks.
Application review / 07
Surface exposure & durability review
Environmental exposure and surface degradation may change the fatigue behaviour of a thermal-service component. TC25 material selection should therefore include the expected storage, handling and service surface conditions.
Products & manufacturing
Machining stock and representative test blanks.
Service & design review
Identify corrosive exposure, cleaning, surface protection and critical fatigue locations. Define any environmental validation required by the design programme.
Purchase & inspection priorities
Control surface damage and retain evidence of the accepted condition. Laboratory exposure results apply only within their tested scope.
Application review / 08
Qualification & recurring supply
A repeatable TC25 order needs stable source, process and drawing requirements. Trial lots should represent the intended production section and material state.
Products & manufacturing
First-article lots and scheduled approved blanks.
Service & design review
Agree controlled variables, inspection hold points, change-review requirements, lot sizes and delivery sequence.
Purchase & inspection priorities
Compile heat, conversion, thermal and final inspection records. Reconcile piece identity and packing documentation before dispatch.
TC25 procurement checklist
Connect the application to the material order.
A useful specification connects the intended component, the supplied stock and the acceptance evidence. Share the drawing and known requirements first.
Define the application
Provide the disc drawing, section map, load and temperature envelope, forging route and final thermal specification. Agree retained test stock before production.
Define the supplied stage
Billet, forged disc blanks and conversion stock. Distinguish raw stock, converted blanks and finished parts. Define who controls subsequent processing.
Define the acceptance evidence
Specify structural acceptance, NDT and directional mechanical tests. Any creep or fatigue qualification must match the project requirements and supplied condition.
Example: a useful TC25 material enquiry
TC25 forged titanium bar; required dimensions and quantity; standard and drawing revision; delivery condition; intended downstream process; mechanical, structural and dimensional acceptance; traceability, destination and required date.
Identify the approved product specification and any project-specific qualification. The grade designation and chemistry standard alone do not define component acceptance.
Discuss your material requirement ↗04 / Standards & documentation
Match the standard
to the product.
Choose the specification by product form, material condition and application. Identify the required edition on the order; a chemistry standard alone does not define a finished forging or component.
| Product / review | International / project route | Chinese reference | Clarify before quotation |
|---|---|---|---|
| Identity & chemistry | Approved product and project specification | GB/T 3620.1-2016View PDF ↗ | Review the complete chemical limits and product requirements; nominal alloy names do not establish automatic interchangeability. |
| TC25 heat treatment and creep research | TC25 heat treatment and creep researchPublisher reference ↗ | Compare the complete ordered Chinese requirements | Original experimental work links TC25 thermal history and microstructure to creep behaviour. Its test conditions are not universal design allowables. |
| TC25 environmental fatigue research | TC25 environmental fatigue researchPublisher reference ↗ | Compare the complete ordered Chinese requirements | Original experimental work examines fatigue after a simulated marine exposure. Application review must remain specific to the approved material, environment and loading. |
| Drawing-based blanks & parts | Approved drawing and controlled manufacturing plan | Agreed product / project specification | Define the supply stage, conversion route, heat treatment, structure, NDT, dimensions and traceability. Material certification is separate from finished component qualification. |
The purchase order must identify the required revision, grade, product form, condition and inspection. Reference documents do not replace design approval, manufacturing qualification or application-specific acceptance.
Request the controlled specification revision for your order. Any substitution, equivalence or dual-certification claim requires a documented comparison and agreement.
05 / Order coordination
Know the scope
before ordering.
Our founder’s 20 years in titanium inform the questions we ask before quotation and the supply options we review with you.

A quotation you can evaluate
Agree the grade, standard edition, dimensions, tolerance, condition and quantity before comparing prices.
- Identify whether inspection, samples and tooling are included.
- Confirm packaging, transport and delivery terms.
- Record items that still need technical confirmation.
Acceptance agreed before supply
Confirm material identity, delivery condition, heat-to-piece traceability, dimensional checks and required testing before production. For converted parts, define inspection after forging, heat treatment and machining, including the specified microstructure and NDT scope.
Independent inspection can be discussed with its scope, timing, acceptance criteria and cost agreed for the order.
Delivery with clear milestones
Review the proposed lead time, approvals, production sequence and dispatch requirements. For several product forms, coordinate document and packing readiness together.
Material substitutions and technical changes require written approval. A schedule deviation should identify the impact, decisions needed and next steps.
One contact when an issue arises
Contact TiHubs with the order reference, affected items and supporting photos or inspection records.
We record the issue, review it against the agreed requirements and coordinate the next steps with the relevant manufacturing parties.
Material records
Grade, standard, test results and heat or batch identity matched to the supplied items.
Inspection records
Dimensional and testing records for the agreed scope, including critical drawing requirements.
Dispatch records
Item identification, packing list, protective packaging and required shipment documents.
06 / Questions before sourcing
Before you specify
TC25 Titanium Alloy.
A clear material designation is the beginning. Product form, specification revision, material condition and acceptance complete the requirement.
A useful first enquiry
- Product and specificationProduct form, standard edition, dimensions and material condition.
- Order and deliveryQuantity, destination and any required delivery date.
- Acceptance requirementsDrawing revision, inspection, certificates and packaging.
Not every detail is finalized? Send the information you have. We can help identify the questions to resolve before quotation.
What happens next: requirement review, technical clarification, then a supply proposal and quotation.
What is TC25 titanium?
TC25 is a heat-resistant alpha-beta titanium alloy containing aluminium, molybdenum, zirconium, tin, tungsten and silicon. Compressor-related forged stock is a priority purchasing direction. Published research shows that thermal history and microstructure affect creep and fatigue behaviour, so a reference test temperature or tensile value must not be presented as a universal component operating limit.
Is TC25 ASTM Grade 25?
No. These designations represent different alloy systems. The Chinese TC25 chemistry must not be confused with the nickel-palladium-containing ASTM grade.
Which products are the priority?
Forged bar, billet and drawing-controlled compressor disc or blade blanks are the main enquiries. Rings and custom blanks require size and route confirmation.
Can you quote a universal TC25 operating temperature?
A universal limit would be misleading. Temperature capability depends on stress, duration, environment, condition and the approved component design.
Why specify creep tests separately?
Short-duration tensile strength does not establish long-duration deformation or rupture behaviour. Use the testing and acceptance required by the design.
What matters for heat treatment?
State the controlled procedure, section, delivered condition, structural requirements and representative sampling. Link tests to the actual supplied state.
Are published fatigue results a component guarantee?
No. Geometry, surface condition, thermal history, loading and environment affect fatigue. Qualification must match the intended application.
What documents should accompany TC25?
Require heat and lot identity, full chemical analysis, delivery condition, dimensional results and the agreed mechanical and structural tests. Define NDT method, coverage and acceptance criteria in the order.
What should a TC25 RFQ include?
Include form, dimensions, quantity, drawing and standard revisions, condition, thermal and load requirements, inspection, destination and source restrictions.
07 / Your next step
Start with the
requirement you have.
Send the product details, drawing or operating conditions you already know. We will identify missing information and discuss a suitable supply route before quotation.
- Requirement review
- Technical clarification
- Supply proposal and quotation
Combine materials and parts in one enquiry.
Send one list of TC25 forms, sizes and quantities. Include drawing revisions, material conditions and items that must be supplied or dispatched together.
Share the service and acceptance priorities.
Include load and temperature conditions, critical sections, required material records, process qualification, inspection, destination and timing.
Baoji, China · info@tihubs.com
Start your TC25 Titanium Alloy enquiry
Send your material form, drawing or process conditions. We will help clarify the remaining requirements.