Grade 11 / TA9-1 titanium-palladium sheet, bars and heat-exchanger tube products on a dark metallic background

Grade 11 · Gr11 · TA9-1 · UNS R52250

Grade 11 / TA9-1 titanium.For corrosion & forming demands.

Source titanium-palladium sheet, bar, tube and drawing-based parts for chemical equipment. We review Gr11 / TA9-1 requirements for heat exchangers, condensers, evaporators and formed components through one technical and commercial contact in Baoji.

Start with a specification, drawing or application. We’ll help identify the details still needed.

Material review. Supply coordination.
One contact in Baoji, China.

Grade 11 / Gr11 / TA9-1Ti-Pd · UNS R52250 · Low-interstitial material route
Corrosion + formabilityMatch the material to the media, geometry and duty
One contact20 years of founder experience · 100+ Baoji factories

01 / Product forms

Find your
Grade 11 / TA9-1 product.

Choose a material form or application. Send the dimensions, service conditions and required records so we can match the manufacturing route to your order.

Grade 11 / TA9-1 titanium sheet & plate with specification reference markings

01 / 06

Grade 11 · Gr11 · TA9-1 · Ti-Pd

Grade 11 / TA9-1 titanium sheet & plate

For corrosion-resistant linings, formed shells and selected heat-transfer plates. Share the finished geometry and operating conditions alongside the starting sheet size.

Specification
ASTM B265 Grade 11 or GB/T 3621 TA9-1 with the ordered edition. State the required route and whether dual certification is needed.
Dimensions
Thickness × width × length, thickness tolerance, flatness, surface and rolling direction. Include cut blanks or finished contours.
Forming
Drawing depth, bend radii, tooling, thinning limits and the required condition. A material elongation value does not guarantee a specific formed shape.
Acceptance
Heat identity, material records, dimensional and surface checks; formed-part inspection agreed separately.
Grade 11 / TA9-1 titanium bar & rod with specification reference markings

02 / 06

Grade 11 · Gr11 · TA9-1 · Ti-Pd

Grade 11 / TA9-1 titanium bar & rod

Starting stock for machined sleeves, stems, connectors and other specified wetted parts. Define the corrosion environment and the finished component requirements together.

Specification
ASTM B348 Grade 11. For TA9-1, use GB/T 3620.1 chemistry with an explicitly agreed bar specification and acceptance scope.
Dimensions
Diameter or section × length, straightness, surface condition, machining allowance and quantity per size.
Condition
Agreed delivery condition and surface; clarify turned, ground or other finish requirements before quotation.
Acceptance
Chemistry including palladium, mechanical requirements, heat or lot identity and any agreed ultrasonic inspection. Do not assume TA9 bar requirements cover TA9-1.
Grade 11 / TA9-1 heat-exchanger & condenser tubes with specification reference markings

03 / 06

Grade 11 · Gr11 · TA9-1 · Ti-Pd

Grade 11 / TA9-1 heat-exchanger & condenser tubes

Discuss straight tubes, U-bends and condenser tubes against the equipment duty. Tube specifications and process-pipe specifications serve different purchasing scopes.

Specification
ASTM B338 Grade 11 or GB/T 3625 TA9-1 for condenser and heat-exchanger tubes. Identify seamless or welded construction.
Dimensions
Outside diameter × wall × length, wall tolerance, straightness and end condition. For U-tubes, include bend radius and leg spacing.
Equipment interface
Tube-to-tubesheet connection, expansion or welding requirements, bundle layout and cleaning access.
Acceptance
Applicable hydrostatic or nondestructive electrical testing, process tests, dimensional records and agreed post-bending inspection.
Application illustration: Titanium coils & formed heat-exchanger plates with specification reference markings

04 / 06

Grade 11 · Gr11 · TA9-1 · Ti-Pd

Titanium coils & formed heat-exchanger plates

Application illustration: Gr11 / TA9-1 coils, bent condenser tubes and formed heat-transfer plates. Material selection and forming feasibility are reviewed for the actual service.

Material route
Tube to the specified heat-exchanger or seamless-tube standard; sheet to ASTM B265 Grade 11 or GB/T 3621 TA9-1.
Coil details
OD, wall, coil diameter, pitch, turns, developed length, connections and support points. Agree ovality and thinning limits.
Plate details
OEM drawing, plate pattern, ports, gasket interface, pressing depth and minimum remaining thickness. Confirm tooling availability.
Acceptance
Post-forming dimensions, surface condition and the agreed integrity test. Raw-material certification alone does not certify a finished coil or plate pack.
Application illustration: Heat exchangers, condensers & evaporation equipment with specification reference markings

05 / 06

Grade 11 · Gr11 · TA9-1 · Ti-Pd

Heat exchangers, condensers & evaporation equipment

Application illustration: material and fabrication coordination for defined titanium wetted parts or an agreed equipment scope. Confirm the design basis before committing to construction.

Service conditions
Both-side media, concentrations, impurities, pH, operating and design temperatures, pressures and cleaning conditions.
Supply boundary
Tube bundle, plates, coil, lining, selected internals or an assembly. Identify which wetted parts must be Grade 11 / TA9-1.
Manufacturing
Equipment drawings, joint design, tubesheet and gasket interfaces, welding requirements and inspection hold points.
Acceptance
Applicable design code, fabrication qualifications, pressure or leak tests and document package. A material specification is not an equipment certification.
Application illustration: Pump, valve & sealing connection components with specification reference markings

06 / 06

Grade 11 · Gr11 · TA9-1 · Ti-Pd

Pump, valve & sealing connection components

Application illustration: machined parts, ring blanks and connecting components for an agreed corrosive duty. Assess loading, wear and sealing as well as material corrosion resistance.

Starting material
ASTM B348 Grade 11 bar, ASTM B381 F-11 forgings or the explicitly agreed Chinese route. GB/T 25137 uses F-11.
Drawing
Revision, wetted surfaces, threads, sealing faces, concentricity, surface finish and machining allowance.
Duty
Pressure, temperature, fluid chemistry, solids, velocity, cavitation risk and contact with dissimilar materials.
Acceptance
Material traceability, critical dimensions and required surface or NDT checks. Finished valve or pump performance testing needs its own agreed scope.

Images illustrate material forms and application possibilities. Reference markings identify specification options; they do not establish dual certification, stock availability or approval of finished equipment.

Define the shape. Share the service.

These details help turn a material enquiry into a comparable quotation.

01 / Drawing review

Formed shells & linings

Send the finished shape, blank size, radii, minimum wall and surface requirements. Identify welds, bonded interfaces and the areas exposed to the process fluid.

Discuss your drawing

02 / Drawing review

Coils, U-bends & plate packs

Include tube or plate drawings, connection details, tooling requirements and post-forming acceptance. State whether the scope is a part, replacement set or assembly.

Discuss your drawing

03 / Drawing review

Machined & forged components

Provide rough and finished drawings, critical sealing features and material callout. Specify the required material records and any component-level testing.

Discuss your drawing

02 / Material identity

What is
Grade 11 / TA9-1 titanium?

Grade 11 titanium, also written Gr11, is a low-interstitial titanium-palladium alloy identified as UNS R52250. It contains 0.12–0.25% palladium. TA9-1 is the Chinese designation for the corresponding low-interstitial Ti-Pd chemistry route. It is considered where corrosion resistance and demanding forming operations must be addressed together.

Order Grade 11 and TA9-1 against their stated product specifications. Similar designation chemistry does not replace a review of dimensions, condition, mechanical properties, testing and traceability, or establish automatic dual certification.

240MPa

Minimum tensile strength
ASTM B265-08 · Grade 11

138MPa

Minimum 0.2% offset yield strength
ASTM B265-08 · Grade 11

24%

Minimum elongation · 50 mm gauge
ASTM B265-08 · Grade 11

Property or condition Reference Ordering implication
Reference scope ASTM B265-08, Table 1 Sheet/plate reference, subject to the table footnotes and ordered condition. For non-annealed material or plate over 25 mm, agree the applicable tensile requirements.
Yield strength range 138–310 MPa · ASTM B265-08 Do not treat the minimum value as an allowable stress for equipment design.
Chinese sheet route GB/T 3621-2022 · TA9-1 · M condition · 0.3–25 mm Listed tensile minimum 240 MPa, 0.2% proof strength 140–310 MPa and elongation minimum 24%. Keep the Chinese acceptance basis explicit.
Forming requirement Finished geometry and process Review draw depth, radii, thinning, springback and surface damage. Tensile elongation alone does not define forming feasibility.
Pressure-equipment requirement Design code and actual wall Select thickness and test requirements using the approved equipment design. Do not transfer raw-material values directly to finished-part ratings.

Source: the supplied ASTM B265-08 and GB/T 3621-2022 files. Values above are product-standard references, not universal values for every Gr11 / TA9-1 product or equipment design allowables.

ASTM B265-08View PDF ↗GB/T 3621-2022View PDF ↗

Selected element · wt % ASTM B265-08 · Grade 11 GB/T 3620.1-2016 · TA9-1
Palladium · Pd 0.12–0.25 0.12–0.25
Oxygen · O 0.18 max. 0.18 max.
Iron · Fe 0.20 max. 0.20 max.
Nitrogen · N 0.03 max. 0.03 max.
Carbon · C 0.08 max. 0.08 max.
Hydrogen · H 0.015 max. 0.015 max.
Titanium · Ti Balance Balance

Selected elements only. Review residual elements, analysis tolerances, sampling and all requirements in the specified product standard. Matching principal chemical limits do not by themselves establish matching delivery or inspection requirements.

ASTM B265-08View PDF ↗GB/T 3620.1-2016View PDF ↗

Grade 11 / Gr11 and TA9-1

Both identify a low-interstitial titanium-palladium route. Specify the exact product standard, edition, condition and test basis in the order; confirm any substitution or dual certification with supporting records.

Grade 11 and Grade 7 / TA9

Both contain palladium. Grade 11 has lower oxygen and iron limits and lower specified strength in the cited sheet standard. It offers a more formable option; Grade 7 / TA9 is a different order designation.

Grade 11 and Grade 1

Grade 11 adds palladium to a low-interstitial titanium base. Palladium can improve performance in certain reducing and crevice-corrosion conditions. Actual compatibility still depends on the full service environment.

Why pay for a palladium grade?

Review the corrosion duty and forming requirement together. Specify Grade 11 where its combination is justified by selection evidence; the grade name alone does not establish a life-cycle benefit for every installation.

03 / Corrosion & forming applications

Grade 11 / TA9-1
in chemical equipment.

Match the material to the medium, geometry and fabrication route. These application reviews show what to define before pricing a Gr11 / TA9-1 requirement.

Application review / 01

Chemical equipment: start with the actual corrosion duty

Grade 11 / TA9-1 is considered for chemical-process equipment when the corrosion requirement also calls for a readily formable titanium-palladium material. The material review must cover the fluid at the metal surface, including stagnant regions and crevices, rather than only the nominal process-stream name. A storage vessel, heated lining and flowing pipe can expose the same alloy to different conditions.

Products to discuss

Sheet for formed shells and linings; tubes, bar and drawing-based wetted parts. Define which surfaces must be titanium and the scope of any assembly.

What we need to review

Full media composition and concentration, impurities, pH, temperature, pressure, aeration, flow, crevice geometry and cleaning chemicals. Include startup, shutdown and upset conditions, plus any service history or corrosion-test requirement.

Send your application details

Application review / 02

Deep-drawn shells, covers & corrosion-resistant linings

Formability is a central reason to evaluate Gr11 rather than choosing a palladium grade on chemistry alone. Deep drawing, flanging and pressed contours need a coordinated review of sheet condition, geometry and tooling. A quotation for flat sheet should be kept distinct from a quotation for a formed part with a specified minimum remaining wall.

Products to discuss

Annealed sheet, cut blanks, formed shells and drawing-based liners; prototype or trial pieces where the production geometry needs confirmation.

What we need to review

Finished and developed drawings, rolling direction, draw depth, radii, thinning limits, springback, tooling ownership and batch size. Agree surface finish, trim allowance, weld interfaces and inspection after forming; identify any required trial approval before production.

Send your application details

Application review / 03

Heat-exchanger tubes, bundles & selected plate systems

A Grade 11 / TA9-1 heat-exchanger enquiry needs both the process-side and utility-side conditions. Confirm which side contacts titanium, the tube-wall or plate conditions, and whether deposits or cleaning can change the exposure. Tube bundles and plate systems have different manufacturing and acceptance requirements even when the same alloy family is specified.

Products to discuss

Straight and U-bent heat-transfer tubes, replacement bundles, coils or selected formed plates. State whether the purchase covers material, fabricated internals or a defined assembly.

What we need to review

Tube OD, wall and length; plate pattern and ports; tube-to-tubesheet expansion or welding; gasket compatibility and cleaning method. Provide pressure and temperature limits, both-side fluids and required integrity tests. Confirm the equipment design and fabrication code separately from the tube or sheet standard.

Send your application details

Application review / 04

Condenser tubes & bent condensation circuits

Condensation duty can involve different exposures in the vapor space, newly formed condensate and cooling circuit. Send the expected composition on each side, including contaminants and non-condensable gases. For a replacement tube order, the original drawing and failure history help distinguish a dimensional replacement from a material-selection change.

Products to discuss

Straight condenser tubes, U-bends, coils and replacement tube sets; new bundle or component work subject to drawing and scope review.

What we need to review

Required tube construction, wall basis, leg length, bend radius, end preparation and tube-to-tubesheet connection. Define inlet velocity, cleaning access, condensate chemistry, thermal cycling and the applicable leak or integrity test. Agree how heat identity will be maintained after bending and cutting.

Send your application details

Application review / 05

Evaporators: review the conditions as concentration changes

Evaporation and concentration equipment should be reviewed across the operating cycle. Feed composition alone is insufficient: dissolved species may concentrate, deposits may form and cleaning may introduce a different environment. The material at a heated surface can face conditions that differ from the bulk liquid. Grade 11 / TA9-1 selection must therefore use the defined process envelope.

Products to discuss

Heating tubes, coils, selected heat-transfer plates, wetted internals and formed components for an agreed evaporator scope. Identify replacement parts and new-build requirements separately.

What we need to review

Feed and final concentrations, salts and solids, pH, temperatures, operating pressure or vacuum, heat-transfer conditions and deposit-control measures. Include cleaning agents, duration and frequency. Define joint details, fabrication inspection, pressure/vacuum design requirements and the records needed for acceptance.

Send your application details

Application review / 06

Coils, U-bends & formed heat-transfer plates

For a coil, the straight tube specification is the starting point; bending can change wall distribution and ovality. For a pressed plate, the finished pattern, ports and gasket interface govern compatibility. Neither an alloy designation nor a raw-material certificate proves that a replacement will fit or perform in a specific heat exchanger.

Products to discuss

Custom coils, serpentine tubes, U-bends and heat-transfer plates where material selection and forming suitability have been confirmed for the application.

What we need to review

Coil diameter, pitch, turn count, total developed length and connections; or released plate drawing, tooling and gasket geometry. Agree minimum remaining wall, ovality, contour tolerances, surface cleanliness and any post-forming integrity test. Review a sample or first article where needed before releasing the batch.

Send your application details

Application review / 07

Process piping with a defined tube, pipe & fitting route

A process-piping enquiry needs more than a nominal bore and alloy name. State whether the design calls for seamless pipe, welded pipe or a tube dimensional system. The pipe, fittings and connections must be reviewed as a system, including weld joints, dissimilar materials and areas that retain fluid.

Products to discuss

Grade 11 seamless pipe to ASTM B861, welded pipe to ASTM B862, or an agreed TA9-1 tube route. Wrought welding fittings may use ASME SB-363 WPT11 when specified.

What we need to review

OD and wall or the required size schedule, lengths, fitting drawings, end preparation and flange interfaces. Include design pressure/temperature, fluid and cleaning conditions, weld procedure requirements, inspection and system-test responsibilities. A tube standard does not automatically establish a piping-code rating.

Send your application details

Application review / 08

Pump, valve & sealing components: corrosion plus mechanics

For pump and valve parts, corrosion resistance is only one selection input. Pressure loads, contact stresses, solids, velocity, cavitation and sliding wear may control the design or require a different surface or material pairing. Gr11 / TA9-1 should be evaluated against the actual component duty, including crevices at seals and connections.

Products to discuss

Specified bar stock, F-11 forging blanks, rings, sleeves, stems, connectors and drawing-based wetted components. Define whether the scope stops at the blank or includes finished machining.

What we need to review

Drawing revision, wetted surfaces, sealing-face finish, concentricity, threads and mating materials. Agree material condition, machining allowance, dimensional and NDT records, and any separate component pressure or leakage test. Identify inspection hold points before critical surfaces are finished.

Send your application details

Material references: Alleima Grade 11 datasheet ↗ and ATI corrosion-resistant titanium alloys ↗. These describe material behavior and application considerations. Selection for a particular fluid and finished equipment requires project-specific review.

Chemical-equipment enquiry checklist

Make the corrosion duty part of the order.

A useful specification connects the environment, the supplied parts and the acceptance evidence. Share existing data first; missing details can be clarified.

01

Define the service envelope

Provide normal, minimum and maximum operating conditions, both-side media, impurities, concentration changes, deposits and cleaning cycles. Include relevant corrosion history or the test evidence your engineering team requires.

02

Define the supplied boundary

List each wetted item, drawing and material route. Separate raw material, formed or machined parts, welded subassemblies and complete equipment. Identify design-code responsibilities, joints and mating materials.

03

Define the evidence and milestones

Agree chemistry and heat identity, product-specific mechanical tests, dimensional and integrity checks, welding records where applicable and inspection hold points. State sample, third-party inspection, packaging and delivery requirements.

Example: a useful Grade 11 condenser-tube enquiry

“Grade 11 titanium tubes to ASTM B338-08b, seamless; OD × wall × length and quantity; straight or U-bent drawing; both-side media, temperature and pressure; tube-to-tubesheet connection; required material records, integrity testing and post-bending checks; destination and target delivery.”

For a TA9-1 order, state GB/T 3625-2007 and the applicable requirements explicitly. Add your actual dimensions and conditions; do not substitute one designation automatically.

Discuss your equipment requirement

04 / Standards & documentation

Match the standard
to the product.

Select the product specification, edition and delivery condition. Grade 11, F-11, WPT11 and TA9-1 belong to defined product routes; use the designation required by the controlling document.

Reference files available on TiHubs · Select a standard to preview or download the supplied edition.
Product form ASTM / ASME route Chinese standard route Clarify before quotation
Material identity & composition United StatesTi-Pd · UNS R52250

Use the chemical requirements in the specified ASTM product standard.

ChinaGB/T 3620.1-2016View PDF ↗

TA9-1 designation and chemistry; use with the applicable product requirements.

Grade designation, complete chemistry, analysis basis and the required material records.
Sheet & plate United StatesASTM B265-08View PDF ↗

Grade 11 strip, sheet and plate.

ChinaGB/T 3621-2022View PDF ↗

TA9-1 plate and sheet.

Thickness, width, length, condition, surface, forming direction and acceptance.
Bar & rod United StatesASTM B348-08aView PDF ↗

Grade 11 bars and billets.

ChinaGB/T 3620.1-2016View PDF ↗

TA9-1 chemistry plus an explicitly agreed bar specification. GB/T 2965-2023 lists TA9, not TA9-1; do not infer full TA9-1 bar coverage.

Section, condition, dimensional limits, mechanical tests, surface and inspection scope.
Heat-exchanger & condenser tubes United StatesASTM B338-08bView PDF ↗

Grade 11; identify seamless or welded construction.

ChinaGB/T 3625-2007View PDF ↗

TA9-1 heat-exchanger and condenser tubes.

OD, wall, length, straight or bent geometry, tube-joint requirements and applicable integrity tests.
Seamless process pipe / tube United StatesASTM B861-10View PDF ↗

Grade 11 seamless pipe.

ChinaGB/T 3624-2023View PDF ↗

TA9-1 seamless tube; review the ordered dimensional system and scope.

OD and wall or specified pipe size, manufacturing route, end preparation and required testing.
Welded process pipe / tube United StatesASTM B862-06b ε1View PDF ↗

Grade 11 welded pipe.

ChinaGB/T 26057-2010View PDF ↗

TA9-1 welded tube; review dimensions and weld-related requirements.

Weld construction, condition, weld inspection, testing and dimensional acceptance.
Forgings & component blanks United StatesASTM B381-08aView PDF ↗

F-11 forging designation.

ChinaGB/T 25137-2010View PDF ↗

F-11 is the designation used in this Chinese forging document.

Rough and finished geometry, allowance, heat treatment, test location and NDT scope.
Wrought welding fittings United StatesASME SB-363 · 2013View PDF ↗

WPT11 under ASME SB-363 in the supplied 2013 BPVC Section II-B file.

ChinaDrawing / agreed specification

Confirm the actual fitting product standard and designation for a Chinese-route enquiry.

Fitting type, dimensions, construction, joints, required product tests and applicable system design code.
Agree the order basis.

These are the supplied file editions. The purchase order must identify the required revision, grade, product form, condition and inspection. Material and product standards do not by themselves establish compliance of a finished pressure vessel, heat exchanger, pump or valve.

Use the file titles shown above. The file named ASME-B363.pdf contains ASME SB-363; its fitting designation is WPT11. Any substitution or dual-certification requirement must be agreed before supply.

05 / Order coordination

Know the scope
before ordering.

Our founder’s 20 years in titanium inform the questions we ask before quotation and the supply options we review with you.

Grade 11 / TA9-1 pump, valve and sealing component application illustration
Component application illustration. Actual material records, inspection and performance tests are defined for the order.
A quotation you can evaluate

Agree the grade, standard edition, dimensions, tolerance, condition and quantity before comparing prices.

  • Identify whether inspection, samples and tooling are included.
  • Confirm packaging, transport and delivery terms.
  • Record items that still need technical confirmation.
Acceptance agreed before supply

Confirm the material certificate, palladium-bearing grade, heat or batch identity, delivery condition, dimensional checks and additional testing before supply starts. For fabricated parts, agree post-forming or weld inspection and the required traceability scope.

Independent inspection can be discussed with its scope, timing, acceptance criteria and cost agreed for the order.

Delivery with clear milestones

Review the proposed lead time, approvals, production sequence and dispatch requirements. For several product forms, coordinate document and packing readiness together.

Material substitutions and technical changes require written approval. A schedule deviation should identify the impact, decisions needed and next steps.

One contact when an issue arises

Contact TiHubs with the order reference, affected items and supporting photos or inspection records.

We record the issue, review it against the agreed requirements and coordinate the next steps with the relevant manufacturing parties.

01 / Material identity

Material records

Grade, standard, test results and heat or batch identity matched to the supplied items.

  • Material certificate
  • Heat / batch ID
  • Test results
02 / Agreed acceptance

Inspection records

Dimensional and testing records for the agreed scope, including critical drawing requirements.

  • Dimensions
  • Agreed testing
  • Acceptance criteria
03 / Ready for dispatch

Dispatch records

Item identification, packing list, protective packaging and required shipment documents.

  • Packing list
  • Item labels
  • Shipping documents

06 / Questions before sourcing

Before you specify
Grade 11 / TA9-1.

A clear material designation is the beginning. Product form, specification revision, material condition and acceptance complete the requirement.

A useful first enquiry

  • Product and specificationProduct form, standard edition, dimensions and material condition.
  • Order and deliveryQuantity, destination and any required delivery date.
  • Acceptance requirementsDrawing revision, inspection, certificates and packaging.

Not every detail is finalized? Send the information you have. We can help identify the questions to resolve before quotation.

Discuss your requirement

What happens next: requirement review, technical clarification, then a supply proposal and quotation.

What is Grade 11 titanium, and what does Gr11 mean?

Grade 11, abbreviated Gr11, is a low-interstitial titanium-palladium alloy identified as UNS R52250. Its palladium range is 0.12–0.25%. It is considered for corrosion-resistant chemical equipment and demanding formed components. The product standard, condition and service environment must still be defined.

Is TA9-1 the Chinese equivalent of Grade 11?

TA9-1 is the Chinese designation for the corresponding low-interstitial Ti-Pd chemistry route. The selected principal chemical limits shown on this page align with Grade 11, but product standards can differ in scope, mechanical requirements and inspection. Specify the exact route; substitution or dual certification requires agreement and supporting material records.

How does Grade 11 differ from Grade 7 / TA9?

Both are palladium-bearing titanium grades. Grade 11 has lower oxygen and iron limits and lower specified strength in the cited sheet standard, making formability an important selection consideration. Grade 7 / TA9 is a different material order. Confirm the required strength, geometry and corrosion duty before changing grades.

Where is Grade 11 / TA9-1 mainly used?

It is considered for chemical corrosion-resistant equipment that also benefits from good formability: selected heat-exchanger and condenser tubes, coils, formed plates, linings and evaporator internals. Pump, valve and sealing components are reviewed against their drawings and duty. Suitability depends on the media, conditions and component design; these are application options, not universal approvals.

What information is needed for a heat exchanger or evaporator enquiry?

Send the drawing or item list, both-side media and concentrations, impurities, operating and design temperatures and pressures, and cleaning conditions. For evaporation, include the final concentration, solids and deposits. Add the tube or plate dimensions, joint details, required design code, inspection scope, quantity and destination. Incomplete information can be clarified before quotation.

Can you coordinate coils, U-bends or formed heat-transfer plates?

We can review the relevant manufacturing route against your drawing. For coils and U-bends, specify tube dimensions, radius, pitch or leg spacing, wall-thinning and ovality limits. For plates, provide the pattern, ports, gasket interface and minimum remaining thickness. Material selection, tooling, sample approval and post-forming inspection are agreed before commitment.

Which standards apply to tube, pipe and forged components?

ASTM B338 Grade 11 and GB/T 3625 TA9-1 cover heat-exchanger and condenser tube routes. ASTM B861 Grade 11 covers seamless pipe, and ASTM B862 Grade 11 covers welded pipe. Chinese tube routes include GB/T 3624 and GB/T 26057 for TA9-1. ASTM B381 and GB/T 25137 use F-11 for forgings; the supplied ASME SB-363 fitting document uses WPT11. Select by actual product scope and edition.

Can you provide certificates, samples and independent inspection?

Required material records, heat or batch identity and testing are agreed during quotation. Samples, forming trials and independent inspection can be discussed with scope, acceptance criteria, timing and cost defined for the order. Finished-part, weld or equipment tests must be specified separately from raw-material certification.

What are your minimum order quantity, lead time and issue-handling process?

Quantity and timing depend on the form, dimensions, stock or production route, tooling and inspection. We confirm the quotation scope and delivery milestones for your requirement. If an issue arises, contact TiHubs with the order reference, affected items and evidence. We record it, compare it with the agreed requirements and coordinate the next steps with the relevant manufacturing parties.

07 / Your next step

Start with the
requirement you have.

Send the product details, drawing or operating conditions you already know. We will identify missing information and discuss a suitable supply route before quotation.

  1. Requirement review
  2. Technical clarification
  3. Supply proposal and quotation

Combine materials and parts in one enquiry.

Send one list of Gr11 / TA9-1 forms, sizes and quantities. Include drawing revisions and items that must be supplied or dispatched together.

Share the service and acceptance priorities.

Include media, temperatures, pressures and cleaning conditions, plus the required material records, forming or fabrication checks, destination and timing.

Baoji, China · info@tihubs.com

Start your Grade 11 / TA9-1 enquiry

Send your material form, drawing or process conditions. We will help clarify the remaining requirements.

Customer Feedback & RFQ Form (#6)