Grade 21 · Gr21 · TB8 · UNS R58210
Grade 21 / TB8 titanium.For formed aerospace components.
Source Grade 21 / TB8 titanium sheet, strip, bar, pipe and wire for reviewed aerospace and engineering requirements. TiHubs coordinates the material condition, forming or fabrication scope and inspection through one contact in Baoji.
Start with a specification, drawing or application. We’ll help identify the details still needed.
Material review. Supply coordination.
One contact in Baoji, China.
01 / Product forms
Find your
Grade 21 / TB8 product.
Choose a material form or application. Send the dimensions, service conditions and required records so we can match the manufacturing route to your order.

Grade 21 / TB8 · Gr21 · Ti-15Mo-3Al-2.7Nb-0.25Si
Grade 21 / TB8 titanium sheet, strip & plate
Material for formed thin-wall structures and drawing-based components. Define the starting condition for forming and the final aging or property requirement before requesting a production quotation.
- Specification
- ASTM B265 Grade 21 or GB/T 3621 TB8 within the stated product scope. AMS 4897 is a sheet-and-strip aerospace option when specified by the drawing.
- Dimensions
- Thickness × width × length, strip or cut-sheet form, thickness tolerance, flatness, rolling direction, surface and edge condition.
- Processing
- Forming sequence, bend or draw geometry, trim allowance, joining requirements and responsibility for final aging or dimensional correction.
- Acceptance
- Required chemical and tensile-test basis, sample orientation, surface quality and dimensional records. State any forming trial or first-article approval.

Grade 21 / TB8 · Gr21 · Ti-15Mo-3Al-2.7Nb-0.25Si
Grade 21 / TB8 titanium bar & rod
Stock for machined components and specified fastener or structural requirements. Send the final drawing with the raw-material size so the section and delivered condition can be reviewed together.
- Specification
- ASTM B348 Grade 21 with the required edition and condition. For TB8, agree the bar product requirements alongside GB/T 3620.1 material identity.
- Dimensions
- Round or rectangular section × length, straightness, surface finish, machining allowance and quantity by size.
- Condition
- Solution-treated or the specified aged strength level. Confirm when heat treatment and finish machining occur in the production sequence.
- Acceptance
- Mechanical-test location and direction, heat identity, surface and dimensions, and any agreed ultrasonic or additional inspection.

Grade 21 / TB8 · Gr21 · Ti-15Mo-3Al-2.7Nb-0.25Si
Grade 21 / TB8 seamless pipe & custom tube
Hollow material for a defined manufacturing or engineering duty. A listed Grade 21 pipe standard establishes a specification route; practical dimensions and production feasibility still need review.
- Specification
- ASTM B861 Grade 21 for seamless pipe. Define an agreed product and acceptance specification for a TB8 tubular requirement.
- Dimensions
- OD × wall × length or the ordered pipe-size system; bore, ovality, straightness, end condition and minimum finished wall.
- Condition
- Solution-treated or solution-treated and aged, as specified. Include subsequent bending, forming, joining or machining requirements.
- Acceptance
- Applicable mechanical, dimensional, pressure or NDT requirements and post-process checks. Aerospace tubing approval is separate from general pipe compliance.

Grade 21 / TB8 · Gr21 · Ti-15Mo-3Al-2.7Nb-0.25Si
Grade 21 / TB8 titanium wire
Wire for drawing-based component or processing requirements. State the purpose, starting condition and final acceptance basis so diameter alone does not determine the quotation.
- Specification
- ASTM B863 Grade 21. For TB8 wire, agree the product requirements and use GB/T 3620.1 for the material designation.
- Supply form
- Coils, spools or straight lengths; diameter, tolerance, coil weight, cast or straightness and packaging.
- Processing
- Required delivery condition, subsequent forming, final heat treatment and surface-cleanliness requirements.
- Acceptance
- Chemistry, diameter, surface and applicable mechanical tests, linked to the supplied lot. Welding filler requires its own specified consumable basis.

Grade 21 / TB8 · Gr21 · Ti-15Mo-3Al-2.7Nb-0.25Si
Aerospace exhaust & nozzle component requirements
Application illustration: sheet supply and fabrication coordination for reviewed exhaust structures. Define the thermal duty, drawing and approved manufacturing requirements before choosing the material and supply scope.
- Thermal duty
- Metal-temperature profile, exposure duration, starts and stops, thermal cycling and any oxidation or life requirements.
- Supply boundary
- Sheet blanks, formed shell segments, nozzle or plug parts, or a defined subassembly. Identify purchaser-supplied drawings and interfaces.
- Manufacturing
- Material and process specifications, forming and joining sequence, heat treatment, tooling and approved special-process requirements.
- Acceptance
- Critical dimensions, weld and surface inspection, material records, first-article requirements and purchaser approval. No flight qualification follows from the alloy name alone.

Grade 21 / TB8 · Gr21 · Ti-15Mo-3Al-2.7Nb-0.25Si
Thin-wall formed shells & heat-shield components
Application illustration: shaped sheet parts with defined material and final-condition requirements. Review the geometry and thermal duty together, including how the part will be supported and joined.
- Starting material
- ASTM B265 Grade 21 or the specified TB8 sheet route. AMS 4897 may apply to sheet and strip within its revision-specific scope.
- Geometry
- Drawing revision, wall thickness, bend or draw radii, flanges, trim lines, holes, attachment points and surface finish.
- Processing
- Starting condition, forming stages, joining, final aging and the sequence for trimming or finish machining.
- Acceptance
- Minimum remaining wall, dimensional profile, surface and weld checks, agreed samples and identification through each processing step.
Images illustrate material forms and application possibilities. Reference markings identify specification options; they do not establish dual certification, stock availability or finished-component approval.
Define the product. Share the requirement.
These details help turn your enquiry into a comparable quotation.
01 / Requirement review
A sheet-forming requirement
Provide the drawing, gauge, forming geometry and final condition. Identify sample approval and the sequence for trimming, joining and aging.
Discuss your requirement02 / Requirement review
An exhaust or warm structure
Share the metal-temperature history, loads, thermal cycles and approved material/process requirements. Define the exact supply boundary.
Discuss your requirement03 / Requirement review
A coordinated material package
List sheet, strip, bar, wire or tubular items with quantities, condition and documentation. Review common approval and dispatch milestones.
Discuss your requirement02 / Material identity
What is
Grade 21 / TB8 titanium?
Grade 21 / Gr21 / TB8 belongs to the Beta 21S titanium alloy family. A useful material review connects starting condition, final aging and thermal duty with the product specification and the part being purchased.
Use the following values as specification references, not design allowables or a universal thermal rating. Sheet, bar, tube and finished assemblies need their own acceptance basis.
Minimum tensile strength · solution-treated sheet
Minimum yield strength · solution-treated sheet
Minimum elongation · solution-treated sheet
ASTM B265-08 · Grade 21 · Table 1, including its product and condition footnotes.
| Property or condition | Reference | Ordering implication |
|---|---|---|
| Reference condition | ASTM B265-08 · Grade 21 · solution treated | The headline values relate to the cited sheet/plate table and its footnotes. Aged properties require a separately agreed basis. |
| Chinese sheet route | GB/T 3621-2022 · TB8 · ST | The cited table lists tensile strength 825–1,000 MPa and proof strength 795–965 MPa, with elongation depending on sheet thickness. |
| TB8 sheet elongation | 6% at 0.3–0.6 mm; 8% above 0.6–2.5 mm | Apply the complete table and test requirements; these are not universal values for thicker plate, bar or finished parts. |
| Bar · moderate-strength STA | 966 MPa tensile min. · 897–1,096 MPa yield · 10% elongation min. | ASTM B348-08a condition-specific reference. State the required strength level, section and sampling basis. |
| Bar · high-strength STA | 1,172 MPa tensile min. · 1,104–1,276 MPa yield · 8% elongation min. | The cited table applies to longitudinal sections up to 76 mm thickness and 64.5 cm² area; larger sections require agreement. |
| Thermal-duty acceptance | Use the component design and process requirements | Room-temperature tensile values do not establish a permissible metal temperature, exposure life, oxidation allowance or finished-assembly rating. |
The cited ASTM and Chinese sheet routes use different acceptance tables. State the required product, thickness, test direction, delivery condition and final processing requirements before comparing quotations.
| Element · wt.% | ASTM B348-08a · Grade 21 | GB/T 3620.1-2016 · TB8 |
|---|---|---|
| Molybdenum · Mo | 14.0–16.0 | 14.0–16.0 |
| Aluminum · Al | 2.5–3.5 | 2.5–3.5 |
| Niobium · Nb | 2.2–3.2 | 2.4–3.2 |
| Silicon · Si | 0.15–0.25 | 0.15–0.25 |
| Oxygen · O | 0.17 max. | 0.17 max. |
| Iron · Fe | 0.40 max. | 0.40 max. |
| Carbon · C | 0.05 max. | 0.05 max. |
| Nitrogen · N | 0.03 max. | 0.05 max. |
| Hydrogen · H | 0.015 max. | 0.015 max. |
| Titanium · Ti | Balance | Balance |
Selected chemical limits are shown in weight percent. Apply the complete ordered specification, including analysis and residual-element requirements. The cited ASTM and TB8 limits differ for niobium and nitrogen.
Grade 21 / Gr21 / TB8 / Beta 21S
These names are used for the corresponding Ti-Mo-Al-Nb-Si alloy family. Use the designation requested by the buyer and the complete product specification, edition and condition on the order.
Grade 21 is not Ti-15-3
Ti-15V-3Cr-3Sn-3Al is a different beta titanium alloy, associated with TB5. Grade 21 / TB8 uses molybdenum, niobium, aluminum and silicon; the two names must not be mixed on drawings or certificates.
Forming condition and final condition
A sheet may be ordered for forming before final aging. Define both stages, the process responsibility and the final mechanical and dimensional acceptance instead of treating one strength value as the whole requirement.
Grade 21 and Grade 5
The two alloys have different composition and processing routes. For a warm structural or formed-sheet application, review the drawing, thermal duty, joining and approved material requirements before considering a change.
03 / Application review
Grade 21 / TB8 for aerospace forming and thermal duties.
Start with the component and its operating conditions. We review how the material, forming sequence, final condition and required records fit the order.
Application review / 01
Exhaust structures: define the metal-temperature history
Grade 21 / TB8 is relevant to aerospace exhaust and nozzle sheet applications where the material and fabrication route are selected for the thermal duty. A procurement review should distinguish the temperature of the surrounding gas from the temperature experienced by the metal, and identify the loads and service cycles the drawing is designed to withstand. TiHubs coordinates the supply scope around those requirements.
Products to discuss
Sheet and strip blanks, formed shell sections, plug or nozzle components and defined subassemblies. The quotation should identify where material supply ends and fabrication or assembly responsibilities begin.
What we need to review
Metal-temperature profile, exposure duration, thermal cycles, pressure or mechanical loads, drawing revision and material/process specifications. Include joint details, inspection class, first-article evidence and the purchaser approval route.
Application review / 02
Thin-wall parts: agree the sequence from sheet to final shape
A Grade 21 / TB8 shell enquiry needs more than finished dimensions. The starting sheet condition, forming stages and final heat treatment determine what must be controlled during production. Specify the wall and shape requirements at final acceptance, and identify where samples or tooling trials are needed to resolve geometry before a production quantity is committed.
Products to discuss
Sheet blanks, curved panels, flanged shells and heat-shield components to a released drawing. Add joining or finish-machining work only where it is included in the supply boundary.
What we need to review
Thickness and tolerance, rolling direction, radii, draw depth, minimum remaining wall, trim allowance and attachment geometry. Agree aging responsibility, dimensional correction, surface requirements and the method used to approve the finished profile.
Application review / 03
Warm structures: connect material records with the design duty
For a warm airframe or engine-structure requirement, use the actual drawing and service envelope to define the material enquiry. The review should cover the delivered condition and the evidence needed for the part, including areas where joints, fasteners or thermal movement affect the manufacturing scope. Do not treat a room-temperature property table as a component life assessment.
Products to discuss
Sheet, bar, forging blanks and drawing-based structural components where the specified material and process route are suitable. Identify raw-stock supply separately from finished parts.
What we need to review
Operating and design temperatures, exposure time, cyclic loads, interfaces, stiffness-related dimensions and final condition. State inspection, traceability, first-article and customer qualification requirements before requesting a production proposal.
Application review / 04
Fluid-exposed assemblies: separate compatibility from approval
Producer data discuss Beta 21S resistance to aircraft hydraulic fluids. For a Grade 21 / TB8 enquiry involving such exposure, identify the fluid and the actual temperature and contact conditions. That compatibility discussion is separate from qualifying a pressure tube, joint or complete hydraulic assembly. The purchase needs the product and component requirements as well as the material name.
Products to discuss
Reviewed sheet or machined components exposed to specified fluids; tube or pipe only where the required product route and dimensional capability are confirmed.
What we need to review
Fluid designation, exposure temperature and duration, pressure, loads, joints and cleaning chemicals. Include the controlling aerospace or purchaser specification and required evidence for the particular component.
Application review / 05
Welded fabrication: define joint and heat-treatment requirements
When a Grade 21 / TB8 component includes welds, define the joint and the final heat-treatment condition early. The quotation should identify which party supplies the released welding and inspection requirements, what sample or procedure evidence is required, and how dimensional acceptance will be checked after fabrication. Material records should remain linked to each fabricated item.
Products to discuss
Formed sheet sections, ducts, panels and specified welded pipe or subassemblies. ASTM B862 is a welded-pipe route; it does not replace an aircraft-assembly drawing or process specification.
What we need to review
Joint design, parent thickness, welding process and shielding requirements, heat-treatment sequence, surface condition, NDT and dimensional limits. Include procedure approval, hold points and any final assembly testing.
Application review / 06
Lightweight panels: specify the thin-material and joining scope
For a Grade 21 / TB8 honeycomb or lightweight-panel enquiry, define whether the requirement is sheet or strip stock, a formed core element, or an assembled panel. The manufacturing and inspection discussions differ for each scope. Provide the geometry and service requirements so material thickness, joining access and the required document package can be reviewed before quotation.
Products to discuss
Thin sheet or strip, formed panel elements and project-specific fabricated items. Quantities, dimensions and available manufacturing routes are reviewed against the actual drawing.
What we need to review
Gauge and tolerance, cell or panel geometry, attachment details, surface, joining requirements and thermal duty. Agree sample evaluation, dimensional and joint inspection, handling protection and the criteria for production approval.
Application review / 07
Machined components: order the final condition explicitly
Grade 21 / TB8 bar or wire enquiries should identify the required finished condition and the manufacturing sequence. A purchaser comparing offers needs to know whether material is supplied before or after aging, whether machining is included and which inspection records accompany the items. State the part and lot requirements so they can be priced on a consistent basis.
Products to discuss
Bar, rod, wire and forging blanks for released machined-part or fastener drawings. Different stock forms should not be assumed to share the same mechanical test basis.
What we need to review
Section, dimensions and tolerances, threads or critical surfaces, machining allowance and heat-treatment responsibility. Define mechanical-test orientation, NDT where required, marking, samples and delivery milestones.
Application review / 08
Development projects: separate feed material from system performance
Beta 21S producer literature includes foil and titanium-matrix-composite development uses. A TiHubs enquiry in this area should define the material being purchased and the trial objective without assuming that a feedstock specification proves the performance of a composite or assembled system. Start with the planned dimensions, condition and evaluation method, then agree a manageable sample scope.
Products to discuss
Specified thin sheet, strip or other reviewed development material, with dimensions and processing requirements confirmed before quotation. Experimental quantities and repeat production are separate discussions.
What we need to review
Required thickness, surface, condition, joining or consolidation constraints and traceability. Identify the trial acceptance criteria, test specimens, permitted substitutions, reporting requirements and who approves progression to the next stage.
Purchasing checklist
Define the route from stock to finished condition.
For Grade 21 / TB8, the purchase should connect the source material, forming or joining steps and the final acceptance requirements.
Material and scope
Grade, edition, form, gauge or section, delivery condition and the items included in the quotation.
Thermal and processing duty
Metal-temperature history, drawing revision, forming, joining, aging and approval responsibilities.
Inspection and records
Chemical and mechanical test basis, dimensions, weld or NDT scope, traceability and the final document package.
“We need TB8 sheet for an exhaust shell.”
We would clarify the sheet gauge and starting condition, released shell drawing, metal-temperature duty, forming and joining sequence, final aging responsibility and the dimensional or weld evidence required for acceptance.
Illustrative requirement review; it is not a claim of an approved aircraft part or a published customer project.
Discuss your requirement04 / Standards & documentation
Match the standard
to the product.
Select the specification for the material form and condition being purchased. The website PDFs retain their actual editions; additional aerospace requirements follow the purchaser’s drawing and approved revision.
| Product form | ASTM / AMS / ASME route | Chinese standard route | Clarify before quotation |
|---|---|---|---|
| Material identity & chemistry | United States / technical reference Grade 21 · UNS R58210 · Ti-Mo-Al-Nb-Si; use the ordered product standard for chemistry and acceptance. | ChinaGB/T 3620.1-2016View PDF ↗ TB8 designation and chemical composition. | Full grade, alloy identity, product form, condition and analysis basis. |
| Sheet, strip & plate | United States / technical referenceASTM B265-08View PDF ↗ Grade 21 ST reference; AMS 4897 is a separate sheet-and-strip option within its specified thickness scope. | ChinaGB/T 3621-2022View PDF ↗ TB8 ST sheet; apply the thickness-specific requirements. | Gauge, surface, rolling direction, forming sequence, final condition and tests. |
| Bar & rod | United States / technical referenceASTM B348-08aView PDF ↗ Select the applicable solution-treated or aged strength level. | ChinaGB/T 3620.1-2016View PDF ↗ TB8 chemistry plus an agreed bar product specification. | Section, machining allowance, straightness, final aging and sampling. |
| Seamless & welded pipe | United States / technical referenceASTM B861-10View PDF ↗ASTM B862-06b ε1View PDF ↗ Separate pipe routes with specified condition, manufacturing and test requirements. | ChinaGB/T 3620.1-2016View PDF ↗ Agree the TB8 tubular product specification and acceptance basis. | OD, wall, length, end condition, downstream processing and NDT. |
| Wire | United States / technical referenceASTM B863-19View PDF ↗ Grade 21 wire; identify any additional component or consumable requirement. | ChinaGB/T 3620.1-2016View PDF ↗ TB8 material identity with agreed wire product requirements. | Diameter, surface, coil or straight lengths, condition and traceability. |
| Forgings & drawing-based parts | United States / technical referenceASTM B381-08aView PDF ↗ F-21 forging reference; finished-component requirements remain drawing-specific. | ChinaGB/T 3620.1-2016View PDF ↗ TB8 identity plus the agreed blank or finished-part requirements. | Blank drawing, final condition, structure, machining and inspection scope. |
| Technical reference | United States / technical referenceTIMETAL 21S · producer technical dataView PDF ↗ Original producer information for the Beta 21S family; typical data are not universal acceptance values. | China Use the ordered TB8 standards and project documents for acceptance. | Review the assumptions relevant to the actual process and thermal duty. |
AMS 4897 catalog information is linked below as an additional aerospace reference. A catalog link is not a free full standard, and a raw-material specification does not establish finished-assembly approval.
Use the document edition, product scope and condition specified in the purchase order. Producer technical references support discussion; they do not replace ordered product acceptance requirements.
05 / Order coordination
Know the scope
before ordering.
Our founder’s 20 years in titanium inform the questions we ask before quotation and the supply options we review with you.

A quotation you can evaluate
Agree the grade, standard edition, dimensions, tolerance, condition and quantity before comparing prices.
- Identify whether inspection, samples and tooling are included.
- Confirm packaging, transport and delivery terms.
- Record items that still need technical confirmation.
Acceptance agreed before supply
Confirm the material certificate, full grade, heat or lot identity, delivery condition, dimensional checks and required testing before supply starts. Define any process records, NDT and purchaser approval points for the ordered product.
Independent inspection can be discussed with its scope, timing, acceptance criteria and cost agreed for the order.
Delivery with clear milestones
Review the proposed lead time, approvals, production sequence and dispatch requirements. For several product forms, coordinate document and packing readiness together.
Material substitutions and technical changes require written approval. A schedule deviation should identify the impact, decisions needed and next steps.
One contact when an issue arises
Contact TiHubs with the order reference, affected items and supporting photos or inspection records.
We record the issue, review it against the agreed requirements and coordinate the next steps with the relevant manufacturing parties.
Material records
Grade, standard, test results and heat or batch identity matched to the supplied items.
Inspection records
Dimensional and testing records for the agreed scope, including critical drawing requirements.
Dispatch records
Item identification, packing list, protective packaging and required shipment documents.
06 / Questions before sourcing
Before you specify
Grade 21 / TB8.
A clear material designation is the beginning. Product form, specification revision, material condition and acceptance complete the requirement.
A useful first enquiry
- Product and specificationProduct form, standard edition, dimensions and material condition.
- Order and deliveryQuantity, destination and any required delivery date.
- Acceptance requirementsDrawing revision, inspection, certificates and packaging.
Not every detail is finalized? Send the information you have. We can help identify the questions to resolve before quotation.
What happens next: requirement review, technical clarification, then a supply proposal and quotation.
What is Grade 21 titanium, and what does Gr21 mean?
Grade 21, abbreviated Gr21, is the Ti-15Mo-3Al-2.7Nb-0.25Si beta titanium alloy identified as UNS R58210. It is associated with the Beta 21S alloy family and the Chinese designation TB8. Include the product specification, edition and delivery condition with the grade when ordering.
Where is Grade 21 / TB8 mainly considered?
Its main focus here is aerospace exhaust and nozzle components, formed thin-wall parts and warm structural applications. Sheet and strip are particularly relevant to these purchasing discussions. The drawing, thermal duty, processing route and required approval determine whether a particular product is suitable.
Is Grade 21 the same as Ti-15-3 titanium?
No. Ti-15-3 means Ti-15V-3Cr-3Sn-3Al, a different beta alloy associated with TB5. Grade 21 / TB8 is the molybdenum-niobium-aluminum-silicon alloy family. Keep the full composition or UNS reference with the grade to avoid mixing these materials in a quotation or purchase order.
Which specification should I use for sheet or strip?
ASTM B265 includes Grade 21 sheet, strip and plate. GB/T 3621-2022 includes TB8 sheet under its listed condition and dimensional requirements. AMS 4897 is an aerospace sheet-and-strip option; the current official scope is limited to 3.18 mm and below. Use the exact revision required by the drawing and do not apply it automatically to thick plate.
Should the sheet be supplied before or after aging?
Specify the condition required for the next manufacturing step and the condition required at final acceptance. Forming, joining, trimming and aging responsibilities need to be agreed together. A quotation should identify whether TiHubs supplies starting stock, coordinates processing, or delivers a part with final-condition test records.
Can you supply Grade 21 / TB8 bar, pipe and wire?
These forms can be reviewed against the required size, quantity, condition and inspection scope. ASTM B348, B861 and B863 include Grade 21 bar, seamless pipe and wire respectively. For the TB8 route, agree the product specification explicitly; the supplied GB/T 2965-2023 and GB/T 3623-2022 files do not list TB8.
What temperature can Grade 21 / TB8 operate at?
There is no single temperature rating for every Grade 21 product or component. Suitability depends on metal temperature, exposure time, load, thermal cycling, oxidation allowance, joints and the final material condition. Send the service profile and the applicable design or purchaser requirements so the material and processing basis can be reviewed.
Can you provide aerospace qualification or inspection documents?
State the required material specification, approved-source or special-process requirements, traceability, testing and first-article documents with the enquiry. TiHubs reviews which supply resources and records are appropriate to that scope. A grade page or material certificate alone does not establish flight approval or compliance with every aerospace requirement.
How do I start an enquiry, and what about MOQ and lead time?
Send the form or drawing, Grade 21 or TB8 designation, standard edition, dimensions, required condition, quantity and destination. Add thermal duty and inspection requirements where relevant. MOQ, samples, inspection costs and delivery milestones are confirmed with the supply proposal. TiHubs remains your contact for follow-up and any order issue.
07 / Your next step
Start with the
requirement you have.
Send the product details, drawing or operating conditions you already know. We will identify missing information and discuss a suitable supply route before quotation.
- Requirement review
- Technical clarification
- Supply proposal and quotation
Combine materials and parts in one enquiry.
Send one list of Grade 21 / TB8 forms, sizes and quantities. Include drawing revisions and items that need to be supplied together.
Define the condition and acceptance priorities.
Include the ordered specification, final application, material condition, inspection and documentation, destination and required delivery milestones.
Baoji, China · info@tihubs.com
Start your Grade 21 / TB8 enquiry
Send your material form, drawing or process conditions. We will help clarify the remaining requirements.