CategoryMaterials & Grade Selection

Titanium or
zirconium 702?

A dip tube, a gasket and a specimen in a beaker can see different environments in the same plant. Specify what the comparison needs to represent before asking for a price.

Chemical equipmentCorrosion assessment
Illustration of metal corrosion coupons beside an empty laboratory vessel and specimen holder
R50400Titanium Grade 2
R60702Zirconium 702
AI illustration; not a production or inspection record.

Quick answer

Compare the two metals against the particular part of the plant that limits service. Match the grade and product form to the order, and choose a sample that represents the metal, finish, weld and location actually exposed. Grade 2 titanium and zirconium 702 can then be compared on a common basis, with published properties kept distinct from measurements returned by the laboratory.

Which metal belongs on the purchase order?

The maintenance crew has removed a corroded dip tube from a chemical tank. On the floor beside it are a spare made years ago, a stained gasket and a sketch labelled “reactive metal.” A distributor offers commercially pure titanium and a fabricator suggests zirconium 702. The first useful exercise is to mark where the old tube was damaged. Was the surface below the liquid level intact while a narrow band near the top was rough? Had metal disappeared under the support clamp? Those observations are more informative than asking which metal is generally more corrosion resistant.

The two candidates here are metallic Grade 2 titanium, UNS R50400, and commercially unalloyed zirconium 702, UNS R60702. Zirconia is zirconium dioxide, a ceramic; it cannot be ordered as a substitute sheet or welded tube under a zirconium metal specification. A requisition copied from a general materials comparison can easily lose that distinction. Put the UNS designation and the required product form together wherever the material is specified, including on sample labels, drawings and the bill of materials. Ask whether a legacy trade name can be linked to a certificate before assigning it to the old component.

For flat stock, ASTM B265 covers titanium and titanium alloy strip, sheet and plate. ASTM B551/B551M covers zirconium and zirconium alloy flat products and identifies the unalloyed grade R60702. These specifications describe mill products; they do not provide a claim about how long the rinse water, acid condensate or cleaning sequence in a particular tank will allow a fabricated item to last. When the order is for a tube, obtain the applicable tubular product specification. A chemistry match to a plate standard does not make a plate certificate into a tube certificate.

What the buyer can establish Grade 2 titanium Zirconium 702
Identity on enquiry and sample register R50400, commercially pure titanium R60702, commercially unalloyed zirconium metal
Flat-product specification for review ASTM B265 ASTM B551/B551M
Reference density used in the example 4.52 g/cm³ from the ATI Grade 2 plate listing 6.51 g/cm³ from the ATI Zircadyne 702/705 physical-property table
Evidence for a welded dip tube Tube and joint records for the actual titanium construction Tube and joint records for the actual zirconium construction

Keep the commercial decision tied to the purchasable item. If the plant needs an unmachined piece of titanium sheet for a test, specify sheet and its traceability. If it needs a replacement assembly, attach the assembly drawing, connection details and the expected acceptance record. A small sheet sample from a convenient heat can answer an initial screening question while leaving the manufacturing scope of the eventual line item completely open. State that distinction on the order so a low-cost coupon trial does not become an accidental approval of a whole assembly.

Divide the vessel into the places the liquid actually touches

Start the service survey with a section through the equipment. Draw the normal and minimum liquid levels, inlet jet, vapour take-off, any cold surface where vapour condenses and the drain point. Show every gasket, support and narrow gap that can hold liquid. Give each region a letter and use the same letters on the failure photographs and proposed specimen positions. The result can fit on one page. It allows a laboratory or supplier to discuss a specific region even if proprietary chemistry must be handled through the owner’s materials engineer.

A bulk liquid sample is convenient to send to a laboratory. Its value depends on the question being asked. A specimen continuously immersed in the sample can represent the submerged wall better than a cold lid receiving drops of condensate. Splash can alternately wet and expose an area, while a crevice can hold solution long after the bulk tank drains. A survey reporting only the average fluid concentration and tank operating temperature misses these distinct exposures. Ask whether the early trial is meant to represent one region or provide evidence for all of them.

Map the process over time as well as space. During a restart the first material through the line may be residual rinse water rather than normal process solution. A standby loop may stagnate. Cleaning may introduce a different chemical or temporarily raise the metal temperature. Give the reviewer the frequency, duration and order of events where available. If a measurement is taken at a remote control point, identify that location. A logged temperature at the storage tank cannot automatically be assigned to the wall beside a heated nozzle.

Manufacturer literature is useful for developing a shortlist. ATI publishes separate zirconium references for several chemical environments. TIMET discusses how titanium’s surface film and local exposure influence corrosion. A chart for an uncontaminated single chemical warrants particular care when real liquor contains traces carried over from an upstream stage. Ask which impurities the analytical sample could actually detect and whether the plant history includes a change in raw material, water source or cleaning agent. Materials specialists can then identify which published comparison is relevant and which conditions call for additional evidence.

Equipment region Information missing from a typical fluid data sheet How to record it for technical review
Submerged straight length Flow pattern, deposits and changes during drain-down Sampling point, level range and time-stamped photograph
Liquid line and splash band Extent of intermittent wetting and drying Mark the band on the recovered part and the vessel sketch
Lid or cold connection Composition and temperature of condensate Separate condensate sample or a recorded reason it could not be obtained
Clamp, gasket or sleeve Materials in contact and geometry of confined liquid Detail view before dismantling, mating part and a section drawing

A useful review may end with a conditional answer. The team could approve a screening trial for the straight submerged length while asking for better information about the clamp. That is progress: purchasing can order the right specimens and engineering retains an explicit open question. It is much harder to recover from a one-line note saying “zirconium approved” when nobody can remember which part of the plant the note referred to.

Cross-section showing submerged wall, liquid line, condensate and a confined contact
Industrial buying guide / 02Four exposure zones in one vessel

A submerged coupon represents only one of these positions. Mark the site where the removed part was damaged.

How to make a comparison the plant can use

A meaningful pair of samples starts with a common question. If the question is whether two parent metals behave differently in the bulk liquid, use comparable exposed geometries and documented surface preparations. If the question concerns a circumferential weld, request representative welded samples and identify the location of the weld and heat-affected zone. A joint exposed horizontally on a bench and a sample suspended in a tank can encounter different drainage, shadowing or deposits. Sketch the actual orientation and explain why it represents the component of interest.

Give each specimen an identifier that survives the test and can be related to its material certificate. Agree whether the location of a hole, wire, hanger or marking introduces a region that must be examined separately. If the material and finish change together between samples, any observed difference may have more than one explanation. Where it matters, plan specimens that allow the variables to be separated. Record any deviations at the time they occur, including a dropped specimen, an altered holder or an interruption in exposure.

Use the test plan to settle practical questions before samples enter the process. Who records the initial dimensions and mass? Who records the solution composition, temperature and position? Will deposits remain in place until an initial photograph is taken? Who decides the cleaning method and how that method could affect the metal? ASTM G31 discusses factors influencing immersion tests, and ASTM G1 addresses preparation, cleaning and evaluation of corrosion specimens. They give the team a common starting point. An acceptance threshold still needs an owner, an appropriate method and a connection to the intended service.

As a drawing exercise, take a plain rectangular specimen measuring 50 × 25 × 2 mm, with no hole, mask or bevel. Its volume is 2,500 mm³, or 2.50 cm³. The exposed area when all six faces are wetted is twice the sum of length times width, length times thickness and width times thickness. That gives 2,800 mm² or 28.00 cm². Counting only the two broad faces gives 25.00 cm². The difference matters when a laboratory divides an observed change by area. This is an illustration of geometry, not a result for either metal.

Quantity calculated for the drawing example Grade 2 titanium Zirconium 702
Solid volume of one specimen 2.50 cm³ 2.50 cm³
Calculated initial mass using the stated density 11.30 g 16.28 g, rounded
Six-face area before suspension or masking 28.00 cm² 28.00 cm²
Broad faces alone 25.00 cm² 25.00 cm²

A real holder may mask part of a face, and a drilled hole removes flat material while introducing a cylindrical surface. Do not copy the table value straight into a test report for a drilled specimen. Have the laboratory state whether its exposed area is measured or calculated and what it excludes. Include a dimensioned sketch with the report. The next person reviewing a series of trials can then understand whether a changed result reflects a change in service or simply a different area convention.

Dimensions of a rectangular 50 by 25 by 2 millimetre specimen, with broad faces and edges identified
Industrial buying guide / 03Account for the narrow faces

Calculated for an unperforated, fully wetted block. A support or hole changes the exposed surface.

What an immersion report can and cannot settle

Read the observations before ranking the numbers. Look for changes in appearance, deposits, staining, local pits, a narrow attack line beside the holder, damage at a weld and differences between the upper and lower faces. Uniform mass loss expresses an average over the reported area. A very small damaged area can be important to a thin-walled component while contributing little to an average. Ask for the position and depth assessment of any local feature the laboratory considers significant. The absence of that information should remain visible when the report goes to purchasing.

A positive mass change deserves interpretation too. Retained oxide or process deposits may add mass; cleaning can remove material as well as deposits. ASTM G1 specifically draws attention to adherent oxide on titanium and zirconium. A raw balance reading with a plus or minus sign, by itself, cannot resolve what has occurred on the substrate. Ask for the initial condition, as-retrieved observations, cleaning history, final measurement and any reference specimen used to assess the procedure. Treat an unresolved mass increase as an open question rather than quietly entering zero corrosion in a comparison sheet.

Consider an illustrative arithmetic check. If a hypothetical clean specimen loses 14 mg over the full 28 cm² in the drawing example, its area-normalized loss is 0.50 mg/cm² for that exposure. If the analyst mistakenly uses only 25 cm², the result becomes 0.56 mg/cm². The mass reading is identical but the second figure is 12% higher. Neither value is a published rate, and neither is a prediction of titanium or zirconium performance. Their purpose is to show why the report must identify the exposed area before an engineer compares two numbers.

A second reporting trap arises when converting mass change into an equivalent average penetration. Equal milligrams per square centimetre on two metals of different density do not imply equal thickness removed. For illustration, the hypothetical 0.50 mg/cm² loss would represent about 1.11 micrometres of uniform Grade 2 titanium or about 0.77 micrometres of uniform zirconium 702 at the densities above. These numbers assume genuine uniform removal of clean metal. They cannot describe local depth, resolve an adherent oxide problem or determine how the next year of operation will proceed.

If a reviewer asks for a lifetime in years, ask which mechanism governs the component, how its condition will be monitored and whether the trial genuinely represents its vulnerable zone. A short stable exposure can support material screening without demonstrating long-term changes in deposits, flushing or operation. Separately record the time basis, measurement uncertainty and actual visual findings. This gives the design authority something more useful than a precise-looking annualized number with no explanation of what the specimen experienced.

Normalized comparison of uniform penetration for an illustrative loss of 0.50 milligrams per square centimetre
Industrial buying guide / 04Equal mass loss, different equivalent depths

The two depths are calculated examples using published densities. No test measurement or service life is implied.

Follow the identity beyond the mill certificate

Suppose the screening work supports further assessment of both candidates. The next document should describe the two fabrication routes for the physical component. For each, list the wetted parts, product forms, drawing revisions, joining methods and any item supplied by the owner. Include the fixture or support if it influences exposure in service. A replacement dip tube may have a machined end, welded attachment, gasketed connection and an area hidden after assembly. One certificate for the tube does not identify every wetted piece in the finished item.

If a trial specimen represented a parent metal, identify which extra evidence is required for the finished joint. The manufacturer may need to propose a procedure and qualification appropriate to the design, base material and joint geometry. Agree how work will be identified and inspected before an inaccessible joint is closed. Collect the records linked to the weld position. If an alternative shop takes over part of the work, retain the link between the original material record, the transfer document and the final assembly mark. That chain matters even when the physical pieces look indistinguishable.

The starting material can change during planning. A supplier may offer plate instead of sheet, propose a different size from stock, or offer to machine a tubular component from solid bar. Every change alters what documents and inspection results are relevant. Ask the supplier to describe the proposed route explicitly. Require the engineering owner to evaluate any effect on wall definition, seams, condition or allowable properties. Once accepted, the revised route belongs on the purchase line and the bill of materials so incoming inspection knows what it will actually receive.

Keep inspection instructions practical. An inspector can match a heat number to a certificate if both are legible. Measuring an internal feature might require access before the final connection is fitted. Checking whether a surface has been contaminated by a previous processing step may need a method agreed in advance. Move these checks to the stage at which evidence can be obtained. Recording the hold point on the fabrication drawing prevents a perfectly assembled part reaching the receiving dock without the only view the owner required.

For an additional lot of test pieces, the Grade 2 titanium material page is a starting point for an enquiry about the titanium side. Identify the requested product form, parent heat, surface condition, number of specimens and whether machining, drilling or joining is included. If the exposure comparison will be performed by an outside laboratory, tell the supplier how the samples must be identified without disturbing the surfaces to be evaluated. This small coordination step can save an entire repeat exposure.

Release the next step that the evidence supports

Use a short decision note with separate entries for each wetted region. Record the candidate, what was reviewed, what remains uncertain, the person responsible for resolving it and the next authorized purchase. The result might be a small coupon order, a prototype, a replacement under an existing approval, or a request for more process data. Put the option and the conditions in the same paragraph. Later readers can then see whether a materials meeting actually approved a production design or only agreed to collect better evidence.

Compare total delivered scope after the technical routes have been identified. A quotation for stock sheet marked and packed for a laboratory differs from one for welded, serialized specimens with measurements and records. For a finished assembly, shipping protection, isolation between dissimilar items and the support during transport can affect whether the delivered component arrives usable. Ask for the planned packaging and for a way to identify the part after unpacking. Treat the inspection package and traceability as deliverables with an agreed due date, rather than documents to request after payment.

Think through the receiving decision using a concrete exception. A shipment arrives with the correct number of coupons, but the labels on two bags have become unreadable. Even if all titanium and zirconium samples could be separated by weight, the receiving team might still be unable to recover the specific heat, finish or weld condition. Isolate the affected pieces and ask the supplier to reconstruct their identity from controlled records. If it cannot do so, do not use them for a trial that depends on that identity. Repeating a small sample order is preferable to basing a plant decision on ambiguous evidence.

For a full production enquiry, send the material designations, drawings, exposure map and relevant test conclusions with the assumptions still attached. Describe which zone and which product condition each finding covers. Identify inspection responsibility, delivery location and whether the offer must include both manufacture and testing. Where TiHubs is being asked for the titanium route only, label the zirconium information as the comparison basis. This keeps budgets, delivery promises and technical decisions tied to the correct supplier and material.

Request traceable specimens or flat stock

State whether this purchase is for comparative test pieces, parent material for an approved fabrication or a finished component. Name the person responsible for technical release and identify the operations and test records to include. When two materials are under review, indicate which one TiHubs should quote and which one appears only as the benchmark.

Information to include

  • UNS and required stock form
  • Wetted zone and orientation
  • Drawing, initial finish and specimen marking
  • Lot identity, quantity and delivery
  • Approver and requested inspection records

Build your RFQ checklist

Choose the product and add the information you have. Copy the resulting brief or send your requirements to TiHubs. Submitting an enquiry does not place an order.

TiHubs — EN — Titanium vs Zirconium 702 in Chemical Equipment: Choosing Samples and Purchasing Plate

Add your details, then copy the checklist or send your requirements to TiHubs.

We use these details to respond to your enquiry. Privacy Policy.

Questions buyers ask

Can a supplier identify the returned specimen from its density alone?

Density can help screen two candidate families if the mass and volume are known accurately. It cannot recover the heat number, distinguish every possible grade or tell you whether the specimen received the same finish as the installed part. Treat an unmarked return as evidence with uncertain identity. Ask for original marking photographs, specimen position records and the machining traveler before deciding whether its result can be associated with a specific heat.

How should a blank control be described in the enquiry?

Tell the laboratory what source of uncertainty the control is intended to investigate. A retained unexposed sibling can document the original appearance and condition. A separate piece taken through a cleaning procedure may help the specialist assess changes introduced by that operation. Agree on quantity and identification before cutting all donated material into exposure specimens. The laboratory can then select suitable controls and account for them in its quotation and report.

Should a small trial order specify the same packaging as production?

Specify packaging to protect the characteristic you need to measure. Individually separated samples may be justified where rubbing would change the finish or transfer foreign residue. If specimens are shipped directly to a laboratory, identify the receiver, the accompanying register and instructions for re-identification after opening the outer package. A production order for full sheets can have different edge protection and lifting requirements, even where the underlying alloy and surface designation are identical.

Who decides whether to move beyond screening?

The plant owner or designated engineering authority should review the trial in the context of the intended component and its exposure. The laboratory can explain what its observations support, the fabricator can identify production variables, and purchasing can reconcile the commercial options. Record the person authorizing a prototype or production order along with the relevant drawing and test references. This avoids interpreting a successful sample delivery as formal acceptance of a different assembly.

Keep the purchase requirements connected.

  1. Map liquid, vapour, splash and contact zones before selecting a representative sample.
  2. Trace both metal and surface condition from the original stock to the retrieved specimen.
  3. Preserve the exposure-area convention whenever mass changes are compared.
  4. Record the limits of the evidence when releasing the next purchase.

Sources and data scope

References reviewed November 20, 2026. Public source summaries support the discussion; the controlled specification, agreed edition and approved project requirements govern acceptance.

  1. ATI Grade 2 titanium — Plate density and UNS identifier.
  2. ATI Zircadyne 702/705 — Physical-property table for metallic zirconium 702.
  3. ASTM B265 — Scope for titanium flat products.
  4. ASTM B551/B551M — Zirconium strip, sheet and plate.
  5. ASTM G31 — Factors influencing laboratory immersion tests.
  6. ASTM G1 — Specimen evaluation and the special problem of adherent oxide.
  7. TIMET corrosion manual — Engineering background on titanium in chemical service.

About TiHubs

TiHubs coordinates titanium material and custom supply enquiries from Baoji, China. Send the product, drawing revision and acceptance requirements so the proposed supply scope can be reviewed. Learn about our sourcing role.

Contents