Titanium stub ends.
Send a section through the joint with the pipe, loose backing flange and gasket identified. A titanium stub end can match the pipe size while its lap, corner radius or face station still prevents the assembled connection from seating.
Select the supply configuration
Use the drawing and the assembly configuration to identify the item to quote.
Type A short pattern
For the quotation, identify lap radius, backing relief, short length.
- Lap radius
- backing relief
- short length
Dimensions and acceptance
Match a titanium stub end to the backing flange, weld end and gasket. Compare short and long patterns, lap diameter, radius and inspection dimensions.
| Order item | Include in your enquiry | Why it matters |
|---|---|---|
| NPS 1, Schedule 10S example | Pipe OD 33.40 mm; listed bore 27.86 mm | Titanium Industries Table 2, selected Grade 2 catalogue item |
| Lap diameter, same example | 50.80 mm | Check gasket and backing ring on their own drawings |
| Overall length, same example | Short 50.80 mm; long 101.60 mm | Weld end shifts 50.80 mm if the sealing face is fixed |
| Lap radius, same catalogue row | Type A 3.18 mm; Type B 0.79 mm | Confirm the actual backing bore and corner relief |
| Tube wall, same catalogue row | 2.77 mm | Specify weld preparation and mating pipe condition |
| Commercial boundary | Stub end alone or matched connection components | Separate backing flange, gasket, studs and assembly |
Your starting specification.
Send a section through the joint with the pipe, loose backing flange and gasket identified. A titanium stub end can match the pipe size while its lap, corner radius or face station still prevents the assembled connection from seating.
The table identifies the basis for the quotation. Confirm material, dimensions, inspection and delivery for the selected part before ordering.
Material and delivery condition
Identify the material on the approved drawing and confirm its product form and condition with the quotation.
Chinese designations and international names are reference routes, not automatic substitutes. Grade, product specification, condition and acceptance requirements must be agreed together.
Open grade cross reference ↗Purchasing situations
A first assembly, a replacement and a repeat order need different evidence.
Type A short pattern
For the quotation, identify lap radius, backing relief, short length. For related supply options, see the parent product guide.
Type B short pattern
For the quotation, identify type on drawing, contact band, bore clearance.
Replacement to drawing
For the quotation, identify actual backing flange, gasket outline, plant datum.
Engineering and purchasing guide
Send a section through the joint with the pipe, loose backing flange and gasket identified. A titanium stub end can match the pipe size while its lap, corner radius or face station still prevents the assembled connection from seating.

Stub end and backing flange. Wetted stub end, Loose backing flange.
Order geometry schematic; not a dimensional drawing.Separate the wetted part from the loose flange
When a maintenance photograph shows a loose flange behind a flared pipe end, identify what the plant actually wants to replace. The short tubular item carrying the lap is the stub end. Its tubular end is welded to the pipe. The separate backing flange bears on the rear of the lap and provides the bolt pattern for the connection. The gasket bears on a process-side face. A requisition describing the entire photograph as a titanium flange can produce an offer for the wrong piece or an incomplete kit.
Give the two metallic parts separate line items, even if the supplier is to deliver them together. For the wetted part identify the titanium grade, starting or finished fitting specification, pipe end and required lap geometry. For the backing flange identify its own material, pattern, bore and contact profile, bolt pattern and applicable flange requirements. Add the gasket and fasteners if they are part of the purchased supply. An exploded section with the delivered pieces shaded makes the commercial boundary clear to a buyer in another office.
Decide whether the backing flange will remain in service. A new titanium stub end may have to mate with an old ring that was modified, coated or purchased to a different dimensional reference. Obtain measurements and a drawing of that actual ring. If removal during a survey would require opening a working line, indicate the access limitation and make the offer conditional on the missing check. A confident quotation based only on a pipe size has not resolved the rear contact or face geometry.
In service the flexible orientation of a loose flange can help line up the bolt holes before tightening. It does not provide an unlimited way to correct misalignment between two pipe axes or two sealing faces. Ask which installation dimension is presently difficult: rotational alignment of bolt holes, axial spacing, angular alignment of faces or clearance behind the lap. Each calls for different evidence. Applying the same solution to all four can consume the limited space available for the weld or the gasket.
The term stub end is widely used alongside names such as lap-joint end or flared collar. Regional purchasing language can also describe a loose flange and a lap as an assembly. Preserve the supplier’s terminology beside the controlled section drawing. If the drawing shows a machined integral flange with bolt holes through the titanium itself, qualify the request again. The product and the way loads pass through it differ from a stub end with a free backing flange.
Read the catalogue by pattern and size
Read a dimensional table from the title down to the individual row. Titanium Industries identifies several Grade 2 options, including short and long patterns and different lap radii. In its Schedule 10S table, the NPS 1 row gives an outside diameter of 33.40 mm, a listed bore of 27.86 mm and a wall of 2.77 mm. The bore agrees with subtracting the two nominal walls from the outside diameter. These are catalogue values for the chosen example. Select the required series and controlled drawing before using them as order dimensions.
The same row lists a lap diameter of 50.80 mm. It lists a short length of 50.80 mm and a long length of 101.60 mm. In this example the lap diameter and the short overall length happen to have the same number. They measure different directions on the component. Label each number with its feature and unit when copying it to an enquiry. A single unlabeled value of 50.8 on a supplier sketch is not a safe way to decide where the weld will meet existing pipe.
The catalogue row also shows different radii, 3.18 mm for Type A and 0.79 mm for Type B. These values belong to this particular nominal size and published reference. They do not establish a general allowance to fit any Type A or Type B product against a flange carrying a similar trade description. A flange bore, its corner relief and the actual lap profile must be considered together. Ask a proposed alternate supplier to mark the radius on a section instead of writing only “equivalent type”.
Choose the controlling units for acceptance. In a printed catalogue, a value expressed to a limited number of decimal places in inches can appear to disagree with a more precise metric figure after conversion. Use the approved dimension and its tolerance rather than combining the largest value from one column with the smallest from another. If the equipment drawing was originally metric and a replacement is offered to an inch series, reconcile the actual controlling geometry before a purchase order is released.
For a nonstandard connection, ask for dimensions that can be independently checked after delivery. State the tubular outside diameter and wall, lap diameter, face-to-weld-end length, face geometry and rear corner detail. Identify the reference face for length, including whether a machining allowance remains. If the drawing specifies inspected values after finishing, a dimension measured before facing or after blasting may refer to a different condition. Record that stage in both the vendor drawing and inspection plan.
Keep the two uses of the word face distinct during inspection. The rear bearing side accepts the force from the backing flange. The process-side sealing face is the reference that the gasket sees. If an item is quoted with an allowance to machine the sealing face, the final distance back to the weld end may change. Ask which measurements the vendor will report before and after that operation. A report can otherwise be dimensionally consistent with the unfinished part while failing to describe the item the installer receives.
Check the lap and backing contact together
Examine the rear side of the lap as though the assembly had been cut through its axis. The backing flange must pass over the pipe and reach a defined annular contact area on the lap. Between the neck and lap there is a transition. If the edge of the flange bore contacts this transition first, the ring may look close to the correct position without actually bearing on its intended area. The question is where the force is transmitted after assembly, not merely whether the flange can be slid over the pipe.
Use a section with both profiles overlaid at their agreed dimensional limits. Mark the minimum bore, the available corner relief, the maximum relevant lap transition and the start and end of the intended contact band. Check the support near any step in the lap or face. Coatings on the backing ring, edge finishing or an actual out-of-round condition can affect a tight fit. If the proposed contact depends on a coating being absent in an area, put that condition on the purchase drawing where the supplier and inspector will see it.
A useful geometric calculation illustrates the distinction between overall land and effective contact. With the NPS 1 catalogue lap diameter of 50.80 mm and tube OD of 33.40 mm, half the difference is 8.70 mm of nominal radial projection on each side. That figure is a geometric envelope. It includes the transition region and says nothing about the ring’s inner radius, actual relief, finish or maximum permitted contact stress. A designer should not enter 8.70 mm as a guaranteed effective bearing width without a mating drawing.
If an existing ring binds during a cold trial fit, record where contact occurs before changing either component. Mark the part orientation and inspect the bore edge and corner. A localized high point and uniform contact all around a radius suggest different issues. Compare with the drawing and any treatment or damage visible on the removed hardware. Do not grind a titanium lap or enlarge a flange bore simply because the parts appear close. The modification could change the bearing area or leave less support for the face.
The order should assign responsibility for the matching check. A vendor delivering only the stub end can verify what its own part drawing controls. A vendor delivering a matched pair can also check the assembled fit against an agreed acceptance method. Where the owner supplies a loose flange, arrange to send its controlled dimensions or a representative item for trial assembly. State whether the check concerns sliding clearance, seating contact, rotational freedom before bolting or all of these features. A single statement that the flange fits gives little help if a later problem appears.
An off-centre trial is worth recording even if the ring can be pushed into place by hand. Measure the proposed clearance at several angular positions and inspect the actual bore and neck for damage or ovality. Determine whether the ring lies flat in its free position. A trial made with the assembly standing vertically can mask a ring that shifts under its own weight in the orientation used on site. The responsible designer can decide whether the observed free movement or contact is acceptable for that joint.
Locate the gasket and the weld end
On the process side, lay the gasket outline over the actual sealing face. Check its inside and outside boundaries and the intended face finish against the selected joint design. A catalogue lap diameter describes the outside of the metal projection. It does not identify the gasket support area after chamfers, radii, recesses or a difference in bore are considered. Obtain the drawing of the mating face too. The gasket contacts two surfaces, and an accepted finish on one face leaves the other face unresolved.
Trace the wetted boundary at the edge of the gasket and at the bore. A joint being purchased to isolate a particular process liquid may need the owner to define which materials can be exposed there. A titanium stub end does not make nearby hardware universally suitable for the environment. External washdown, leakage during maintenance or the surrounding atmosphere may also influence the material and coating selected for the backing flange. Have the responsible engineer specify the service assumptions instead of relying on the trade name of the joint.
Keep the location of the sealing face and the weld station distinct. For the NPS 1 catalogue example, changing from the 50.80 mm short pattern to the 101.60 mm long pattern moves the weld end by 50.80 mm if the sealing face stays fixed. If the weld station stays fixed, the sealing face moves instead. A drawing that holds both locations fixed cannot accept that substitution without another change in the spool. This is an ideal nominal comparison before any allowance for fitting, weld preparation or machining.
For a replacement between fixed lines, a longer neck could move the weld closer to a support, an earlier joint or a region that cannot be accessed with the specified tooling. A shorter neck could deprive the fabricator of space to grip or align the part. Ask the installer to mark the usable weld zone and the space needed for its method and inspection. The plant design authority decides whether relocating a weld or trimming another component is permissible.
Protect the sealing face through the actual work sequence. A face received in good condition may later rest against a steel bench, a clamp or unprotected packing. The chosen handling protection must remain removable without damaging the specified surface. If an inspector finds a mark, locate it relative to the gasket footprint and request a disposition to the agreed criterion. Taking material off the face to remove the mark can also change the face station and lap thickness. Any such correction should be evaluated as a dimensional change, as well as a surface repair.
Plan the assembly sequence and inspection
A free backing flange often has to be placed on the correct side before the stub end is welded. Check the planned assembly sequence on the real spool. After a second joint has been completed, there may be no route for a closed one-piece ring to pass over the lap or around a bend. If the system uses a special split backing arrangement, identify that separately on the drawing. It is a different supply configuration requiring its own approved design and parts.
At incoming inspection, identify the stub end, the loose ring and the gasket before laying out a trial assembly. Check that the part labels refer to the required material and dimensional series. Record the dimensions the order defines for the weld end, lap and reference face. If two components are supplied as a matched set, maintain that relationship in storage and at the work station. A free flange moved to another nominally similar stub end during fabrication can defeat a trial fit already carried out by the supplier.
Maintain access for the checks that matter. Before the weld closes an assembly, confirm the ring is present, correctly oriented and free to occupy its intended position. After joining, inspect the required weld and recheck any face location, squareness or surface condition that the process could have affected. A loose ring that rotates comfortably before welding may become trapped by the arrangement of adjacent equipment even if its geometry is unchanged. Check its usable movement on the delivered assembly where this is a requirement.
Specify the inspection record in terms of feature and method. A calliper can help check a lap outside diameter, but cannot establish conformity of every point on a sealing face or the geometry of an inaccessible radius. Identify how the inspector should check the transition and compare it with the mating corner. State the section drawing and revision used to assess the fit. Where a representative test assembly forms part of acceptance, identify which parts participated and whether they belong to the production batch.
For pressure or leak testing, distinguish the starting fitting, the shop spool and the installed joint. A supplier’s dimensional inspection does not set the plant test pressure or release the gasketed joint. The approved piping design and test procedure control what will be tested and under whose authority. Specify any supplier documents that must be available before the next assembly hold point. Returning to a completed spool to recover a missing backing-ring identification or an unrecorded weld-end dimension can involve disproportionate dismantling.
Compare kits, spares and site work
Prepare a commercial comparison with a separate row for each item and service. The first vendor may offer a titanium stub end only. A second may offer the same nominal size with a drilled backing flange, gasket and bolts. A third may weld it to a pipe pup and provide inspection records for the assembly. Their total prices cannot be compared until the buyer assigns responsibility for the remainder of the connection. Identify which party owns the compatibility of pieces sourced from different vendors.
Ask how manufactured length is determined on the delivered item. A stock long-pattern piece offered for trimming may appear versatile, but trimming changes the weld end, marking position and relationship to the original controlled dimensions. A shop offering a finished cut-to-length item should identify the post-cut examination and any new end preparation. Keep the drawing and acceptance conditions with the quotation so a purchasing substitution does not become an unapproved modification to the pipe spool.
Plan spares by failure or maintenance need. If a gasket is routinely replaced when the equipment is opened, it may belong in a service kit. A damaged titanium lap or a backing ring with an unsuitable corner requires a different replacement. Retaining a complete matched pair may help where a nonstandard profile is difficult to reproduce. On the other hand, stock held without its drawing or traceable mark may be impossible to approve years later. Package the reference and mating requirements with the spare and record which plant locations use the same configuration.
A receiving team can encounter two short-pattern ends having the same nominal pipe size but visibly different rear radii. Do not separate them solely by a handwritten A or B on the outer carton. Inspect the actual profile against the specified series, recover the material traceability and identify the mating ring intended for each. If the two offers use different naming conventions, the controlled profile is a more reliable reference than a translated catalogue label. Keep the receipt discrepancy open until the combination is positively identified.
For a quotation, include pipe size and wall, material grade, selected pattern, length, lap diameter, transition and face requirements. Attach the mating flange and gasket references, direction of installation, available weld access and inspection requirements. State how many pieces or matched sets are required, the delivery location, and whether the vendor is to supply loose components or a joined assembly. The result can then be priced, manufactured and inspected against the same physical interfaces the plant will use.
When suppliers propose different materials for a loose flange, compare the actual environment it will see. The flange may be outside the intended process boundary yet exposed to cleaning liquid, condensate or weather. The owner should define the external condition and any treatment on the backing metal. Keep that material decision separate from the titanium specification for the stub end. The purchase can then identify a permissible combination without implying that every piece in the assembly must share the same grade or corrosion behaviour.
Inspection points
Agree the acceptance evidence before the first part is released.
Traceable from heat to shipment.
Titanium Industries Table 2, selected Grade 2 catalogue item
Pipe OD 33.40 mm; listed bore 27.86 mmCheck gasket and backing ring on their own drawings
50.80 mmWeld end shifts 50.80 mm if the sealing face is fixed
Short 50.80 mm; long 101.60 mmConfirm the actual backing bore and corner relief
Type A 3.18 mm; Type B 0.79 mmSpecify weld preparation and mating pipe condition
2.77 mmSeparate backing flange, gasket, studs and assembly
Stub end alone or matched connection componentsSource documents
Check the applicable series, revision and scope against the purchase drawing.
Library PDFs may be earlier editions. Check the document cover and your contractual revision. A reference file does not certify a supplied product.
Explore all downloads ↗Technical sources
- Titanium Industries — Stub Ends, Table 2 — Selected Grade 2 Schedule 10S NPS 1 catalogue dimensions; scope limited to the stated example.
- ASME B16.9 — Scope and exclusions for factory-made wrought buttwelding fittings.
- ASTM B363 — Scope of titanium welding fitting material specification.
- Standard Titanium — stub end — Manufacturer description of a stub end welded to pipe and used with a free backing flange.
Baoji.
One contact.
TiHubs coordinates titanium sourcing through a local manufacturer network. Your specification guides the supplier review, technical discussion and delivery requirements.
Clarify the requirement
Confirm grade, dimensions, state, quantity and the purpose of the stock.
Review the supply route
Discuss manufacturing, finishing, inspection and documentation with the relevant supplier.
Agree the commercial scope
Confirm the quotation, lead time, acceptance requirements and delivery terms.
Coordinate inspection & delivery
Follow the agreed checks, marking, packing and shipment documentation.
Before you order
Match a titanium stub end to the backing flange, weld end and gasket. Compare short and long patterns, lap diameter, radius and inspection dimensions.

TITANIUM STUB ENDS · BAOJI SOURCING
Send your specification.
Send a section through the joint with the pipe, loose backing flange and gasket identified. A titanium stub end can match the pipe size while its lap, corner radius or face station still prevents the assembled connection from seating.