Ti-6242S · TA19 · UNS R54620
Ti-6242S / TA19 titanium.For compressor forgings and formed aerospace parts.
Source Ti-6242S / TA19 titanium sheet, bar, forging blanks and wire for specified aerospace requirements. TiHubs connects the material form, heat-treatment condition, drawing and inspection scope through one contact in Baoji.
Start with a specification, drawing or application. We’ll help identify the details still needed.
Material review. Supply coordination.
One contact in Baoji, China.
01 / Product forms
Find your
Ti-6242S / TA19 product.
Choose a material form or application. Send the dimensions, service conditions and required records so we can match the manufacturing route to your order.

Ti-6242S / TA19 · Ti-6242S · Ti-6Al-2Sn-4Zr-2Mo-0.08Si
Ti-6242S / TA19 titanium sheet & plate
Flat material for defined aerospace forming and machining requirements. Provide the finished drawing together with the starting thickness so the rolling direction, forming allowance and final condition can be reviewed.
- Specification
- AMS 4919 is a Ti-6Al-2Sn-4Zr-2Mo-0.08Si sheet, strip and plate route in the duplex-annealed condition. Specify the drawing-required revision and thickness scope.
- Geometry
- Thickness × width × length, flatness, grain direction, surface and trim allowance. Identify critical bend radii, formed wall thickness and holes or cut-outs.
- Processing
- Define supplied-sheet condition, forming, joining and any subsequent heat treatment. Agree where raw material supply ends and fabrication responsibilities begin.
- Acceptance
- Material records, test direction, surface, dimensions and the required inspection or forming samples. For TA19, identify the agreed sheet product specification as well as chemistry.

Ti-6242S / TA19 · Ti-6242S · Ti-6Al-2Sn-4Zr-2Mo-0.08Si
Ti-6242S / TA19 titanium bar & rod
Starting stock for machined aerospace components and reviewed forging routes. The required delivered condition and the test condition should be clear before a price is compared.
- Specification
- AMS 4975 covers the specified alloy in bars and wire, with a separate flash-welded-ring scope. GB/T 2965-2023 provides a TA19 bar route.
- Geometry
- Diameter or section, length, straightness, surface finish, machining allowance and quantity per size. State whether bars are for machining or further conversion.
- Condition
- Specify the AMS heat-treated delivery route or the TA19 hot-/cold-worked route. The cited Chinese bar standard tests heat-treated specimen blanks; it does not describe all bars as supplied annealed.
- Acceptance
- Chemistry, test specimen treatment and orientation, mechanical records, agreed NDT, surface and traceability through cutting or machining.

Ti-6242S / TA19 · Ti-6242S · Ti-6Al-2Sn-4Zr-2Mo-0.08Si
Ti-6242S / TA19 forging blanks & rings
Billets and drawing-based forging blanks for compressor and structural requirements. Send the blank and finished-part envelopes so the forming route, machining allowance and inspection access can be discussed.
- Specification
- AMS 4976 is the solution- and precipitation-heat-treated forging route. Apply its dimensional limits and the ordered revision; forging stock is a distinct supply category.
- Geometry
- Forging drawing, disc or ring dimensions, section transitions, minimum stock allowance, grain-flow requirements and quantity.
- Processing
- Specify the intended microstructure, forging and final heat-treatment requirements. Different forging routes should not be treated as equivalent solely because the chemistry matches.
- Acceptance
- Test locations, orientation, structure, agreed ultrasonic examination and surface inspection. TA19 forgings require an agreed forging specification alongside GB/T 3620.1 identity.

Ti-6242S / TA19 · Ti-6242S · Ti-6Al-2Sn-4Zr-2Mo-0.08Si
Ti-6242S / TA19 titanium structural wire
Wire for the product or component route stated on the drawing. Specify the diameter, straight or coiled form and downstream manufacturing requirements; identify welding filler as a separate enquiry.
- Specification
- AMS 4975 includes Ti-6Al-2Sn-4Zr-2Mo-0.08Si wire. State the required revision, diameter range and delivered condition.
- Supply form
- Diameter and tolerance, coil or straight lengths, coil weight, surface, straightness and packaging requirements.
- Processing
- Required forming or machining steps, final heat treatment and surface requirements. Agree any sample evaluation before a production quantity.
- Acceptance
- Chemistry, mechanical tests, dimensions, surface and lot traceability. A structural-wire description does not establish compliance with a welding-filler classification.

Ti-6242S / TA19 · Ti-6242S · Ti-6Al-2Sn-4Zr-2Mo-0.08Si
Aerospace compressor disc & ring forging requirements
Application illustration: source material and processing coordination for released compressor-part requirements. The material enquiry must connect the finished geometry with the specified heat treatment, inspection and customer approval route.
- Supply boundary
- Forging stock, rough forging, heat-treated blank or machined component. Identify the exact stage to be purchased and the responsible parties for the remaining stages.
- Operating duty
- Design metal temperature, rotational and cyclic loads, required life-related evidence and the drawing-defined critical zones.
- Manufacturing
- Blank geometry, grain-flow or microstructure requirements, thermal processing, machining allowance and the specification for any special process.
- Acceptance
- Specified NDT class, test locations, dimensional records, traceability and purchaser approval. A raw-material specification alone does not qualify a rotating engine part.

Ti-6242S / TA19 · Ti-6242S · Ti-6Al-2Sn-4Zr-2Mo-0.08Si
Ti-6242S / TA19 formed shells & aerospace panels
Application illustration: sheet blanks and drawing-based formed components for approved aerospace designs. Clarify the starting sheet and the complete fabrication sequence before requesting a repeat-production quotation.
- Starting material
- AMS 4919 sheet or plate when specified, or the agreed TA19 product route. Identify thickness, condition and rolling direction.
- Forming
- Shape, bend radii, draw depth, final wall, trim allowance and dimensional datums. State whether tooling, samples and assembly fixtures are included.
- Joining
- Joint geometry, joining procedure requirements, post-process condition and inspection access. Record any purchaser hold points.
- Acceptance
- Final profile and dimensions, surface, joint inspection where applicable, source-material records and defined first-article evidence.
Images illustrate material forms and application possibilities. Reference markings identify specification options; they do not establish dual certification, stock availability or finished-component approval.
Define the product. Share the requirement.
These details help turn your enquiry into a comparable quotation.
01 / Requirement review
A compressor forging
Send the blank and finished drawings, critical sections, structure and inspection requirements. Identify the required delivery stage.
Discuss your requirement02 / Requirement review
A formed sheet component
Provide gauge, rolling direction, final geometry, forming and joining requirements. Agree samples and post-process dimensional checks.
Discuss your requirement03 / Requirement review
A machining-stock package
List each size, condition, test basis and quantity. Specify cut-piece marking, material records and coordinated delivery requirements.
Discuss your requirement02 / Material identity
What is
Ti-6242S / TA19 titanium?
Ti-6242S / TA19 is a silicon-containing near-alpha titanium alloy. A useful purchase specification links its chemistry with the product form, manufacturing route and required high-temperature or cyclic performance.
The headline values below are the TA19 bar test reference from GB/T 2965-2023. They apply to heat-treated specimen blanks, not automatically to stock in its delivered worked condition.
Minimum tensile strength · heat-treated test specimen
Minimum proof strength · heat-treated test specimen
Minimum elongation · heat-treated test specimen
GB/T 2965-2023 · TA19 · clause 5.3 and Table 2; TA19 bars are delivered in R or Y condition.
| Property or condition | Reference | Ordering implication |
|---|---|---|
| Headline reference | TA19 bars · GB/T 2965-2023 | 895 MPa tensile, 825 MPa proof strength and 10% elongation are minimum values from the cited TA19 test table, evaluated on heat-treated specimen blanks. |
| Delivered bar condition | Hot worked or cold worked | The cited Chinese standard specifically limits TA19 bar delivery to R or Y condition. Confirm specimen treatment separately from delivered-stock condition. |
| Sheet route | Duplex annealed | AMS 4919 addresses a different product and condition from AMS 4975 bar/wire or AMS 4976 forgings. Apply the ordered product table and thickness scope. |
| Density | Approximately 4.54 g/cm³ | Producer reference useful for preliminary mass calculations. Confirm the actual blank dimensions and machining allowance for material estimates. |
| Elevated-temperature duty | Time, load and condition matter | Specify metal temperature, exposure duration, thermal cycles, creep or fatigue acceptance and final condition. A producer temperature reference is not a component operating approval. |
| Forging evaluation | Structure and sampling are part of the order | Agree the required process route, microstructure, test orientation and inspection zone instead of selecting stock by tensile strength alone. |
Product-specific specifications and the ordered revision govern acceptance. Mechanical references are not design allowables or proof of a finished component’s operating life.
| Element · wt.% | Ti-6242S · nominal identity | GB/T 3620.1-2016 · TA19 limits |
|---|---|---|
| Aluminum · Al | 6 nominal | 5.5–6.5 |
| Tin · Sn | 2 nominal | 1.5–2.5 |
| Zirconium · Zr | 4 nominal | 3.6–4.4 |
| Molybdenum · Mo | 2 nominal | 1.5–2.5 |
| Silicon · Si | 0.08 nominal in cited AMS titles | 0.06–0.10 |
| Oxygen · O | Apply the ordered product specification | 0.12 max. |
| Iron · Fe | Apply the ordered product specification | 0.25 max. |
| Carbon · C | Apply the ordered product specification | 0.08 max. |
| Nitrogen · N | Apply the ordered product specification | 0.05 max. |
| Hydrogen · H | Apply the ordered product specification | 0.015 max. |
| Titanium · Ti | Balance | Balance |
The middle column identifies nominal alloy additions; it is not an AMS acceptance table. Apply the complete ordered specification, including residual elements, analysis basis and product-specific exceptions.
Ti-6242S / TA19 / Ti-6Al-2Sn-4Zr-2Mo-Si
These names identify the silicon-containing near-alpha alloy family discussed on this page. Specify TA19 or the full aerospace designation together with the required product standard and condition.
Ti-6242S and Ti-6246
Ti-6246 contains a higher nominal molybdenum addition and follows different product and processing requirements. An abbreviated 6242 or 6246 name should remain linked to the full alloy designation on drawings and orders.
Sheet, bar and forging routes
AMS 4919, AMS 4975 and AMS 4976 address different forms and conditions. A sheet certificate cannot automatically establish acceptance of a forging or an engine component.
Stock condition and test condition
The TA19 bar reference distinguishes hot-/cold-worked delivery from heat-treated specimen testing. State both conditions so quotations and records describe the same material scope.
03 / Application review
Ti-6242S / TA19 for compressor and aerospace structures.
Define the component, manufacturing stage and acceptance evidence. We review the source material and processing scope around the purchaser’s released requirements.
Application review / 01
Compressor forgings: begin with the critical section
Ti-6242S / TA19 enquiries for compressor disc and ring blanks should begin with the released drawing and the material specification required by the engine programme. Review the thickest section, changes in section and the intended machining sequence before selecting a blank. The purchasing scope should identify the manufacturing stage at delivery and the evidence required before the next stage is approved.
Products to discuss
Forging stock, rough disc and ring blanks, heat-treated forgings and defined machining work. Separate source stock from finished rotating components in the quotation.
What we need to review
Material and process revisions, blank drawing, required structure and grain flow, test locations and orientations, critical-zone NDT, machining allowance and approval hold points. Identify temperature, rotational duty and cyclic acceptance where these drive the specified requirements.
Application review / 02
Blade and impeller stock: retain the drawing requirements
For a blade or impeller enquiry, material identity is only the start of the order definition. The geometry may create thin features beside a comparatively thick hub or root, so the purchaser should identify which material, dimensional and surface requirements apply at each critical area. TiHubs reviews the requested supply stage and the records needed for the buyer’s subsequent processing.
Products to discuss
Bar or forging blanks and drawing-based machining where the ordered specifications permit the selected route. A development blank and an approved production part require different evidence.
What we need to review
Blank dimensions, orientation, root or hub stock, surface finish, heat-treatment responsibility, NDT access and datum scheme. State required process approvals, first-article documents and any customer-source restrictions.
Application review / 03
Engine cases: define the ring, shell or assembled route
A casing request may refer to a forged ring, a machined housing or a sheet-fabricated shell. These are separate manufacturing scopes. Provide the released geometry and design requirements so the enquiry can identify an appropriate material form, the included processing and the inspection stages. Do not price every case using a generic ring or sheet description.
Products to discuss
Forged ring or housing blanks, sheet-based shell sections and specified machined interfaces. Define whether joining, final machining or assembly is included.
What we need to review
Wall transitions, flanges, sealing and mounting faces, tolerances, thermal duty and required structure. Agree dimensional checks after heat treatment, weld requirements where relevant, surface inspection and the final record package.
Application review / 04
Formed panels: connect the sheet condition to the final shape
For Ti-6242S / TA19 formed-panel work, request a quotation against the final geometry and the specified starting sheet. The review should identify how stock thickness, rolling direction, forming allowance and later trimming relate to the part being accepted. Where a trial is needed, separate sample approval from the production release so the buyer can assess the result before committing a series.
Products to discuss
AMS 4919 sheet or plate when specified, cut blanks, formed panels and drawing-based shell sections. A flat sheet enquiry can be priced separately from tooling and forming.
What we need to review
Drawing revision, gauge tolerance, radii, draw depth, minimum remaining wall, trim allowance, heat treatment, attachment details and final dimensional datums. Identify trial parts, tooling ownership and inspection reports.
Application review / 05
Thermal structures: order against metal temperature and time
The 6-2-4-2 alloy family appears in producer references for afterburner sheet structures. For a purchasing enquiry, define the actual part and the design-specified material rather than treating an application name as a temperature rating. Metal temperature, exposure duration, stresses and joints affect what evidence the designer requires from the material and fabrication route.
Products to discuss
Specified sheet, formed sections and agreed fabricated items for released thermal-structure drawings. Finished-assembly qualification remains within the purchaser’s approval process.
What we need to review
Metal-temperature history, thermal cycles, required life evidence, joint details and surface requirements. Agree forming and joining procedures, final condition, inspection access and the scope of any thermal or mechanical testing.
Application review / 06
Machining stock: confirm allowance and condition together
A buyer ordering Ti-6242S / TA19 machining stock should identify the finished part, even when machining is performed elsewhere. The drawing helps define an economical stock envelope, the needed surface condition and the relationship between test orientation and the final part. Agree how cut pieces remain traceable so the delivered package can enter the buyer’s production process without missing identification.
Products to discuss
Bar, plate and forging blanks for specified brackets, fittings or other structural parts. Review each form against its own product and condition requirements.
What we need to review
Finished envelope, roughing and finishing allowance, material condition, critical threads or interfaces, cutting length, marking and test-certificate linkage. State required approved-source or special-process restrictions at the enquiry stage.
Application review / 07
Wire and ring enquiries: define the product actually purchased
Ti-6242S structural wire and ring-stock enquiries require the diameter, supplied shape and downstream process to be identified. A flash-welded ring, a seamless forged ring and straight wire do not describe the same product. Keep the chosen route visible in the enquiry and quotation so dimensional, heat-treatment and inspection requirements can be assigned to the correct stage.
Products to discuss
AMS 4975 wire or its specified flash-welded-ring route, and separately reviewed forging rings. State when the enquiry is only for source stock.
What we need to review
Diameter or section, ring geometry, joint requirement, condition, surface and quantity. Agree manufacturing responsibility, joint inspection where applicable, final dimensional checks and lot traceability.
Application review / 08
Development work: make the trial acceptance measurable
For a Ti-6242S / TA19 development project, define what the first material or part delivery is intended to demonstrate. The purchase might test forming geometry, machining allowance or an inspection method. Record that objective and the evidence required, then identify which changes need approval before repeat production. This makes sample costs and later production scope easier to compare.
Products to discuss
Small batches of specified stock, forging or forming trials and drawing-based test articles, subject to supply-route review. Trial availability and production capacity are confirmed separately.
What we need to review
Material identity, condition, sample count, test or inspection plan, reporting format and approval criteria. Identify destructive-test pieces, retained samples, permitted changes and the schedule for evaluating the results.
Purchasing checklist
Connect material, process and acceptance before ordering.
A Ti-6242S / TA19 quotation should describe what arrives, how it is tested and which manufacturing stages are included.
Material route
Full alloy identity, standard revision, product form, section and supplied condition.
Manufacturing scope
Blank drawing, forming or forging route, heat treatment, machining allowance and approval responsibilities.
Acceptance evidence
Test condition, orientation, structure, NDT, traceability and required customer documents.
“We need TA19 blanks for a compressor ring.”
We would clarify the released blank geometry, finished envelope, specified forging and heat-treatment route, critical sections, test locations, NDT class, machining scope and purchaser approval milestones before preparing a comparable quotation.
Illustrative requirement review; it does not claim an approved engine part or a completed customer project.
Discuss your requirement04 / Standards & documentation
Match the standard
to the product.
Choose the standard for the actual product and delivered condition. Available PDFs are linked below; aerospace catalog references identify additional scopes without presenting them as free full standards.
| Product form | ASTM / AMS / ASME route | Chinese standard route | Clarify before quotation |
|---|---|---|---|
| Material identity | United States / technical reference Ti-6242S · UNS R54620; use the ordered product specification for complete acceptance. | ChinaGB/T 3620.1-2016View PDF ↗ TA19 composition, including silicon. | Full alloy, chemistry limits, analysis basis and residual requirements. |
| Sheet, strip & plate | United States / technical reference AMS 4919 duplex-annealed route; see official catalog reference below. | ChinaGB/T 3620.1-2016View PDF ↗ TA19 identity plus the specified sheet product requirements. | Revision, thickness, surface, rolling direction, forming and final condition. |
| Bars & rods | United States / technical reference AMS 4975 heat-treated bar route; verify ordered section and revision. | ChinaGB/T 2965-2023View PDF ↗ TA19 R/Y delivery, with heat-treated specimen testing. | Delivered condition, specimen treatment, dimensions and test orientation. |
| Forgings & stock | United States / technical reference AMS 4976 forgings and forging stock have separate supply and size requirements. | ChinaGB/T 3620.1-2016View PDF ↗ TA19 identity plus the agreed forging specification. | Blank dimensions, structure, grain flow, process and inspection. |
| Structural wire & rings | United States / technical reference AMS 4975 wire and flash-welded-ring scope; separate any forged-ring or filler request. | ChinaGB/T 3620.1-2016View PDF ↗ Agree product requirements for the actual TA19 form. | Diameter, joint route, condition, surface and lot identity. |
| Producer reference | United States / technical referenceTi-6Al-2Sn-4Zr-2Mo · producer technical dataView PDF ↗ Original alloy-family technical information, including typical data. | China Use the ordered TA19 requirements for acceptance. | Compare reference conditions with the actual order. |
AMS catalog references do not replace the purchased standard or drawing revision. Finished-part acceptance and purchaser approval are defined separately from source-material conformity.
Use the document edition, product scope and condition specified in the purchase order. Producer technical references support discussion; they do not replace ordered product acceptance requirements.
05 / Order coordination
Know the scope
before ordering.
Our founder’s 20 years in titanium inform the questions we ask before quotation and the supply options we review with you.

A quotation you can evaluate
Agree the grade, standard edition, dimensions, tolerance, condition and quantity before comparing prices.
- Identify whether inspection, samples and tooling are included.
- Confirm packaging, transport and delivery terms.
- Record items that still need technical confirmation.
Acceptance agreed before supply
Confirm the material certificate, full grade, heat or lot identity, delivery condition, dimensional checks and required testing before supply starts. Define any process records, NDT and purchaser approval points for the ordered product.
Independent inspection can be discussed with its scope, timing, acceptance criteria and cost agreed for the order.
Delivery with clear milestones
Review the proposed lead time, approvals, production sequence and dispatch requirements. For several product forms, coordinate document and packing readiness together.
Material substitutions and technical changes require written approval. A schedule deviation should identify the impact, decisions needed and next steps.
One contact when an issue arises
Contact TiHubs with the order reference, affected items and supporting photos or inspection records.
We record the issue, review it against the agreed requirements and coordinate the next steps with the relevant manufacturing parties.
Material records
Grade, standard, test results and heat or batch identity matched to the supplied items.
Inspection records
Dimensional and testing records for the agreed scope, including critical drawing requirements.
Dispatch records
Item identification, packing list, protective packaging and required shipment documents.
06 / Questions before sourcing
Before you specify
Ti-6242S / TA19.
A clear material designation is the beginning. Product form, specification revision, material condition and acceptance complete the requirement.
A useful first enquiry
- Product and specificationProduct form, standard edition, dimensions and material condition.
- Order and deliveryQuantity, destination and any required delivery date.
- Acceptance requirementsDrawing revision, inspection, certificates and packaging.
Not every detail is finalized? Send the information you have. We can help identify the questions to resolve before quotation.
What happens next: requirement review, technical clarification, then a supply proposal and quotation.
What is Ti-6242S / TA19 titanium?
Ti-6242S / TA19 is the silicon-containing Ti-6Al-2Sn-4Zr-2Mo alloy family used in elevated-temperature aerospace material discussions. Ti-6242S is associated with UNS R54620. Order using the full designation, product specification, revision and required condition.
Where is Ti-6242S / TA19 mainly used?
Key application discussions include compressor discs, blades and impellers, engine structures and specified formed sheet parts. The exact drawing, thermal duty and purchaser material/process requirements determine the acceptable product route.
Which standards apply to sheet, bar and forgings?
AMS 4919 addresses sheet, strip and plate; AMS 4975 addresses bar, wire and flash-welded rings; AMS 4976 addresses forgings and forging stock. Each has its own condition and size scope. GB/T 3620.1 defines TA19 chemistry, and GB/T 2965-2023 provides a TA19 bar route.
Are TA19 bar strength values the as-delivered properties?
The cited GB/T 2965-2023 standard supplies TA19 bars in hot- or cold-worked condition and tests mechanical properties on heat-treated specimen blanks. Specify delivery condition and specimen treatment separately. Do not describe every delivered TA19 bar as annealed or as having the tested specimen properties without qualification.
Can you provide ring forgings or engine-casing blanks?
Send the blank and finished drawings, material/process specifications, section, quantity and required supply stage. TiHubs reviews suitable resources, machining allowance, structure, heat treatment and inspection requirements before quoting. Any engine-programme qualification or approved-source requirement must be stated.
Can Ti-6242S wire be used as welding filler?
The structural-wire route shown here does not establish welding-filler compliance. A filler enquiry must include the relevant consumable specification and classification, parent material, welding process and required approval. Do not substitute wire solely because the alloy names look similar.
What is the maximum operating temperature?
There is no single approved operating temperature for every part. Define metal temperature, exposure duration, loads, creep and fatigue requirements, final condition and joints. Producer data support preliminary material review; the component design and qualification establish the permitted service envelope.
Which inspection and aerospace documents can be discussed?
List chemistry and mechanical records, heat-treatment evidence, microstructure, NDT, test orientation, traceability and first-article requirements. TiHubs reviews the required scope and applicable supply resources. Material certification does not by itself establish approval for a finished aircraft or engine part.
How do I request price and lead time?
Send the form or drawing, Ti-6242S or TA19 designation, specification revision, size, condition, quantity and destination. Add inspection and approval requirements. We clarify missing details, separate material and processing costs, and confirm proposed samples and delivery milestones with the quotation.
07 / Your next step
Start with the
requirement you have.
Send the product details, drawing or operating conditions you already know. We will identify missing information and discuss a suitable supply route before quotation.
- Requirement review
- Technical clarification
- Supply proposal and quotation
Combine materials and parts in one enquiry.
Send one list of Ti-6242S / TA19 forms, sizes and quantities. Include drawing revisions and items that need to be supplied together.
Define the condition and acceptance priorities.
Include the ordered specification, final application, material condition, inspection and documentation, destination and required delivery milestones.
Baoji, China · info@tihubs.com
Start your Ti-6242S / TA19 enquiry
Send your material form, drawing or process conditions. We will help clarify the remaining requirements.