TC6 Titanium Alloy · Alpha-beta titanium alloy
TC6 Titanium Alloy. Forged stock for compressor parts.
Source TC6 forged bar, billet and drawing-controlled blanks for compressor and aerospace component manufacturing. Define structure, heat treatment and inspection together.
Start with a specification, drawing or application. We’ll help identify the details still needed.
Material review. Supply coordination.
One contact in Baoji, China.
01 / Product forms
Find your TC6 product.
Choose a material form or application. Send the dimensions, service conditions and required records so we can match the manufacturing route to your order.

TC6 Titanium Alloy
TC6 forged titanium bar
Forged round stock for compressor-part machining and approved conversion routes.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Diameter, usable length, straightness and surface condition.
- Manufacturing review
- State delivered thermal condition, subsequent forging or machining and minimum stock allowance.
- Inspection priorities
- Structure, directional mechanical testing, surface quality and specified ultrasonic examination.

TC6 Titanium Alloy
TC6 conversion billet
Cut billet for qualified forging programmes and controlled preform manufacture.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Section, cut weight, length and cropping allowance.
- Manufacturing review
- Define final section, deformation direction, thermal sequence and retained test material.
- Inspection priorities
- Chemistry, incoming structure, surface defects and agreed internal inspection.

TC6 Titanium Alloy
TC6 structural forgings
Application illustration: stepped forgings supplied at the agreed manufacturing stage.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Drawing envelope, datum faces, critical radii and finish allowance.
- Manufacturing review
- Review die or open-forging route, grain-flow expectations and inspection access.
- Inspection priorities
- Require heat and lot identity, full chemical analysis, delivery condition, dimensional results and the agreed mechanical and structural tests. Define NDT method, coverage and acceptance criteria in the order.

TC6 Titanium Alloy
TC6 compressor blade blanks
Application illustration: rough blade-shaped preforms for an approved compressor design.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Airfoil envelope, root geometry, length and machining allowance.
- Manufacturing review
- Identify forging orientation, final treatment, surface removal and critical transition requirements.
- Inspection priorities
- Root and airfoil dimensions, surface integrity, structure and specified NDT.

TC6 Titanium Alloy
TC6 compressor disc blanks
Application illustration: disc-shaped forging blanks with a defined bore and rim allowance.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Outside diameter, bore, web thickness, rim section and test-stock provisions.
- Manufacturing review
- Agree the forging route, thermal history, sampling positions and machining sequence.
- Inspection priorities
- Internal soundness, directional properties, structure and drawing-controlled dimensions.

TC6 Titanium Alloy
TC6 custom machining blanks
Application illustration: stepped blanks for drawing-specific aerospace hardware.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Rough and final drawings, datums, minimum usable stock and quantity.
- Manufacturing review
- Separate rough machining, thermal processing, finishing and final-component release.
- Inspection priorities
- Require heat and lot identity, full chemical analysis, delivery condition, dimensional results and the agreed mechanical and structural tests. Define NDT method, coverage and acceptance criteria in the order.
Images illustrate material forms and application possibilities. Reference markings identify specification options; they do not establish dual certification, stock availability or approval of finished equipment.
Define the shape. Share the service.
These details help turn a material enquiry into a comparable quotation.
01 / Drawing review
Drawing-controlled blanks
Provide rough and finished drawings, datum positions, critical sections, machining allowance and the intended conversion route.
Discuss your drawing02 / Drawing review
Heat treatment & process sequence
Identify the required delivery condition and subsequent manufacturing steps. Agree process records, sampling stages and dimensional checks after thermal processing.
Discuss your drawing03 / Drawing review
Component inspection planning
Specify surface integrity, microstructure, NDT, dimensional acceptance and traceability. Identify which tests apply to raw material and which apply to the finished component.
Discuss your drawing02 / Material identity
What is TC6 Titanium Alloy titanium?
TC6 is an aluminium-chromium-molybdenum titanium alloy with iron and silicon additions. Compressor discs and blades are documented application directions, making forged stock and conversion blanks the priority procurement forms. The purchase specification must connect the supplied section and thermal condition to the approved component drawing; nominal chemistry alone does not establish flight-part acceptance.
Specify the exact standard edition, form and delivery condition. Nominal chemistry is only one part of an order; strength, microstructure, dimensional acceptance and traceability also need to be defined.
| Review item | Order basis | What to confirm |
|---|---|---|
| Material condition | Define the ordered heat-treatment state | Tie test results to the same conversion and thermal history as the supplied product. |
| Strength and ductility | Product- and section-dependent | Specify tensile, proof strength, elongation, sampling location and test direction in the purchase requirement. |
| Microstructure | Agree acceptance limits | Review grain structure, alpha morphology, surface alpha case and metallographic sampling for the manufacturing route. |
| Fatigue and fracture | Application-specific validation | A material tensile certificate does not establish component life. Specify any fatigue, toughness or crack-growth evaluation separately. |
| Non-destructive examination | Drawing / product specification | Define method, calibration, coverage, acceptance class and reporting before production. |
| Selected element · wt % | Reference composition |
|---|---|
| Aluminium · Al | 5.5–7.0 |
| Chromium · Cr | 0.8–2.3 |
| Molybdenum · Mo | 2.0–3.0 |
| Iron · Fe | 0.2–0.7 |
| Silicon · Si | 0.15–0.40 |
| Oxygen · O | 0.18 max |
| Titanium · Ti | Balance |
Selected composition limits, wt %, from GB/T 3620.1-2016. Use the complete ordered standard for all impurity, residual-element and analysis requirements.
TC6 is a specific alloy
Do not substitute TC4 / Ti-6Al-4V simply because both are alpha-beta titanium alloys. Chromium, molybdenum, iron and silicon change the alloy system.
Forged stock versus finished part
A forged bar certificate supports incoming stock acceptance. Disc, blade and other finished components need the drawing-specific process and inspection release.
Section and sampling
Large sections require an agreed structural and testing plan. Identify test direction, location, machining allowance and NDT coverage before production.
Thermal state matters
Compare strength and ductility only for the same product condition and relevant section. Reference data do not define universal operating limits.
03 / Application priorities
TC6 in application.
Review each main use through its service conditions, material choice, manufacturing route and acceptance plan. These are sourcing discussions; approved drawings and qualification requirements govern the final component.
Application review / 01
Compressor disc forgings
Disc stock is a central TC6 procurement direction. The bore, web and rim represent different sections and loading locations, so a single generic bar property is not an adequate acceptance plan.
Products & manufacturing
Forged disc blanks, suitable billet and bar for approved conversion.
Service & design review
Provide the disc drawing, section map, forging route, grain-flow requirements and heat-treatment specification. Agree specimen positions before material is cut.
Purchase & inspection priorities
Specify internal examination, structure, directional mechanical testing and dimensional stock allowance. Finished-disc fatigue and life assessment remain within the approved component programme.
Application review / 02
Compressor blade preforms
Blade manufacture places particular emphasis on root-to-airfoil transitions and the removal of surface-affected material. TC6 preforms should be purchased against the actual finished envelope and approved forging route.
Products & manufacturing
Forged bar, conversion stock and blade-shaped blanks.
Service & design review
Define blade geometry, root form, orientation, finishing allowance and subsequent thermal treatment. Identify surfaces that require additional process control.
Purchase & inspection priorities
Agree structure, surface inspection, critical dimensions and the specified examination after final treatment. Raw-stock certification does not release a finished rotating blade.
Application review / 03
Forged aerospace hardware
TC6 may be ordered for other drawing-approved hardware where its alloy and processing route are explicitly specified. Begin with the accepted material requirement instead of choosing by a generic strength label.
Products & manufacturing
Bar, stepped forgings and custom machining blanks.
Service & design review
Provide load directions, section transitions, required condition, source restrictions and the supply stage. Confirm that the proposed producer can meet the complete product specification.
Purchase & inspection priorities
Require traceable material records, structural acceptance, NDT and dimensional results appropriate to the delivered blank.
Application review / 04
Billet-to-preform conversion
Conversion stock must support the intended deformation and final section. TC6 billet enquiries should include enough information to plan cropping, test stock and surface preparation before the usable material quantity is priced.
Products & manufacturing
Cylindrical billet and cut conversion stock.
Service & design review
Share final envelope, cut weight target, deformation orientation and thermal route. Identify retained material for qualification or production tests.
Purchase & inspection priorities
Set incoming chemistry, structure and surface acceptance; define separate inspection after forging and heat treatment.
Application review / 05
Heat-treatment consistency
The delivered thermal state connects TC6 stock to its next manufacturing step. Two quotations with different conditions may require different downstream processing and cannot be compared on price per kilogram alone.
Products & manufacturing
Bar and forgings in the explicitly ordered condition.
Service & design review
List the controlling process specification, section range, processing responsibility and any post-treatment straightening or machining.
Purchase & inspection priorities
Tie mechanical and metallographic results to the delivered condition and representative sampling. Record later thermal processing separately.
Application review / 06
Critical-section inspection
For compressor blanks, access to internal and surface inspection can change as machining progresses. Agree inspection stages while the blank geometry still allows the required coverage.
Products & manufacturing
Disc, blade and structural blanks with suitable examination allowance.
Service & design review
Define NDT method, reference calibration, coverage, acceptance level and report format. Identify any reinspection after rough machining or final treatment.
Purchase & inspection priorities
Link the results to piece identity and the agreed processing stage. A generic statement of ultrasonic testing does not define adequate coverage.
Application review / 07
First-article component lots
A new TC6 source or manufacturing route may require representative first-article evidence. The trial material should reproduce the intended section, condition and processing sequence.
Products & manufacturing
Trial bar, billet and drawing-controlled blanks.
Service & design review
Agree controlled variables, inspection hold points, approval responsibility and the permitted scope of later changes.
Purchase & inspection priorities
Compile incoming material, forging, heat-treatment and final inspection records against the project plan.
Application review / 08
Recurring forged-stock orders
Repeat procurement benefits from consistent drawing revisions, material conditions and heat segregation. Separate disc, blade and general bar lines so their different testing and delivery requirements remain visible.
Products & manufacturing
Scheduled bar and approved blank lots.
Service & design review
Provide quantities, standard editions, marking, packaging, delivery sequence and certificate language.
Purchase & inspection priorities
Reconcile heat and piece markings with test reports and packing lists before shipment.
TC6 procurement checklist
Connect the application to the material order.
A useful specification connects the intended component, the supplied stock and the acceptance evidence. Share the drawing and known requirements first.
Define the application
Provide the disc drawing, section map, forging route, grain-flow requirements and heat-treatment specification. Agree specimen positions before material is cut.
Define the supplied stage
Forged disc blanks, suitable billet and bar for approved conversion. Distinguish raw stock, converted blanks and finished parts. Define who controls subsequent processing.
Define the acceptance evidence
Specify internal examination, structure, directional mechanical testing and dimensional stock allowance. Finished-disc fatigue and life assessment remain within the approved component programme.
Example: a useful TC6 material enquiry
TC6 forged titanium bar; required dimensions and quantity; standard and drawing revision; delivery condition; intended downstream process; mechanical, structural and dimensional acceptance; traceability, destination and required date.
Identify the approved product specification and any project-specific qualification. The grade designation and chemistry standard alone do not define component acceptance.
Discuss your material requirement ↗04 / Standards & documentation
Match the standard
to the product.
Choose the specification by product form, material condition and application. Identify the required edition on the order; a chemistry standard alone does not define a finished forging or component.
| Product / review | International / project route | Chinese reference | Clarify before quotation |
|---|---|---|---|
| Identity & chemistry | Approved product and project specification | GB/T 3620.1-2016View PDF ↗ | Review the complete chemical limits and product requirements; nominal alloy names do not establish automatic interchangeability. |
| BaoTi forged-stock catalogue | BaoTi forged-stock cataloguePublisher reference ↗ | Compare the complete ordered Chinese requirements | Manufacturer catalogue identifies TC6 forged stock and compressor-disc and blade uses. The catalogue is a reference, not a statement of TiHubs inventory or source approval. |
| Drawing-based blanks & parts | Approved drawing and controlled manufacturing plan | Agreed product / project specification | Define the supply stage, conversion route, heat treatment, structure, NDT, dimensions and traceability. Material certification is separate from finished component qualification. |
The purchase order must identify the required revision, grade, product form, condition and inspection. Reference documents do not replace design approval, manufacturing qualification or application-specific acceptance.
Request the controlled specification revision for your order. Any substitution, equivalence or dual-certification claim requires a documented comparison and agreement.
05 / Order coordination
Know the scope
before ordering.
Our founder’s 20 years in titanium inform the questions we ask before quotation and the supply options we review with you.

A quotation you can evaluate
Agree the grade, standard edition, dimensions, tolerance, condition and quantity before comparing prices.
- Identify whether inspection, samples and tooling are included.
- Confirm packaging, transport and delivery terms.
- Record items that still need technical confirmation.
Acceptance agreed before supply
Confirm material identity, delivery condition, heat-to-piece traceability, dimensional checks and required testing before production. For converted parts, define inspection after forging, heat treatment and machining, including the specified microstructure and NDT scope.
Independent inspection can be discussed with its scope, timing, acceptance criteria and cost agreed for the order.
Delivery with clear milestones
Review the proposed lead time, approvals, production sequence and dispatch requirements. For several product forms, coordinate document and packing readiness together.
Material substitutions and technical changes require written approval. A schedule deviation should identify the impact, decisions needed and next steps.
One contact when an issue arises
Contact TiHubs with the order reference, affected items and supporting photos or inspection records.
We record the issue, review it against the agreed requirements and coordinate the next steps with the relevant manufacturing parties.
Material records
Grade, standard, test results and heat or batch identity matched to the supplied items.
Inspection records
Dimensional and testing records for the agreed scope, including critical drawing requirements.
Dispatch records
Item identification, packing list, protective packaging and required shipment documents.
06 / Questions before sourcing
Before you specify
TC6 Titanium Alloy.
A clear material designation is the beginning. Product form, specification revision, material condition and acceptance complete the requirement.
A useful first enquiry
- Product and specificationProduct form, standard edition, dimensions and material condition.
- Order and deliveryQuantity, destination and any required delivery date.
- Acceptance requirementsDrawing revision, inspection, certificates and packaging.
Not every detail is finalized? Send the information you have. We can help identify the questions to resolve before quotation.
What happens next: requirement review, technical clarification, then a supply proposal and quotation.
What is TC6 titanium?
TC6 is an aluminium-chromium-molybdenum titanium alloy with iron and silicon additions. Compressor discs and blades are documented application directions, making forged stock and conversion blanks the priority procurement forms. The purchase specification must connect the supplied section and thermal condition to the approved component drawing; nominal chemistry alone does not establish flight-part acceptance.
Which TC6 products are the priority?
Forged bar, billet and drawing-controlled compressor disc or blade blanks are the main enquiries. Actual size and processing capability are confirmed against your order.
Is TC6 interchangeable with TC4?
No automatic substitution is appropriate. Compare the complete alloy chemistry, product specification, condition and component requirements.
Can I order finished compressor parts?
Send the drawing and required supply stage. Raw stock, rough blanks and fully released components have different capability and qualification requirements.
What matters for disc blanks?
Provide bore, web and rim dimensions, forging route, sampling positions, thermal condition and NDT requirements. Include stock and test-material allowances.
What matters for blade blanks?
Define airfoil and root envelopes, forging orientation, critical transitions, surface removal, final treatment and inspection stages.
Are published strengths guaranteed for every size?
No. Mechanical requirements depend on the ordered specification, condition, section and sampling. Agree the acceptance values in the purchase order.
What documents should accompany TC6?
Require heat and lot identity, full chemical analysis, delivery condition, dimensional results and the agreed mechanical and structural tests. Define NDT method, coverage and acceptance criteria in the order.
What should a TC6 RFQ include?
Include form, dimensions, quantity, drawing and standard revisions, thermal condition, conversion route, inspection, destination and any approved-source restrictions.
07 / Your next step
Start with the
requirement you have.
Send the product details, drawing or operating conditions you already know. We will identify missing information and discuss a suitable supply route before quotation.
- Requirement review
- Technical clarification
- Supply proposal and quotation
Combine materials and parts in one enquiry.
Send one list of TC6 forms, sizes and quantities. Include drawing revisions, material conditions and items that must be supplied or dispatched together.
Share the service and acceptance priorities.
Include load and temperature conditions, critical sections, required material records, process qualification, inspection, destination and timing.
Baoji, China · info@tihubs.com
Start your TC6 Titanium Alloy enquiry
Send your material form, drawing or process conditions. We will help clarify the remaining requirements.