CategorySourcing & Buying Guides
Titanium sputtering targets:
specify the complete supply.
Connect purity and impurity evidence with target geometry, cathode fit, backing, bonding and the approved qualification plan.

Quick answer
Specify a titanium sputtering target with an explicit purity basis, critical impurity limits and lot-linked analysis, then confirm the complete cathode interface. Distinguish a bare disk from a bonded assembly, including backing material, drawing, total thickness, bond requirements and inspection evidence. Preserve cleaning and packaging requirements and agree the process qualification plan before changing suppliers or configurations. A larger purity number alone does not establish compatibility, film performance or an approved operating envelope.
01 / Process requirement
Define the target the process actually needs.
A coating laboratory asks purchasing for a two-inch titanium sputtering target. One quotation offers a bare disk, another includes a bonded backing plate, and a third lists a higher purity without an impurity report. The descriptions sound comparable, but they may represent different installed assemblies and acceptance requirements. Start with the approved target drawing, cathode identification and process specification. Then define material, geometry, backing, bonding, cleanliness and evidence as connected purchasing fields.
Identify whether the order replaces an approved consumable, supports a controlled material change or supplies an exploratory trial. A repeat order should preserve the accepted part reference and revision. A development order should state which requirements remain provisional and who will assess the trial. Keep the intended coating application visible without assuming that the application name alone determines target purity, thickness or operating conditions.
Specify elemental titanium separately from titanium alloys, titanium nitride and titanium oxides. A film containing titanium does not necessarily require a target with the same compound formula as the final film. Reactive processes and compound-target processes have different requirements. The process owner must identify the approved route; purchasing should not substitute Ti, TiN or TiO2 because the desired coating contains titanium. For an alloy, state the composition basis and permitted variation rather than supplying only a trade nickname.
Separate the target’s supply specification from the deposition recipe. The supplier needs the interface and agreed operating envelope to assess the offered assembly, but a material quotation should not invent gas flow, power, conditioning time or film performance. A target with the correct dimensions and chemistry still needs approval within the actual equipment and process. Preserve the qualification responsibility and the trial acceptance criteria in the purchasing record.
| Order situation | Information to preserve |
|---|---|
| Repeat consumable | Accepted part number, drawing and revision |
| Alternative supplier | Same acceptance requirements and defined comparison trial |
| New target assembly | Cathode interface, approved configuration and qualification plan |
| Exploratory material | Provisional composition, test objective and release authority |
Verify standards status rather than copying an old catalogue claim. ASTM lists F1709-97(2016), the historical high-purity titanium target specification, as withdrawn in 2023 without replacement. If an existing controlled specification invokes that edition, identify it explicitly and have the responsible technical authority confirm the purchase basis. Do not advertise it as a current active standard or silently replace the customer’s requirement with an unrelated titanium product specification. [1]
The first useful output is a one-page requirement with known values, unresolved fields and approval owners. It lets suppliers quote the same deliverable and prevents a price comparison between a material disk and a qualified assembly. Keep this record attached to the enquiry, subsequent drawing review and final order so clarification is not lost when purchasing changes hands.
02 / Purity and impurities
Read the basis behind the purity number.
A purity label is incomplete until its calculation basis is known. Ask whether the percentage refers to metallic impurities, a defined analytical suite or another stated basis. Thermo Fisher’s titanium target listing explicitly uses a metals-basis assay. That wording is meaningful: it should not be rewritten as a guarantee covering every possible nonmetallic constituent. Preserve the supplier’s analytical basis and compare it with the process requirement before accepting a higher-looking number. [2]
The arithmetic is straightforward when the basis is fixed. A nominal 99.99% titanium fraction corresponds to a 0.01% remainder, or 100 parts per million on that same basis. Similarly, 99.995% corresponds to 50 ppm and 99.999% to 10 ppm. These conversions explain the labels; they do not establish which elements were measured, how nondetects were counted or whether oxygen was included. Do not add or compare figures taken from incompatible calculation bases.
Request limits for impurities that matter to the approved process, with units and analytical methods. Keep oxygen, nitrogen, hydrogen and carbon visible where required rather than assuming that the headline metal purity controls them. Dexerials publishes separate elemental limits and test methods for its titanium target product. Its figures demonstrate how a product-specific specification is structured; they should not become universal TiHubs limits or be copied into a customer’s order without approval. [3]
Separate a maximum specification limit, a typical value and a measured lot result. A brochure may describe a product family; the certificate should identify the delivered material and the required analysis. If a report gives less-than values, retain the reporting or detection limit and the agreed calculation rule. A nondetect is not automatically zero. Ask the laboratory or supplier to clarify the meaning instead of calculating a favorable purity from incomplete fields.
| Purity field | Required clarification |
|---|---|
| Headline percentage | Basis and included analytical suite |
| Critical impurity | Element, maximum, units and method |
| Less-than result | Reporting limit and treatment in the total |
| Certificate | Lot identity, sampling basis and actual results |
| Acceptance | Approved process limits, not a generic premium label |
For a qualification comparison, create a requested-versus-offered table rather than ranking suppliers only by the number of nines. Two offerings with the same headline purity can differ in a critical impurity, reporting limit or sampling scope. Conversely, an increased headline purity may not address the contaminant that caused a previous film problem. Identify the specific requirement and evidence needed to decide whether the proposed material change is useful.
Keep units explicit. Mass ppm and atomic percent are different quantities; converting between them requires the relevant composition and atomic masses. Do not move a value from one column to another just by changing the label. For alloy targets, confirm whether composition is specified by mass or atoms and whether impurity totals exclude intended alloying elements. These simple checks make quotations comparable before analytical or deposition trials consume time.

Arithmetic equivalents on the same stated basis: 99.99% leaves 100 ppm, 99.995% leaves 50 ppm and 99.999% leaves 10 ppm. This does not define oxygen or any excluded constituent.
03 / Geometry and fit
Match the complete cathode interface.
A nominal target diameter is only one dimension of the installed part. Request the controlled drawing or the exact OEM reference together with the relevant revision. Include diameter or length and width, target thickness, flatness where specified, edge profile, steps, recesses, holes and mounting details. If a backing plate is included, distinguish its dimensions from the titanium disk. A correct disk diameter cannot compensate for an assembly that is too thick or has the wrong retaining feature.
Maintain the drawing’s original units and conversion precision. Two inches equals 50.8 mm, not 50 mm. The difference is 0.8 mm across the diameter. This is an exact unit conversion and a simple dimensional comparison, not a recommended fit or tolerance. Whether a proposed alternative is acceptable depends on the approved cathode drawing. Likewise, 0.250 inch converts to 6.35 mm; do not round it to a convenient stock thickness without a documented review.
Describe target thickness, backing thickness, bond-line contribution and total installed thickness separately where relevant. If the system has a controlled maximum assembly envelope, compare the full stack at its specified limits. Ask which face provides the locating reference and which area contacts the cooling interface. Do not infer these details from a photograph or assume that all cathodes using the same nominal target size share the same mounting design.
| Drawing area | Fields to check |
|---|---|
| Titanium target | Shape, dimensions, tolerances and edge detail |
| Backing plate | Material, dimensions, recesses and mounting features |
| Bonded assembly | Alignment, overall thickness and acceptance scope |
| Cathode interface | Retaining method, contact face and approved reference |
| Inspection | Measurement references and required report |
For a custom profile, mark the sputtering face and distinguish it from the rear and peripheral surfaces. Identify any areas that must remain free of markings, handling damage or assembly material. Provide the approved drawing rather than asking the supplier to reconstruct a complex target from a nominal diameter and a used sample. A sample can support identification, but erosion and earlier rework may make it an unreliable manufacturing master.
Do not obtain extra usable life by simply increasing thickness. The cathode geometry and magnetic arrangement are part of the equipment requirements, and the proposed target must fit the approved operating configuration. Ask the equipment owner to review any thickness change before quoting it as an upgrade. The same principle applies when changing from a monolithic disk to a bonded target: it is an assembly change, not merely a different packaging option.
Receiving inspection should use the same drawing revision that the supplier accepted. Record the delivered target and backing identities and verify the specified dimensions without compromising the agreed cleanliness controls. If the enclosure must be opened for inspection, define who performs that step and how it is repackaged. A dimensional report is useful evidence, but the physical item and label must still correspond to the reported part.

Two inches equals 50.8 mm, while 0.250 inch equals 6.35 mm. These conversions are not recommended fit tolerances.
04 / Backing and bonding
Specify the delivered assembly and its evidence.
State whether the purchase is a bare titanium target, a separate backing plate, a bonded assembly or a rebonding service. These scopes involve different responsibilities and cannot be compared by target mass alone. Identify the backing material, drawing, ownership and condition. If the customer supplies a used backing plate, agree inspection and acceptance before the quotation assumes that it can be reused without repair or replacement.
The bond is part of the thermal and mechanical path between target and cooling interface. Select its method and acceptance requirements for the actual assembly and equipment. Lesker describes target bonding and separate backing-plate supply as distinct services. Its titanium guidance also qualifies power recommendations by target configuration and thermal conditions. Treat those as equipment-specific guidance, not a universal wattage that can be transferred to every titanium disk or bonded assembly. [4] [5]
Ask for the approved bond material or method, required coverage, permitted defects and verification evidence. If a percentage coverage is specified, define the evaluated area and inspection method. A single percentage without a mapped acceptance basis may hide differences in location or size of unbonded regions. Avoid inventing a universal coverage threshold; the responsible assembly specification must establish what is acceptable for the particular configuration.
Keep overall thickness and alignment requirements in the bonded-assembly drawing. A dimensionally correct target can still produce the wrong installed envelope when backing and bond-line contributions are added. If the assembly requires identified leak, dimensional or bond inspections, state their scope and acceptance criteria separately. Do not describe a visual check as proof of an internal bond condition or imply that one test certifies every aspect of the assembly.
| Supply option | Boundary to define |
|---|---|
| Bare target | Disk only; installation responsibility remains identified |
| Target plus loose backing | Separate components; bonding scope stated explicitly |
| Bonded assembly | Drawing, method and agreed acceptance evidence |
| Rebonding | Returned-part condition, reuse decision and new records |
For returns, identify the previous material, service history where relevant and the condition of the backing. Follow the supplier’s return requirements and the site’s handling procedure. A quotation should state whether cleaning, debonding, dimensional recovery and new bonding are included. If inspection may reject the backing, agree the replacement decision and commercial allowance before shipment so the turnaround plan does not rely on an unverified reusable component.
Keep the operating instructions attached to the accepted assembly rather than to a generic material name. The equipment owner must approve cooling, mounting and operating conditions. Purchasing can request that the supplier identify applicable limits and documentation, but should not prescribe a commissioning recipe from an article. After a change in bond method, backing or target geometry, retain a clear record of the required review before the assembly enters routine production.

Schematic layers distinguish titanium target, bond and backing plate. Actual materials, dimensions and inspection requirements follow the approved assembly drawing.
05 / Quality and handling
Link material condition to lot-level records.
Microstructure and processing condition may be part of a controlled target specification. If grain size, texture or uniformity matters to the approved process, define the metric, sampling locations, measurement method and acceptance limits. A statement such as fine grain is not a complete inspection requirement. Umicore’s technical sheet discusses titanium target microstructure and analytical methods as separate characteristics. Its product data is an example of a defined offering, not a universal specification for every sputtering application. [6]
Distinguish bulk analysis from surface condition. A lot can meet its chemical limits while the delivered surface has handling contamination or damage that needs disposition. Specify the accepted finish, cleaning condition, packaging and marking locations. Do not equate mirror appearance with process cleanliness, and do not order unnecessary polishing simply because it looks more professional. The controlled process should determine the surface requirement and any subsequent preparation.
Protect the link between material lot, target identity and assembly records. If several targets share one material analysis, the documentation should explain the sampling basis and relationship. If backing or bonding has its own identification, preserve that relationship as well. A receiving team should be able to determine which target belongs to which record without opening every package or relying on an unmarked supplier photograph.
| Evidence | Question it answers |
|---|---|
| Analysis certificate | Which lot and measured impurity results? |
| Dimensional report | Which drawing and inspected characteristics? |
| Microstructure record, if required | Which method, sample and acceptance limits? |
| Assembly report, if required | Which target, backing and bond verification? |
| Package label | Which delivered item and handling instructions? |
Agree packaging with the required delivery condition. State individual identification, surface protection, bag or enclosure requirements and any specified storage instructions. If sealed packaging is required, define how damage or loss of seal is handled at receipt. Do not assume that every target needs the same gas-filled package or storage period. Those details belong to the accepted supply specification and should be confirmed before shipment.
Keep the target protected until the approved inspection or installation step. Use the site’s handling and preparation procedure; an improvised solvent wipe or unapproved abrasive treatment can alter the condition being qualified. When damage, residue or an unclear label is found, retain identity and record the discrepancy. Ask for a disposition before removing evidence or installing the part, especially if the target is being compared in a supplier qualification trial.
Film performance depends on the wider deposition process as well as the supplied material. Lesker’s technical notes identify handling and vacuum-system sources of contamination in addition to starting-material purity. Therefore, investigate a failed film with the target records, equipment state and process history together. Replacing the target with a higher purity alone is not a complete diagnosis, and a satisfactory trial does not remove the need to control subsequent lots and handling. [7]
06 / RFQ and qualification
Compare supply against one acceptance plan.
Build the enquiry around the delivered part and the decision it must support. Include target material, purity basis, individual impurity limits, drawing revision, cathode reference, target and assembly dimensions, backing and bond scope, quantity, packaging and records. Identify the intended trial or repeat-order status. A supplier can then respond with confirmed requirements, proposed alternatives and unresolved items instead of giving a price for an assumed generic disk.
Separate mandatory requirements from preferences. If the process requires a particular impurity limit or approved assembly, mark it as mandatory. If an alternative package, lead time or optional inspection can be considered, list it separately. Ask for exceptions in a visible deviation table. This makes it easier to compare the actual scope and prevents a commercial acceptance from being interpreted as technical approval of every proposed change.
For an alternative supplier, agree the qualification plan before buying the production batch. Identify baseline material, equipment, controlled process conditions, evaluation method and acceptance authority. The plan may compare relevant film or process outcomes, but those criteria must come from the application owner. Define the number and purpose of trial targets without claiming that one successful run establishes all future performance. Preserve target identity alongside the trial record.
| Quotation check | Requested versus offered |
|---|---|
| Material | Purity basis and critical impurity limits |
| Fit | Drawing, dimensions and mounting interface |
| Assembly | Backing, bond and verification scope |
| Delivery | Quantity, packaging, records and schedule |
| Release | Trial criteria, deviations and responsible approver |
Compare cost over the same delivered boundary. A bare disk price excludes services that a complete bonded assembly may include. A rebonding offer may depend on backing acceptance. State inspection charges, trial quantities, packaging and return obligations where relevant. Evaluate cost per accepted usable supply rather than declaring a supplier cheaper from a nominal price per kilogram that ignores the required assembly and documentation.
Define the replacement and return criteria through the equipment procedure. Erosion pattern, remaining thickness and backing condition cannot be reduced to one generic discard dimension for all systems. Record the applicable inspection and removal limits from the approved equipment documentation. Do not continue operation to a percentage utilization claimed in marketing if the system’s own acceptance limit has been reached. Purchasing needs the expected replacement process to plan supply, not an invented operating threshold.
For a supply review, use the enquiry below and the TiHubs titanium sputtering target page. Provide the approved drawing and a concise list of material, interface and evidence requirements. TiHubs can review the requested scope and identify items needing confirmation. After acceptance, retain the final specification and deviation record for repeat orders so the next batch reproduces the approved supply rather than only the same product name.
07 / Build your RFQ
Prepare a titanium sputtering target enquiry.
Send the target drawing, cathode or accepted part reference and required material specification. Include purity basis, impurity limits, target and backing dimensions, bonding scope, quantity, packaging and documentation. TiHubs can review the requested supply and identify fields needing confirmation. State whether this is an approved repeat order or a qualification trial, and list proposed changes separately from mandatory requirements.
Information to include
- Elemental or alloy composition and calculation basis
- Purity and individual impurity limits with methods
- Target drawing, cathode reference and dimensions
- Bare target, backing or bonded-assembly scope
- Inspection, lot records, cleaning and packaging
- Trial status, quantity, delivery and approval criteria
Build your RFQ checklist
Choose the product and add the information you have. Copy the resulting brief or send your requirements to TiHubs. Submitting an enquiry does not place an order.
08 / FAQs
Questions buyers ask
Does 99.99% purity automatically limit oxygen to 100 ppm?
No. The arithmetic remainder is 100 ppm only on the stated calculation basis. If the figure is based on metallic impurities, it does not by itself specify oxygen. Request the applicable oxygen limit and analytical evidence separately, together with the other impurities required by the approved process.
Are a two-inch target and a 50 mm target interchangeable?
Two inches equals 50.8 mm, so the nominal diameters differ by 0.8 mm. Interchangeability depends on the cathode drawing and its tolerances, not a rounded catalogue description. Confirm thickness, edge profile, retention and any backing dimensions as well as diameter.
Is a backing plate included in a target quotation?
Only if the scope explicitly includes it. A bare disk, loose target and backing, bonded assembly and rebonding service are different deliverables. State the required configuration, ownership of any returned backing and the drawing and verification requirements before comparing prices.
What should the analysis certificate identify?
It should connect the delivered material to the required analysis through lot identity, sampling basis, units, methods and reported results. Distinguish specification maxima from measured values and preserve reporting limits for nondetects. Ask for clarification when the certificate does not establish the required acceptance field.
Is ASTM F1709 a current active target specification?
ASTM identifies F1709-97(2016) as withdrawn in 2023 without replacement. An existing controlled requirement may still name that edition, but its use must be explicit and reviewed by the responsible authority. Do not describe the historical document as a currently active standard.
Can a higher-purity target guarantee a better film?
No single purity figure guarantees the film result. The relevant impurity limits, assembly, handling, equipment condition and deposition process must satisfy the application. Define an appropriate qualification comparison and retain target identity with the trial record before changing routine supply.
09 / Key takeaways
Keep the purchase requirements connected.
- Read the purity basis and critical impurity limits.
- Match the complete cathode and assembly drawing.
- Separate bare-target and bonded-assembly scopes.
- Retain lot-linked analysis and inspection records.
- Approve changes through the actual process qualification plan.
Technical references
Sources and data scope
References reviewed November 13, 2026. Public source summaries support the discussion; the controlled specification, agreed edition and approved project requirements govern acceptance.
- ASTM F1709-97(2016) — Withdrawn 2023 — Official status and historical scope; not a claim of current active-standard compliance.
- Thermo Fisher — Titanium target, metals-basis assay — Primary product specification illustrating an explicitly stated assay basis.
- Dexerials — Titanium target impurity data — Product-specific elemental limits and analytical methods; not universal purchasing limits.
- Kurt J. Lesker — Target bonding and backing plates — Primary description of bonding and backing-plate supply services.
- Kurt J. Lesker — Titanium sputtering targets — Material and configuration guidance with equipment-dependent operating qualifications.
- Umicore — Titanium for semiconductor applications — Technical product sheet discussing analysis, microstructure and target configurations.
- Kurt J. Lesker — Deposition materials technical notes — Explains starting-material and process-related contamination considerations.