Gr9 · TA18 · Ti-3Al-2.5V · UNS R56320
Grade 9 / TA18 titanium.Built around your requirements.
Ti-3Al-2.5V seamless tubing for aerospace hydraulic lines and premium bicycle frames, plus sheet, bar and wire. TiHubs coordinates your material, inspection and delivery requirements through one contact in Baoji.
Start with a specification, drawing or application. We’ll help identify the details still needed.
Material review. Supply coordination.
One contact in Baoji, China.
01 / Product forms
Find your
Grade 9 / TA18 product.
Select a starting form. We review dimensions, condition, inspection and delivery before confirming a suitable supply route.
Grade 9 / Gr9 · TA18 · Ti-3Al-2.5V
Grade 9 / TA18 seamless titanium tube & pipe
Gr9 tube combines low mass with useful strength and formability. Start with the intended service: hydraulic line, frame tube, heat-transfer tube or process pipe. Each needs its own specification and acceptance scope.
- Specification
- ASTM B861-10 Grade 9 for seamless pipe; ASTM B338-08b for heat-exchanger tubing; GB/T 3624-2023 for TA18 seamless tubes. Aerospace requests use the specified AMS route.
- Dimensions
- OD × wall thickness × length; minimum wall or nominal wall basis, ID, ovality, straightness and end condition.
- Condition
- State annealed or cold-worked and stress-relieved where permitted by the selected specification. Include later bending, flaring or welding.
- Acceptance
- Heat and lot records, dimensional checks and specified surface, NDT, pressure or leak testing. A pipe standard does not establish aerospace acceptance.
Grade 9 / Gr9 · TA18 · Ti-3Al-2.5V
Grade 9 / TA18 titanium sheet & plate
For formed details, welded assemblies and drawing-based industrial components. State whether the material will be cut, bent, drawn or machined so condition, surface and usable size can be reviewed.
- Specification
- ASTM B265-08 Grade 9, or TA18 to GB/T 3621-2022. Confirm the product form and thickness-dependent requirements.
- Dimensions
- Thickness × width × length; thickness tolerance, flatness, rolling direction, cut-edge requirements and quantity per size.
- Condition
- Required delivery condition and surface finish; forming sequence and any subsequent heat treatment.
- Acceptance
- Chemical and mechanical records, heat identity, dimensions and additional inspection required by the drawing.
Grade 9 / Gr9 · TA18 · Ti-3Al-2.5V
Grade 9 / TA18 titanium bar & rod
Machining stock for sleeves, fittings, shafts and custom components. Coordinate bar condition with the finished-part drawing, machining allowance and inspection requirements.
- Specification
- ASTM B348-08a Grade 9 or TA18 to GB/T 2965-2023. Specify bar or billet and the required supply condition.
- Dimensions
- Diameter or section × usable length; diameter tolerance, straightness and allowance for machining.
- Condition
- Annealed or other permitted condition; turned, ground or agreed surface finish.
- Acceptance
- Heat traceability, material certificate, mechanical tests and any required ultrasonic or other inspection.
Grade 9 / Gr9 · TA18 · Ti-3Al-2.5V
Grade 9 / TA18 titanium wire
For specified forming and component-manufacturing requirements. Identify the end use early: general wire and welding consumables have different chemistry, surface and qualification requirements.
- Specification
- ASTM B863-19 Grade 9 or the applicable TA18 requirements of GB/T 3623-2022. Confirm intended use and product-specific chemistry.
- Dimensions
- Diameter and tolerance, coil or straight length, coil weight, length accuracy and quantity.
- Condition
- Supply condition, surface cleanliness, straightness and packaging suitable for the subsequent process.
- Acceptance
- Heat or lot identification, chemical and mechanical records and diameter checks. Welding filler needs the required consumable classification and procedure review.
Grade 9 / Gr9 · TA18 · Ti-3Al-2.5V
Ti-3Al-2.5V aerospace hydraulic tubing
A core Grade 9 alloy application: lightweight seamless tube for specified aircraft hydraulic lines. Send the released material callout and approval requirements before selecting a supply route.
- Specification
- AMS 4943L: annealed. AMS 4944H: cold worked and stress relieved. AMS 4945H: cold worked and stress relieved with controlled contractile strain ratio.
- Dimensions
- OD × wall × length; tolerances, bend radii, end-forming or flare details, fitting interfaces and usable straight lengths.
- Condition
- Keep annealed and CWSR conditions separate. Contractile strain ratio, texture or other directional requirements must be stated where specified.
- Acceptance
- Required material source, heat/lot traceability, NDT and test records, tube cleanliness and end protection. Material conformity alone is not approval for aircraft installation.
Grade 9 / Gr9 · TA18 · Ti-3Al-2.5V
Grade 9 / TA18 titanium bicycle frame tubing
Ti-3Al-2.5V is used for premium road, gravel, touring and mountain-bike frame tubes. The frame builder’s geometry, wall profile, joining process and validation plan define the useful purchase specification.
- Specification
- Specify Grade 9 / Gr9 or TA18, the agreed tube material standard and the frame-builder drawing. A material standard does not certify a completed bicycle frame.
- Dimensions
- Tube-by-tube OD, wall and cut length. For butted tubes, give end walls, centre wall, butt lengths, transition positions and miter allowances.
- Condition
- Straight-gauge, butted, tapered, ovalized or bent requirements are reviewed for feasibility. State condition and surface finish before forming or welding.
- Acceptance
- Wall-profile and straightness checks, surface condition, lot traceability and prototype acceptance. Frame fatigue, impact and assembly validation remain part of the finished-frame programme.
Grade 9 / Gr9 · TA18 · Ti-3Al-2.5V
Gr9 / TA18 tubing for marine & offshore projects
Review Grade 9 tubing for specified seawater-contact equipment, hydraulic lines and offshore control or process systems where mass and corrosion resistance matter. Suitability depends on the actual fluid and duty.
- Specification
- ASTM B861-10 Grade 9 seamless pipe or TA18 to GB/T 3624-2023, with the project’s additional design, testing and documentation requirements.
- Dimensions
- OD, wall, length, coil or straight delivery, bend geometry and interface dimensions.
- Condition
- Agree the delivery condition and forming route; identify later welding, assembly or pressure testing.
- Acceptance
- State fluid composition, pressure, temperature, cyclic duty and any sour-service or operator requirements. No blanket seawater, sour-service or offshore approval is implied.
Grade 9 / Gr9 · TA18 · Ti-3Al-2.5V
Grade 9 titanium heat-exchanger tube & process pipe
For equipment designers comparing tube strength, wall thickness, corrosion conditions and fabrication needs. Define tube supply separately from the requirements for a completed exchanger or piping assembly.
- Specification
- ASTM B338-08b Grade 9 for condenser/heat-exchanger tubes; ASTM B861-10 Grade 9 for seamless pipe. TA18 seamless tube uses GB/T 3624-2023 where specified.
- Dimensions
- OD × wall × length, tube-sheet interface, straightness, end preparation and any drawing-based bends.
- Condition
- Required material condition and surface; tube expansion, joining and fabrication requirements.
- Acceptance
- Agreed chemistry, tensile, dimensional and NDT records; required pressure/leak tests and the equipment design code. Tube material certification is not equipment certification.
Images illustrate product forms and application possibilities. Markings show material specification options; they do not establish stock, dual certification or approval of a completed hydraulic system, bicycle frame or pressure assembly.
Need more than straight tubing?
Send the finished geometry and acceptance requirements for a feasibility review.
01 / Custom requirement
Tube bending & end forming
Bends, flares and formed ends need a controlled drawing. Include bend radius, wall thinning, ovality limits, end geometry and any post-forming checks.
02 / Custom requirement
Frame tube sets & butted profiles
Send a bill of materials for top, down and seat tubes, chainstays and seatstays. Define each profile, transition and allowance; prototype approval comes before a production commitment.
03 / Custom requirement
Machined connectors & assemblies
For sleeves, fittings, spacers and joined assemblies, include the part drawing, mating materials, surface condition and the applicable component or assembly standard.
02 / Material identity
What is Grade 9 / TA18 titanium?
Grade 9 titanium, also written Gr9 or Gr. 9, is Ti-3Al-2.5V (UNS R56320): a titanium alloy with nominally 3% aluminium and 2.5% vanadium. TA18 is the Chinese Ti-3Al-2.5V designation. Its combination of strength, cold formability and weldability makes tubing a central application.
Specify the designation together with the product standard, revision and delivery condition. Grade 9 and TA18 belong to the same nominal alloy family; their specification limits and acceptance requirements must still be checked for the order.
Published minimum tensile strength
Annealed Ti-3Al-2.5V reference
Published minimum yield strength
Annealed Ti-3Al-2.5V reference
Published minimum elongation
Annealed Ti-3Al-2.5V reference
| Property / condition | Reference | Purchasing implication |
|---|---|---|
| Density | Approximately 4.48 g/cm³ | Useful for preliminary mass calculations; finished tube weight also depends on dimensions and tolerances. |
| Annealed | 620 MPa UTS · 483 MPa YS · 15% elongation | TIMET published minimum reference. Product-form, dimension and test requirements govern the order. |
| Cold worked, stress relieved (CWSR) | 862 MPa UTS · 724 MPa YS · 10% elongation | TIMET published minimum reference for this condition. Do not substitute it for an annealed requirement or use it as a universal Grade 9 guarantee. |
| TA18 seamless tube | GB/T 3624-2023, annealed: ≥620 MPa UTS, ≥483 MPa YS, ≥15% elongation | Tube values are not automatically the values for TA18 sheet, bar or wire. Review the relevant product table. |
| Aerospace hydraulic tube | AMS 4943L / 4944H / 4945H | Condition, dimensions, inspection and any contractile strain ratio requirements must match the specified AMS revision. |
Source: TIMET TIMETAL 3-2.5 technical data ↗ and the supplied GB/T 3624-2023 file. Reference values are not pressure ratings, fatigue allowables or finished-part design approval.
| Element | Symbol | Grade 9 reference, wt % | TA18 designation reference, wt % |
|---|---|---|---|
| Aluminium | Al | 2.50–3.50 | 2.0–3.5 |
| Vanadium | V | 2.00–3.00 | 1.5–3.0 |
| Iron | Fe | ≤0.25 | ≤0.25 |
| Oxygen | O | ≤0.15 | ≤0.15 |
| Carbon | C | ≤0.08 | ≤0.05 |
| Nitrogen | N | ≤0.03 | ≤0.05 |
| Hydrogen | H | ≤0.015 | ≤0.0125 |
| Other elements, each | — | ≤0.10 | ≤0.10 |
| Other elements, total | — | ≤0.40 | ≤0.30 |
| Titanium | Ti | Balance | Balance |
Grade 9: TIMET technical data and the supplied ASTM material references. TA18: GB/T 3620.1-2016 designation table. Product standards can add or change requirements for a particular use: review, for example, the wire requirements in GB/T 3623-2022. A shared Ti-3Al-2.5V name does not establish compliance with both columns.
Grade 9 / Gr9 and TA18
These names identify the nominal Ti-3Al-2.5V family under different specification systems. Order ASTM Grade 9, the required AMS alloy specification, or Chinese TA18 explicitly. Dual conformity requires comparison and supporting records.
Grade 9 versus Grade 5
Ti-3Al-2.5V is commonly selected for formable, weldable tubing. Ti-6Al-4V serves a different strength and manufacturing balance. Choose by the drawing, fabrication route and service requirements, not grade number alone.
Annealed versus CWSR
Cold work and stress relief can raise tube strength. The resulting tube still needs the specified forming, dimensional and test properties. Do not assume the same bend or end-forming process works in both conditions.
TA18 is not ASTM Grade 18
Chinese TA18 is Ti-3Al-2.5V. ASTM Grade 18 is a separate palladium-bearing titanium designation. Keep the standard system beside the grade in every RFQ and material record.
03 / Aerospace, bicycle & industrial applications
Grade 9 tubing. Two demanding applications.
Aerospace hydraulic lines and premium bicycle frames both use Ti-3Al-2.5V, but they need different purchasing details. Start with the application, then define the material and acceptance requirements.
Application review / 01
Grade 9 aerospace hydraulic tubing
Ti-3Al-2.5V seamless tubing is used for aircraft hydraulic lines where low mass, strength and fabrication capability matter together. A hydraulic line also sees pressure cycling, vibration, bends and fitting loads, so the material callout must be read with the assembly drawing.
Products to discuss
Annealed tube to AMS 4943L, CWSR tube to AMS 4944H, or controlled-contractile-strain-ratio tube to AMS 4945H when specified. Straight stock, bent lines and fitted assemblies are separate supply scopes.
What we need to review
Send the required AMS revision, OD and wall, delivery condition, pressure and temperature context, bend/end details, approved-source restrictions, inspection requirements and traceability package.
Application review / 02
Grade 9 / TA18 tubing for premium bicycle frames
Ti-3Al-2.5V is an established bicycle tube material. A successful frame tube set balances mass, stiffness, forming, joint design and fatigue requirements. The useful enquiry is a tube schedule or drawing, rather than a request for the thinnest possible wall.
Products to discuss
Top, down and seat tubes plus chainstays and seatstays; straight-gauge or specified butted and shaped profiles subject to feasibility review. The frame image illustrates an application.
What we need to review
Identify frame type, tube-by-tube dimensions, butt profile, transition lengths, orientation, miter allowance, bending and ovalization, finish and prototype/production quantities. Define who validates the finished frame.
Application review / 03
Formed tubes for lightweight structures
Use Grade 9 / TA18 when the drawing calls for a strength and fabrication balance suited to thin-walled members. Stiffness and buckling depend strongly on the section geometry and cannot be established from tensile strength alone.
Products to discuss
Round or drawing-based tube profiles, bent members and connecting details.
What we need to review
Loads, unsupported lengths, joints, forming limits, tolerances and the structural acceptance plan.
Application review / 04
Tubing for defined offshore service
Grade 9 tubing can be considered where the project requires titanium’s corrosion behaviour together with alloy strength. Fluid chemistry, temperature, crevices, joining and service loading need a project-specific review.
Products to discuss
Seamless pipe, straight tube and project-specified coiled or formed lines.
What we need to review
Fluid composition, chloride or sour-service conditions, design pressure and temperature, fitting materials, cyclic duty and operator documentation requirements.
Application review / 05
Grade 9 heat-transfer tubes
For a heat exchanger, evaluate the material together with wall thickness, tube-sheet connection, fluid exposure and fabrication. Grade 9 is an option when the equipment design calls for its strength and corrosion behaviour.
Products to discuss
Heat-exchanger tubing to the specified ASTM B338 Grade 9 requirements; TA18 seamless tube under the specified Chinese route.
What we need to review
Tube size, length, straightness, surface condition, joining/expansion method, inspection and required pressure or leak testing.
Application review / 06
Seamless pipe for specified process systems
A process line needs an agreed material standard and a separate design basis for pressure, corrosion, joints and supports. Avoid treating a tube material certificate as approval of an assembled pressure system.
Products to discuss
ASTM B861 Grade 9 seamless pipe and drawing-based fittings or spools under an agreed fabrication scope.
What we need to review
Fluid and temperature range, pressure/cyclic duty, pipe dimensions, end preparation, welding, NDT, test records and design-code requirements.
Application review / 07
TA18 / Grade 9 formed sheet components
Sheet and plate are starting forms for specified formed or welded components. Review thickness, rolling direction and surface before defining the blank or forming route.
Products to discuss
Sheet, plate and cut blanks; forming or joining reviewed against the drawing.
What we need to review
Blank dimensions, bend geometry, allowable thinning, joining process, final condition, surface and acceptance criteria.
Application review / 08
Material matched to your manufacturing process
Bar and wire requirements should reflect the intended machining or forming operation and the final component’s inspection needs. State any separate consumable or component classification.
Products to discuss
Bar for machined sleeves and fittings; wire for defined forming or component manufacture.
What we need to review
Drawing revision, critical tolerances, delivery condition, material records, surface requirements and lot quantities.
Aerospace hydraulic tube / procurement detail
Specify the tube. Control the hydraulic-line requirements.
The three supplied AMS files describe distinct material conditions. We review your exact drawing callout before discussing manufacturers, quotation and the inspection package.
Start with the controlling revision
AMS 4943L is the annealed route. AMS 4944H covers cold-worked, stress-relieved tube. AMS 4945H adds controlled contractile strain ratio to a CWSR route. Do not switch between them based only on alloy composition or a higher tensile value.
Connect geometry with fabrication
Give OD, wall, tolerances and finished length, plus bend radii, flare or end-forming details and fitting interfaces. Identify the required condition after forming and any limits on wall thinning, ovality or surface damage.
Define evidence and delivery condition
List required material-source approvals, heat/lot traceability, tensile and dimensional records, NDT and applicable pressure or leak tests. Agree internal cleanliness, end caps, identification and protective packaging for delivery.
Example RFQ: aerospace hydraulic seamless tube
“Ti-3Al-2.5V seamless hydraulic tube to AMS 4944H; OD × wall × length; quantity; drawing and revision; CWSR condition; required dimensional/NDT/test records; source restrictions; internal cleanliness and end caps; destination and required date.”
Replace the specification with your released callout. If AMS 4945H is required, retain its controlled contractile strain ratio requirements. A raw-tube order and a finished bent, fitted or qualified hydraulic assembly are separate scopes.
Premium bicycle frame tube / procurement detail
Build a tube set around the frame design.
Grade 9 / TA18 tube supply begins with the frame builder’s bill of materials. Geometry, wall distribution and fabrication affect the finished frame as much as the alloy designation.
Specify each frame member
List the top tube, down tube, seat tube, chainstays and seatstays separately. Include OD, wall, cut length, straightness and the required orientation of bends or ovalized sections. Head-tube and bottom-bracket interfaces need their own dimensions and material callouts.
Define the butted profile
For a single-, double- or other specified butted tube, show the end and centre walls, butt lengths and transition locations. Include miter and forming allowances so a later cut does not remove the intended thicker joint region. Availability and tooling are confirmed after review.
Agree prototype acceptance
Define wall-profile measurement, surface checks, trial forming, joint preparation and prototype quantities. Frame fabrication needs an appropriate titanium welding and shielding procedure. Finished-frame fatigue, impact and assembly tests belong to the frame manufacturer’s validation plan.
Example RFQ: Grade 9 titanium bicycle frame tube set
“Grade 9 / Ti-3Al-2.5V seamless frame tubing, or TA18 to the agreed specification; road/gravel/MTB frame; tube schedule attached; OD and end/centre wall profile; butt and cut lengths; bend/ovalization drawings; surface finish; prototype quantity and projected batch quantity; inspection records; destination.”
ASTM B338 is a condenser/heat-exchanger tube standard. If used as part of a frame builder’s material purchase requirement, it still needs the agreed geometry, condition and inspection details; it does not certify a bicycle frame.
04 / Standards & documentation
Match the standard
to the product.
Choose the specification for the actual product. Grade 9 / Gr9, AMS Ti-3Al-2.5V and Chinese TA18 requirements are presented together so you can identify the correct order route.
| Product form | ASTM / AMS route | Chinese standard route | Clarify before quotation |
|---|---|---|---|
| Material identity & composition | United StatesGrade 9 / Gr9 · Ti-3Al-2.5V · UNS R56320
Apply the chemistry required by the selected ASTM or AMS product standard. |
ChinaGB/T 3620.1-2016 View PDF ↗ | Name the standard system. TA18 is not ASTM Grade 18; dual conformity requires supporting records. |
| Aerospace hydraulic tube | United StatesAMS 4943L View PDF ↗AMS 4944H View PDF ↗AMS 4945H View PDF ↗ | ChinaTA18 material designation
GB/T 3624-2023 may be a specified tube route, but it does not replace an AMS callout or an aircraft approval requirement. |
Exact AMS revision, annealed/CWSR condition, contractile strain ratio where required, dimensions, NDT, cleanliness and source approvals. |
| Seamless tube & pipe | United StatesASTM B861-10 View PDF ↗ | ChinaGB/T 3624-2023 View PDF ↗ | Pipe/tube dimensional basis, OD, wall, length, condition, testing and intended service. |
| Heat-exchanger tubing | United StatesASTM B338-08b View PDF ↗ | ChinaGB/T 3624-2023 View PDF ↗ | Tube versus completed equipment; dimensional, surface, joining and pressure/leak-test requirements. |
| Bicycle frame tubing | United StatesGrade 9 + agreed tube specification
ASTM B338 can form part of a material purchase specification; it is not a bicycle-frame standard. |
ChinaGB/T 3624-2023 View PDF ↗ | Frame-builder tube schedule, wall profile, butted transitions, forming and prototype acceptance. |
| Sheet & plate | United StatesASTM B265-08 View PDF ↗ | ChinaGB/T 3621-2022 View PDF ↗ | Thickness, width, length, condition, rolling direction and agreed inspection. |
| Bar & rod | United StatesASTM B348-08a View PDF ↗ | ChinaGB/T 2965-2023 View PDF ↗ | Section, usable length, straightness, condition, surface and inspection. |
| Wire | United StatesASTM B863-19 View PDF ↗ | ChinaGB/T 3623-2022 View PDF ↗ | Diameter, coil or straight form, condition, surface and intended manufacturing or consumable use. |
Publisher scope references: SAE AMS 4943L ↗ · SAE AMS 4944H ↗ · SAE AMS 4945H ↗. Material specifications and finished-system approvals are separate requirements.
05 / Order coordination
Know the scope
before ordering.
Our founder’s 20 years in titanium inform the questions we ask before quotation and the supply options we review with you.
A quotation you can evaluate
Agree the grade, standard edition, dimensions, tolerance, condition and quantity before comparing prices.
- Identify whether inspection, samples and tooling are included.
- Confirm packaging, transport and delivery terms.
- Record items that still need technical confirmation.
Acceptance agreed before supply
Confirm material certificates, heat and production-lot identity, delivery condition, dimensions and required testing before supply. Hydraulic tube orders may also call for NDT, contractile strain ratio and cleanliness records; frame tubes may need wall-profile and prototype checks.
Independent inspection can be discussed with its scope, timing, acceptance criteria and cost agreed for the order.
Delivery with clear milestones
Review the proposed lead time, approvals, production sequence and dispatch requirements. For several product forms, coordinate document and packing readiness together.
Material substitutions and technical changes require written approval. A schedule deviation should identify the impact, decisions needed and next steps.
One contact when an issue arises
Contact TiHubs with the order reference, affected items and supporting photos or inspection records.
We record the issue, review it against the agreed requirements and coordinate the next steps with the relevant manufacturing parties.
Material records
Grade, standard, test results and heat or batch identity matched to the supplied items.
Inspection records
Dimensional, wall-profile and agreed test records linked to the supplied tube, bar, sheet or wire lots.
Dispatch records
Item identification, packing list, protective packaging and required shipment documents.
06 / Questions before sourcing
Before you specify
Grade 9 / TA18.
A clear material designation is the beginning. Product form, specification revision, material condition and acceptance complete the requirement.
A useful first enquiry
- Product and specificationGrade 9 / Gr9 or TA18, product form, standard revision and condition.
- Order and deliveryQuantity, destination and any required delivery date.
- Acceptance requirementsDrawing revision, inspection, certificates and packaging.
Not every detail is finalized? Send the information you have. We can help identify the questions to resolve before quotation.
What happens next: requirement review, technical clarification, then a supply proposal and quotation.
What is Grade 9 titanium, and what does Gr9 mean?
Grade 9, Gr9 and Gr. 9 refer to the Ti-3Al-2.5V titanium alloy, identified as UNS R56320 in ASTM specifications. It contains nominally 3% aluminium and 2.5% vanadium. Its key applications include aerospace hydraulic tubing and premium bicycle frame tubing.
Is TA18 the Chinese designation for Grade 9?
TA18 is the Chinese Ti-3Al-2.5V designation. It is discussed with Grade 9 on this page because they share the nominal alloy family. Their chemistry limits, product standards, delivery conditions and acceptance requirements are not identical in every case. Specify the required route; substitution or dual conformity needs agreement and evidence.
How do AMS 4943L, AMS 4944H and AMS 4945H differ?
AMS 4943L covers annealed Ti-3Al-2.5V seamless hydraulic tubing. AMS 4944H covers cold-worked and stress-relieved tubing. AMS 4945H specifies a CWSR route with controlled contractile strain ratio. Use the revision required by the drawing rather than treating these specifications as interchangeable.
What should I send for an aerospace hydraulic tube quotation?
Send the exact material specification and revision, OD, wall, length, quantity and delivery condition. Include drawing and bend/end details, required source approvals, inspection and test scope, traceability, cleanliness, packaging and destination. State whether the order is for straight raw tube or a finished assembly.
Why is Ti-3Al-2.5V used for bicycle frame tubing?
It offers a useful balance of strength, low density, corrosion behaviour, formability and weldability for tubular frames. Tube diameter, wall distribution, joint design and fabrication control still determine frame performance. Selecting Grade 9 does not itself prove fatigue life or completed-frame compliance.
Can you review butted, tapered or shaped bicycle tubes?
Yes. Send the tube drawing with end and centre walls, butt lengths and transitions, OD, length, bending or ovalization details and prototype quantity. We assess manufacturing feasibility, tooling, tolerances and inspection before confirming the supply scope. The illustrated frame is not a statement of finished-frame stock.
Does ASTM B338 certify a bicycle frame or an aircraft hydraulic line?
No. ASTM B338 covers titanium tubes for condensers and heat exchangers. If a buyer uses it as a tube material requirement, application-specific geometry, condition and acceptance must still be defined. An aircraft drawing may require a particular AMS specification; a completed bicycle frame needs its own validation.
Is TA18 the same as ASTM Grade 18?
No. TA18 is a Chinese Ti-3Al-2.5V designation. ASTM Grade 18 is a separate palladium-bearing titanium alloy designation. Include the standard system and full grade name to prevent an incorrect material order.
What are your minimum order quantity and lead time?
They depend on product form, size, condition, quantity, tooling and inspection. Send your prototype or production requirement and destination. We confirm the quantity basis, proposed lead time and approval milestones with the quotation; this page is not a live stock list.
Can you provide samples, certificates or independent inspection?
The required material records and inspection scope are agreed during quotation. Samples and independent inspection can be discussed with acceptance criteria, timing and costs defined for the order. Records must relate to the supplied heat, lot or items.
Can Grade 9 wire automatically be used as welding filler?
No. General wire identification does not establish the required welding-consumable classification or suitability for a qualified procedure. Specify the filler classification, chemistry, surface, packaging and joining procedure requirements for that use.
Who coordinates several products or an order issue?
TiHubs remains your technical and commercial contact in Baoji. We coordinate specifications, relevant manufacturing resources, inspection and delivery communication. If an issue arises, we record it, review the agreed requirements and coordinate the next steps with the relevant manufacturing parties.
07 / Your next step
Start with the
requirement you have.
Send the product details, drawing or operating conditions you already know. We will identify missing information and discuss a suitable supply route before quotation.
- Requirement review
- Technical clarification
- Supply proposal and quotation
Combine several items in one enquiry.
Send one tube schedule or list of forms, sizes and quantities. Include the AMS callout for hydraulic tubing or the profile drawings for a bicycle frame tube set.
Share delivery and acceptance priorities.
Include the destination, target date, prototype approval stage, inspection scope, traceability and any customer source restrictions.
Baoji, China · info@tihubs.com
Start your Grade 9 / TA18 enquiry
Tell us what you need. Details can be clarified after your first enquiry.