Illustration of Titanium Pipe Tees

Titanium pipe tees.

Mark the two run ends and the branch on the piping isometric. Send the three end dimensions, centerline position and mating pipe details for a quotation covering the fitting you can actually install.

View specifications
20 years in titanium100+ Baoji factory connections
Equal butt-weld tee · Reducing tee

Select the supply configuration

Use the drawing and the assembly configuration to identify the item to quote.

Equal butt-weld tee

Equal butt-weld tee

For the quotation, identify run OD, branch OD, wall schedule.

  • Run OD
  • branch OD
  • wall schedule

Dimensions and acceptance

Specify a titanium butt-weld tee by run and branch size, wall at each end, center-to-face dimensions, material, fabrication route and inspection.

Order itemInclude in your enquiryWhy it matters
Run and branchEqual or reducing branchIdentify ends A, B and C on an isometric
NPS 1/2 straight tee, Sch 10SOD 21.34 mm; wall 2.11 mmCatalogue center to face 25.40 mm
NPS 3/4 straight tee, Sch 10SOD 26.67 mm; wall 2.11 mmCatalogue center to face 28.58 mm
End boreCompare actual bores at all three jointsUse the drawing for mismatch acceptance
Fitting materialASTM B363 where specifiedConfirm exact grade and seamless or welded route
Installation envelopeRun center-to-face and branch center-to-faceRecord orientation and reference planes separately

Your starting specification.

TiHubs — EN — Titanium Pipe Tees — inline

Mark the two run ends and the branch on the piping isometric. Send the three end dimensions, centerline position and mating pipe details for a quotation covering the fitting you can actually install.

The table identifies the basis for the quotation. Confirm material, dimensions, inspection and delivery for the selected part before ordering.

Material and delivery condition

Identify the material on the approved drawing and confirm its product form and condition with the quotation.

Chinese designations and international names are reference routes, not automatic substitutes. Grade, product specification, condition and acceptance requirements must be agreed together.

Open grade cross reference ↗

Purchasing situations

A first assembly, a replacement and a repeat order need different evidence.

Equal butt-weld tee

For the quotation, identify run OD, branch OD, wall schedule. For related supply options, see the parent product guide.

What to sendRun OD / branch OD / wall schedule.

Reducing tee

For the quotation, identify both run ends, branch bore, branch center to face.

What to sendBoth run ends / branch bore / branch center to face.

Replacement in a spool

For the quotation, identify as-found dimensions, available closure, weld access.

What to sendAs-found dimensions / available closure / weld access.

Engineering and purchasing guide

Mark the two run ends and the branch on the piping isometric. Send the three end dimensions, centerline position and mating pipe details for a quotation covering the fitting you can actually install.

Locate the branch centerline — Run center to face, Branch face position
Equal and reducing tees — Equal branch, Reducing branch

Equal and reducing tees. Equal branch, Reducing branch.

Order geometry schematic; not a dimensional drawing.

Read the isometric as three separate interfaces

A tee ordered for an existing titanium line has to meet three pipes at once. A straight coupling can accommodate only a single run direction. With a tee, correcting the position of one end can move the branch away from a fixed valve or bring the opposite end too close to a support. Draw the actual installation before sending sizes. A small isometric showing the run, branch, flow arrows where useful, nearby restraints and the intended field closure communicates more than a photograph of a fitting on a bench.

Label the straight-through ends A and B and the branch C. Put the nominal pipe size, actual outside diameter and wall or schedule beside each one. If the line list references separate drawings for the main line and branch, include both revisions. A description such as “two-inch titanium reducing tee” identifies at most part of the order. It leaves the branch size open and can conceal a difference between the two existing run ends caused by a past repair. Specify which end faces which item in the system.

An equal or straight tee generally identifies a fitting whose three nominal end sizes match. A reducing tee combines a nominal run with a smaller nominal branch. Those descriptions alone do not establish a manufacturer’s take-out dimensions, material specification or pressure design. If the installation demands an unusual angle, an offset or a particular arrangement made from pieces, show that configuration as a drawing-led fitting. A standard forming route and a fabricated branch assembly may both connect three pipes but require different approval and examination.

Ask how the installer can verify orientation before cutting the old line. A take-off serving equipment above a pipe rack may appear vertical on one elevation while the actual run slopes towards a drain. Give the designer’s required angle and reference plane. In a prefabricated spool with other fittings, record where rotation is measured from. An apparent clock position on a photograph is ambiguous unless the viewing direction is known. A short note such as “looking from A towards B” makes the position usable by the receiving shop.

Keep the quotation boundary visible. A factory tee with three prepared ends, a tee already welded into two pipe pups and an installed spool ready for a site tie-in are different purchases. Indicate who supplies the adjacent pipe, on which joints field work remains, and which pieces need identification after cutting. A buyer can then separate the cost and responsibility of the actual fitting from the work required to make it usable within the plant.

If branch orientation is handed, label the viewing direction on both the request and the returned drawing. A branch shown to the right when looking from end A will appear on the left when looking from end B. This becomes important when a tee is attached to an asymmetric spool, a sampling connection or a support lug. A simple witness mark on a preliminary assembly may help during fabrication, but the controlled drawing must still preserve the orientation after that temporary mark disappears.

Compare the catalogue with the adjacent pipes

Titanium Industries publishes a Grade 2 straight-tee table for Schedule 10S that illustrates how nominal size differs from a measured outside diameter. Its NPS 1/2 entry lists 21.34 mm outside diameter, 2.11 mm wall and 25.40 mm from center to face. Its NPS 3/4 entry lists 26.67 mm outside diameter, 2.11 mm wall and 28.58 mm from center to face. The table on this page uses those catalogue examples. They describe selected equal tees and cannot be transferred directly to a reducing branch or a custom fabrication.

The first entry also offers a useful dimensional cross-check. For an ideal concentric circular pipe end, subtract twice the wall from the outside diameter to obtain the nominal bore. At 21.34 mm outside and 2.11 mm wall, the calculation gives 17.12 mm. For 26.67 mm outside and the same wall, it gives 22.45 mm. Both agree with the corresponding published entries. The calculation confirms what the columns represent. It does not give the permitted variation of an actual end or the minimum wall at a formed intersection.

At a real tie-in, inspect both mating ends. A difference in outside diameter, wall or ovality may leave an internal step despite an apparently acceptable external fit. If the line has been machined, lined, eroded or repaired, a nominal schedule from the original specification may no longer represent the measured bore. Mark the measurement stations in relation to the weld end. A reading taken behind a bevel and a reading taken on the thin edge of the bevel should not be treated as the same dimension.

If a procurement system accepts only one schedule field, attach a three-end schedule to the enquiry. That is particularly important for reducing tees where the adjoining branch can belong to a different line class or thickness requirement. Ask the responsible engineer how local mismatch is to be assessed and which transitions are permitted. Do not authorize a shop to remove material from a titanium end merely to make the bores look flush. The modification must preserve the geometry and wall required by the approved design.

Confirm which edition and dimensional system govern the purchase. NPS and DN are nominal designations, while millimetres or inches on the drawing can represent actual dimensions. An outside diameter expressed as “one half inch” could be a tube measurement or a nominal pipe callout depending on the speaker. Resolve this ambiguity before comparing stock. If a vendor cites an equal-tee table, ask it to mark the precise row and the values it will use for the selected part.

Review the catalogue rounding convention as well. A displayed inch value may have fewer significant figures than the adjacent metric value. Converting the rounded inch entry back into millimetres can create a small apparent discrepancy. Pick the controlling units from the agreed drawing or specification and use that column consistently. Where a receiving tolerance is tight relative to the apparent discrepancy, request the unambiguous controlling dimension instead of rejecting a fitting on the basis of a rounded catalogue display.

Locate the branch before fixing the cut lengths

The center-to-face dimension describes where a welding face lies relative to the relevant centerline intersection. For the catalogue NPS 1/2 straight tee with a 25.40 mm run center-to-face dimension on each side, the nominal run face-to-face span is 50.80 mm. Adding those two distances is appropriate for that symmetric example. It does not establish the face-to-face span of an item with unequal end details or a welded-on extension. Obtain a marked drawing when one side has been adapted.

The position that matters on site may be the center of a valve, a face of a flange or a previously installed instrument, not the bare tee face. Choose a project datum and work through all components between it and the branch. Include the specified end preparation, mating fitting and field fit-up requirements where the design calls for them. A dimension taken on an assembly photograph contains neither the datum nor the allowances used in fabrication. Distinguish a design dimension from a field measurement and report the uncertainty of the latter.

As a drawing exercise, imagine the planned center of a branch is 220 mm from a fixed reference plane along the run. The fitting drawing puts the relevant run face 25.40 mm before that center. Its nominal face station is then 194.60 mm from the reference. That station locates a face. It is not automatically the adjacent pipe’s finished cut length, because the actual mating face, weld preparation and fit-up have their own definitions. Mark the station first, then have the fabricator calculate the cut from the approved details.

A similar arithmetic mistake occurs when the branch is measured from the outside wall of the run instead of its centerline. On a small drawing the difference may be visually subtle, especially if the pipe is shown as a single line. Specify the measurement origins at both ends of every critical dimension. If the branch ties into existing equipment, check the elevation and lateral position as well as the distance along its axis. A correct axial take-out alone will not resolve a lateral offset.

Resolve tolerances before assigning the field closure. The fitter may be able to absorb a permitted variation in one loose pipe length but not between two fixed nozzles. Ask which piece remains available for trimming and who may authorize changes. If the assembly is supplied as a spool, specify the final interface coordinates or drawing dimensions required at delivery. Receiving inspection can then check the geometry of the assembled spool instead of assuming that three satisfactory individual component records guarantee the final fit.

Define material, construction and examination scope

ASTM B363 addresses seamless and welded titanium and titanium alloy welding fittings. Confirm the specific grade, construction and ordered edition for the proposed tee. ASME B16.9 addresses factory-made wrought buttwelding fittings within its stated scope and exclusions. A reference to one document answers a different question from a reference to the other. The plant designer must determine which references and piping requirements apply. A website example or a matching outside diameter does not establish a rating for the completed line.

Ask where the fitting began and what records identify its finished condition. A quotation for a formed tee from suitable stock can have a different manufacturing route from one for a fabricated branch connection. A supplier proposing an alternative should identify the base product, any longitudinal or branch seams, forming operations and the examinations offered. The owner can then compare the proposal with the design requirements. A raw tube certificate does not describe the condition at the branch intersection after forming or joining.

If the fitting is specified as seamless, clarify which feature and which document that requirement refers to. An installed tee will still have assembly welds to adjoining pipes. Conversely an offer saying the three site joints are included does not identify whether there are manufacturing welds inside the supplied fitting. Use different marks on the drawing for factory seams, shop spool welds and field joints. Keep responsibility for preparing, examining and documenting each group alongside it.

For process service, agree any surface and cleanliness requirements defined by the owner. The inside of a tee can be less accessible than an open length of pipe. Describe whether the plant requires inspection of internal intersections or preservation of a particular surface condition during transport. Specify caps or other protection appropriate to the order without assuming that an end cap certifies cleanliness. If residual material or damage is found under protection on arrival, the receiving team needs a documented route to inspect and resolve the issue before welding.

The inspection package should follow the actual product identity. Depending on the order, it may include material records, traceability of starting stock, a dimensional report, manufacturing or seam records, agreed examination results and final identification. Agree the documents and their timing. A report produced after the fitting has been incorporated into a spool may arrive too late for a hold point the owner intended to witness. Define any required presentation of the bare fitting before the adjacent pipe obscures its marking or access.

Plan fit-up and receiving inspection

Use an incoming sketch with the three ends labelled in the same way as the purchase drawing. Record outside diameter, end wall or agreed wall measurements, face positions and any required preparation checks for A, B and C. The tool and measuring location depend on the feature. An external calliper cannot establish minimum wall throughout a formed junction. If the design calls for local wall verification or another specialized examination, agree the method, coverage and acceptance criterion with the supplier in advance.

Check for ovality and orientation with a defined reference. A single diameter across the most convenient axis does not describe an out-of-round end. The inspection plan can identify the axes or method required by the approved specification. Record which end had the measurement and what condition it was in, particularly if it carried a protective cap or was supported on a fixture. A short list of results disconnected from the three end labels can make the receiving report nearly impossible to apply on the shop floor.

When possible, arrange a trial fit using representative mating ends or a fixture reflecting the project datums. The intent is to reveal conflicts before a permanent joint is made. Do not draw a branch into position with load applied through connected equipment merely to prove it can be attached. If the gap or orientation differs from the drawing, record the free position, review the dimensional chain and return the issue to the person authorized to approve a change. A forced fit can mask the origin of the mismatch.

Inspection after installation answers different questions. A satisfactory shop check of the three welding ends does not release the site welds. A successful system test does not retrospectively identify an undocumented material substitution inside a fitting. Keep component inspection, shop welding, field work and installed-system testing as separate entries in the turnover records. This gives the operator a way to trace an indication found years later to either the original tee, a shop joint or a site modification.

Consider a receiving exception. Two tees arrive with similar dimensions, but one part marking is no longer legible after handling. The box labels identify two lots. Matching an outside diameter will not distinguish them. Separate the affected fitting and ask the supplier to recover its identity through controlled records. Once traceability has been restored or another disposition has been authorized, document the outcome. Keeping a suspect part out of a prefabricated spool is far easier than establishing its identity after all three ends have been welded.

End protection should stay with the part until its condition has been recorded. If a bevel arrives dented, photograph the location and identify the end before blending or cleaning it. Removing a mark can change the root face, move the effective end plane or reduce local wall. Obtain a documented disposition for any proposed correction and repeat the measurements affected by the work. This preserves the relationship between what the original supplier delivered and what the spool fabricator eventually installed.

Compare the delivered scope and prepare the RFQ

A useful quotation comparison starts with the actual level of completion. A formed tee shipped with plain cut ends, a tee with agreed weld preparation and a spool complete with adjoining pieces are different products even if all use Grade 2 titanium. List manufacturing route, material, supplied ends, surface condition and documentation on separate lines. If the buyer already holds suitable adjoining pipe, identify who assumes responsibility for verifying its compatibility with the offered tee.

The treatment of one field dimension can outweigh a small difference in material price. Suppose a branch must meet a fixed flange while the run is accessible through a narrow maintenance opening. An offer based on catalogue geometry might require site trimming or a new closure piece. An offer based on a surveyed spool may include that coordination work. Ask each vendor to mark its final delivery interfaces, any site measurements the customer must provide and its process for resolving a discrepancy. Then compare the offers on the same installed scope.

If the quantity includes a first-off and a series, set out how the first unit will be approved and how the approval carries into production. Keep the drawing revision, material and route linked to that sample. A later proposal to use another manufacturing route or a different outside diameter to obtain stock quickly should be reported before the change reaches the production lot. If the first unit was installed before full documentation was available, preserve representative measurements or photographs with the equipment reference.

Packaging a tee is another three-ended problem. Protect prepared faces against contact with the crate, keep caps or covers identifiable and support the fitting without loading the branch as a handle. Ask for identification that remains visible when several sizes arrive together. Where the customer needs a kit of fittings for a line number, list the tee tag and the matching pipe pieces on the packing record. Correct allocation across two similar spools can save more time than a general claim about expedited delivery.

A complete enquiry gives the run and branch nominal sizes, actual end dimensions or schedules, center-to-face requirements, grade, construction route and applicable controlled reference. Attach the isometric with orientation and tie-in constraints. List inspection and document requirements, quantity, destination and timing. State whether the quotation includes only the fitting or also preparation, testing, pipe pups and site work. The supplier can then return a marked-up proposal with specific exceptions, and the purchaser can see which questions must be resolved before releasing the order.

For a repeat order, attach the last accepted drawing alongside the current line revision. Highlight the few dimensions that changed, including adjacent pipe replacements. If the replacement part was previously trimmed in the field, retain both the supplied dimension and the final installed dimension. Otherwise the supplier may quote yesterday’s catalogue fitting while the maintenance team expects a ready-to-install copy of a modified spool. Naming the delivery condition avoids that misunderstanding before the new parts arrive.

Inspection points

Agree the acceptance evidence before the first part is released.

Three weld interfaces — Run end A, Run end B, Branch end C
Order documentationTiHubs

Traceable from heat to shipment.

Material identificationGrade + specification
Batch identificationHeat / lot reference
Inspection scopeAgreed tests & results
Shipment identificationMarks + packing list
Illustrative document checklist. Not a certificate or test report.
01Run and branch

Identify ends A, B and C on an isometric

Equal or reducing branch
02NPS 1/2 straight tee, Sch 10S

Catalogue center to face 25.40 mm

OD 21.34 mm; wall 2.11 mm
03NPS 3/4 straight tee, Sch 10S

Catalogue center to face 28.58 mm

OD 26.67 mm; wall 2.11 mm
04End bore

Use the drawing for mismatch acceptance

Compare actual bores at all three joints
05Fitting material

Confirm exact grade and seamless or welded route

ASTM B363 where specified
06Installation envelope

Record orientation and reference planes separately

Run center-to-face and branch center-to-face

Source documents

Check the applicable series, revision and scope against the purchase drawing.

Library PDFs may be earlier editions. Check the document cover and your contractual revision. A reference file does not certify a supplied product.

Explore all downloads ↗

Technical sources

Baoji.
One contact.

TiHubs coordinates titanium sourcing through a local manufacturer network. Your specification guides the supplier review, technical discussion and delivery requirements.

20 yearsTitanium industry experience
100+Baoji factory connections
  1. Clarify the requirement

    Confirm grade, dimensions, state, quantity and the purpose of the stock.

  2. Review the supply route

    Discuss manufacturing, finishing, inspection and documentation with the relevant supplier.

  3. Agree the commercial scope

    Confirm the quotation, lead time, acceptance requirements and delivery terms.

  4. Coordinate inspection & delivery

    Follow the agreed checks, marking, packing and shipment documentation.

Before you order

Specify a titanium butt-weld tee by run and branch size, wall at each end, center-to-face dimensions, material, fabrication route and inspection.

TITANIUM PIPE TEES · BAOJI SOURCING

Send your specification.

Mark the two run ends and the branch on the piping isometric. Send the three end dimensions, centerline position and mating pipe details for a quotation covering the fitting you can actually install.

You do not need to finalize every detail before contacting us.

Start your RFQ

Required fields *

TiHubs — EN — Titanium Pipe Tees — modal