TB2 Titanium Alloy · Metastable beta titanium alloy
TB2 Titanium Alloy. Stock for rivets and cold forming.
Source TB2 wire, bar, sheet and strip for qualified rivet and formed-component manufacturing. Agree the starting condition, deformation route and final inspection.
Start with a specification, drawing or application. We’ll help identify the details still needed.
Material review. Supply coordination.
One contact in Baoji, China.
01 / Product forms
Find your TB2 product.
Choose a material form or application. Send the dimensions, service conditions and required records so we can match the manufacturing route to your order.

TB2 Titanium Alloy
TB2 rivet wire
Coiled or straight wire for approved cold-headed rivet manufacturing routes.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Diameter, tolerance, coil mass, straight-length option, cast and helix.
- Manufacturing review
- Define head geometry, forming sequence and the material state required during heading.
- Inspection priorities
- Diameter consistency, surface quality, formability checks and traceable material condition.

TB2 Titanium Alloy
TB2 titanium bar
Round stock for rivet, pin and small precision-component machining programmes.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Diameter, cut length, straightness and surface finish.
- Manufacturing review
- Identify machining allowance, subsequent forming and any final ageing treatment.
- Inspection priorities
- Require heat and lot identity, full chemical analysis, delivery condition, dimensional results and the agreed mechanical and structural tests. Define NDT method, coverage and acceptance criteria in the order.

TB2 Titanium Alloy
TB2 forming sheet
Flat stock for drawing-approved sheet-metal components and forming trials.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Thickness, width, length, flatness, rolling direction and surface finish.
- Manufacturing review
- Provide bend geometry, edge preparation and the thermal sequence before and after forming.
- Inspection priorities
- Directional properties, thickness uniformity, surface defects and agreed forming evidence.

TB2 Titanium Alloy
TB2 titanium strip
Narrow flat stock for controlled forming and project-specific component development.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Thickness, width tolerance, coil diameter, edge condition and delivery length.
- Manufacturing review
- Define slitting, levelling, bending and any intermediate thermal processing.
- Inspection priorities
- Edge and surface integrity, width consistency, condition and lot identification.

TB2 Titanium Alloy
TB2 rivet blanks
Application illustration: uninstalled rivet manufacturing blanks to an approved drawing.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Head form, shank diameter, grip length, end geometry and sample quantity.
- Manufacturing review
- Separate heading, final condition and installation requirements; identify the qualified manufacturing route.
- Inspection priorities
- Head and shank geometry, surface integrity and required finished-rivet and joint tests.

TB2 Titanium Alloy
TB2 formed & machined blanks
Application illustration: simple formed brackets and precision pin blanks.
- Specification
- Approved grade-specific product specification, drawing revision and delivery condition; confirm supply feasibility.
- Size & delivery
- Drawing envelope, datums, bend radii and remaining machining stock.
- Manufacturing review
- Confirm the permitted forming or machining route and the delivered material condition.
- Inspection priorities
- Dimensions, springback, critical surfaces, specified mechanical evidence and traceability.
Images illustrate material forms and application possibilities. Reference markings identify specification options; they do not establish dual certification, stock availability or approval of finished equipment.
Define the shape. Share the service.
These details help turn a material enquiry into a comparable quotation.
01 / Drawing review
Drawing-controlled blanks
Provide rough and finished drawings, datum positions, critical sections, machining allowance and the intended conversion route.
Discuss your drawing02 / Drawing review
Heat treatment & process sequence
Identify the required delivery condition and subsequent manufacturing steps. Agree process records, sampling stages and dimensional checks after thermal processing.
Discuss your drawing03 / Drawing review
Component inspection planning
Specify surface integrity, microstructure, NDT, dimensional acceptance and traceability. Identify which tests apply to raw material and which apply to the finished component.
Discuss your drawing02 / Material identity
What is TB2 Titanium Alloy titanium?
TB2 is a Chinese metastable beta titanium alloy with nominal composition Ti-5Mo-5V-8Cr-3Al. Rivet manufacture and cold-formed parts are priority sourcing directions. The solution-treated starting state and any subsequent ageing are different material conditions; procurement should identify the approved process and the stage at which properties are accepted.
Specify the exact standard edition, form and delivery condition. Nominal chemistry is only one part of an order; strength, microstructure, dimensional acceptance and traceability also need to be defined.
| Review item | Order basis | What to confirm |
|---|---|---|
| Material condition | Define the ordered heat-treatment state | Tie test results to the same conversion and thermal history as the supplied product. |
| Strength and ductility | Product- and section-dependent | Specify tensile, proof strength, elongation, sampling location and test direction in the purchase requirement. |
| Microstructure | Agree acceptance limits | Review grain structure, alpha morphology, surface alpha case and metallographic sampling for the manufacturing route. |
| Fatigue and fracture | Application-specific validation | A material tensile certificate does not establish component life. Specify any fatigue, toughness or crack-growth evaluation separately. |
| Non-destructive examination | Drawing / product specification | Define method, calibration, coverage, acceptance class and reporting before production. |
| Selected element · wt % | Reference composition |
|---|---|
| Aluminium · Al | 2.5–3.5 |
| Molybdenum · Mo | 4.7–5.7 |
| Vanadium · V | 4.7–5.7 |
| Chromium · Cr | 7.5–8.5 |
| Iron · Fe | 0.30 max |
| Titanium · Ti | Balance |
Selected composition limits, wt %, from GB/T 3620.1-2016. Use the complete ordered standard for all impurity, residual-element and analysis requirements.
TB2 is a specific beta alloy
Do not treat TB2 as interchangeable with TB3, TB6, TB8 or Ti-15-3. Similar broad alloy classification does not replace chemistry and process comparison.
Solution-treated and aged states
Cold forming may require a different state from the final component. Specify the starting condition, ageing responsibility and final acceptance stage.
Wire and strip require separate orders
Rivet wire and narrow flat strip have different dimensional, surface and processing requirements. Identify the product form explicitly rather than using a generic beta-titanium description.
Rivet material versus joint performance
A material certificate does not establish the strength or fatigue life of a riveted assembly. Joint geometry, installation and qualification remain drawing-specific.
03 / Application priorities
TB2 in application.
Review each main use through its service conditions, material choice, manufacturing route and acceptance plan. These are sourcing discussions; approved drawings and qualification requirements govern the final component.
Application review / 01
Aircraft rivet manufacture
TB2 is a documented titanium rivet material. A useful purchasing requirement links wire condition to heading and finished-rivet geometry, then separates manufacturing acceptance from installation in the aircraft joint.
Products & manufacturing
Rivet wire, bar-derived blanks and drawing-controlled rivet preforms.
Service & design review
Provide head and shank dimensions, grip range, forming method, required condition and the approved rivet specification. Identify who performs heading, final treatment and inspection.
Purchase & inspection priorities
Agree material and surface tests on incoming stock and separate finished-rivet dimensional, mechanical and installation checks.
Application review / 02
Cold-headed hardware
Cold heading concentrates deformation near the head and transitions. The TB2 starting state, surface preparation and actual geometry should be reviewed together instead of relying on a generic statement of cold formability.
Products & manufacturing
Wire and cut lengths for qualified heading routes.
Service & design review
State reduction stages, head shape, tooling sequence, lubrication and any intermediate treatment. Use representative trials for a new size or source where required.
Purchase & inspection priorities
Inspect surface defects and formed-head integrity, then check dimensions and final material condition.
Application review / 03
Riveted thin-sheet joints
The performance of a riveted joint depends on more than the rivet alloy. Sheet stack, hole quality, grip length and installation method must be included in the qualification plan.
Products & manufacturing
TB2 rivet blanks to the approved joint drawing.
Service & design review
Provide mating sheets, hole preparation, grip range, installation sequence and permissible deformation. Define the authority responsible for accepting the completed joint.
Purchase & inspection priorities
Evaluate installed geometry and specified static or fatigue tests on representative joints. Raw-material testing cannot replace this evidence.
Application review / 04
Cold-formed sheet components
TB2 sheet and strip can be reviewed for formed components when the design calls for this alloy and a qualified process. Bending response depends on thickness, direction, surface and material condition.
Products & manufacturing
Sheet, narrow strip and cut forming blanks.
Service & design review
Share bend radii, flange dimensions, rolling direction, edge preparation and springback limits. Identify any post-forming ageing or joining steps.
Purchase & inspection priorities
Inspect cracking, geometry and surface integrity after forming, then perform the agreed tests in the final delivered state.
Application review / 05
Precision pins & small parts
Machined TB2 components need a clear stock condition and usable dimensional envelope. Subsequent ageing or forming may change the finishing and inspection sequence.
Products & manufacturing
Bar, straight lengths and rough-machined pin blanks.
Service & design review
Specify fits, critical radii, surface finish, final condition and the machining allowance required after thermal processing.
Purchase & inspection priorities
Require material identity, dimensional results and examination of critical surfaces. Tie final acceptance to the correct process stage.
Application review / 06
Condition & ageing control
A solution-treated TB2 lot and an aged lot are not interchangeable purchasing conditions. The order should state whether the objective is further forming or release in the final material state.
Products & manufacturing
Wire, sheet, strip and bar in the explicitly agreed condition.
Service & design review
Identify thermal specifications, processing responsibility, section and lot definitions, and any permitted straightening or finishing after treatment.
Purchase & inspection priorities
Match mechanical tests and structural examination to the delivered state; retain records for later conversion.
Application review / 07
Forming and installation trials
A new TB2 supply route may require trials representative of production wire, rivet geometry or sheet thickness. Qualification should address the variables that matter to the actual component.
Products & manufacturing
Trial lots and retained stock for material and process evaluation.
Service & design review
Agree specimen sizes, forming or installation method, test sequence, acceptance criteria and approval authority before sample manufacture.
Purchase & inspection priorities
Record source, chemistry, condition and manufacturing variables alongside the results. Keep recurring supply within the approved scope.
Application review / 08
Recurring rivet-stock supply
Stable condition and surface quality are central to repeated TB2 wire and blank purchases. Itemized order lines help distinguish forming stock from finished rivet blanks.
Products & manufacturing
Scheduled wire, straight bar and approved blanks.
Service & design review
List drawing and specification revisions, dimensions, quantities, condition, lot segregation, packaging and delivery sequence.
Purchase & inspection priorities
Reconcile material records and physical markings with the dispatch list, and review source or process changes through the agreed procedure.
TB2 procurement checklist
Connect the application to the material order.
A useful specification connects the intended component, the supplied stock and the acceptance evidence. Share the drawing and known requirements first.
Define the application
Provide head and shank dimensions, grip range, forming method, required condition and the approved rivet specification. Identify who performs heading, final treatment and inspection.
Define the supplied stage
Rivet wire, bar-derived blanks and drawing-controlled rivet preforms. Distinguish raw stock, converted blanks and finished parts. Define who controls subsequent processing.
Define the acceptance evidence
Agree material and surface tests on incoming stock and separate finished-rivet dimensional, mechanical and installation checks.
Example: a useful TB2 material enquiry
TB2 rivet wire; required dimensions and quantity; standard and drawing revision; delivery condition; intended downstream process; mechanical, structural and dimensional acceptance; traceability, destination and required date.
Identify the approved product specification and any project-specific qualification. The grade designation and chemistry standard alone do not define component acceptance.
Discuss your material requirement ↗04 / Standards & documentation
Match the standard
to the product.
Choose the specification by product form, material condition and application. Identify the required edition on the order; a chemistry standard alone does not define a finished forging or component.
| Product / review | International / project route | Chinese reference | Clarify before quotation |
|---|---|---|---|
| Identity & chemistry | Approved product and project specification | GB/T 3620.1-2016View PDF ↗ | Review the complete chemical limits and product requirements; nominal alloy names do not establish automatic interchangeability. |
| TB2 rivet study | TB2 rivet studyPublisher reference ↗ | Compare the complete ordered Chinese requirements | Original research investigates TB2 rivet forming and thin-sheet joint properties. It is an application reference, not a product release specification or qualification for a new joint. |
| Drawing-based blanks & parts | Approved drawing and controlled manufacturing plan | Agreed product / project specification | Define the supply stage, conversion route, heat treatment, structure, NDT, dimensions and traceability. Material certification is separate from finished component qualification. |
The purchase order must identify the required revision, grade, product form, condition and inspection. Reference documents do not replace design approval, manufacturing qualification or application-specific acceptance.
Request the controlled specification revision for your order. Any substitution, equivalence or dual-certification claim requires a documented comparison and agreement.
05 / Order coordination
Know the scope
before ordering.
Our founder’s 20 years in titanium inform the questions we ask before quotation and the supply options we review with you.

A quotation you can evaluate
Agree the grade, standard edition, dimensions, tolerance, condition and quantity before comparing prices.
- Identify whether inspection, samples and tooling are included.
- Confirm packaging, transport and delivery terms.
- Record items that still need technical confirmation.
Acceptance agreed before supply
Confirm material identity, delivery condition, heat-to-piece traceability, dimensional checks and required testing before production. For converted parts, define inspection after forging, heat treatment and machining, including the specified microstructure and NDT scope.
Independent inspection can be discussed with its scope, timing, acceptance criteria and cost agreed for the order.
Delivery with clear milestones
Review the proposed lead time, approvals, production sequence and dispatch requirements. For several product forms, coordinate document and packing readiness together.
Material substitutions and technical changes require written approval. A schedule deviation should identify the impact, decisions needed and next steps.
One contact when an issue arises
Contact TiHubs with the order reference, affected items and supporting photos or inspection records.
We record the issue, review it against the agreed requirements and coordinate the next steps with the relevant manufacturing parties.
Material records
Grade, standard, test results and heat or batch identity matched to the supplied items.
Inspection records
Dimensional and testing records for the agreed scope, including critical drawing requirements.
Dispatch records
Item identification, packing list, protective packaging and required shipment documents.
06 / Questions before sourcing
Before you specify
TB2 Titanium Alloy.
A clear material designation is the beginning. Product form, specification revision, material condition and acceptance complete the requirement.
A useful first enquiry
- Product and specificationProduct form, standard edition, dimensions and material condition.
- Order and deliveryQuantity, destination and any required delivery date.
- Acceptance requirementsDrawing revision, inspection, certificates and packaging.
Not every detail is finalized? Send the information you have. We can help identify the questions to resolve before quotation.
What happens next: requirement review, technical clarification, then a supply proposal and quotation.
What is TB2 titanium alloy?
TB2 is a Chinese metastable beta titanium alloy with nominal composition Ti-5Mo-5V-8Cr-3Al. Rivet manufacture and cold-formed parts are priority sourcing directions. The solution-treated starting state and any subsequent ageing are different material conditions; procurement should identify the approved process and the stage at which properties are accepted.
What are the main TB2 applications?
The main focus is rivet manufacture and drawing-approved cold-formed parts. This page connects wire, bar, sheet and strip to their required processing and inspection.
Is TB2 the same as TB6 or Ti-15-3?
No. These are different beta-titanium alloy systems with different chemistry and processing requirements. Use the full specified grade and product standard.
Which condition should I order?
Specify the state required by your manufacturing route, such as the approved solution-treated starting condition or final aged state. Identify all later thermal processing.
Can TB2 wire be cold headed?
Review the intended head geometry, wire size, surface quality and condition against the qualified process. A representative trial may be required for a new source or product size.
Does material certification qualify a riveted joint?
No. The joint requires its own drawing, installation and test requirements. Sheet stack, hole preparation and installed geometry influence performance.
Can I enquire about TB2 sheet and strip?
Yes. Provide thickness, width, delivery form, condition, edge quality and intended forming route so the actual supply capability can be confirmed.
What inspection should be specified?
Require heat and lot identity, full chemical analysis, delivery condition, dimensional results and the agreed mechanical and structural tests. Define NDT method, coverage and acceptance criteria in the order. For forming stock, include the agreed surface and forming checks; finished rivets need a separate acceptance plan.
What information helps obtain a TB2 quote?
Send form, dimensions, quantity, specification, condition, drawing revision, forming or machining route, inspection and destination. Identify any project source restrictions.
07 / Your next step
Start with the
requirement you have.
Send the product details, drawing or operating conditions you already know. We will identify missing information and discuss a suitable supply route before quotation.
- Requirement review
- Technical clarification
- Supply proposal and quotation
Combine materials and parts in one enquiry.
Send one list of TB2 forms, sizes and quantities. Include drawing revisions, material conditions and items that must be supplied or dispatched together.
Share the service and acceptance priorities.
Include load and temperature conditions, critical sections, required material records, process qualification, inspection, destination and timing.
Baoji, China · info@tihubs.com
Start your TB2 Titanium Alloy enquiry
Send your material form, drawing or process conditions. We will help clarify the remaining requirements.