TC20 / Ti-6Al-7Nb · Alpha-beta titanium alloy
TC20 / Ti-6Al-7Nb. For implant-material manufacturing.
Source TC20 / Ti-6Al-7Nb bar, wire and drawing-based blanks for implant manufacturing. Coordinate material identity, microstructure, surface condition and traceability with one technical and commercial contact in Baoji.
Start with a specification, drawing or application. We’ll help identify the details still needed.
Material review. Supply coordination.
One contact in Baoji, China.
01 / Product forms
Find your TC20 product.
Choose a material form or application. Send the dimensions, service conditions and required records so we can match the manufacturing route to your order.

TC20 / Ti-6Al-7Nb
TC20 titanium bar & rod
Precision starting stock for implant screws, abutments and machined component blanks. Quote by size and required material condition.
- Specification
- ASTM F1295 / ISO 5832-11 / GB/T 13810 TC20, as specified; confirm each edition and size range.
- Dimensions & supply
- Diameter, length, tolerance, straightness, turned or ground finish and lot quantities.
- Manufacturing review
- Define machining allowance, surface contamination limits and any process qualification coupons.
- Acceptance
- Chemical and tensile records, microstructure, surface checks, specified NDT and heat-to-piece traceability.

TC20 / Ti-6Al-7Nb
Ti-6Al-7Nb wire
Wire and straight lengths for validated medical component manufacturing; identify the finished function before selecting condition.
- Specification
- ASTM F1295 or the applicable TC20 requirements of GB/T 13810.
- Dimensions & supply
- Diameter, tolerance, coil or straight lengths, cast, helix, package size and handling requirements.
- Manufacturing review
- Drawing, forming and subsequent thermal processing can change strength and ductility; define the delivered state.
- Acceptance
- Diameter, surface integrity, lot testing and cleanliness. Product wire is not automatically a qualified welding filler.

TC20 / Ti-6Al-7Nb
TC20 forging & machining blanks
Billets and oversize blanks for conversion into drawing-controlled implant components.
- Specification
- Agree the blank specification, chemistry and conversion route; identify which final material-standard requirements are verified after processing.
- Dimensions & supply
- Blank envelope, minimum section, forging stock, machining allowance and sample quantity.
- Manufacturing review
- Define deformation route, intermediate condition and final heat treatment with the responsible manufacturer.
- Acceptance
- Material pedigree, conversion records and agreed inspection stages. Do not accept a chemistry-only certificate as implant-material release.

TC20 / Ti-6Al-7Nb
Hip stem manufacturing blanks
Application illustration: forged and machined blanks for femoral stem designs specified in Ti-6Al-7Nb.
- Specification
- The approved implant drawing, material specification and manufacturing control plan govern.
- Dimensions & supply
- Stem envelope, datum system, neck and taper geometry, machining stock and lot identification areas.
- Manufacturing review
- Review forging flow, stock removal, surface treatment and the sequence of dimensional and fatigue qualification.
- Acceptance
- Agree component inspection separately from raw material tests; design validation and device release remain with the responsible manufacturer.

TC20 / Ti-6Al-7Nb
Bone fixation component blanks
Application illustration: material and machining coordination for specified bone plates, screws and fixation components.
- Specification
- Use the specified TC20 / Ti-6Al-7Nb material route and released component drawings.
- Dimensions & supply
- Plate thickness, contour, hole geometry, thread profile, critical radii and drawing revision.
- Manufacturing review
- Review plate forming, thread manufacturing, deburring and protection of fatigue-sensitive surfaces.
- Acceptance
- Dimensional reports, surface integrity, process records and traceability. Finished assembly performance requires its own validation.

TC20 / Ti-6Al-7Nb
Dental implant & abutment blanks
Application illustration: precision stock and component blanks for dental designs that explicitly specify Ti-6Al-7Nb.
- Specification
- Material selection must follow the device drawing; TC20 is not an automatic replacement for CP titanium or TC4 ELI.
- Dimensions & supply
- Blank size, connection geometry, threads, concentricity, surface allowance and quantity.
- Manufacturing review
- Agree machining, cleaning and surface-treatment responsibilities before producing qualification samples.
- Acceptance
- Material identity plus critical dimensional and surface checks; device-specific fatigue and biological assessment are separate.
Images illustrate material forms and application possibilities. Reference markings identify specification options; they do not establish dual certification, stock availability or approval of finished equipment.
Define the shape. Share the service.
These details help turn a material enquiry into a comparable quotation.
01 / Drawing review
Drawing-controlled blanks
Provide rough and finished drawings, datum positions, critical sections, machining allowance and the intended conversion route.
Discuss your drawing02 / Drawing review
Heat treatment & process sequence
Identify the required delivery condition and subsequent manufacturing steps. Agree process records, sampling stages and dimensional checks after thermal processing.
Discuss your drawing03 / Drawing review
Component inspection planning
Specify surface integrity, microstructure, NDT, dimensional acceptance and traceability. Identify which tests apply to raw material and which apply to the finished component.
Discuss your drawing02 / Material identity
What is TC20 / Ti-6Al-7Nb titanium?
TC20 / Ti-6Al-7Nb is an aluminium-niobium titanium alloy used as starting material for surgical implant manufacturing. Also identified as UNS R56700, it uses niobium as a beta stabilizer rather than the intentional vanadium addition in Ti-6Al-4V. The purchase requirement must identify the product form, material condition and implant-material specification.
Specify the exact standard edition, form and delivery condition. Nominal chemistry is only one part of an order; strength, microstructure, dimensional acceptance and traceability also need to be defined.
Minimum tensile strength
Minimum proof strength
Minimum elongation
GB/T 13810-2017 TC20 annealed bar reference, diameter over 7 mm through 90 mm. Apply the complete table, sampling and test requirements; do not extrapolate to every wire or finished implant.
| Review item | Order basis | What to confirm |
|---|---|---|
| Material condition | Define the ordered heat-treatment state | Tie test results to the same conversion and thermal history as the supplied product. |
| Strength and ductility | Product- and section-dependent | Specify tensile, proof strength, elongation, sampling location and test direction in the purchase requirement. |
| Microstructure | Agree acceptance limits | Review grain structure, alpha morphology, surface alpha case and metallographic sampling for the manufacturing route. |
| Fatigue and fracture | Application-specific validation | A material tensile certificate does not establish component life. Specify any fatigue, toughness or crack-growth evaluation separately. |
| Non-destructive examination | Drawing / product specification | Define method, calibration, coverage, acceptance class and reporting before production. |
| Selected element · wt % | Reference composition |
|---|---|
| Aluminium · Al | 5.5–6.5 |
| Niobium · Nb | 6.5–7.5 |
| Iron · Fe | 0.25 max. |
| Oxygen · O | 0.20 max. |
| Tantalum · Ta | 0.50 max. |
| Titanium · Ti | Balance |
Selected Ti-6Al-7Nb limits from the TIMET TIMETAL 367 datasheet; confirm the complete chemistry against the ordered ASTM F1295 / ISO 5832-11 / GB/T 13810 edition.
TC20 and Ti-6Al-7Nb
TC20 is the Chinese alloy designation discussed alongside Ti-6Al-7Nb. Specify ASTM F1295, ISO 5832-11 or GB/T 13810 with the required edition, product form and condition. Dual compliance must be demonstrated against both complete requirements.
Compared with TC4 / Grade 5
Both belong to the alpha-beta titanium family, but their alloying systems differ. TC20 contains niobium; TC4 contains vanadium. A generic TC4 certificate cannot release TC20 material.
Compared with TC4 ELI / Grade 23
Grade 23 is an ELI Ti-6Al-4V route, not a shortened name for Ti-6Al-7Nb. Choose the specified material based on the approved device design and manufacturing validation.
Material versus finished device
Material-standard compliance does not establish the safety, fatigue life, sterilization validation or regulatory approval of a finished implant. Define the supply boundary and the device manufacturer’s responsibilities.
03 / Application priorities
TC20 in application.
Review each main use through its service conditions, material choice, manufacturing route and acceptance plan. These are sourcing discussions; approved drawings and qualification requirements govern the final component.
Application review / 01
Hip stems & femoral components
Ti-6Al-7Nb has an established role in femoral-component material selection. For a stem procurement project, useful material strength must be considered together with geometry, cyclic loading and surface processing. A material certificate alone does not describe the fatigue performance of the finished neck, taper or stem.
Products & manufacturing
Bar, forging stock and drawing-based stem blanks. Distinguish oversize forging, rough-machined blank and finished component in the RFQ.
Service & design review
Provide drawing revision, critical sections, stock allowance, forging route, material condition and the required qualification sequence. Identify whether coatings, roughening or polishing occur after delivery.
Purchase & inspection priorities
Agree heat traceability through forging and machining, microstructural acceptance, dimensional inspection and surface controls. The device manufacturer defines design validation and final release.
Application review / 02
Bone plates & fracture fixation
TC20 can be considered for fixation components when it is specified by the device design. Plate contouring, screw holes and local transitions create manufacturing requirements that a raw tensile value cannot capture. Buyers should define the delivered manufacturing stage so that forming and finishing obligations are clear.
Products & manufacturing
Specified sheet/plate, bar, screws or machined blanks. Sheet and plate can be quoted under a suitable implant-material route after dimensions are reviewed.
Service & design review
State thickness, rolling direction where relevant, bend radii, hole pattern, thread details and minimum remaining sections. Identify forming temperature, subsequent heat treatment and cosmetic versus functional surfaces.
Purchase & inspection priorities
Agree plate and thread inspection, burr limits, lot records and qualification samples. Assembly strength and cyclic performance must be validated for the actual design.
Application review / 03
Spinal fixation components
Rod, screw and connector enquiries require clarity about the approved alloy and final mechanical condition. A TC20 raw-material order should remain traceable through cutting, machining and any bending or finishing operation; mixing similar-looking titanium grades creates avoidable release problems.
Products & manufacturing
Bar and wire/rod stock for drawing-specified spinal fixation elements, or component blanks within an agreed manufacturing scope.
Service & design review
Provide thread and connection geometry, rod size, bending requirements, fatigue-critical radii and the required material condition. State whether the order is development material or released production.
Purchase & inspection priorities
Define dimensional sampling, surface inspection, chemistry confirmation and heat/lot marking. System-level fatigue testing, compatibility and regulatory acceptance are separate from supply of the alloy.
Application review / 04
Dental implants & abutments
Ti-6Al-7Nb is a possible material route for dental components whose design specifies it. It should not be substituted into a CP-titanium or TC4 ELI design solely because the dimensions are similar. Small connections and threaded sections make surface condition and dimensional consistency central purchasing concerns.
Products & manufacturing
Precision bar, implant blanks, abutment blanks and drawing-based machined samples. Illustrations show a manufacturing use, not an approved device catalogue.
Service & design review
Share the connection type, thread profile, datum structure, runout limits, surface treatment and cleaning sequence. Confirm who controls biological evaluation and mechanical qualification.
Purchase & inspection priorities
Specify inspection of critical fits, material traceability, contamination controls and sample approval. No clinical lifetime or device approval is inferred from the material designation.
Application review / 05
Precision machining of implant stock
Stable incoming stock helps a medical component manufacturer control its machining process. Straightness, skin removal and diameter tolerance affect workholding and yield; quoting only by alloy and weight can leave these costs unresolved.
Products & manufacturing
Ground or turned bar, cut lengths and machined blanks matched to the actual nesting and machining plan.
Service & design review
Provide minimum usable length, saw allowance, diameter tolerance, surface finish, end condition and preferred identification position. State restrictions on marking and contact materials.
Purchase & inspection priorities
Agree incoming inspection and certificate fields before supply. Keep individual cut pieces linked to the original heat and test lot throughout subcontract processing.
Application review / 06
Wire forming & small components
A thin wire order needs a clear distinction between strength in the delivered state and ductility required for downstream forming. The name Ti-6Al-7Nb alone does not specify either. Fine surface defects may also become significant after severe bending.
Products & manufacturing
Straight wire or coils for a defined medical manufacturing process, with diameter and condition selected by the buyer.
Service & design review
Describe forming strain, bend geometry, straightness or cast/helix, spool handling and any subsequent thermal process. Welding consumables require a separate qualification basis.
Purchase & inspection priorities
Confirm tensile sampling, surface criteria, diameter checks and packaging protection. Assess the finished part after its complete processing sequence.
Application review / 07
Development lots & validation samples
Development material should represent the proposed production route closely enough to make qualification results useful. A sample made from a different condition or source may machine well but fail to establish a repeatable production supply basis.
Products & manufacturing
Small trial lots, representative blanks, machining coupons and retained samples with documented identity.
Service & design review
Identify which variables may change after trials: melt source, conversion route, heat treatment, size or surface finish. Define approval criteria and the evidence required to move into production.
Purchase & inspection priorities
Keep sample and production records connected. Agree how any later material or process change is reviewed before shipment rather than assuming the first sample approves all variants.
Application review / 08
Traceable repeat production
For recurring implant-material purchases, consistency of documentation can be as important as consistent dimensions. The order should state the exact evidence needed by the receiving quality team, so missing records do not delay material release.
Products & manufacturing
Scheduled lots of bar, wire and approved blanks with stable item codes and controlled specifications.
Service & design review
Provide the approved supplier and process requirements, certificate format, revision control, lot separation, marking and packaging rules. Confirm whether third-party inspection is required.
Purchase & inspection priorities
Review material and inspection records against the purchase order before dispatch. Device approval, sterilization and finished-product labelling remain outside an unqualified raw-material supply claim.
Chemical-equipment enquiry checklist
Make the corrosion duty part of the order.
A useful specification connects the environment, the supplied parts and the acceptance evidence. Share existing data first; missing details can be clarified.
Define the service envelope
Provide normal, minimum and maximum operating conditions, both-side media, impurities, concentration changes, deposits and cleaning cycles. Include relevant corrosion history or the test evidence your engineering team requires.
Define the supplied boundary
List each wetted item, drawing and material route. Separate raw material, formed or machined parts, welded subassemblies and complete equipment. Identify design-code responsibilities, joints and mating materials.
Define the evidence and milestones
Agree chemistry and heat identity, product-specific mechanical tests, dimensional and integrity checks, welding records where applicable and inspection hold points. State sample, third-party inspection, packaging and delivery requirements.
Example: a useful TC20 heat-exchanger tube enquiry
“TC20 titanium seamless tubes to ASTM B338-08b; OD × wall × length and quantity; straight or U-bent drawing; both-side media, temperature and pressure; tube-to-tubesheet connection; required material records, integrity tests and post-bending checks; destination and target delivery.”
For TC20, specify the agreed Chinese product route, such as GB/T 3624-2023 for seamless tube, and all equipment-specific requirements. Do not assume GB/T 3625-2007 covers TC20.
Discuss your equipment requirement04 / Standards & documentation
Match the standard
to the product.
Choose the specification by product form, material condition and application. Identify the required edition on the order; a chemistry standard alone does not define a finished forging or component.
| Product / review | International / project route | Chinese reference | Clarify before quotation |
|---|---|---|---|
| Identity & chemistry | ASTM F1295Publisher reference ↗ISO 5832-11:2024Publisher reference ↗ | GB/T 3620.1-2016View PDF ↗ | Full alloy designation, chemical limits, melt identity and agreed product route. |
| Bar, rod & starting stock | ASTM F1295Publisher reference ↗ISO 5832-11:2024Publisher reference ↗ | GB/T 13810-2017View PDF ↗ | Grade and dimensional coverage, condition, sampling, tensile testing, surface and required NDT. |
| Forgings & drawing-based parts | Approved drawing and controlled process specification | Agreed Chinese aerospace / product specification, where applicable | Do not release the component against chemistry alone. Agree forging route, heat treatment, microstructure, NDT and drawing inspection. |
The purchase order must identify the required revision, grade, product form, condition and inspection. Reference documents do not replace design approval, manufacturing qualification or application-specific acceptance.
Request the controlled specification revision for your order. Any substitution, equivalence or dual-certification claim requires a documented comparison and agreement.
05 / Order coordination
Know the scope
before ordering.
Our founder’s 20 years in titanium inform the questions we ask before quotation and the supply options we review with you.

A quotation you can evaluate
Agree the grade, standard edition, dimensions, tolerance, condition and quantity before comparing prices.
- Identify whether inspection, samples and tooling are included.
- Confirm packaging, transport and delivery terms.
- Record items that still need technical confirmation.
Acceptance agreed before supply
Confirm material identity, delivery condition, heat-to-piece traceability, dimensional checks and required testing before production. For converted parts, define inspection after forging, heat treatment and machining, including the specified microstructure and NDT scope.
Independent inspection can be discussed with its scope, timing, acceptance criteria and cost agreed for the order.
Delivery with clear milestones
Review the proposed lead time, approvals, production sequence and dispatch requirements. For several product forms, coordinate document and packing readiness together.
Material substitutions and technical changes require written approval. A schedule deviation should identify the impact, decisions needed and next steps.
One contact when an issue arises
Contact TiHubs with the order reference, affected items and supporting photos or inspection records.
We record the issue, review it against the agreed requirements and coordinate the next steps with the relevant manufacturing parties.
Material records
Grade, standard, test results and heat or batch identity matched to the supplied items.
Inspection records
Dimensional and testing records for the agreed scope, including critical drawing requirements.
Dispatch records
Item identification, packing list, protective packaging and required shipment documents.
06 / Questions before sourcing
Before you specify
TC20 / Ti-6Al-7Nb.
A clear material designation is the beginning. Product form, specification revision, material condition and acceptance complete the requirement.
A useful first enquiry
- Product and specificationProduct form, standard edition, dimensions and material condition.
- Order and deliveryQuantity, destination and any required delivery date.
- Acceptance requirementsDrawing revision, inspection, certificates and packaging.
Not every detail is finalized? Send the information you have. We can help identify the questions to resolve before quotation.
What happens next: requirement review, technical clarification, then a supply proposal and quotation.
What is TC20 / Ti-6Al-7Nb titanium?
TC20 / Ti-6Al-7Nb is an aluminium-niobium titanium alloy used as starting material for surgical implant manufacturing. Also identified as UNS R56700, it uses niobium as a beta stabilizer rather than the intentional vanadium addition in Ti-6Al-4V. The purchase requirement must identify the product form, material condition and implant-material specification.
Is TC20 the same as TC4 or Grade 23?
Both belong to the alpha-beta titanium family, but their alloying systems differ. TC20 contains niobium; TC4 contains vanadium. A generic TC4 certificate cannot release TC20 material. Grade 23 is an ELI Ti-6Al-4V route, not a shortened name for Ti-6Al-7Nb. Choose the specified material based on the approved device design and manufacturing validation.
Which standards should I specify?
Specify ASTM F1295, ISO 5832-11 or GB/T 13810 TC20 with the required edition, form and condition. Use GB/T 3620.1 for Chinese designation chemistry, not as a substitute for the complete implant-material product requirements.
What are the main application directions?
The principal direction is material for surgical implant manufacturing, particularly femoral stems. Drawing-approved bone fixation, spinal and dental components can also be discussed. The material choice and device validation belong to the responsible device manufacturer.
Can you supply sheet and plate as well as bar and wire?
Yes, sheet/plate enquiries can be reviewed against the specified implant-material standard and dimensions. GB/T 13810-2017 includes TC20 sheet/plate requirements. Availability, quantity and processing route are confirmed in the quotation; catalogue illustrations do not establish stock.
Does material compliance mean the implant is approved?
No. Material chemistry, properties and microstructure are one part of the manufacturing requirement. Device design, biological evaluation, fatigue validation, surface processing, sterilization and regulatory release require their own controls.
What records should accompany the material?
Agree chemical and mechanical results, heat and lot identity, product dimensions, condition, microstructure, surface inspection and NDT where specified. Record the required certificate format and maintain traceability through any conversion or machining.
What should I send for a quotation?
Provide the material designation, standard edition, form, dimensions, tolerances, condition and quantity. For blanks, add the drawing revision, manufacturing stage, critical surfaces, inspection scope, sample requirements and destination.
How are samples, MOQ and lead time determined?
These depend on form, size, melt/conversion route, available stock, tooling and inspection. TiHubs confirms the proposed scope and milestones in the quotation; representative samples and written approval can be agreed before production.
07 / Your next step
Start with the
requirement you have.
Send the product details, drawing or operating conditions you already know. We will identify missing information and discuss a suitable supply route before quotation.
- Requirement review
- Technical clarification
- Supply proposal and quotation
Combine materials and parts in one enquiry.
Send one list of TC20 forms, sizes and quantities. Include drawing revisions, material conditions and items that must be supplied or dispatched together.
Share the service and acceptance priorities.
Include load and temperature conditions, critical sections, required material records, process qualification, inspection, destination and timing.
Baoji, China · info@tihubs.com
Start your TC20 / Ti-6Al-7Nb enquiry
Send your material form, drawing or process conditions. We will help clarify the remaining requirements.