CategoryManufacturing & Customization
Titanium grinding,
what must be measured?
Circle the surface that locates, slides or seals. Give that surface its own dimension, geometric requirement and texture callout before asking a grinder for a price.

Quick answer
On a round bar, a 0.20 mm reduction in diameter is 0.10 mm per side for ideal concentric removal. On a plate, specify how much may be removed from each face. Diameter, flatness, runout and surface texture require their own inspection evidence.
01 / Specify the surface that performs the work
Specify the surface that performs the work
A purchasing note that says “grind titanium to a smooth finish” leaves the supplier to guess what the surface must do. A shaft seat may need to locate a bearing at a controlled diameter. A sliding strip may need a profile texture measured in a particular direction. A plate may need two faces that establish a repeatable working height. A decorative face may simply need a consistent visible pattern. These requirements can coexist, but the evidence needed to accept each is different. Begin with a marked drawing showing the working surface and its relationship to the rest of the component. Then decide which limits belong to size, geometric form, texture and visible defects.
Identify the article being delivered. Ground stock can mean a full-length bar with a controlled outside surface, a short blank finished on two faces or a nearly completed component with selected surfaces ground after machining. In the first case the buyer may remove part of the surface in later operations. In the second, the finished face may become the primary workshop datum. In the third, existing shoulders, holes or bores may already control where a new surface must lie. Give the supplier the actual sequence and identify which parts it will receive and return. An offer to grind loose stock and an offer to finish a customer-owned component expose the bidders to different work and responsibilities.
Ask why grinding appears on the drawing. It may be the required manufacturing route, a shorthand inherited from an earlier supplier or simply a way to meet an inspection requirement. If the customer requires a particular route, state it explicitly and request the associated records. If the requirement is functional and the route can vary, invite an alternative on a separate quote line for design approval. A polished part may look brighter than a ground one but still fail a dimensional or texture requirement. Conversely, an acceptable ground locating seat need not resemble a mirror. A drawing should indicate the required outcome even when the process is also prescribed.
Define the material supplied to the grinder. Identify grade, product form, condition, starting dimensions and traceability. Record which faces are already finished, how the component may be held and what identifying marks must remain. A subcontractor needs to know whether it can use an end as a handling extension or whether that end is already a finished datum. A simple shaded region indicating where contact and processing are permitted can avoid an otherwise expensive misunderstanding. For a repeat item retain the drawing and accepted reference evidence in addition to any photographs. A photograph can communicate appearance but cannot preserve a tolerance or a measurement setup on its own.
02 / Calculate stock removal and residual allowance
Calculate stock removal and residual allowance
Keep diametral removal separate from radial removal. For a round bar reduced concentrically from 20.20 to 20.00 millimetres outside diameter, the change in diameter is 0.20 millimetre. Material removed at each side is 0.10 millimetre in the ideal geometry. A drawing note calling for “0.20 grind allowance” without stating whether it is on diameter or per side leaves two possible finished sizes. Write the starting and finished limits and name the convention. If a surface must remain in a particular relationship to a bore or existing journal, include that datum. The simple half-difference applies to concentric geometry and cannot establish how much is removed around an eccentric incoming blank.
For a flat plate taken from 8.40 to 8.00 millimetres, total thickness reduction is 0.40 millimetre. Removing 0.20 millimetre from each face is only one possible allocation. A process intended to preserve an existing datum might remove most or all of the material from the opposite face. Specify which face is retained, which face is worked and the permitted condition of the finished edges. A part that meets total thickness after removal from the wrong side can still mislocate a shoulder or an existing cross-hole. Locate holes and steps relative to the face that will actually be present after finishing.
Review the incoming minimum size as well as the nominal stock size. Suppose an order requires a cleanup cut around the entire outside of a long bar. A nominal stock diameter alone cannot confirm that enough metal is present at every position once incoming bow, taper or local marks are considered. Ask what incoming inspection the supplier requires and how it will report unsuitable blanks before working them. Put the disposition of customer material in the purchase order. It may be appropriate to return a short blank, hold it for a revised dimension or reject it, but the person authorised to decide should be known before the original surface disappears.
For an illustrative fit, take a stationary bore from 20.03 to 20.05 millimetres and a finished bar from 19.99 to 20.00 millimetres. The diametral clearance ranges from 0.03 to 0.06 millimetre when the input limits are paired in the adverse directions. This arithmetic uses assumed dimensions and does not prescribe a fit for a bearing or sliding application. It shows how a procurement team can check that both parties are using the same limits. A dimensional clearance calculation does not account for every geometric error, alignment condition or thermal effect in the assembled machine. Those characteristics need their own review where they affect service.
| Illustrative drawing or reference | Input | Interpretation |
|---|---|---|
| Ideal round bar | From 20.20 mm OD to 20.00 mm OD concentrically | 0.20 mm diametral removal, 0.10 mm per side |
| Ideal plate | From 8.40 mm to 8.00 mm thick | 0.40 mm total, or 0.20 mm per face only if divided equally |
| Illustrative shaft/ring fit | Ring bore 20.03–20.05 mm, bar OD 19.99–20.00 mm | Diametral clearance 0.03–0.06 mm. No general fit recommendation is implied. |
| Profile texture | ISO 21920-2 covers terms, definitions and parameters | Identify the parameter, unit, evaluation conditions and drawing edition |
| Surface integrity | TIMET discusses heat effects and abrasive contamination in titanium finishing | Agree what evidence the finished application requires |

The concentric outlines are separated for clarity. The radial allowance is half the change in diameter.
03 / Separate profile texture, size and geometric form
Separate profile texture, size and geometric form
Surface texture describes relatively small features of the measured surface profile under defined evaluation conditions. Size describes a dimensional characteristic such as diameter or thickness. Form describes geometry such as flatness, straightness or roundness. A bar can have acceptable local diameter measurements and still be bowed along its length. A plate can have a smooth local texture while its surface departs from a plane. Do not use a single finish adjective to stand for all three. Enter each characteristic on the purchase drawing with an appropriate tolerance, measurement zone and supporting reference where required.
ISO 21920-2 defines terms and parameters for profile surface texture. Specify the parameter that the drawing actually requires, its unit and the agreed evaluation conditions. Ra is an average roughness parameter. Two profiles can yield similar averages while one contains an isolated defect of importance to the user. Where a scratch, pit or local mark matters, give it an independent inspection requirement and define how much of the surface is covered. A report from a short profile trace provides valuable evidence about its path, but cannot prove that no defect exists elsewhere on an entire component.
Texture direction also matters. A profile taken along visible grinding marks can differ from one taken across them. Identify the direction relative to the working motion or a drawing datum and identify the zone in which the measurement can be taken. If the part is too narrow or curved for a proposed measuring setup, discuss a suitable method or a representative witness area before manufacture. One supplier may quote a value measured on a flat coupon while another proposes a direct measurement on the component. Those approaches must be assessed for how well they represent the controlled surface and its actual production history.
A legacy drawing may specify an older standard, a parameter convention or an inspection practice established with an earlier supplier. Keep that context intact. An updated instrument menu or a current standards family does not automatically change the acceptance basis of a controlled drawing. Ask the responsible engineer to approve any change of reference and describe how old and new records can be compared. The manufacturer guides cited below help explain terms and instruments. The contractual definition must be the one agreed for the component. This is particularly important when old reports recorded only a number with no unit, parameter or measurement direction.

A specified final thickness does not determine how removal is divided between the two faces.
04 / Choose how a ground part will be measured
Choose how a ground part will be measured
Plan the dimensional checks around the surfaces used in service. For a bar, identify the axial stations where diameter is measured and the orientations required at each station. Several readings along the same line can reveal a size change along the length. Readings in different directions at one station provide different information. A two-point diameter measurement is not a complete roundness evaluation. Ask for the method appropriate to the specified geometric characteristic. State whether end zones affected by handling or a subsequent cut are included in the finished length. A drawing that excludes those zones should identify how much usable length remains.
For a plate, define the support condition and the surfaces used to assess thickness, flatness or parallelism. A thin piece on an uneven bench can adopt the shape of its support. A part clamped flat for measurement can spring to a different shape when released. If the drawing controls a free or installed condition, identify it. Thickness at several points describes separation between the faces at those locations. It does not by itself establish that one face is flat or that the faces are parallel to a specified datum. Record the measurement pattern so two inspectors can compare results at equivalent positions.
For runout, name the reference axis and the feature being indicated. A shaft rotated on its functional centres and the same shaft supported on an unqualified external surface may produce different readings. Identify whether the requirement applies to a particular circular section or to the surface over a stated length. A dial indicator can be a useful part of an agreed check, but a photograph of an indicator touching the work does not define the setup. Record how the component is located and which reading is reported. This makes a result reproducible when the buyer repeats the check after transport.
Build a first-article report with a drawing reference for each controlled feature. Add the method, measuring location, support, units, actual reported result and agreed limits. If an instrument produces a trace, link it to the part and measurement position. A single average from several measurements can hide one outlying location when the drawing requires each location to comply. Clarify whether sampling applies to the number of parts, the number of traces per part or both. If the remaining stock is to be cut into short pieces later, distribute measurement positions to represent the delivered useful length. A near-end reading may be easy to take and still poorly represent the middle of the purchased bar.
A practical disagreement can arise when two reports both say the surface passed but list different units. One micrometre is one thousandth of a millimetre. A drawing entry in micrometres and a report in millimetres should be converted explicitly before comparison. Keep the original value in the report and add a separate converted value for the purchasing review. A decimal shifted without its unit can turn a reasonable texture result into an apparently impossible dimensional tolerance. Apply the same care when an older drawing uses microinches and the instrument exports metric data. A unit conversion changes the expression of a value without changing its parameter, filtering or direction of measurement.
For a disputed batch, ask both inspectors to measure an identified part at a marked position in the agreed orientation, using the required support and evaluation settings. Compare their records before extending the conclusion to the rest of the lot. If the disagreement disappears, identify which condition had differed. If it remains, the responsible metrology team can consider uncertainty, instrument suitability and the agreed decision rule. This is more informative than selecting the more favourable number or averaging unlike results. Where the surface will be consumed in later work, preserve a representative item or its trace long enough to complete the review. Record whether an agreed deviation applies only to the affected lot or changes the drawing for later releases.

The inspection drawing should identify both the measurement zone and the direction relative to the surface lay.
05 / Control surface integrity and downstream operations
Control surface integrity and downstream operations
Discuss surface integrity separately from roughness. TIMET’s fabrication guidance draws attention to contamination and heat effects in abrasive finishing of titanium. For purchasing, the practical question is which surface condition the downstream operation requires and what evidence is appropriate. A bright appearance or a satisfactory profile value alone cannot establish a surface’s chemical cleanliness or subsurface condition. Tell the supplier if the part will be joined, coated, inspected or used as a controlled contact face. The specialist can then propose a defined finishing and cleaning boundary for the buyer’s engineering review.
Do not assign a universal removal depth to every incoming titanium product. The starting process matters. A mill-finished bar, a thermally affected cut edge and a forging with a separate surface-removal requirement do not necessarily have the same condition at the same depth. Identify the incoming history that is known and distinguish it from an assumption. If removal of an affected layer is a drawing requirement, state the evidence or inspection method that establishes completion for the particular product. A nominal reduction in diameter can remove a specified amount of metal while leaving the question about the initial surface condition unresolved.
Preserve protected features during outsourced finishing. Mark threads, edges, identification areas, bores and surfaces that are already accepted. A general instruction to break all edges may conflict with a specific locating corner, a seal interface or an adjacent small feature. Identify the permitted edge treatment on the drawing and any area where a protective covering may be applied. If the material undergoes marking again after grinding, specify the permitted marking zone and retention of lot identity. A readable mark on the original surface offers little traceability if it vanishes during processing and is never transferred under control.
Check the state in which the part moves to its next operation. A ground plate may be wrapped with a protective film suitable for transport but unsuitable for a subsequent cleaning or bonding step. A bar may require separators to protect its controlled surface in transit. Define who removes temporary protection and who performs final cleaning where cleanliness is critical. Ask how the supplier separates evidence for material identity, dimensional conformity, profile texture and surface integrity. This lets the buyer select the checks it actually needs and avoids interpreting a routine appearance inspection as evidence for an unrelated chemical or metallurgical requirement.
Read the related technical guide for the companion product or property.
06 / Compare quotations and receive the finished stock
Compare quotations and receive the finished stock
Compare quotes from the incoming condition to the accepted output. Include the material owner, stock dimensions, quantity, areas to grind, finished limits, inspection coverage, protection and responsibility for nonconforming input. A price for grinding the outer surface of a full stock bar may exclude cutting, end finishing and individual part marking. A price for completed short blanks may include all three. Calculate the price per accepted usable part as well as the price per length. If the buyer supplies expensive blanks, include the agreed procedure for first-piece approval and handling of parts that cannot clean up within the permitted limits.
Consider a plate with one finished reference face and a pattern of holes located from that face. The supplier receives stock above final thickness and proposes equal removal from both faces. That would achieve the thickness target yet move the reference face relative to the holes. A drawing showing the preserved face resolves the ambiguity before a part is scrapped. For a separate bar order the reverse problem can arise. A request to preserve one side of the starting material may be incompatible with a finished diameter concentric to an existing bore. The technical owner must choose which datum and stock disposition the finished part will satisfy.
At receipt, protect the finished surface while matching the material and process records. Record the part or lot identity, verify the drawing revision and confirm the measuring condition before treating a difference as a failure. Measurements taken through protective film, over a burr or on a different support may answer a different question. Repeat the agreed setup if necessary and preserve the original readings for review. If both parties agree that a result exceeds the contract limit, document the feature and location and obtain disposition before a further operation removes the evidence. A polished repair can make the history of the original discrepancy impossible to reconstruct.
Close the purchase with a repeatable description of the next order. Retain the drawing, approved input condition, stock allocation, inspection setup and examples of accepted surface appearance where relevant. If the next release calls for a different grade or starting form, reopen the questions affected by that change instead of copying an old allowance by habit. When asking TiHubs for a quote, attach the marked drawing and identify the functional surface in a single sentence. Include the quantity, stock source, applicable standards and reports expected at delivery. The result is an enquiry that different suppliers can price on the same basis and that receiving can verify using the requirements actually agreed.
For example, a 6,000 mm bar with 20 mm reserved for holding at each end has 5,960 mm in the controlled zone. If each 300 mm piece uses a 3 mm cut allowance, each consumes 303 mm. Nineteen pieces use 5,757 mm and leave 203 mm. Twenty would require 6,060 mm under the same convention. These assumed allowances are planning examples. Ask whether the grinder supplies the entire bar with holding zones identified or trims them off. If a newly cut end serves as an installation datum, identify who verifies or finishes that face after cutting.
07 / Build your RFQ
Request a technical quotation
Circle the surface that locates, slides or seals. Give that surface its own dimension, geometric requirement and texture callout before asking a grinder for a price.
Information to include
- Incoming and finished dimensions
- Allowance per face or per side
- Geometric datum and support
- Profile parameter and measurement direction
- Material and inspection traceability
Build your RFQ checklist
Choose the product and add the information you have. Copy the resulting brief or send your requirements to TiHubs. Submitting an enquiry does not place an order.
08 / FAQs
Questions buyers ask
Does a ground finish establish straightness?
Specify and inspect straightness for the relevant feature independently. A smooth local trace or an acceptable diameter does not establish the shape over the full supported length.
Does Ra identify every scratch?
Ra is an average profile parameter. If an isolated scratch, pit or surface defect matters, give it an appropriate independent acceptance criterion and inspection coverage.
Which face keeps its original location?
Show the datum and allocation of stock on the drawing. A total thickness reduction alone does not identify whether one face stays intact or both are processed.
09 / Key takeaways
Keep the purchase requirements connected.
- Incoming and finished dimensions
- Allowance per face or per side
- Geometric datum and support
- Profile parameter and measurement direction
- Material and inspection traceability
Technical references
Sources and data scope
References reviewed November 20, 2026. Public source summaries support the discussion; the controlled specification, agreed edition and approved project requirements govern acceptance.
- TIMET — Fabricating Titanium — Manufacturer context for grinding, contamination and surface condition.
- ISO 21920-2 — Surface texture, profile parameters — Official scope of the profile surface-texture parameters. Specify the drawing’s applicable edition and evaluation conditions.
- Mitutoyo — Quick Guide to Surface Roughness Measurement — Instrument manufacturer’s explanation of profile measurement and roughness parameters.