Conceptual titanium dowel pins with smooth cylindrical locating surfaces and one extraction hole

Dowel pins.
In titanium.

Source titanium locating pins against the assembly drawing. Define the pin and mating hole together, then agree material condition, geometric tolerances, surface requirements and lot inspection.

View specifications
20 years in titanium100+ Baoji factory connections
Fit definition · Precision geometry · Drawing-led supply

Choose the locating construction

Identify the functional cylindrical surfaces, end details and removal requirements.

Straight solid dowel pins

Straight solid dowel pins

Specify the working diameter, length datum and both end profiles. Identify the mating hole limits and whether the pin is retained in one component or removable from both. The word precision does not define an acceptance interval. Send numerical limits or a complete tolerance designation with the applicable drawing convention.

  • Working diameter and limits
  • Length and end geometry
  • Mating-hole relationship

Specify the complete fit

Nominal diameter alone cannot define interchangeability or assembly behavior.

Order itemInclude in your enquiryWhy it matters
FunctionLocation, retention or defined load transferIdentify the design responsibility
DiameterNominal size and upper/lower limitsInclude units and tolerance convention
Mating holeSize limits, material and surface conditionEvaluate the pair, not the pin alone
LengthMeasurement datum and usable engagementDefine end allowance separately
EndsChamfer, radius, flat or other profileControl insertion and bottom clearance
GeometryRoundness, straightness and feature relationshipsUse functional datums
SurfaceFinish, treatment and final inspection stageAccount for dimensional effects
ExtractionThread, depth and access where requiredDo not assume a lifting rating
MaterialGrade, specification and delivered conditionPreserve heat or lot traceability
AcceptanceMethods, sampling and report contentAgree before production

Your starting specification.

TiHubs — EN — Titanium Dowel Pins — inline

Pin drawing and revision; titanium grade and condition; diameter limits; length datum; end geometry; mating hole limits and materials; geometric tolerances; finish; extraction features; assembly method; inspection and sampling; quantity and destination.

Dimensions, material condition, quantity, testing and delivery are confirmed in the quotation and order.

Retain the exact material condition

Grade selection must suit the approved assembly, contact and loading conditions.

Chinese designations and international names are reference routes, not automatic substitutes. Grade, product specification, condition and acceptance requirements must be agreed together.

Open grade cross reference ↗

Connect the pin to its assembly

The same pin dimensions can serve different locating, retention and load-transfer functions.

Fixture and component location

Identify the surfaces and holes that establish assembly position. Explain which component retains the pin and which must separate during maintenance. Include repeated assembly requirements where relevant. Locating accuracy depends on the whole datum scheme and mating features, not solely on a narrow pin diameter tolerance.

What to sendAssembly datums, hole limits and removal sequence.

Corrosion-sensitive assemblies

Specify the actual medium, temperature and mating materials for material review. Keep corrosion selection separate from contact wear and fit design. For a broader drawing-controlled component enquiry, see titanium machined parts and identify whether pins are supplied individually or within an assembly.

What to sendService conditions, contact materials and finish requirements.

Pin stock versus finished pins

A cut length of bar is not automatically a finished locating pin. If procurement covers feedstock, the titanium bar page defines that separate supply route. Finished pins need their own diameter, form, ends, surface and inspection requirements after machining.

What to sendSupply stage, final drawing and inspection responsibility.

Turn a drawing into an inspectable order

Resolve size, form, mating geometry and acceptance before comparing supply routes.

Conceptual illustration of smooth titanium locating pins, including an extraction-hole variant; final geometry follows the drawing.

Specify the working diameter, length datum, end profile and actual cylindrical engagement.

Order geometry schematic; not a dimensional drawing.

Define what the pin must do

Start with the assembly function. A pin may establish relative position, retain a component, carry a defined transverse load or combine several duties. These functions require different evidence. A drawing that controls only the pin diameter does not describe every load case or the position of the mating holes. Identify the responsible design authority and preserve the approved assembly requirements in the enquiry.

Explain whether the pin remains in one component during disassembly and whether repeated insertion is expected. Include access restrictions, cleaning requirements and the intended replacement method. A pin that works in a permanent assembly may be inconvenient in a fixture that is opened frequently. These operating details help the supplier review end geometry and extraction features without redesigning the assembly by assumption.

Do not use titanium as a stand-alone performance specification. The selected alloy, delivered condition, contacting materials, geometry and environment all matter. If the original design uses hardened steel, replacing it with a titanium pin of identical nominal size is a material change requiring review. Matching dimensions does not establish equivalent stiffness, surface hardness, wear behavior or permissible load.

Read a standard designation within its scope

ISO 2338 identifies parallel pins of unhardened steel and austenitic stainless steel. ISO 8734 identifies hardened steel and martensitic stainless steel dowel pins. Their titles matter when preparing a titanium enquiry: adopting a dimensional pattern does not make a titanium part fully compliant with a steel-material standard. State the adopted dimensional requirements and the separately approved material requirements instead of making an unsupported blanket conformity claim.

ASME B18.8.2 addresses several inch-series pin constructions. Its catalogue also notes that included sizes do not imply stock availability. Where a drawing invokes this standard, retain the edition and applicable construction. Do not assume that a metric designation, an inch designation and a supplier catalogue description represent the same end geometry or length convention.

The purchase order should identify which document governs if requirements differ. A buyer drawing may set the titanium material, selected dimensions and additional inspection while referring to a standard for specific features. Make those references precise. Resolve conflicts before production so receiving inspection does not have to decide retrospectively whether a catalogue value or the drawing takes precedence.

Calculate fit from both size intervals

Use the pin and hole limits together. Let Dmin and Dmax represent the smallest and largest permitted hole diameters, and dmin and dmax the corresponding pin limits. At the size-limit level, minimum diametral clearance is Cmin = Dmin − dmax and maximum diametral clearance is Cmax = Dmax − dmin. Use the same units and reference conditions for all four values. Negative clearance denotes interference in this sign convention.

These equations compare permitted sizes, not installation forces or actual three-dimensional surface contact. If the whole clearance interval is positive, the size limits provide clearance. If the whole interval is negative, they provide interference. If it spans negative and positive values, the permitted size combinations include both possibilities. Zero at a boundary is a limiting line-to-line case that should be handled under the selected fit definition.

ISO 286 provides the terminology and code system for linear-size tolerances and fits. When the drawing uses a designation such as a hole and shaft tolerance class, obtain the applicable limits for the actual nominal-size interval and edition. Do not reuse numerical deviations from another diameter band. Record the resolved limits in the inspection plan to prevent a letter-and-number callout from being interpreted differently by buyer and supplier.

Fit information and its limits

Symbolic size-limit relationships, not advertised manufacturing tolerances or a stock-size table.
InformationWhat it establishesWhat still needs review
Pin size intervalPermitted finished diameter limitsRoundness, straightness and surface requirements
Hole size intervalPermitted mating-hole size limitsHole form, location and assembly alignment
Cmin = Dmin − dmaxSmallest signed diametral clearance by size limitsActual contact and installation method
Cmax = Dmax − dminLargest signed diametral clearance by size limitsLocation accuracy of the complete assembly
Fit designationA standardized way to identify size intervalsCorrect nominal-size range and applicable edition

Keep size and geometric controls distinct

A diameter measurement does not establish every aspect of cylindrical form. A pin can require separate controls for roundness, straightness or the relationship between two working diameters. Likewise, a hole may meet its size limits while its orientation or position prevents the intended assembly. Use the selected geometric-dimensioning system consistently and identify the functional datums on the drawing.

Choose controls because they support a function. A long locating surface, a stepped pin and a short simple dowel may need different inspection arrangements. Avoid adding very tight geometric tolerances without explaining the mating relationship; doing so can increase cost without addressing the feature that actually controls assembly. Conversely, an unspecified form requirement should not be assumed to follow automatically from a small size tolerance.

Review the acceptance method alongside the drawing. Two-point diameter checks, functional gauges and form measurement answer different questions. Agree which features each method verifies and how the result is reported. If a functional gauge is required, identify its definition and acceptance use rather than asking the supplier to interpret an unnamed shop fixture as a universal conformity test.

Define the usable length and end profile

State how length is measured and distinguish overall length from the cylindrical engagement available to locate the mating component. Chamfers, radii and other end details can occupy part of the total length. The required engagement should therefore be checked against the actual end profile and assembly depth, not inferred from an overall-length figure alone.

For blind holes, define the required bottom clearance and the permitted seated position. Include any shoulder or stop that establishes the final location. A pin that bottoms before the intended surface seats can give an apparently firm assembly while leaving the functional relationship incorrect. The drawing should make the intended contact surfaces visible so manufacturing and inspection use the same reference.

Specify end geometry with dimensions or an applicable drawing reference. A general request for easy insertion does not determine a chamfer angle, edge radius or acceptable burr condition. Review the entry geometry of the mating hole as well. End treatment should support the approved assembly process without reducing functional engagement or concealing a mismatch in the diameter limits.

Plan insertion, venting and extraction

Define how the pin is installed and removed, including access to the opposite end. If the hole is blind, review how trapped air, liquid or assembly compounds are managed. Any vent, relief or extraction feature must be part of the approved design. Do not add a groove or drilled passage informally if it changes the functional surface, cleanliness requirement or remaining section.

Where an extraction thread is specified, state its thread designation, usable engagement, depth and inspection requirement. Describe the intended pulling arrangement and access around the pin. A thread intended for maintenance extraction should not be represented as a certified lifting point. The permissible removal method and any load limitations belong to the approved assembly instructions.

Keep installation-force assumptions separate from a simple fit calculation. Interference, surface state, contact length, material response and the assembly method can influence the process. The size-limit equations alone do not provide a press-force guarantee. For a new assembly, agree the trial conditions and the observations required before releasing repeat production.

Review the contact pair and final surface

Identify both mating materials and their final surface conditions. Titanium selection for corrosion service does not automatically resolve friction, adhesive wear or galling in a close contact. Where sliding or repeated assembly is expected, the design review should address the actual contact pair and the approved surface or lubrication requirements. Do not prescribe a universal lubricant without considering the service environment and cleanliness constraints.

Any coating or treatment must be included in the dimensional definition. Specify whether diameter acceptance applies before or after the final operation and which layer thickness or surface characteristics are controlled. A dimensional report on an unfinished pin cannot establish the final delivered fit if a later process changes the working surface.

Define surface texture in the drawing convention used by the project and identify the relevant functional area. A polished appearance is not a complete texture specification. Also address handling damage: a local raised mark on a precision working diameter can affect assembly even when the bulk material and nominal dimensions are correct. Packaging should protect the locating surfaces through transport and storage.

Treat temperature as part of the measurement basis

The drawing and inspection plan should identify the reference conditions used for dimensional acceptance. The pin, mating component and measuring equipment may not be at the same temperature immediately after machining, handling or transport. For a close fit, uncontrolled measurement conditions can create disagreement that is not resolved by repeating the same reading on another warm part.

Distinguish acceptance at the specified reference condition from the fit during service. Different materials and temperature changes can alter the relationship between the pin and hole. Any thermal fit calculation must use applicable material data, geometry and temperature ranges; a room-temperature clearance result alone does not qualify the assembly throughout operation.

When a service-temperature review is needed, supply both component materials and the expected temperature conditions to the responsible designer. Record the resulting requirements in the drawing or assembly specification. The supplier should receive a defined finished-part acceptance basis rather than an instruction to achieve an unspecified fit at every temperature.

Match metrology to the specified feature

Agree the measurement locations and method for diameter, length and geometric characteristics. A single reading at one end of a pin may not represent its complete working surface. The inspection plan should explain how the selected measurements address the drawing requirements and how parts with special features are supported without distorting or obscuring the result.

Instrument resolution alone is not proof that a measurement process is suitable. Consider the method, calibration status, environment and uncertainty relative to the acceptance requirement. If a limit is difficult to resolve reliably, agree an appropriate decision rule and method before production. This is more useful than receiving a report with many decimal places but no explanation of how the result was obtained.

Material identification and dimensional inspection should remain linked through the lot record. A chemistry record does not measure straightness; a dimensional report does not identify the alloy. Specify the documents needed for each purpose and ensure they refer to the delivered parts. If direct marking would damage a functional surface, agree package identification or another suitable traceability method.

Separate locating accuracy from load capacity

A close fit can support repeatable location, but it does not by itself establish a permissible pin load. If the pin transfers force, the design must consider the actual arrangement, engagement and loading direction. Material properties from a bar data sheet should not be copied into a finished-pin capacity table without an applicable design and test basis.

Specify any required finished-part or assembly tests with their conditions and acceptance criteria. Identify whether the test concerns material properties, a particular shear arrangement, retention or repeated assembly. Results from different fixtures or load paths should not be compared as interchangeable values. Keep typical data, calculated design values and measured acceptance results clearly identified.

For an existing approved assembly, retain the required material and source controls. A proposed alternative grade, condition or geometry should be submitted as a deviation for the responsible review. Procurement can compare the cost and lead time of a proposal while still keeping the original technical requirement visible.

Control samples, lots and repeat orders

For first-piece approval, agree the sample identity, drawing revision, material condition and inspection report in advance. If assembly trials are required, use representative mating components and document their condition. An accepted fit with one selected hole does not automatically demonstrate interchangeability across every permitted pin-and-hole size combination.

After approval, preserve the manufacturing and acceptance definition for repeat orders. Record changes in material condition, finishing route, dimensions or inspection method and review them before supply. Keep trial pieces and production lots distinguishable. A sample approval should lead to a controlled production specification rather than a permanent instruction to copy an unlabeled reference part.

Receiving inspection should protect that control. Separate similar-looking pins by part number, revision and lot, especially where diameter differences are small. Preserve package identity when quantities are divided for assembly. If a fit problem occurs later, the records should allow the actual pin batch and mating component to be identified rather than requiring assumptions based on appearance.

Send a quotation package that can be compared

Provide the pin drawing and revision, grade and condition, diameter limits, length convention, end geometry and any extraction details. Include the mating-hole limits, component materials and assembly function. State the quantity, delivery destination, required records and whether the request concerns prototypes, first-piece approval or established production. Mark unresolved requirements clearly for technical review.

Ask suppliers to identify deviations and exclusions separately from price. Compare the same finished condition, inspection scope and documentation. A quotation for machined pins with measured final diameters is a different scope from a quotation for cut bar blanks, even if both use the same alloy and approximate dimensions. Confirm which party performs any remaining finishing or assembly trial.

TiHubs can review titanium dowel-pin drawings through its Baoji sourcing network. The useful outcome is a defined supply proposal with material, geometry, inspection and open technical questions made explicit. Confirm that proposal against the approved assembly requirements before ordering. This supports a repeatable purchasing decision without presenting unverified fits, stock sizes or load ratings as guaranteed product capabilities.

Measure the features that control assembly

Diameter, form, position and surface condition require appropriate inspection methods.

Illustrative acceptance map for pin size, form, surface and traceability; not a measurement report.
Order documentationTiHubs

Traceable from heat to shipment.

Material identificationGrade + specification
Batch identificationHeat / lot reference
Inspection scopeAgreed tests & results
Shipment identificationMarks + packing list
Illustrative document checklist. Not a certificate or test report.
01Material identity

Connect grade and condition to the delivered lot.

Material record
02Diameter limits

Verify the finished working surface against stated limits.

Size acceptance
03Geometry

Check the specified form and feature relationships.

Functional geometry
04Ends and length

Use the defined datum and end profile.

Engagement control
05Surface condition

Inspect after the required final operations.

Delivered fit
06Lot records

Preserve identity, sampling and measurement evidence.

Repeatable supply

Separate dimensions from material approval

Use standards within their scope and keep any titanium-specific departures explicit.

Library PDFs may be earlier editions. Check the document cover and your contractual revision. A reference file does not certify a supplied product.

Explore all downloads ↗

Technical sources

Baoji.
One contact.

TiHubs coordinates titanium sourcing through a local manufacturer network. Your specification guides the supplier review, technical discussion and delivery requirements.

20 yearsTitanium industry experience
100+Baoji factory connections
  1. Clarify the requirement

    Confirm grade, dimensions, state, quantity and the purpose of the stock.

  2. Review the supply route

    Discuss manufacturing, finishing, inspection and documentation with the relevant supplier.

  3. Agree the commercial scope

    Confirm the quotation, lead time, acceptance requirements and delivery terms.

  4. Coordinate inspection & delivery

    Follow the agreed checks, marking, packing and shipment documentation.

Before you order

Resolve the mating geometry and inspection basis before choosing a finished titanium locating pin.

TITANIUM DOWEL PINS · BAOJI SOURCING

Send your specification.

Source titanium locating pins against the assembly drawing. Define the pin and mating hole together, then agree material condition, geometric tolerances, surface requirements and lot inspection.

You do not need to finalize every detail before contacting us.

Start your RFQ

Required fields *

TiHubs — EN — Titanium Dowel Pins — modal