TC10 / Ti-662 · Alpha-beta titanium alloy
TC10 / Ti-662. Strength for structures and fasteners.
Source TC10 / Ti-662 bar, billet, plate and fastener wire for high-strength structural manufacturing. Coordinate the specification, heat-treatment state, machining stock and inspection before placing an order.
Start with a specification, drawing or application. We’ll help identify the details still needed.
Material review. Supply coordination.
One contact in Baoji, China.
01 / Product forms
Find your TC10 product.
Choose a material form or application. Send the dimensions, service conditions and required records so we can match the manufacturing route to your order.

TC10 / Ti-662
TC10 titanium bar & rod
Machining stock for high-strength fittings, pins and structural hardware. Compare quotations on usable dimensions and the same heat-treatment state.
- Specification
- TC10 agreed bar specification or Ti-662 AMS 4971 where the ordered product meets its scope.
- Size & delivery
- Diameter, cut length, straightness, tolerance, surface finish and quantity per heat.
- Manufacturing review
- State whether the bar will be machined in the delivered condition or heat treated later; retain allowance for distortion and final inspection.
- Inspection priorities
- Require heat and lot identity, chemical analysis, delivery condition, dimensional results and the agreed mechanical and metallographic tests. Define any NDT method, coverage and acceptance class in the order.

TC10 / Ti-662
TC10 forging billet
Conversion stock for structural forgings, preforms and larger-section parts. Billet acceptance should support the downstream forging process.
- Specification
- AMS 4971 stock for forging where applicable, or an agreed TC10 billet specification.
- Size & delivery
- Billet diameter or section, length, cut weight, end allowance and surface preparation.
- Manufacturing review
- Share forging temperature control requirements, deformation route, final section and test-stock location. The finished forging needs its own acceptance plan.
- Inspection priorities
- Melt and billet identity, chemistry, incoming structure, surface quality and specified ultrasonic examination.

TC10 / Ti-662
TC10 plate & machining stock
Plate and cut blanks for drawing-approved structural machining. Confirm actual thickness and supply feasibility before committing a delivery schedule.
- Specification
- Agree a plate-specific specification, condition and test plan. AMS 4971 is not the plate release standard.
- Size & delivery
- Thickness, width, length, flatness, cut-edge condition and rolling direction.
- Manufacturing review
- Define pocketing, bending or thermal processing after delivery and the required machining allowance.
- Inspection priorities
- Thickness and flatness, directional tensile tests, surface condition, traceability and any specified internal examination.

TC10 / Ti-662
TC10 fastener wire
Wire or straight lengths for approved aircraft fastener manufacturing routes. Surface condition and forming behaviour matter alongside tensile strength.
- Specification
- AMS 4971 wire or the customer-approved TC10 fastener-stock specification.
- Size & delivery
- Diameter, tolerance, coil or straight length, cast and helix, package mass and handling method.
- Manufacturing review
- Provide heading, forming and thread-making route, intermediate annealing needs and final heat-treatment sequence.
- Inspection priorities
- Diameter consistency, surface defects, material condition and lot testing. Finished fastener acceptance is separate from wire certification.

TC10 / Ti-662
TC10 fastener machining blanks
Application illustration: bar and wire converted into bolt, pin and high-strength hardware blanks to an approved drawing.
- Specification
- Fastener drawing plus the specified raw-material and manufacturing requirements.
- Size & delivery
- Head and shank geometry, grip length, thread allowance, datum system and inspection sample plan.
- Manufacturing review
- Review head-to-shank transitions, thread rolling or machining, thermal processing and surface treatment responsibilities.
- Inspection priorities
- Critical dimensions, surface integrity, required proof or fatigue tests and raw-material-to-part traceability.

TC10 / Ti-662
TC10 structural forging blanks
Application illustration: near-net or oversize blanks for lugs, brackets and load-transfer fittings.
- Specification
- Approved structural drawing, forging route and TC10 material specification.
- Size & delivery
- Blank envelope, principal load directions, thickest section, stock allowance and test prolongations.
- Manufacturing review
- Agree grain-flow objectives, roughing stages and heat treatment before comparing blank prices.
- Inspection priorities
- Directional properties, structure, ultrasonic and surface inspection at the defined manufacturing stages.
Images illustrate material forms and application possibilities. Reference markings identify specification options; they do not establish dual certification, stock availability or approval of finished equipment.
Define the shape. Share the service.
These details help turn a material enquiry into a comparable quotation.
01 / Drawing review
Drawing-controlled blanks
Provide rough and finished drawings, datum positions, critical sections, machining allowance and the intended conversion route.
Discuss your drawing02 / Drawing review
Heat treatment & process sequence
Identify the required delivery condition and subsequent manufacturing steps. Agree process records, sampling stages and dimensional checks after thermal processing.
Discuss your drawing03 / Drawing review
Component inspection planning
Specify surface integrity, microstructure, NDT, dimensional acceptance and traceability. Identify which tests apply to raw material and which apply to the finished component.
Discuss your drawing02 / Material identity
What is TC10 / Ti-662 titanium?
TC10 is the Chinese designation associated with Ti-6Al-6V-2Sn, commonly called Ti-662 or Ti-6-6-2. This heat-treatable alpha-beta alloy gives buyers a distinct high-strength titanium route for structural parts and fastener manufacture. The nominal alloy name does not replace a product specification: bars, forging stock, plate and wire need their own condition and acceptance requirements.
Specify the exact standard edition, form and delivery condition. Nominal chemistry is only one part of an order; strength, microstructure, dimensional acceptance and traceability also need to be defined.
| Review item | Order basis | What to confirm |
|---|---|---|
| Material condition | Define the ordered heat-treatment state | Tie test results to the same conversion and thermal history as the supplied product. |
| Strength and ductility | Product- and section-dependent | Specify tensile, proof strength, elongation, sampling location and test direction in the purchase requirement. |
| Microstructure | Agree acceptance limits | Review grain structure, alpha morphology, surface alpha case and metallographic sampling for the manufacturing route. |
| Fatigue and fracture | Application-specific validation | A material tensile certificate does not establish component life. Specify any fatigue, toughness or crack-growth evaluation separately. |
| Non-destructive examination | Drawing / product specification | Define method, calibration, coverage, acceptance class and reporting before production. |
| Selected element · wt % | Reference composition |
|---|---|
| Aluminium · Al | 5.50–6.50 |
| Vanadium · V | 5.50–6.50 |
| Tin · Sn | 1.50–2.50 |
| Iron · Fe | 0.35–1.00 |
| Copper · Cu | 0.35–1.00 |
| Titanium · Ti | Balance |
Selected TC10 composition limits, wt %, from GB/T 3620.1-2016. Full impurity, residual-element and analysis requirements remain part of the ordered specification. Do not assume every Ti-662 producer datasheet uses identical limits.
TC10 and Ti-662
Ti-662 and Ti-6Al-6V-2Sn are useful international search names for this alloy family. Compare the full Chinese and international specifications before claiming dual certification.
Compared with TC4 / Ti-6Al-4V
The higher vanadium and additional tin, copper and iron distinguish this alloy from TC4. Existing TC4 process qualifications and material certificates do not automatically transfer.
Annealed versus heat-treated
An annealed, heat-treatable product is not a finished solution-treated-and-aged component. Identify the delivered state and who performs subsequent thermal processing.
Choose a product route
AMS 4971 covers defined bars, wire, forgings, flash-welded rings and conversion stock. It is not a blanket plate specification; confirm the applicable scope and section limit.
03 / Application priorities
TC10 in application.
Review each main use through its service conditions, material choice, manufacturing route and acceptance plan. These are sourcing discussions; approved drawings and qualification requirements govern the final component.
Application review / 01
Airframe fittings & brackets
TC10 / Ti-662 is a procurement route for high-strength titanium structural parts where the approved design calls for this alloy. Fittings transfer load through holes, fillets and section changes; the value of the blank depends on its process history as well as its nominal strength.
Products & manufacturing
Bar for smaller machined fittings; billet and near-net forgings for larger load-transfer features. Plate is a separate, drawing-approved option.
Service & design review
Provide load direction, bearing features, fatigue-sensitive surfaces, maximum section and final heat-treatment state. Establish whether machining from bar is permitted or a specified forging route is mandatory.
Purchase & inspection priorities
Agree directional tensile testing, structure, NDT and critical dimensional reports. Preserve heat identity when one blank produces several parts.
Application review / 02
Aircraft fasteners
Fastener manufacture is a priority use for TC10 wire and bar. A useful RFQ identifies the forming route and final fastener class, because head formation, thread manufacture and thermal treatment can change the properties established on the starting-stock certificate.
Products & manufacturing
Wire for a qualified forming route; bar and straight lengths for machined bolts, pins and hardware.
Service & design review
State head and shank dimensions, grip length, thread method, required ductility during forming and the final material condition. Agree lubrication, surface protection and any thermal processing with the responsible manufacturer.
Purchase & inspection priorities
Inspect incoming wire diameter and surface quality, then define separate finished-fastener proof, tensile, fatigue and dimensional requirements where the drawing calls for them.
Application review / 03
Pins, lugs & bearing joints
Load-transfer pins and lugs can combine bending, shear and contact loading. TC10 material selection must therefore be connected to the joint geometry and fatigue evaluation; a higher tensile number alone does not establish a better assembly.
Products & manufacturing
Round bar for pins; forged or rough-machined blanks for lugs and clevises.
Service & design review
Identify bearing surfaces, fit, hole orientation, critical radii and mating materials. Define which surface treatments and final inspections are included in the supply scope.
Purchase & inspection priorities
Require material condition, dimensional reports and examination of fatigue-sensitive surfaces. Define the appropriate sample orientation for each load-carrying section.
Application review / 04
Forged structural preforms
Billet procurement supports a later conversion process. The incoming TC10 condition may intentionally differ from the final part, so the purchase order should separate billet acceptance from the properties developed after forging and heat treatment.
Products & manufacturing
Cut billet, preforms and drawing-specific structural forging blanks.
Service & design review
Provide the intended deformation route, usable volume, cropping allowance, test-stock positions and final section size. Resolve changes in source or processing before production.
Purchase & inspection priorities
Specify melt pedigree, billet structure, surface preparation and incoming NDT. Retain conversion records and establish the final-part testing stage.
Application review / 05
Plate-machined components
Where the approved design allows TC10 plate, a flat blank can support machined brackets and structural profiles. Plate availability, rolling direction and distortion during metal removal need early review.
Products & manufacturing
Plate, cut rectangles and rough-machined structural stock, subject to the confirmed supply range.
Service & design review
Share finished wall thickness, pocket depth, datums, nesting and acceptable plate direction. Define stabilization and inspection after rough machining.
Purchase & inspection priorities
Use a plate-specific release basis and directional sampling. Confirm flatness, usable thickness, surface condition and any through-thickness examination required by the order.
Application review / 06
Heat-treatment coordination
Heat treatment is part of the material definition for high-strength Ti-662 parts. Buyers need an explicit handover between annealed stock, intermediate processing and final component condition to avoid comparing certificates from different states.
Products & manufacturing
Bar, wire, billet and forgings supplied to the agreed stage.
Service & design review
Identify the approved process specification, section range, thermal records and who performs each treatment. Include machining allowance and distortion limits after heating and cooling.
Purchase & inspection priorities
Tie tensile and structural tests to the specified delivery condition. Any later thermal treatment may require a separate final acceptance step.
Application review / 07
First-article qualification
A trial lot should represent the intended TC10 production route, especially where a new source or forming process is being introduced. Convenient small coupons do not necessarily reproduce the behaviour of a thicker finished section.
Products & manufacturing
Representative wire lots, bar, forgings and retained test material.
Service & design review
Agree the evidence package, specimen locations, manufacturing stages and approval authority before making samples. Record variables that must remain controlled for recurring orders.
Purchase & inspection priorities
Provide the agreed material, process and dimensional results. A successful sample supports the defined project and does not establish unrestricted aerospace approval.
Application review / 08
Repeat structural supply
Recurring orders benefit from stable drawings, clear material-condition codes and traceable pieces. Consolidating different TC10 forms under one enquiry is useful when their separate release requirements remain visible.
Products & manufacturing
Coordinated bar, wire, plate and forging lots against an itemized bill of materials.
Service & design review
List item numbers, standard editions, condition, quantity, delivery sequence and required document language. Identify any approved-source restrictions or inspection hold points.
Purchase & inspection priorities
Reconcile piece markings, heat numbers, test results and packing lists before dispatch. Keep any substitution or process change subject to the agreed approval route.
TC10 procurement checklist
Connect the application to the material order.
A useful specification connects the intended component, the supplied stock and the acceptance evidence. Share the drawing and known requirements first.
Define the application
Provide load direction, bearing features, fatigue-sensitive surfaces, maximum section and final heat-treatment state. Establish whether machining from bar is permitted or a specified forging route is mandatory.
Define the supplied stage
Bar for smaller machined fittings; billet and near-net forgings for larger load-transfer features. Plate is a separate, drawing-approved option. Distinguish raw stock, converted blanks and finished parts. Define who controls subsequent processing.
Define the acceptance evidence
Agree directional tensile testing, structure, NDT and critical dimensional reports. Preserve heat identity when one blank produces several parts.
Example: a useful TC10 material enquiry
TC10 titanium bar & rod; required dimensions and quantity; standard and drawing revision; delivery condition; intended downstream process; mechanical, structural and dimensional acceptance; traceability, destination and required date.
Identify the approved product specification and any project-specific qualification. The grade designation and chemistry standard alone do not define component acceptance.
Discuss your material requirement ↗04 / Standards & documentation
Match the standard
to the product.
Choose the specification by product form, material condition and application. Identify the required edition on the order; a chemistry standard alone does not define a finished forging or component.
| Product / review | International / project route | Chinese reference | Clarify before quotation |
|---|---|---|---|
| Identity & chemistry | AMS 4971NPublisher reference ↗ | GB/T 3620.1-2016View PDF ↗ | Verify the full composition and ordered product requirements. A Chinese grade name alone does not establish international or dual certification. |
| Bar, wire & forging stock | AMS 4971NPublisher reference ↗ | GB/T 2965-2023View PDF ↗ | AMS 4971N: annealed, heat-treatable Ti-6Al-6V-2Sn bars, wire, forgings and flash-welded rings within its section scope, plus stock for conversion. Confirm all dimensional and condition requirements. |
| Plate & cut flat stock | Agreed plate-specific material specification | Approved Chinese / project plate requirements | Confirm plate availability, thickness, condition, directional tests and surface acceptance. AMS 4971 is not a plate specification. |
| Drawing-based blanks & parts | Approved drawing and controlled manufacturing plan | Agreed product / project specification | Define the supply stage, conversion route, heat treatment, structure, NDT, dimensions and traceability. Material certification is separate from finished component qualification. |
The purchase order must identify the required revision, grade, product form, condition and inspection. Reference documents do not replace design approval, manufacturing qualification or application-specific acceptance.
Request the controlled specification revision for your order. Any substitution, equivalence or dual-certification claim requires a documented comparison and agreement.
05 / Order coordination
Know the scope
before ordering.
Our founder’s 20 years in titanium inform the questions we ask before quotation and the supply options we review with you.

A quotation you can evaluate
Agree the grade, standard edition, dimensions, tolerance, condition and quantity before comparing prices.
- Identify whether inspection, samples and tooling are included.
- Confirm packaging, transport and delivery terms.
- Record items that still need technical confirmation.
Acceptance agreed before supply
Confirm material identity, delivery condition, heat-to-piece traceability, dimensional checks and required testing before production. For converted parts, define inspection after forging, heat treatment and machining, including the specified microstructure and NDT scope.
Independent inspection can be discussed with its scope, timing, acceptance criteria and cost agreed for the order.
Delivery with clear milestones
Review the proposed lead time, approvals, production sequence and dispatch requirements. For several product forms, coordinate document and packing readiness together.
Material substitutions and technical changes require written approval. A schedule deviation should identify the impact, decisions needed and next steps.
One contact when an issue arises
Contact TiHubs with the order reference, affected items and supporting photos or inspection records.
We record the issue, review it against the agreed requirements and coordinate the next steps with the relevant manufacturing parties.
Material records
Grade, standard, test results and heat or batch identity matched to the supplied items.
Inspection records
Dimensional and testing records for the agreed scope, including critical drawing requirements.
Dispatch records
Item identification, packing list, protective packaging and required shipment documents.
06 / Questions before sourcing
Before you specify
TC10 / Ti-662.
A clear material designation is the beginning. Product form, specification revision, material condition and acceptance complete the requirement.
A useful first enquiry
- Product and specificationProduct form, standard edition, dimensions and material condition.
- Order and deliveryQuantity, destination and any required delivery date.
- Acceptance requirementsDrawing revision, inspection, certificates and packaging.
Not every detail is finalized? Send the information you have. We can help identify the questions to resolve before quotation.
What happens next: requirement review, technical clarification, then a supply proposal and quotation.
What is TC10 titanium?
TC10 is the Chinese designation associated with Ti-6Al-6V-2Sn, also called Ti-662. It is a heat-treatable alpha-beta titanium alloy used for specified high-strength structural and fastener applications.
Are TC10 and Ti-662 automatically interchangeable?
No. The names identify the related alloy family, but chemistry limits, product scope, condition and inspection may differ between specifications. Review both complete requirements before approving substitution or dual certification.
Which TC10 products can I enquire about?
Start with bar, forging billet, plate and fastener wire. Include dimensions and the required specification so TiHubs can confirm the available supply route. Drawing-based blanks require a separate manufacturing review.
Does AMS 4971 cover TC10 plate?
AMS 4971 addresses defined Ti-6Al-6V-2Sn bars, wire, forgings, flash-welded rings and conversion stock. Plate needs its own agreed specification and acceptance requirements.
Can TC10 wire be used for aircraft fasteners?
It can be sourced for a qualified fastener manufacturing route. State the drawing, forming process, wire condition and final fastener requirements. Wire certification does not replace finished-fastener testing.
Should I order annealed or heat-treated material?
Use the state required by the approved manufacturing plan. Identify any later forging, forming, machining or heat treatment and agree which properties must be demonstrated at delivery.
Can TiHubs coordinate structural forgings?
Send the finished drawing and required blank stage. We review dimensions, material route, forging and heat-treatment requirements, inspection and traceability with the supply partners before confirming scope.
What inspection records should the order include?
Define chemical analysis, condition, tensile sampling, structure, dimensional inspection and any ultrasonic or surface examination. Specify methods and acceptance criteria rather than requesting an undefined aerospace certificate.
What information is needed for a TC10 quotation?
Provide product form, dimensions, quantity, specification edition, material condition, drawing revision, test requirements and destination. For fastener wire or structural blanks, include the intended manufacturing route.
07 / Your next step
Start with the
requirement you have.
Send the product details, drawing or operating conditions you already know. We will identify missing information and discuss a suitable supply route before quotation.
- Requirement review
- Technical clarification
- Supply proposal and quotation
Combine materials and parts in one enquiry.
Send one list of TC10 forms, sizes and quantities. Include drawing revisions, material conditions and items that must be supplied or dispatched together.
Share the service and acceptance priorities.
Include load and temperature conditions, critical sections, required material records, process qualification, inspection, destination and timing.
Baoji, China · info@tihubs.com
Start your TC10 / Ti-662 enquiry
Send your material form, drawing or process conditions. We will help clarify the remaining requirements.